At least 1,207 records · Page 67

Microstructure and Mechanical Properties of Friction Stir Process Derived Al-TiO{sub 2} Nanocomposite

Aluminum-based composites have many advantages over their conventional counterparts. A major problem in such composites is the clustering of particles in the matrix. Friction stir processing (FSP) can homogenize particle distribution in aluminum-based composites. In this study, unannealed TiO{sub 2} particles were used to prepare Al-TiO{sub 2} nanocomposite using FSP. The TiO{sub 2} particles, about 1 µm, were dispersed into an aluminum matrix by 6 passes of FSP. The TiO{sub 2} particles were fractured by multiple FSP passes, leading to a nano-size particle distribution in the matrix. Nanoscale dispersion was confirmed by scanning electron microscopy and transmission electron microscopy. The fractured TiO{sub 2} particles reacted with the aluminum matrix to form Al{sub 3}Ti intermetallic and Al{sub 2}O{sub 3} ceramic. The progression of the Al-TiO{sub 2} reaction from the fourth to the sixth pass of FSP was revealed by x-ray diffraction. Due to the nanoscale dispersion, the yield and ultimate tensile strength of the composite increased to 97 and 145 MPa, respectively. Ductility of the composite decreased marginally compared to the as-received aluminum. As the dispersed particles pin dislocations, the strain-hardening rate of the composite was considerably increased and the same was seen in the Kocks-Mecking plot. The TiO{sub 2} particles are mechanically activated due to their fracture during FSP, hence leading to reaction with the matrix. The particle refinement and dispersion lead to a homogeneous matrix with higher strength.

36 MATERIALS SCIENCE↗

Improving Joint Formation and Tensile Properties of Dissimilar Friction Stir Welding of Aluminum and Magnesium Alloys by Solving the Pin Adhesion Problem

Friction stir welding (FSW), as a solid-state welding technology invented by TWI in 1991, has potential to join dissimilar Al/Mg alloys. In this study, the pin adhesion phenomenon affecting joint quality during FSW of 6061-T6 aluminum and AZ31B magnesium alloys was investigated. The adhesion phenomenon induced by higher heat input easily transformed the tapered-and-screwed pin into a tapered pin, which greatly reduced the tool’s ability to drive the plasticized materials and further deteriorated joint formation. Under the condition without the pin adhesion, the complex intercalated interlayer at the bottom of stir zone was beneficial to mechanical interlocking of Al/Mg alloys, improving tensile properties. However, the formation of intermetallic compounds was still the main reason of the joint fracture, significantly deteriorating tensile properties. Under the welding speed of 60 mm/min without the pin adhesion phenomenon, the maximum tensile strength of 107 MPa and elongation of 1.2% were achieved.

36 MATERIALS SCIENCE↗

Friction Stir Welding of Low-Carbon AISI 1006 Steel: Room and High-Temperature Mechanical Properties

Friction stir welding (FSW) is an ecologically benign solid-state joining process. In this work, FSW of low-carbon AISI 1006 steel was carried out to study the microstructure and mechanical properties of the resulting joints at both room temperature (RT) and 200 °C. In the parameter space investigated here, a rotational tool speed and translation feed combination of 1200 rpm and 60 mm/min produced a defect-free weld with balanced mechanical properties and a superior Vickers microhardness profile compared to all other conditions and to base metal (BM). At faster translation feeds (100 and 150 mm/min), wormhole defects were observed in the weld microstructure and were attributed to higher strain rate experienced by the weld zone. Under tensile loading, welded material exhibited yield strength that was up to 86 and 91% of the BM at RT and 200 °C, respectively. On the other hand, tensile strength of welded material was nearly similar to that of the base metal at both RT and 200 °C. However, at both temperatures the tensile ductility of the welded joints was observed to be significantly lower than the BM. Annealing of the 1200 rpm and 60 mm/min FSW specimen resulted in tensile strength of 102% compared to base material and 47% increase in the strain at failure compared to the as-welded specimen. The Charpy impact values revealed up to 62 and 53% increase in the specific impact energy for the 1200 rpm and 60 mm/min welded joints as compared with the BM.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Characterization of Friction-Stir-Welded Dual-Phase Brass

