Irradiation-Driven Restructuring of UO 2 Thin Films: Amorphization and Crystallization

Combustion synthesis in uranyl nitrate–acetylacetone–2-methoxyethanol solutions was used to deposit thin UO 2 films on aluminum substrates to investigate the irradiation-induced restructuring processes. Thermal analysis revealed that the combustion reactions in these solutions are initiated at ~160 °C. The heat released during the process and the subsequent brief annealing at 400 °C allow the deposition of polycrystalline films with 5–10 nm UO 2 grains. The use of multiple deposition cycles enables tuning of the film thicknesses in the 35–260 nm range. Irradiation with Ar 2+ ions (1.7 MeV energy and a fluence of up to 1 × 10 17 ions/cm 2 ) is utilized to generate a uniform distribution of atomic displacements within the films. X-ray fluorescence (XRF) and alpha-particle emission spectroscopy showed that the films were stable under irradiation and did not undergo sputtering degradation. X-ray photoelectron spectroscopy (XPS) showed that the stoichiometry and uranium ionic concentrations remain stable during irradiation. The high-resolution electron microscopy imaging and electron diffraction analysis demonstrated that at the early stages of irradiation (below 1 × 10 16 ion/cm 2 ) UO 2 films show complete amorphization and beam-induced densification (sintering), resulting in a pore-free disordered film. Prolonged irradiation (5 × 10 16 ion/cm 2 ) is shown to trigger a crystallization process at the surface of the films that moves toward the UO 2 /Al interface, converting the entire amorphous material into a highly crystalline film. This work reports on an entirely different radiation-induced restructuring of the nanoscale UO 2 compared to the coarse-grained counterpart. The preparation of thin UO 2 films deposited on Al substrates fills an area of national need within the stockpile stewardship program of the National Nuclear Security Administration and fundamental research with actinides. Here, the method reported in this work produces pure, robust, and uniform thin-film actinide targets for nuclear science measurements

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Picosecond magneto-optic thermometry measurements of nanoscale thermal transport in AlN thin films

The thermal conductivity Λ of wide bandgap semiconductor thin films, such as AlN, affects the performance of high-frequency devices, power devices, and optoelectronics. However, accurate measurements of Λ in thin films with sub-micrometer thicknesses and Λ > 100 W m -1 K -1 is challenging. Widely used pump/probe metrologies, such as time–domain thermoreflectance (TDTR) and frequency–domain thermoreflectance, lack the spatiotemporal resolution necessary to accurately quantify thermal properties of sub-micrometer thin films with high Λ. In this work, we use a combination of magneto-optic thermometry and TiN interfacial layers to significantly enhance the spatiotemporal resolution of pump/probe thermal transport measurements. We use our approach to measure Λ of 100, 400, and 1000 nm AlN thin films. We coat AlN thin films with a ferromagnetic thin-film transducer with the geometry of (1 nm-Pt/0.4 nm-Co) x3 /(2 nm-TiN). This PtCo/TiN transducer has a fast thermal response time of <50 ps, which allows us to differentiate between the thermal response of the transducer, AlN thin film, and substrate. For the 100, 400, and 1000 nm thick AlN films, we determine Λ to be 200 ± 80, 165 ± 35, and 300 ± 70 W m -1 K -1 , respectively. We conclude with an uncertainty analysis that quantifies the errors associated with pump/probe measurements of thermal conductivity, as a function of transducer type, thin-film thermal conductivity, and thin-film thickness. Time resolved magneto-optic Kerr effect experiments can measure films that are three to five times thinner than is possible with standard pump/probe metrologies, such as TDTR. This advance in metrology will enable better characterization of nanoscale heat transfer in high thermal conductivity material systems like wide bandgap semiconductor heterostructures and devices.

