Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “GRAIN ORIENTATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,207 records · Page 67

Influence of strain and grain boundary variations on magnetism of Cr-doped AlN films

Cr-doped AlN films are prepared by reactive dc magnetron cosputtering under a negative substrate bias ranging from 50 to 110 V. The bias induces variation of the texture from (002) to (110) orientation, enhances the stress and reduces the grain size in the films. All of the samples are ferromagnetic. The atomic magnetic moment (AMM) of Cr increases with the bias from 50 to 90 V and reaches the maximum of 0.18mu{sub B}/Cr at a bias of 90 V. As the bias increases further to 110 V, the AMM decreases. The dielectric constant also changes in the same trend with the bias, as well as the AMM does. The variations in these two properties are determined by the collective effects of the lattice deformations induced by the changing stress, the amount of boundary defects and the grain size in the films.

36 MATERIALS SCIENCE↗

TEM observations on grain boundaries in sintered silicon, part 1

Grain boundaries in silicon with a predetermined orientation were prepared by the sintering of two single crystals. A combination of standard transmission electron microscopy and lattice imaging was used to investigate the structure of the boundaries produced. Low angle grain boundaries on (100) and (111) planes, and twin boundaries on (111) planes are discussed in detail.

Ast, D. G.↗

Coupled phase field damage and crystal plasticity analysis of intragranular fracture: The role of crystallographic orientation and voids

Damage evolution in engineering metal alloys at the grain scale exhibits significant microstructural heterogeneity and anisotropy. These heterogeneities create local hotspots for stress and strain localization, leading to void nucleation. Crystal orientation influences the active slip systems around voids, affecting lattice rotation and potentially forming discontinuities. At low triaxiality, voids may change shape due to lower stress, rotation, elongation, and coalescence. At high triaxiality, the correlation between crystal orientation and void growth rate becomes stronger, resembling the behavior observed in isolated single crystals. Therefore, understanding the effects of crystal orientation, heterogeneous strain, and defect evolution is crucial for single crystal fracture characterization. Here, in this work, a coupled phase-field damage (PFD) and crystal plasticity (CP) model is implemented within a finite element framework to analyze crystal deformation and failure. The CP method employs a dislocation density-based constitutive model, while intragranular failure is modeled using an anisotropic PFD method. The PFD model considers both the stored energy due to elastic stretching and the energy release due to defect formation and crack formation. A single crystal Al2219 with an intracrystalline spherical void is chosen to analyze fracture. The study finds that fracture propagation is strongly correlated with crystal orientations. This coupled CP-PFD model provides accurate failure prediction in crystalline materials by incorporating the effects of crystal orientations and existing voids. This study demonstrates how the local microstructure and defects influence plastic deformation and failure mechanisms in metal alloys.

Aluminum alloy↗

Investigation of the shear response and geometrically necessary dislocation densities in shear localization in high-purity titanium

The influence of microstructural anisotropy on shear response of high-purity titanium was studied using the compact forced-simple-shear specimen (CFSS) loaded under quasi-static loading conditions. Post-mortem characterization reveals significant difference in shear response of different directions in the same material due to material crystallographic texture anisotropy. Shear bands are narrower in specimens in which the shear zone is aligned along the direction with a strong {0001} basal texture. Twinning was identified as an active mechanism to accommodate strains in the shear region in both orientations. This paper confirms the applicability of the CFSS design for the investigation of differences in the shear response of materials as a function of process-induced crystallographic texture. A detailed, systematic approach to quantifying shear band evolution by evaluating geometrically necessary dislocations (GND) associated with crystallographic anisotropy is presented. Finally, the results show that: i) line average GND density profiles, for Ti samples that possess a uniform equiaxed-grain structure, but with strong crystallographic anisotropy, exhibit significant differences in GND density close to the shear band center; ii) GND profiles decrease steadily away from the shear band as the plastic strain diminishes, in agreement with Ashby's theory of work hardening, where the higher GND density in the through-thickness (TT) orientation is a result of restricted < a > type slip in the shear band compared with in-plane (IP) samples; iii) the anisotropy in deformation response is derived from initial crystallographic texture of the materials, where GND density of < a > GNDs are higher adjacent to the shear band in the through-thickness sample oriented away from easy slip, but the density of < c+a > type GNDs are very similar in these two samples; and iv) the increase in grain average GND density was determined to have strong correlation to an increase in the Euler Φ angle of the grain average orientation, indicating an increased misorientation angle evolution.

