Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ELONGATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,207 records · Page 67

Microstructure and Mechanical Properties of Spray-Formed 7075 Alloy During Retrogression

The mechanical properties, conductivity, microstructure, precipitation behavior and evolution process of elements and phases of spray-formed 7075 alloy during retrogression are studied by the tensile test, electric test, hardness test, transmission electron microscope (TEM), x-ray diffraction (XRD) analysis, electron-dispersive spectroscopy (EDS) and lattice parameter measurements. The results show that the mechanical properties and conductivity of the alloy can be effectively improved when treated at a suitable retrogression temperature and time. According to the TEM observations, XRD analysis, EDS and an accurate measurement of the lattice parameter, the redissolution of elements and precipitated phases can be readily observed. From the optimization selection of the RRA treatment for the 7075 alloy, the regularity of redissolution and precipitation of the elements and phases are evaluated. The ultimate tensile strength, yield strength, hardness, elongation and conductivity of the spray-formed 7075 alloy after preaging at 120 °C for 16 h, retrogression at 200 °C for 8 min and reaging at 120 °C for 24 h are 791, 736 MPa, 181 HBW, 8.5% and 22.6 MS/m, respectively.

36 MATERIALS SCIENCE↗

Microstructural Evolution and Mechanical Behavior of Lead-Free Silicon Brass Manufactured by Low-Pressure Die Casting

Low-pressure die casting (LPDC) has been widely used to process aluminum and magnesium alloys; however, it has yet to be applied to manufacture brass alloys. This study investigates the microstructural evolution and mechanical behavior of a lead-free CuZnSiAl silicon brass via a variable-controlling approach on the basis of a faucet casting by LPDC. The manufactured silicon brass castings are predominantly composed of bcc β-CuZn(Si, Al) and minor fcc α-Cu(Zn, Si) solid solutions. The silicon brass castings also predominantly exhibit short rod-like or granular α phases, which distinctly differ from the acicular α morphology obtained by conventional gravity casting. The manufactured silicon brass castings which contain finer β grains and short rod-like or granular α phase exhibit superior mechanical properties. Their optimal mechanical properties—elongation of 15.0%, yield strength of 359.8 MPa, and ultimate tensile strength of 598.9 MPa—are far superior to those of the typical lead brass HPb59-1. The results obtained in this study provide insight into the manufacture and design of lead-free silicon brass castings by LDPC.

36 MATERIALS SCIENCE↗

Enhanced Strength of 304 SS-Ti6Al4V Laser-Welded Joints Containing Composite Interlayers

This paper investigates the microstructural characterization of the fracture propagation edge during laser beam welding of Ti6Al4V and 304 stainless steel using Cu, V, and Ni interlayers as a single Cu interlayer and composite interlayer structures with different Cu interlayer thicknesses. This study attempts to increase the Ti-SS joint strength through the use of the composite interlayers. X-ray diffraction characterization based on a 0.5-mm-thick Cu interlayer showed that the SS/Cu/Ti joint contained considerable brittle IMCs; however, the fracture surface of the SS/Cu-V/Ti composite interlayer sample did not contain any Fe-Ti IMCs or Cr{sub 2}Ti. EBSD observation indicated that the crack propagated transgranularly from solidified CuTi in the interdendritic regions of the FeTi compounds in the composite interlayer sample; however, the crack propagated intergranularly along Fe{sub 2}Ti grain boundaries in the single interlayer sample. The investigation based on a 1-mm-thick Cu interlayer showed that the SS/Ni-Cu1/Ti sample was stronger than the SS/Cu1/Ti sample due to a lack of CuTi at 3.5 kW. The tensile strength of the SS/Cu1-V/Ti joint was greater than that of the SS/Ni-Cu1/Ti joint due to the formation of ductile NiTi instead of brittle NiTi{sub 2}. The microstructures of the fracture edges after tensile testing illustrated that the eutectic CuTi + CuTi{sub 2} fractured at the SS/Cu1/Ti joint after tensile testing, while CuTi{sub 2} and eutectoid αTi + CuTi{sub 2} compounds fractured during the tensile experiment at the SS/Ni-Cu1/Ti and SS/Cu1-V/Ti joints, respectively. Investigations based on both the 0.5- and 1-mm-thick Cu interlayers showed that the tensile strength and elongation of the composite interlayer joints at a laser power of 3.5 kW were greater than those of the single interlayer joints.