36 MATERIALS SCIENCE↗

Characterizing the marker-dye correction for Gafchromic EBT2 film: A comparison of three analysis methods

Purpose: Gafchromic EBT2 film has a yellow marker dye incorporated into the active layer of the film that can be used to correct the film response for small variations in thickness. This work characterizes the effect of the marker-dye correction on the uniformity and uncertainty of dose measurements with EBT2 film. The effect of variations in time postexposure on the uniformity of EBT2 is also investigated. Methods: EBT2 films were used to measure the flatness of a {sup 60}Co field to provide a high-spatial resolution evaluation of the film uniformity. As a reference, the flatness of the {sup 60}Co field was also measured with Kodak EDR2 films. The EBT2 films were digitized with a flatbed document scanner 24, 48, and 72 h postexposure, and the images were analyzed using three methods: (1) the manufacturer-recommended marker-dye correction, (2) an in-house marker-dye correction, and (3) a net optical density (OD) measurement in the red color channel. The field flatness was calculated from orthogonal profiles through the center of the field using each analysis method, and the results were compared with the EDR2 measurements. Uncertainty was propagated through a dose calculation for each analysis method. The change in the measured field flatness for increasing times postexposure was also determined. Results: Both marker-dye correction methods improved the field flatness measured with EBT2 film relative to the net OD method, with a maximum improvement of 1% using the manufacturer-recommended correction. However, the manufacturer-recommended correction also resulted in a dose uncertainty an order of magnitude greater than the other two methods. The in-house marker-dye correction lowered the dose uncertainty relative to the net OD method. The measured field flatness did not exhibit any unidirectional change with increasing time postexposure and showed a maximum change of 0.3%. Conclusions: The marker dye in EBT2 can be used to improve the response uniformity of the film. Depending on the film analysis method used, however, application of a marker-dye correction can improve or degrade the dose uncertainty relative to the net OD method. The uniformity of EBT2 was found to be independent of the time postexposure.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Evaluation of the accuracy of 3DVH software estimates of dose to virtual ion chamber and film in composite IMRT QA

Purpose: A novel patient-specific intensity modulated radiation therapy (IMRT) QA system, 3DVH software and mapcheck 2, purports to be able to use diode array-measured beam doses and the patient's DICOM RT plan, structure set, and dose files to predict the delivered 3D dose distribution in the patient for comparison to the treatment planning system (TPS) calculated doses. In this study, the composite dose to an ion chamber and film in phantom predicted by the 3DVH and mapcheck 2 system is compared to the actual measured chamber and film doses. If validated in this context, then 3DVH can be used to perform an equivalent dose analysis as that obtained with film dosimetry and ion chamber-based composite IMRT QA. This is important for those losing their ability to perform film dosimetry for true composite IMRT QA and provides a measure of confidence in the accuracy of 3DVH 3D dose calculations which may replace phantom-based IMRT QA. Methods: The dosimetric results from 15 consecutive patient-specific IMRT QA tests performed by composite field irradiation of ion chamber and EDR2 film in a solid water phantom were compared to the predicted doses for those virtual detectors based on the calculated 3D dose by the 3DVH software using mapcheck 2 measured doses of each beam within each plan. For each of the 15 cases, immediately after performing the ion chamber plus film measurements, the mapcheck 2 was used to measure the dose for each beam of the plan. The dose to the volume of the virtual ion chamber and the dose distribution in the plane of the virtual film calculated by the 3DVH software was extracted. The ratio of the measured to 3DVH or eclipse-predicted ion chamber doses was calculated. The same plane in the phantom measured using film and calculated with eclipse was exported from 3DVH and the 2D gamma metric was used to compare the relationship between the film doses and the eclipse or 3DVH predicted planar doses. Also, the 3D gamma value was calculated in the 3DVH software which compares the eclipse dose to the 3DVH predicted dose distribution. For the 2D and 3D gamma metrics, 2% dose and 2 mm distance to agreement (DTA) were used. In addition, a simple dose difference was performed using either a 2% or 3% dose difference tolerance. Results: The mean ratio {+-} standard deviation of the measured vs 3DVH or vs eclipse-predicted dose to the ion chamber was 1.013 {+-} 0.015 and 1.003 {+-} 0.012, respectively. For 3DVH vs eclipse, the mean percentage of pixels failing the 3D gamma metric was 1.2% {+-} 1.4% while the failure rate for the 2D gamma metric was 1.1% {+-} 0.9%. When either 3DVH or eclipse was compared to EDR2 film, the gamma failure rate was 2.3% {+-} 2.0% and 1.6% {+-} 1.7%, respectively. Mean dose difference failures were 9%-27% {+-} 5%-15% for 2 or 3% dose difference tolerances, depending on the combination of systems tested. No statistically significant differences were found for any of the planar dosimetric comparisons. Conclusions: 3DVH + mapcheck 2 predicts the same absolute dose, the percent of pixels failing the gamma metric, and the percent of pixels failing 2% or 3% dose difference tolerance tests as one would have obtained had one made measurements in solid water phantom using an ion chamber and coronal film instead of a diode array. This is also a necessary although not sufficient condition for validation of the accuracy of 3DVH predictions of the 3D dose using beam-by-beam measurements.