36 MATERIALS SCIENCE↗

Facet-Dependent Cold Welding of Au Nanorods Revealed by Liquid Cell Transmission Electron Microscopy

Cold welding of metals at the nanoscale has been demonstrated to play a significant role in bottom-up manufacturing and self-healing processes of nanostructures and nanodevices. However, the welding mechanism at the nanoscale is not well understood. In this study, a comprehensive demonstration of the cold welding process of gold nanorods with different modes is presented through in situ liquid cell transmission electron microscopy. The experimental results and molecular dynamics simulations reveal that the nanorods are welded through the facet-dependent atomic surface diffusion and rearrangement along {100} facets. The density functional theory calculations indicate that the preferred coalescence of two {100} surfaces is thermodynamically favorable. Unlike the prevalent “oriented attachment” in the nanoparticle coalescence, the misalignment of nanorod orientations and local stresses can induce grain boundaries and stacking faults in the welded interface.

42 ENGINEERING↗

Local Multimodal Electro-Chemical-Structural Characterization of Solid-Electrolyte Grain Boundaries

Typical models of polycrystalline ionic materials treat the grain boundary properties as single valued, without consideration of the full range of values that define the macroscopically measured average. Here a unique experimental platform suitable for local multimodal characterization of individual grain boundaries in bicrystal fibers is reported. A variation of three orders of magnitude in the grain boundary conductivity of ceria is observed, as measured across six individual bicrystals by both alternating current impedance spectroscopy and direct current (D.C.) linear sweep voltammetry. Nonlinear behavior of the D.C. measurements is consistent with resistance due to a space charge effect. Time-of-flight secondary ion beam spectroscopy reveals a correlation between grain boundary resistance and the concentration of impurities Si, Al, and Ca segregated at the grain boundaries, although the bulk concentrations of these impurities are negligible. Electron backscatter diffraction analysis of the crystal orientations suggests a correlation between the misorientation across the grain boundaries and grain boundary resistance. These correlations point towards a grain boundary resistance that arises from impurity-generated space charge effects and variations in impurity concentration and hence resistivity driven by the energetics of impurity segregation to grain boundaries of differing surface energies.

36 MATERIALS SCIENCE↗

Modeling Microstructural Effects on Heterogeneous Temperature Fields within Polycrystalline Explosives

The paper addresses the role of crystal anisotropy on the evolution of heterogeneous temperature fields in plastic-bonded explosives (PBXs) under conditions of weak shock. The modeling approach is based on simplified idealizations of PBX microstructure including RDX grains and estane binder regions subjected to velocity boundary conditions representative of impact conditions in situ. The constitutive description of the microstructure constituents includes a dislocation-based, anisotropic, single crystal plasticity model for the explosive grains and a linear viscoelastic model to represent the estane binder. Large suites of simulations were used to systematically study the correlation in heating of the grains with local wave dynamics, crystal orientation, and the microstructural neighborhood. These correlations were identified through the selection of characteristics of crystal anisotropy including oriented wave speeds and Taylor factor. A key observation is that the wave dispersion within a certain distance from the impact interface plays a dominant role in the temperature field. Beyond this distance, individual crystal orientations play a more dominant role, but cannot entirely account for the observed heterogeneity without consideration of the local microstructure neighborhood.