Friction stir welding (FSW) is an ideal process to join brass to avoid the evaporation of zinc. In the present investigation, 6-mm-thick dual-phase brass plates were joined efficiently using FSW at various tool rotational speeds. The microstructures were studied using optical microscopy, electron backscattered diffraction and transmission electron microscopy. The optical micrographs revealed the evolution of various zones across the joint line. The microstructure of the heat-affected zone was similar to that of base metal. The weld zone exhibited finer grains due to dynamic recrystallization. The recrystallization was inhomogeneous and the inhomogeneity reduced with increased tool rotational speed. The dual phase was preserved in the weld zone due to the retention of zinc. The severe plastic deformation created a lot of dislocations in the weld zone. The weld zone was strengthened after welding. The role of tool rotational speed on the joint strength is further reported.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Dissimilar Joints of Al-Mg{sub 2}Si and 5052 Aluminum Alloy by Friction Stir Welding

Al-Mg{sub 2}Si alloy and 5052 Al alloy were welded successfully by friction stir welding (FSW) in this study. The results show that the alloy consists of three distinct zones after FSW: the base material zone (BMZ), the transitional zone, and the weld nugget (WN). The morphologies of the primary Mg{sub 2}Si phases are identified as coarse equiaxed crystals for Al-Mg{sub 2}Si alloys in the BMZ. The WN is a mixture of rich Al-Mg{sub 2}Si and rich 5052 alloy, and a banded structure is formed in the zone. Interestingly, in the WN, the equiaxed crystals changed to polygonal particles with substantially reduced sizes in the rich Al-Mg{sub 2}Si zone. However, in addition to the white rich Mg phase appearing in the rich 5052 zone near the interface, the 5052 alloy does not show obvious changes. The hardness gradually increases from the BMZ of the 5052 to the welded joint to the Al-Mg{sub 2}Si BMZ. In addition, the ultimate tensile strength (UTS) of the welded joint is higher than that of the base material of the Al-Mg{sub 2}Si, whereas it is lower than that of the 5052 base alloy. The results of the elongation are similar to the UTS results. The fracture mechanism is also investigated.

36 MATERIALS SCIENCE↗

Interfacial Microstructure and Mechanical Properties of Friction Stir Welded Joints of Commercially Pure Aluminum and 304 Stainless Steel

In the present investigation, friction stir welding of commercially pure aluminum and 304 stainless steel was carried out at varying tool rotational speeds from 200 to 1000 rpm in steps of 200 rpm using 60 mm/min traverse speed at 2 (degree) tool tilt angle. Microstructural characterization of the interfacial zone was carried out using optical microscope and scanning electron microscope. Energy-dispersive spectroscopy indicated the presence of FeAl{sub 3} intermetallic phase. Thickness of the intermetallic layer increased with the increase in tool rotational speed. X-ray diffraction studies indicated the formation of intermetallic phases like FeAl{sub 2}, Fe{sub 4}Al{sub 13}, Fe{sub 2}Al{sub 5}, and FeAl{sub 3}. A maximum tensile strength of ~ 90% that of aluminum along with ~ 4.5% elongation was achieved with the welded sample at tool rotational speed of 400 rpm. The stir zone showed higher hardness as compared to base metals, heat affected zone, and thermo-mechanically affected zone due to the presence of intermetallics. The maximum hardness value at the stir zone was achieved at 1000 rpm tool rotational speed.