61 RADIATION PROTECTION AND DOSIMETRY↗

SU-E-T-498: Initial Characterization of the New EBT XD Gafchromic Film

Purpose To assess the dosimetric accuracy of the new EBT XD (eXtended Dose) Gafchromic film and to compare the lateral scan effect between EBT XD and EBT3 film. Methods: All films were exposed in solid water using a 6 MV beam and were analyzed with FilmQA Pro software and an Epson 10000 XL scanner. Calibration was performed using films exposed to 8 known doses from 0–3000 cGy. To assess dosimetric accuracy, a 15×18 cm{sup 2} 60° EDW delivered a dose range of 200–2900 cGy to 4 separate EBT XD films. Comparison to treatment planning system (TPS) predictions was made using a gamma analysis with 2%/2mm passing criteria. To assess the lateral scan effect, 21 × 21 cm{sup 2} open fields delivered doses of 1000, 2000, and 3000 cGy isocentrically to both EBT3 and EBT XD films at 10 cm depth. Films were centered and scanned such that the widest parts of the exposed film extended lateral to the center of the scanner bed in order to maximize the lateral scan effect. Ratios of measured to TPS predicted doses for EBT3 and EBT XD film were calculated at 5 cm and 8 cm lateral from the center of the scanner bed to quantitatively assess the lateral scan effect. Results The average gamma passing rate for the EDW was 98.9% (range 98.7 – 99.1%). EBT XD film exhibited minimal lateral scan effect (<1%) up to 30 Gy. In contrast, EBT3 showed an under-response of 13% and 25% at lateral positions of 5 cm and 8 cm respectively for the 30 Gy exposure. Conclusion EBT XD can accurately measure dose over a wide dynamic range. The non-polarizing structure of its active ingredient essentially eliminates the lateral scan effect up to at least 30 Gy. EBT XD film is therefore well suited for SRS/SBRT verification measurements.

60 APPLIED LIFE SCIENCES↗

Energy dependent calibration of XR-QA2 radiochromic film with monochromatic and polychromatic x-ray beams

Purpose: This work investigates the energy response and dose-response curve determinations for XR-QA2 radiochromic film dosimetry system used for synchrotron radiation work and for quality assurance in diagnostic radiology, in the range of effective energies 18–46.5 keV. Methods: Pieces of XR-QA2 films were irradiated, in a plane transverse to the beam axis, with a monochromatic beam of energy in the range 18–40 keV at the ELETTRA synchrotron radiation facility (Trieste, Italy) and with a polychromatic beam from a laboratory x-ray tube operated at 80, 100, and 120 kV. The film calibration curve was expressed as air kerma (measured free-in-air with an ionization chamber) versus the net optical reflectance change (netΔR) derived from the red channel of the RGB scanned film image. Four functional relationships (rational, linear exponential, power, and logarithm) were tested to evaluate the best curve for fitting the calibration data. The adequacy of the various fitting functions was tested by using the uncertainty analysis and by assessing the average of the absolute air kerma error calculated as the difference between calculated and delivered air kerma. The sensitivity of the film was evaluated as the ratio of the change in net reflectance to the corresponding air kerma. Results: The sensitivity of XR-QA2 films increased in the energy range 18–39 keV, with a maximum variation of about 170%, and decreased in the energy range 38–46.5 keV. The present results confirmed and extended previous findings by this and other groups, as regards the dose response of the radiochromic film XR-QA2 to monochromatic and polychromatic x-ray beams, respectively. Conclusions: The XR-QA2 radiochromic film response showed a strong dependence on beam energy for both monochromatic and polychromatic beams in the range of half value layer values from 0.55 to 6.1 mm Al and corresponding effective energies from 18 to 46.5 keV. In this range, the film response varied by 170%, from a minimum sensitivity of 0.0127 to a maximum sensitivity of 0.0219 at 10 mGy air kerma in air. The more suitable function for air kerma calibration of the XR-QA2 radiochromic film was the power function. A significant batch-to-batch variation, up to 55%, in film response at 120 kV (46.5 keV effective energy) was observed in comparison with published data.