42 ENGINEERING↗

Subgrains, Texture Evolution, and Dynamic Abnormal Grain Growth in a Mo Rod Material

The roles of subgrains, texture, and surface energy during dynamic abnormal grain growth (DAGG) were examined in a commercial-purity Mo rod material. DAGG was confirmed in this material during tensile deformation at 2023 K (1750 °C). Cooling of specimens after tensile testing was sufficiently rapid to preserve both subgrain structures developed during deformation and several abnormal grains at early stages of growth. These and other microstructural features were characterized to evaluate how subgrains and boundary character influence the early stages of DAGG. Subgrains were observed in the deformed polycrystalline material but were generally absent in newly formed abnormal grains. This was identified as the cause of the sudden drop in flow stress observed at the initiation of DAGG. It is proposed that subgrain intersections with abnormal grain boundaries provide a driving pressure for DAGG. Subgrains within the deformed polycrystals were observed to locally change the boundary curvature at their intersections with abnormal grain boundaries, which likely encouraged growth of the abnormal grains into the deformed polycrystals. Abnormal grains produced by DAGG retained crystallographic orientations and boundary characters that closely resembled those of the polycrystalline material from which they grew. This indicates that neither differences in orientation nor boundary character were important to DAGG in this material.

36 MATERIALS SCIENCE↗

Effect of Different Thermomechanical Processes on the Microstructure, Texture, and Mechanical Properties of API 5L X70 Steel

A commercial API 5L X70 steel plate was subjected to different thermomechanical processes to propose a novel thermomechanical rolling path to achieve improved mechanical properties. Scanning electron microscopy, electron backscatter diffraction, and x-ray texture analysis were employed for microstructural characterization. The results showed that strain-free recrystallized {001} ferrite grains that developed at higher rolling temperature could not meet the American Petroleum Institute (API) requirements. Also, refined and work-hardened grains that have formed in the intercritical region with high stored energy do not provide suitable tensile properties. However, fine martensite–austenite constituents dispersed in ferrite matrix with grains having predominantly {111} and {110} orientations parallel to the normal direction that developed under isothermal rolling at 850 °C provided an outstanding combination of tensile strength and ductility.

36 MATERIALS SCIENCE↗

Effects of homogenization treatment on recrystallization behavior of 7150 aluminum sheet during post-rolling annealing

The effects of two homogenization treatments applied to the direct chill (DC) cast billet on the recrystallization behavior in 7150 aluminum alloy during post-rolling annealing have been investigated using the electron backscatter diffraction (EBSD) technique. Following hot and cold rolling to the sheet, measured orientation maps, the recrystallization fraction and grain size, the misorientation angle and the subgrain size were used to characterize the recovery and recrystallization processes at different annealing temperatures. The results were compared between the conventional one-step homogenization and the new two-step homogenization, with the first step being pretreated at 250 °C. Al{sub 3}Zr dispersoids with higher densities and smaller sizes were obtained after the two-step homogenization, which strongly retarded subgrain/grain boundary mobility and inhibited recrystallization. Compared with the conventional one-step homogenized samples, a significantly lower recrystallized fraction and a smaller recrystallized grain size were obtained under all annealing conditions after cold rolling in the two-step homogenized samples. - Highlights: • Effects of two homogenization treatments on recrystallization in 7150 Al sheets • Quantitative study on the recrystallization evolution during post-rolling annealing • Al{sub 3}Zr dispersoids with higher densities and smaller sizes after two-step treatment • Higher recrystallization resistance of 7150 sheets with two-step homogenization.

36 MATERIALS SCIENCE↗

Spherical nanoindentation stress–strain curves

Although indentation experiments have long been used to measure the hardness and Young's modulus, the utility of this technique in analyzing the complete elastic–plastic response of materials under contact loading has only been realized in the past few years – mostly due to recent advances in testing equipment and analysis protocols. This paper provides a timely review of the recent progress made in this respect in extracting meaningful indentation stress–strain curves from the raw datasets measured in instrumented spherical nanoindentation experiments. These indentation stress–strain curves have produced highly reliable estimates of the indentation modulus and the indentation yield strength in the sample, as well as certain aspects of their post-yield behavior, and have been critically validated through numerical simulations using finite element models as well as direct in situ scanning electron microscopy (SEM) measurements on micro-pillars. Much of this recent progress was made possible through the introduction of a new measure of indentation strain and the development of new protocols to locate the effective zero-point of initial contact between the indenter and the sample in the measured datasets. As a result, this has led to an important key advance in this field where it is now possible to reliably identify and analyze the initial loading segment in the indentation experiments.