36 MATERIALS SCIENCE↗

Phase-Field Modeling of Nugget Zone for a AZ31-Mg-Alloy Friction Stir Weld

This work presents simulation of microstructure evolution in the nugget zone (NZ) of a AZ31-Mg-alloy friction stir weld. The process parameters (tool geometrical characteristics, rotational speed, travel speed, applied load) have been correlated with the resulting microstructural features in the NZ of the weld (grain size and population) with the aid of the MICRESS software, which provides the ability to simulate both nucleation and grain growth during dynamic recrystallization phenomena evolving in the NZ during the weld thermal cycle. The input parameters of the developed model include the tool geometry, the welding conditions as well as the recrystallization energy, the grain boundary mobility and specific material properties. NZ microstructure obtained by simulation shows good agreement with experimental measurements for both grain population and size.

36 MATERIALS SCIENCE↗

Process Parameter Optimization in Refill Friction Spot Welding of 6061 Aluminum Alloys Using Response Surface Methodology

6061-T6 aluminum alloy joint was fabricated by refill friction stir spot welding (RFSSW) on which three process parameters of tool rotation speed, sleeve moving rate, and plunge depth make an important effect. The response surface methodology (RSM) was applied to establish a mathematical model to study the effect of process parameters on lap shear fracture load (LSFL) of the RFSSWed joints which were performed in Box–Behnken designs with three factors, three levels and 15 runs. Analysis of variance used to check the adequacy of the developed model indicates that the mathematical model is significant. LSFL increases with the increase in tool rotation speed, sleeve plunge depth, and sleeve moving rate to maximum and then decreases. Sleeve plunge depth makes the most effect on LSFL in all process parameters. The RFSSW process parameters were also optimized using RSM to predict maximize LSFL. The joint produced using a tool rotational speed of 1506 rpm, sleeve moving rate of 1.01 mm/s and sleeve plunge depth of 2.46 mm displays higher LSFL.

36 MATERIALS SCIENCE↗

Influence of Welding Combined Plastic Forming on Microstructure Stability and Mechanical Properties of Friction Stir-Welded Al-Cu Alloy

A new tailor-welded process, which combines stages of welding, plastic forming, and heat treatment strengthening, was developed to produce a friction stir-welded (FSW) Al-alloy joint. The Al-Cu sheets were FSW under different welding parameters and then were plastic-deformed. The microstructural evolution and mechanical properties of the FSW joint were investigated by scanning electron microscopy and tensile tests. It was found that high heat input during FSW and low solution temperature suppress the abnormal grain growth (AGG) of the joint due to the differential in grain size and grain boundary energy. The microstructure heterogeneity of the FSW joint is effectively improved, as no AGG occurs. The retention of fine equiaxed grains and the increase in the density of precipitates result in excellent mechanical properties. The increase in the strength and micro-hardness of the joint mainly depends on the plastic deformation prior to aging treatment.

36 MATERIALS SCIENCE↗

Enhancing Formability of AA2219 Aluminum Alloy Friction Stir Welded Blanks with Preheating Treatment

The deformation behaviors of FSW blank are complicated due to the incompatibility of the mechanical property and microstructure for the weld and base material. In order to improve the formability of friction stir welded (FSW) blanks, the weld and base material in this paper were subjected to preheating treatments of 250, 300, 350, 400, and 450 °C, plus a solution treatment of 535 °C. The deformation behavior of the AA2219 FSW blank was characterized using uniaxial tension, microhardness test, hydro-bulging test and electron backscattered diffraction to determine the relationship of the deformation property and microstructure for the FSW blanks. Full strain fields of the tensile and bulging specimens were used to analyze the deformation uniformity of the weld and base material under uniaxial tension and biaxial tension stress states. With the limiting bulging height under various preheating temperatures, the formability behavior of the weld and base material was analyzed during the whole bulging process. The optimum preheating temperature can increase the formability and refrain from abnormal grain growth of the weld on the premise of maintaining the weld strength. The limiting bulging height of FSW blank is obviously improved by the lower preheating temperature from 300 to 350 °C. Additionally, the weld position has a significant impact on the deformation of the whole FSW blanks.