61 RADIATION PROTECTION AND DOSIMETRY↗

Real time intelligent process control system for thin film solar cell manufacturing

This project addresses the problem of lower solar conversion efficiency and waste in the typical solar cell manufacturing process. The work from the proposed development will lead toward developing a system which should be able to increase solar panel conversion efficiency by an additional 12-15% resulting in lower cost panels, increased solar technology adoption, reduced carbon emissions and reduced dependency on foreign oil. All solar cell manufacturing processes today suffer from manufacturing inefficiencies that currently lead to lower product quality and lower conversion efficiency, increased product cost and greater material and energy consumption. This results in slower solar energy adoption and extends the time solar cells will reach grid parity with traditional energy sources. The thin film solar panel manufacturers struggle on a daily basis with the problem of thin film thickness non-uniformity and other parameters variances over the deposited substrates, which significantly degrade their manufacturing yield and quality. Optical monitoring of the thin films during the process of the film deposition is widely perceived as a necessary step towards resolving the non-uniformity and non-homogeneity problem. In order to enable the development of an optical control system for solar cell manufacturing, a new type of low cost optical sensor is needed, able to acquire local information about the panel under deposition and measure its local characteristics, including the light scattering in very close proximity to the surface of the film. This information cannot be obtained by monitoring from outside the deposition chamber (as traditional monitoring systems do) due to the significant signal attenuation and loss of its scattering component before the reflected beam reaches the detector. In addition, it would be too costly to install traditional external in-situ monitoring systems to perform any real-time monitoring over large solar panels, since it would require significant equipment refurbishing needed for installation of multiple separate ellipsometric systems, and development of customized software to control all of them simultaneously. The proposed optical monitoring system comprises AccuStrata’s fiber optics sensors installed inside the thin film deposition equipment, a hardware module of different components (beyond the scope of this project) and our software program with iterative predicting capability able to control material bandgap and surface roughness as films are deposited. Our miniature fiber optics monitoring sensors are installed inside the vacuum chamber compartments in very close proximity where the independent layers are deposited (an option patented by us in 2003). The optical monitoring system measures two of the most important parameters of the photovoltaic thin films during deposition on a moving solar panel - material bandgap and surface roughness. In this program each sensor array consists of two fiber optics sensors monitoring two independent areas of the panel under deposition. Based on the monitored parameters and their change in time and from position to position on the panel, the system is able to provide to the equipment operator immediate information about the thin films as they are deposited. This DoE Supply Chain program is considered the first step towards the development of intelligent optical control system capable of dynamically adjusting the manufacturing process “on-the-fly” in order to achieve better performance. The proposed system will improve the thin film solar cell manufacturing by improving the quality of the individual solar cells and will allow for the manufacturing of more consistent and uniform products resulting in higher solar conversion efficiency and manufacturing yield. It will have a significant impact on the multibillion-dollar thin film solar market. We estimate that the financial impact of these improvements if adopted by only 10% of the industry ($7.7 Billion) would result in about $1.5 Billion in savings by 2015 (at the assumed 20% improvement). This can be achieved by optimizing the manufactured product and process in real time without changing the manufacturing technology.

14 SOLAR ENERGY↗

Atmospheric Pressure Plasma CVD of Amorphous Hydrogenated Silicon Carbonitride (a-SiCN:H) Films Using Triethylsilane and Nitrogen

Amorphous hydrogenated silicon carbonitride (a-SiCN:H) thin films are synthesized by atmospheric pressure plasma enhanced chemical vapor (AP-PECVD) deposition using the Surfx Atomflow{trademark} 250D APPJ source with triethylsilane (HSiEt{sub 3}, TES) and nitrogen as the precursor and the reactive gases, respectively. The effect of the substrate temperature (T{sub s}) on the growth characteristics and the properties of a-SiCN:H films was evaluated. The properties of the films were investigated via scanning electron microscopy (SEM), atomic force microscopy (AFM) for surface morphological analyses, Fourier transform infrared spectroscopy (FTIR), and X-ray photoelectron spectroscopy (XPS) for chemical and compositional analyses; spectroscopic ellipsometry for optical properties and thickness determination and nanoindentation to determine the mechanical properties of the a-SiCN:H films. Films deposited at low T{sub s} depict organic like features, while the films deposited at high T{sub s} depict ceramic like features. FTIR and XPS studies reveal that an increases in T{sub s} helps in the elimination of organic moieties and incorporation of nitrogen in the film. Films deposited at T{sub s} of 425 C have an index of refraction (n) of 1.84 and hardness (H) of 14.8 GPa. A decrease in the deposition rate between T{sub s} of 25 and 250 C and increase in deposition rate between T{sub s} of 250 and 425 C indicate that the growth of a-SiCN:H films at lower T{sub s} are surface reaction controlled, while at high temperatures film growth is mass-transport controlled. Based on the experimental results, a potential route for film growth is proposed.