36 MATERIALS SCIENCE↗

Film Thickness and Composition Effects in Symmetric Ternary Block Copolymer/Homopolymer Blend Films: Domain Spacing and Orientation

We report thickness and homopolymer molar mass dependencies in thin film blends of a compositionally symmetric 75 kg/mol lamellar polystyrene-block-poly(methyl methacrylate) diblock copolymer (PS-b-PMMA) with near-equal volume fractions of PS and PMMA homopolymers on “neutral” surfaces that promote a vertical domain orientation. PS and PMMA homopolymers with equal molar masses of 1, 3, and 22 kg/mol are blended in a 1:1 mass ratio. To efficiently explore this parameter space, we prepared combinatorial samples with gradient homopolymer concentrations using electrospray deposition (ESD) and gradient film thicknesses using flow coating; these samples were subsequently characterized by grazing-incidence small-angle X-ray scattering and scanning electron microscopy, respectively. Our results demonstrate that the added homopolymers increase or reduce domain spacings with respect to the neat (unblended) block copolymer depending on their molar masses, in line with previous reports; a simple heuristic to estimate the domain scaling in ternary blends based on the homopolymer molar mass agrees well with data for the thinnest blend films studied here. More surprisingly, we observe that the measured domain spacing in blends also depends on film thickness, with thicker films exhibiting larger domain spacings than thinner films at the same homopolymer concentration. Furthermore, thickness gradients at fixed homopolymer concentrations reveal a change in lamellae orientation from vertical to horizontal as film thickness is increased beyond the nominal lamellar domain spacing. Coarse-grained molecular dynamics simulations indicate that this change in orientation is induced by homopolymer segregation to film surfaces. Finally, tying these effects together, we hypothesize that the observed dependence of domain spacing on film thickness is a consequence of changes in the vertical homopolymer composition profile in thicker films during lamellae reorientation and the conformational asymmetry between PMMA and PS segments.

36 MATERIALS SCIENCE↗

Taking three-dimensional x-ray diffraction (3DXRD) from the synchrotron to the laboratory scale

Three-dimensional x-ray diffraction (3DXRD), a rotating x-ray diffraction technique, is a powerful tool for studying the micromechanical behavior of polycrystalline materials, capable of measuring the volume, position, orientation, and strain of thousands of grains simultaneously. However, its application has been historically limited to synchrotron facilities. Here, we present the first demonstration of laboratory-scale 3DXRD (Lab-3DXRD) using a liquid-metal-jet source. Lab-3DXRD achieves accuracy comparable to synchrotron-based 3DXRD, as validated against laboratory diffraction contrast tomography (LabDCT) and synchrotron-3DXRD. Over 96% of the grains detected with Lab-3DXRD are cross-validated, particularly for coarse grains (> ~60 μm), while the results suggest that finer grains should be accessible by taking advantage of high-efficiency detectors. We further demonstrate that its sensitivity to finer grains is enhanced by incorporating pre-characterization into the analysis. This study establishes Lab-3DXRD as a practical alternative to synchrotron techniques, making 3DXRD accessible to a wider range of academic and industrial researchers.

characterization and analytical techniques↗

Atom-by-atom imaging of moiré transformations in 2D transition metal dichalcogenides

Understanding the atomic-scale mechanisms that govern the structure of interfaces is critical across materials systems but particularly so for two-dimensional (2D) moiré materials. Here, we image, atom-by-atom, the thermally induced structural evolution of twisted bilayer transition metal dichalcogenides using in situ transmission electron microscopy. We observe low-temperature, local conversion of moiré superlattice into nanoscale aligned domains. Unexpectedly, this process occurs by nucleating a new grain within one monolayer, whose crystal orientation is templated by the other. The aligned domains grow through collective rotation of moiré supercells and hopping of 5|7 defect pairs at moiré boundaries. This provides mechanistic insight into the atomic-scale interactions controlling moiré structures and illustrates the potential to pattern interfacial structure and properties of 2D materials at the nanoscale.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Characterization of Titanium Alloys Produced by Electron Beam Directed Energy Deposition