36 MATERIALS SCIENCE↗

Achieving Excellent Strength–Ductility and Impact Toughness Combination by Cyclic Quenching in Medium Mn TRIP-Aided Steel

A novel heat treatment process combined cyclic quenching (CQ) with austenite reversion treatment (ART) is proposed to obtain high strength–ductility and high-impact toughness combination in Fe-0.18C-8.92Mn-3.43Al (in mass%) steel. The process referred as CQ-ART was designed for accomplishing the following objectives: (i) refine the prior austenite grains during cyclic quenching process, (ii) further obtain the refined austenite–ferrite block and (iii) improve the stabilities of retained austenite with Mn/C enrichment during ART process. The outstanding product of tensile strength and total elongation of CQ-ART-treated steels was 41.53 and 37.39 GPa%, respectively, and higher than the ART steel of 27.45 GPa%. The highest Charpy impact toughness of CQ-ART steel can reach to 221 J, which is mainly attributed to the refined grains and discontinuous transformation-induced plasticity (TRIP) effect.

36 MATERIALS SCIENCE↗

Grain Refinement, Microstructure and Mechanical Properties Homogeneity of Mg-Gd-Y-Nd-Zr Alloy During Multidirectional Forging

Multidirectional forging (MDF) of Mg-Gd-Y-Nd-Zr alloy was performed under decreasing temperature condition. The grain refinement, microstructure and mechanical properties homogeneity of Mg-Gd-Y-Nd-Zr alloy during MDF process were investigated. The results show that the grain refinement mechanism of Mg-Gd-Y-Nd-Zr alloy during MDF process was dynamic recrystallization. The dynamic precipitations were observed after MDF process, which were mainly located at the grain boundaries and had a significant influence on the grain refinement, and the amount of dynamic precipitations increased as the MDF passes increase. The microstructure of the billet was not homogeneous due to the deformation and temperature inhomogeneity during MDF process. Optimization MDF process has been proposed, which benefited the microstructure homogeneity and reduced the amount of the dynamic precipitations. Based on the optimization MDF process, the elongation to fracture significantly increased.

36 MATERIALS SCIENCE↗

Effects of Mg Content on the Fatigue Strength and Fracture Behavior of Al-Si-Mg Casting Alloys

In order to investigate the influence of Mg content on the fatigue properties in Al-Si-Mg alloy, uniaxial tensile tests and rotating bending fatigue tests were conducted on two Al-7Si-Mg casting alloys, with different Mg contents of 0.3 and 0.6 wt.%. The fracture surfaces of the specimens were observed by scanning electron microscopy, and the fatigue crack growth process was obtained by the replica method. The results indicate that the increase in Mg content enhances the yield strength and tensile strength of the alloy, whereas it reduces its elongation. There is an obvious knee point in the S–N curves of Al-7Si-0.6Mg alloy while that of Al-7Si-0.3Mg alloy shows continuous decrease. The fatigue strength at 5 × 10{sup 5} cycles is 60 MPa for Al-7Si-0.3Mg alloy and 80 MPa for Al-7Si-0.6Mg alloy. For the two types of specimens, the fatigue failure can initiate from crystal slip and casting defects. The replica results suggest that cracks in Al-7Si-0.6Mg alloy grow more slowly than that in Al-7Si-0.3Mg alloy.