36 MATERIALS SCIENCE↗

Effect of Substrate Temperature on Structural, Morphological, Magnetic, and Electrical Properties of Fe{sub 2}CoSi Heusler Alloy Thin Films for Spin-Based Device Applications

Fe{sub 2}CoSi based Heusler alloy thin films are deposited on single crystal Si (111) substrate at different substrate temperatures varying from room temperature to 600 °C using ultrahigh vacuum DC magnetron sputtering. Structural analysis of the prepared thin films is carried out using GI-XRD measurement and it conform ordered L2{sub 1} crystal structure of the films deposited at 450 °C and above. The atomic force microscopic (AFM) images of Fe{sub 2}CoSi thin films exhibiting 3D-like growth on Si (111) substrate at varying temperatures. The magnetic property of the thin films is studied using vibrating sample magnetometer (VSM). At 450 °C of substrate temperature, the prepared thin film exhibits high saturation magnetization (M{sub s} = 948 emu/cc) and low coercivity (H{sub c} = 8 Oe). The self-energy magnetization of the film and its own field is very high, when the temperature of the substrate was maintained at 450 °C and switching field ratio for this film was obtained as ~ 0.9 due to its high crystallinity and atomic ordering. The electrical property of Fe{sub 2}CoSi thin film is investigated using four-probe technique and a positive magnetoresistive behavior was observed for thin film deposited at a substrate temperature of 450 °C which indicates the possible half-metallic nature at room temperature. The enhanced magnetic and electrical properties obtained for the thin film prepared at 450 °C substrate temperature is highly suitable for spin based device applications.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Relation between carriers hopping rate and structural constants in amorphous carbon nickel films with different nickel nanoparticles distributions

In this paper, the films were prepared by radio frequency magnetron co-sputtering technique. The effect of different mosaic targets made of nickel strips and graphite pure on the dielectric relaxation time, the carriers hopping rate, the fractal dimensions and the optical loss of films were studied. The values of the optical band gap of films using the cross-point between the tangent of the plot of lower and higher values of the photon energy were calculated. The films deposited at 4.64% have maximum hopping rate of about 8.6 × 10{sup 12} S{sup −1}. It can be seen that the films deposited at 3.92% have minimum value of fractal dimension of 2.27. With increasing Ni content of films a nonmetal–metal transition is observed which it is explainable by the power law of percolation theory. Critical metal content and the critical exponent of films were 87.25% and 1, respectively. With increasing Ni content, the carriers effective mass of films decreased and average lattice separation values of films increased. Films deposited at 3.92% have minimum value of Debye frequency ν{sub D} of about 1.09 × 10{sup 12} Hz. The value of energy loss by free charge carriers when traversing the bulk and surface of films at 3.92% has maximum value and it has an increasing function behavior with energy.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Properties of Nb3Sn films fabricated by magnetron sputtering from a single target

Superconducting Nb3Sn films were fabricated on sapphire and fine grain Nb substrates by magnetron sputtering from a single stoichiometric Nb3Sn target. The structural, morphological and superconducting properties of the films annealed for 24 h at temperatures of 800-1000 {\deg}C were investigated. The effect of the annealing time at 1000 {\deg}C was examined for 1, 12, and 24 h. The film properties were characterized by X-ray diffraction, scanning electron microscopy, atomic force microscopy, energy dispersive X-ray spectroscopy, and Raman spectroscopy. The DC superconducting properties of the films were characterized by a four-point probe measurement down to cryogenic temperatures. The RF surface resistance of films was measured over a temperature range of 6-23 K using a 7.4 GHz sapphire-loaded Nb cavity. As-deposited Nb3Sn films on sapphire had a superconducting critical temperature of 17.21 K, which improved to 17.83 K when the film was annealed at 800 {\deg}C for 24 h. For the films annealed at 1000 {\deg}C, the surface Sn content was reduced to ~11.3 % for an annealing time of 12 h and to ~4.1 % for an annealing time of 24 h. The Raman spectra of the films confirmed the microstructural evolution after annealing. The RF superconducting critical temperature of the as-deposited Nb3Sn films on Nb was 16.02 K, which increased to 17.44 K when the film was annealed at 800 {\deg}C for 24 h.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Understanding non-stochiometric deposition of multi-principal elemental NiCoCr thin films