Functionally graded materials offer the potential to improve structural efficiency by allowing the material composition and/or microstructural features to spatially vary within a component. Additive manufacturing techniques enable the fabrication of such graded materials and structures. While examining several titanium alloys, this paper focuses on Ti-8Al-1Er as it has a unique microstructure that is only feasible when produced by rapid solidification methods like electron beam directed energy deposition, an additive manufacturing process. The results show that, when mixed, Ti-8Al-1Er and commercially-pure titanium uniformly mix at various ratios and the resultant static tensile properties of the mixed alloys behave according to rule-of-mixtures. At discontinuous interfaces between Ti-8Al-1Er and commercially-pure titanium, the crack growth behavior progresses smoothly across the discontinuity as the crack transitions from one crack growth regime into another. Studies on monolithic samples shows the mechanisms of damage in the Ti-8Al-1Er; specifically, that strain localization occurs near grain boundaries of high mis-orientation on the microscale and that twinning and dislocation density is concentrated near erbia-strengthening particles (Er2O3) on the nanoscale.

Newman, John A.↗

TEMPERATURE CONSTRAINT OF THE MISTASTIN LAKE IMPACT STRUCTURE IMPACT MELT ROCKS

Impact melt is a product of hypervelocity cratering events formed by the instantaneous melting of near-surface target rocks. The temperatures of impact melt upon formation are believed to be superheated, vastly exceeding the liquidus temperature of igneous rocks formed via endogenic processes. However, quantitative understanding of the formation and duration of superheated temperatures remains incomplete. To date, only one datum on the hottest post-shock temperature (>2370 °C) has been derived by Timms et al. (2017) [1]. These authors studied the microstructures and crystallographic orientations preserved within a rim of vermicular ZrO2 of a zircon grain entrained within impact glass at the Mistastin Lake impact structure, Canada. Diagnostic crystallographic orientation indicated the presence of cubic zirconia, requiring a minimum temperature for the impact melt of >2370°C from the dissociation of zircon to cubic zirconia and liquid SiO2. With only one temperature datum, it cannot be stated whether the temperature of the impact melt sheet was homogenous across the entire structure or if the thermal history of the melt varied with spatial distribution. In this study, we present a preliminary investigation of 70 zircon grains, 22 of which exhibit rims of vermicular ZrO2 dissociation textures, similar to those studied by Timms et al. (2017). To acquire a more accurate temperature profile representative of impact melt, zircon crystals were collected from different types of impact melt bearing units, including additional samples of the impact glass studied by Timms et al. (2017). Of the 22 zircon grains with dissociation textures, at least 4 grains in the impact glass show diagnostic evidence of pre-existing cubic zirconia, and 1 grain from a glass-bearing breccia exhibits granular zircon textures, possible evidence of a transition from high-P to high-T conditions. These results show the heterogeneous post-shock temperature distribution of superheated impact melt within the Mistastin impact structure. [1] Timms, N.E., Erickson, T.M., Zanetti, M.R., Pearce, M.A., Cayron, C., Cavosie, A.J., Reddy, S.M., Wittmann, A. and Carpenter, P.K., 2017. Cubic zirconia in> 2370° C impact melt records Earth's hottest crust. Earth and Planetary Science Letters, 477, pp.52-58.

rock↗

High frequency ultrasonic characterization of sintered SiC

High frequency (60 to 160 MHz) ultrasonic nondestructive evaluation was used to characterize variations in density and microstructural constituents of sintered SiC bars. Ultrasonic characterization methods included longitudinal velocity, reflection coefficient, and precise attenuation measurements. The SiC bars were tailored to provide bulk densities ranging from 90 to 98 percent of theoretical, average grain sizes ranging from 3.0 to 12.0 microns, and average pore sizes ranging from 1.5 to 4.0 microns. Velocity correlated with specimen bulk density irrespective of specimen average grain size, average pore size, and average pore orientation. Attenuation coefficient was found to be sensitive to both density and average pore size variations, but was not affected by large differences in average grain size.

Baaklini, George Y.↗