36 MATERIALS SCIENCE↗

Effect of Rotation Speed on the Microstructure and Mechanical Properties of Friction-Stir-Welded CuSn6 Tin Bronze

Four-mm-thick CuSn6 tin bronze plates were friction stir welded at a constant tool traverse speed of 100 mm min{sup −1}. Favorable joints could be obtained with rotation speeds ranging from 600 to 1000 rev min{sup −1}, and groove was found on the surface of the joint under 400 rev min{sup −1}. The microstructure of the weld nugget zone was characterized by equiaxed recrystallized grains with heterogeneity along the thickness direction. Moreover, the grain size of the thermo-mechanically affected zone and stir zone increased with the increase in rotation speed. Hardness of the stir zone was higher than that of other zones due to microstructural refinement. There was little change in tensile properties of the defect-free welded joints. During tensile test, all of the defect-free joints were fractured at heat-affected zone with typical plastic fracture.

36 MATERIALS SCIENCE↗

Effect of Zinc Interlayer in Microstructure Evolution and Mechanical Properties in Dissimilar Friction Stir Welding of Aluminum to Titanium

The welding of aluminum (Al) and titanium (Ti) is difficult and challenging due to the differences in their chemical and physical properties, and the formation of brittle intermetallic phases. In the present experiment, a zinc (Zn) interlayer was used during friction stir welding of Al to Ti. The weld was characterized in detail to understand the mechanisms associated with microstructural evolution and improvement in mechanical properties of the weld. X-ray computed tomography results reveal three-dimensional distribution of particles and flakes of titanium in the weld nugget. It was also observed that Ti particles are inhomogeneously distributed in the weld and the distribution depends on their morphology. Such a distribution of Ti was informative in understanding material flow. In addition, the consolidation of Zn in the Al matrix reveals the nature of material flow in the weld nugget as well. The importance of the Zn interlayer and mechanism of phase formation was explored in this study. It was characterized that the mechanical mixing of Zn with Al and Ti alters phase evolution and restricts the formation of conventional Al{sub 3}Ti intermetallic phase. The presence of zinc homogenizes elemental distribution and inhibits the formation of brittle intermetallic phases, which leads to a substantial improvement in mechanical properties of the weld.

36 MATERIALS SCIENCE↗

Reducing Intermetallic Compounds of Mg/Al Joint in Friction Stir Lap Welding

To reduce intermetallic compounds (IMCs) of Al{sub 12}Mg{sub 17} and Al{sub 3}Mg{sub 2} in Mg/Al friction stir lap welding joint, pin tip was plunged into the lower sheet at a small distance. Results showed that at a fixed welding speed of 50 mm/min, sound joints were obtained using rotating speeds from 750 to 500 rpm, and the IMCs zones were rather small. Cracks easily appeared inside IMCs inside onion ring and at lap interface. Therefore, reducing the IMC was beneficial for reducing the crack. Joint lap shear stress firstly increased and then decreased with decrease in the rotating speed. The maximum shear stress of 50.2 MPa was attained at a rotating speed of 500 rpm because of reduced IMC.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Friction Stir Welded Q235 Low-Carbon Steel

Three-millimeter-thick Q235 steel plates were friction stir welded using a tool made of tungsten-rhenium alloy in the present study. The microstructure and mechanical properties of welded joints at various traverse speeds from 50 to 150 mm/min were analyzed. It was demonstrated that traverse speed had great impacts on microstructure and mechanical properties of the joints. Phase transformation accompanied with recrystallization occurred during FSW process which resulted in different microstructures in the WNZ, and the grain size in other zones was significantly affected by traverse speed. The highest hardness was located in the nugget zone, while the lowest hardness was found in the heat-affected zone. The transverse tensile test suggested that all the joints showed slightly lower tensile strength than that of the base material, and the tensile strength increased with increasing traverse speed. All the joints fractured in the heat-affected zone with ductile fracture mode. The impact test showed that the impact toughness decreased with the increasing traverse speed and the impact fracture surface could be divided into shear lip zone and fibrous zone which showed a typical ductile fracture.