Multi-principal elemental NiCoCr thin films with compositional flexibility have potential applications as a thermal barrier, corrosion-resistant coatings, and functional energy materials. In this study, the non-stochiometric multi-principal element alloy thin film formation behavior from an equiatomic ablation target of NiCoCr using pulsed laser deposition has been reported. Here, the effect of varying laser fluence on compositions of constituent elements in the NiCoCr thin films is systematically investigated. The increase in laser fluence typically increases the likelihood of acquiring undesirable particulates in thin films. Therefore, to maintain the film quality the laser fluences are adjusted within the range of 1.3–3.3 J·cm -2 , while the film thicknesses are kept constant at ~30 nm. Results show that the constituent elements are well-distributed in the formed NiCoCr thin films, however, having average atomic percentages of Ni and Cr twice as high as Co irrespective of the equiatomic composition of individual elements in the ablation target. This stochiometric alteration in the as-deposited thin films is governed by the rate of ablation and subsequent evaporation of each element, which is facilitated by the optical properties and vapor pressure of individual constituent elements. Additionally, electron energy-loss spectroscopy and x-ray absorption spectroscopy analysis reveal that the thin films have partially oxidized, with the Cr oxidation contributing the most to the O-K edge in comparison to Ni and Co. Finally, this study presents a laser-assisted pathway for fabricating compositionally flexible NiCoCr thin films and develops an understanding of the non-equilibrium laser-material interactions and how the intrinsic properties of constituent elements affect the stoichiometric flow of materials from the target to the final film deposition.

36 MATERIALS SCIENCE↗

Effects of substrate temperature on properties of ITO-ZnO composition spread films fabricated by combinatorial RF magnetron sputtering

We have fabricated ITO-ZnO composition spread films to investigate the effects of substrate temperature on their electrical and optical properties by using combinatorial RF magnetron sputtering. It turned out by X-ray measurement that the film with zinc contents above 16.0 at% [Zn/(In+Zn+Sn)] showed amorphous phase regardless of substrate temperature. The amorphous ITO-ZnO film had lower resistivity than polycrystalline films. When the films were deposited at 250 deg. C, the minimum resistivity of 3.0x10{sup -4} OMEGA cm was obtained with the zinc contents of 16.0 at%. The indium content could be reduced as high as {approx}30 at% compared to that of ITO for the films having similar resistivity ({approx}10{sup -4} OMEGA cm). However, a drastic increase of resistivity was observed for the ITO-ZnO films deposited at 350 deg. C, having zinc contents below 15.2 at%. - Graphical abstract: The effects of substrate temperature on properties of ITO-ZnO films were investigated by using combinatorial RF magnetron sputtering. The amorphous ITO-ZnO film had lower resistivity than polycrystalline films. The minimum resistivity of 3.0x10{sup -4} OMEGA cm was obtained with the substrate temperature of 250 deg. C and the zinc contents of 16.0 at%. The electronic states of ITO-ZnO films were discussed with related to the formation of transparent amorphous oxide semiconductor (TAOS).