36 MATERIALS SCIENCE↗

Microstructure and Tensile Properties of the Fe-32%Ni-4%Co Alloy During Cryorolling and Subsequent Annealing

The Fe-32%Ni-4%Co alloy was cryorolled to produce thickness reductions of 10, 40, 60 and 90%; then, the strips with a final thickness of 0.52 mm were annealed at 893, 923 and 943 K for different soaking times. The x-ray diffraction measurements indicated that both thermally induced α′-martensite (α′-M) and deformation-induced α′-M were present in the tested alloy. The thermally induced α′-M was mainly lath-shaped, while the morphology of the deformation-induced α′-M gradually changed from lath-shaped to irregular-shaped according to transmission electron microscopy observations. After the 90% reduction due to cryorolling, the total volume fraction of α′-M reached 75.6%, and the average ultimate tensile strength (UTS{sub av.}) was significantly improved from 430.3 to 1306.8 MPa. Upon subsequent annealing at 923 K for 5 min, the tested alloy mainly consisted of a large number of fine grains and a few coarse grains (CGs). In addition, several deformed structures were also observed. As the annealing time increased to 10 and 30 min, the fraction of CGs increased, and a bimodal grain size distribution was obtained, while the deformed structures were still present. The temperature of the reverse phase transformation of α′-M → γ was lower than the recrystallization temperature, which may be the main reason for the bimodal grain distribution. With this bimodal grain structure, the alloy exhibited a combination tensile strength of 543.3 MPa and an average elongation of 34.1%.

36 MATERIALS SCIENCE↗

Achieving Grain Refinement and Related Mechanical Property Improvement of an Al-Zn-Mg-Cu Alloy Through Severe Plastic Deformation

Microstructural features and mechanical properties of an Al-Zn-Mg-Cu alloy processed by equal-channel angular pressing (ECAP) have been investigated. The equivalent plastic strain obtained from the simulation agrees well with that from the analytical calculation in a way that both increase with an increase in deformation, but the strain distribution is non-uniform, appearing as a strain gradient along the norm direction. Microstructure investigation shows that grain refinement is achieved in frequency of low-angle grain boundaries fabricated by ECAP. The pole density is reduced by ECAP, during which the Brass and Goss type textures are introduced. TEM results show chain-like recrystallized grains formed at the grain boundaries and broken second-phase particles come into being due to the heavy shear force. After ECAP, the hardness and strength increase significantly while the elongation is reduced. Besides, an extreme strengthening is confirmed because of the balance between dynamic hardening and softening. The microstructure evolution mechanism is revealed in terms of grain refinement, precipitate phase breakage and texture evolution.

36 MATERIALS SCIENCE↗

Processing of Ultrafine-Grained Steels by Warm Rolling and Annealing

Low-carbon microalloyed steel was subjected to warm rolling followed by rapid transformation annealing (RTA) at 800-850 °C and subcritical annealing (SCA) at 600 °C to develop ultrafine ferrite grain structures (UFFG) with grain size less than 3 μm. The present study investigated the influence of light (40%) and heavy (80%) warm rolling deformation (LWR and HWR) applied during the finishing pass of two-pass rolling schedules on the microstructural evolution after rolling and subsequent annealing treatments. RTA treatment of HWR sample at a lower intercritical temperature for an optimum duration (800 °C, 30 s) developed UFFG-martensite dual-phase structure that offered the best combination of strength (YS ~ 900 MPa and UTS ~ 1200 MPa) and ductility (25% elongation). The SCA treatment provided sufficient time to achieve a uniform distribution of carbide particles throughout the ferrite matrix. SCA treatment of HWR at 600 °C for 4 h developed UFFG-carbide structure achieving YS of 800 MPa with 20% ductility. The SCA of LWR resulted in coarser ferrite grain structures (grain size > 5 μm) having higher ductility (more than 30%) but lower strength (UTS of 400-550 MPa) as compared to RTA.