36 MATERIALS SCIENCE↗

Optimization of Tensile and Corrosion Properties of Dissimilar Friction Stir Welded AA2024-7075 Joints

In this work, we performed some joining experiments of dissimilar aluminum alloys AA2024-T351 and AA7075-T651 using friction stir welding (FSW) technique with different process parameters (rotational speed, welding speed and plunge depth). Response surface methodology based on a central composite rotatable design was used to establish the mathematical models predicting the tensile properties and corrosion rate of dissimilar FSW joints with some high confidence level. Analysis of variance method was employed to verify the developed models. Besides, the influences of FSW process parameters on tensile and corrosion properties of joints were analyzed. In order to obtain a desirable combination property of the dissimilar FSW joints, the optimum process parameters after experimental verification were proposed as: rotational speed 1495 rev/min, welding speed 187 mm/min and plunge depth 0.03 mm. This verification illustrated that the developed models are appropriate for the modeling and optimization of process.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Characterization of Friction-Stir-Welded 316L Austenitic Stainless Steels

Fusion welding of austenitic stainless steels (ASSs) causes undesirable metallographic changes. An attempt has been made to join 3-mm-thick 316L ASS plates using friction stir welding and correlate the microstructural evolution and the mechanical properties under various welding conditions. Tungsten alloy (W-Re) tool was employed for welding. Successful joints were obtained within a range of traverse speeds (45-85 mm/min) used in this work. Various zones were observed across the joint line. The stir zone exhibited considerable grain refinement and traces of delta ferrite phase. EBSD images showed a decreasing grain size with increased traverse speed. XRD patterns and TEM images confirmed the existence of delta ferrite. The mechanical properties of the joints including microhardness, tensile strength, impact toughness and bending were further reported.

36 MATERIALS SCIENCE↗

Effect of Friction Stir Processing on the Microstructure, Damping Capacity, and Mechanical Properties of Al-Si Alloy

Friction stir processing (FSP) was conducted on an Al-Si casting alloy. The Si phase and Al grains of an Al-Si casting alloy were refined through FSP. Furthermore, FSP with high rotation rate led to the precipitation of Mg and Si atoms and the formation of Mg{sub 2}Si phase in the Al-Si alloy. Precipitation improved the low-strain damping capacity but deteriorates high-strain damping capacity of the FSP sample at room temperature. At low rotation rate, the FSP sample exhibited excellent high-temperature damping capacity mainly because of its fine grain structure and the low density of its pinning points. The plastic instability of the Al-Si alloy was eliminated by FSP because of the refinement of the Si phase. The increase in the strength of each FSP sample was attributed to the increase in second-phase and boundary strengthening effects. Thus, the mechanical properties and damping capacity of Al-Si were enhanced after FSP.

36 MATERIALS SCIENCE↗

Effect of Tool Pin Eccentricity on the Microstructure and Mechanical Properties of Friction Stir Processed Al-6061 Alloy

Three different stir tools with the pin eccentricity of 0, 0.4 and 0.8 mm were applied to the friction stir processing (FSP) of Al-6061 alloy. Results show that the pin-affected zone (PAZ) enlarges and the grain size in the stir zone (SZ) decreases as the pin eccentricity increases. Moreover, the low peak FSP temperature induced by the pin eccentricity gives rise to the coarsening of strengthening precipitates in the SZ. Compared with the pin-eccentric FSP samples, the SZ produced without pin eccentricity exhibits the highest hardness and yield strength due to the high amount of fine precipitates. However, the application of pin eccentricity elevates the overall tensile properties of FSP samples through changing the failure location from heat-affected zone (HAZ) to SZ.

36 MATERIALS SCIENCE↗