36 MATERIALS SCIENCE↗

Combinatorial study of WInZnO films deposited by rf magnetron co-sputtering

The compositional dependence of co-sputtered tungsten indium zinc oxide (WInZnO) film properties was first investigated by means of a combinatorial technique. Indium zinc oxide (IZO) and WO{sub 3} targets were used with different target power. W composition ratio [W/(In+Zn+W)] was varied between 3 and 30 at% and film thickness was reduced as the sample position moved toward WO{sub 3} target. Furthermore, the optical bandgap energy increased gradually, which might be affected by the reduction in film thickness. All the WInZnO films showed an amorphous phase regardless of the W/(In+Zn+W) ratio. As the W/(In+Zn+W) ratio in WInZnO films increased, the carrier concentration was restricted, causing the increase in electrical resistivity. W cations worked as oxygen binders in determining the electronic properties, resulting in suppressing the formation of oxygen vacancies. Consequentially, W metal cations were effectively incorporated into the WInZnO films as a suppressor against the oxygen vacancies and the carrier generation by employing the combinatorial technique. - Graphical abstract: The film thickness and the sheet resistance (R{sub s}) with respect to the sample position of WInZnO films, which is compositionally graded by rf power for each target, are exhibited. Highlights: > The compositional dependence of co-sputtered WInZnO film properties is first investigated. > W cations work as oxygen binders in determining the electronic properties. > All the WInZnO films show an amorphous phase regardless of the W/(In+Zn+W) ratio. > W metal cations are effectively incorporated into the WInZnO films by the combinatorial technique.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Characterization of niobium-doped titania epitaxial films deposited by metalorganic chemical vapor deposition

Highlights: • The undoped and Nb-doped TiO{sub 2} films were deposited on SrTiO{sub 3} (100) substrates. • The epitaxial growth relationship between TiO{sub 2} film and the substrate was confirmed. • The microstructures of the films were explored. • The electrical and optical properties of the films were revealed. - Abstract: Titania (TiO{sub 2}) films with different niobium (Nb) doping concentrations were deposited on SrTiO{sub 3} (STO) (100) substrates by metalorganic chemical vapor deposition (MOCVD). The crystal structures, surface morphologies, electrical and optical properties of the Nb-doped TiO{sub 2} (TiO{sub 2}:Nb) films varying with Nb content were investigated. The single crystal TiO{sub 2} films with anatase structure were obtained at low Nb doping levels. The highest Hall mobility of the prepared films reached as high as 16.50 cm{sup 2} V{sup −1} s{sup −1}. The lowest resistivity of 5.75 × 10{sup −2} Ω cm with a Hall mobility of 7.40 cm{sup 2} V{sup −1} s{sup −1} and a carrier concentration of 1.47 × 10{sup 19} cm{sup −3} were obtained from the 1.20% Nb-doped TiO{sub 2} film. This resistivity was about 6 orders of magnitude lower than the undoped TiO{sub 2} film. Moreover, all the deposited films exhibited high average transmittances of over 88% in the visible wavelength range.

36 MATERIALS SCIENCE↗

Structure and properties of ternary manganese nitride Mn{sub 3}CuN{sub y} thin films fabricated by facing target magnetron sputtering

Graphical abstract: This figure reveals the dependence of the texture coefficient TC{sub (111)} and TC{sub (200)} of the Mn{sub 3}CuN{sub y} thin films on T{sub sub}. These results indicate that the preferred orientation of the Mn{sub 3}CuN{sub y} thin films dramatically changed from (1 1 1) to (2 0 0) with the increase of T{sub sub}. In one word, the orientation of Mn{sub 3}CuN{sub y} thin film can be tailored by adjusting the magnetron sputtering processing parameters and substrate. It is the first time to report the deposition of Mn{sub 3}CuN{sub y} thin films on single crystal Si (1 0 0) at various substrate temperatures (T{sub sub}) by facing target magnetron sputtering. The influences of substrate temperature on crystal structure and morphology are discussed. The temperature dependences of magnetization, lattice parameters and resistivity for the resulting film are systematically investigated, which shows several different physical properties from those of previous work. Highlights: {yields} Variation of the substrate temperatures adjusted the preferred orientation from (1 1 1) to (2 0 0) of the Mn{sub 3}CuN{sub y} thin films. {yields} There exists a magnetic ordering transition at 225 K from paramagnetic (PM) to ferrimagnetic (FI), which is different than previous results. {yields} It shows a positive thermal expansion behavior with average linear thermal expansion coefficient 2.49 x 10{sup -5} K{sup -1}. However there was no crystal phase transition occurred around the magnetic transition in the film. {yields} The temperature dependence of resistivity displayed a semiconductor-like behavior, which is quite different from the bulk sample. {yields} We believe that our findings may provide an important role to further utilize the potential of antiperovskite manganese nitride film. -- Abstract: Deposition of Mn{sub 3}CuN{sub y} thin films on single crystal Si (1 0 0) at various substrate temperatures (T{sub sub}) by facing target magnetron sputtering is reported. The crystal structure and composition were characterized by X-ray diffraction (XRD) and X-ray photoelectron spectroscopy (XPS). The results confirmed that the crystalline antiperovskite Mn{sub 3}CuN{sub y} thin film with (2 0 0) highly preferred texture had been obtained at T{sub sub} = 180 {sup o}C. Furthermore, for the resulting Mn{sub 3}CuN{sub y} thin film, it showed different properties compared with the bulk counterpart. There was a paramagnetic to ferrimagnetic transition at 225 K with decreasing temperature. The change of the lattice constant with temperature presented positive thermal expansion behavior and no structural transition was observed. The average linear thermal expansion coefficient ({alpha}) is 2.49 x 10{sup -5} K{sup -1} from 123 K to 298 K. More interestingly, the temperature dependence of resistivity displayed a semiconductor-like behavior, i.e. an obvious monotonous decrease of resistivity with increasing temperature.

36 MATERIALS SCIENCE↗

Structural and pyroelectric properties of sol-gel derived multiferroic BFO thin films

Highlights: Black-Right-Pointing-Pointer We fabricated multiferroic BFO/PZT multilayer films by spin-coating method. Black-Right-Pointing-Pointer The trap centers of carriers were formed at the interfaces between BFO and PZT films. Black-Right-Pointing-Pointer The ferroelectric properties were superior to those of single composition BFO film. -- Abstract: Multiferroic BFO/PZT multilayer films were fabricated by spin-coating method on the (1 1 1)Pt/Ti/SiO{sub 2}/Si substrate alternately using PZT(30/70), PZT(70/30) and BFO alkoxide solutions. The structural and ferroelectric properties were investigated for uncooled infrared detector applications. The coating and heating procedure was repeated six times to form BFO/PZT multilayer films. All films showed the typical XRD patterns of the perovskite polycrystalline structure without presence of the second phase such as Bi{sub 2}Fe{sub 4}O{sub 3}. The thickness of BFO/PZT multilayer film was about 200-220 nm. The ferroelectric properties such as dielectric constant, remnant polarization and pyroelectric coefficient were superior to those of single composition BFO film, and those values for BFO/PZT(70/30) multilayer film were 288, 15.7 {mu}C/cm{sup 2} and 9.1 Multiplication-Sign 10{sup -9} C/cm{sup 2} K at room temperature, respectively. Leakage current density of the BFO/PZT(30/70) multilayer film was 3.3 Multiplication-Sign 10{sup -9} A/cm{sup 2} at 150 kV/cm. The figures of merit, F{sub V} for the voltage responsivity and F{sub D} for the specific detectivity, of the BFO/PZT(70/30) multilayer film were 6.17 Multiplication-Sign 10{sup -11} Ccm/J and 6.45 Multiplication-Sign 10{sup -9} Ccm/J, respectively.

36 MATERIALS SCIENCE↗

Chemical bath deposition and characterization of electrochromic thin films of sodium vanadium bronzes

Highlights: Black-Right-Pointing-Pointer We report a new chemical bath method for the deposition of vanadium bronze thin films. Black-Right-Pointing-Pointer The films are phase mixture of NaV{sub 6}O{sub 15} and Na{sub 1.1}V{sub 3}O{sub 7.9} with 10.58% lattice water. Black-Right-Pointing-Pointer The as-deposited vanadium bronze films exhibit two-step electrochromism. Black-Right-Pointing-Pointer They change their yellow-orange color to green and then from green to blue color. Black-Right-Pointing-Pointer The method allows the preparation of films on substrates with low melting point. -- Abstract: Thin yellow-orange films of sodium vanadium oxide bronzes have been prepared from a sodium-vanadium solution (1:1) at 75 Degree-Sign C and pH = 3. The composition, structure and morphology of the films have been studied by XRD, IR spectroscopy, TG and SEM-EDX analyses. It has been established that the prepared films are a phase mixture of hydrated NaV{sub 6}O{sub 15} (predominant component) and Na{sub 1.1}V{sub 3}O{sub 7.9} with total water content of 10.58%. The sodium vanadium bronze thin films exhibit two-step electrochromism followed by color change from yellow-orange to green, and then from green to blue. The cyclic voltammetry measurements on the as-deposited and annealed vanadium bronze films reveal the existence of different oxidation/reduction vanadium sites which make these films suitable for electrochromic devices. The annealing of the films at 400 Degree-Sign C changes the composition, optical and electrochemical properties.

36 MATERIALS SCIENCE↗