36 MATERIALS SCIENCE↗

Importance of Martensite Spatial Distribution at Large Volume Fractions in Imparting Ductility in High-Strength Dual-Phase Steel

Controlled austenite decomposition in a cold-rolled steel was carried out in a hot-dip process simulator with different inter-critical annealing process parameters to produce dual-phase steel consisting of martensite phase fraction above 50%. The evolving microstructure was characterized by using scanning electron microscope and electron backscattered diffraction techniques. Macro- and micro-texture was characterized by using x-ray diffraction and electron backscattered diffraction techniques, respectively. Uniaxial tensile deformation showed a very good combination of ultra-high strength above 900 MPa with uniform elongation of above 7%. An anomalous increase in ductility was observed for steel with high martensite volume fraction of 62.2% compared to that of lower fraction of 52.3%, indicating the influence of size and spatial distribution arrangement of ferrite and martensite phases. The enhancement in the ductility with high strength was attributed to the improved plastic deformability of hard fine martensite phase along with fine ferrite surrounding it. The nature of micro- and macro-texture was also found to affect strain partitioning compatibility between ferrite and martensite in this study.

36 MATERIALS SCIENCE↗

Effect of Martensite Content on Failure Behavior of Laser Welded Dual-Phase Steel Joints During Deformation

Laser welding was applied to three types of dual-phase (DP) steel sheets (DP590, DP780, and DP980) with different martensite contents. The microstructure of laser welded joints was observed by optical microscope and scanning electron microscope, and the hardness of welded joints was measured by a microhardness tester. The tensile testing machine and the Erichsen test machine were employed to measure the tensile properties and forming properties of welded joints, respectively. The microstructure model showed that the welded joints of three different materials all contained a hardened zone (HZ) that was composed of a fusion zone, a coarse-grained heat-affected zone, and fine-grained heat-affected zone. The microstructure of the HZ contained mainly martensite such that the average martensite content of welded joints was increased by 1.9-9.8%, and the microhardness of the HZ was 1.2-1.9 times that of the base metal (BM). Moreover, the elongation of welded joints decreased with decreasing martensite content in the BM, and the effect was severe for the DP590 welded joint (21.8%) compared to the other two welded joints. During the Erichsen test, deformation failure varied among the welded joints with different martensite contents, and it was determined by the HZ and softened zone. The fracture occurred in the softened zone and ran parallel along the zone for DP980 welded joints, whereas the fracture occurred in the HZ and ran perpendicular to this zone for the other two welded joints. The Erichsen values of the DP590, DP780, and DP980 welded joints were 81.1, 91.7, and 85.0% of the BM, respectively.

36 MATERIALS SCIENCE↗

The Application of Canned Deformation to a Hard-Deformed Spray-Deposited Al-Zn-Mg-Cu Alloy

A wide variety of industrial applications require Al-Zn-Mg-Cu alloys with high strength and ductility. However, Zn-rich Al-Zn-Mg-Cu alloys prepared by rapid solidification methods usually show excellent strength but poor formability, which restricts their wide application in complex forming. In this study, we developed a new deformation method for the spray-deposited Zn-rich Al-Zn-Mg-Cu alloy to avoid crack formation and achieve isotropic properties. The microstructure evolution and crystallographic textures were analyzed and compared with the results of a normal deformation process. Crack-free forgings with the ultimate tensile strength (UTS), yield strength (YS) and elongation of 727 ± 5 MPa, 690 ± 3 MPa, 5.0 ± 0.7% along the radial direction and 735 ± 2 MPa, 693 ± 3 MPa, 6.3 ± 0.2% along the tangential direction were finally obtained. The improvement in the mechanical properties can be attributed to the larger amount of subgrains and substructures generated in the canned deformed alloy. The results of this study show excellent advantages and potential application prospects of the canned deformation to hard-deformed Al-Zn-Mg-Cu alloys.

36 MATERIALS SCIENCE↗

Deformation Behavior and Microstructural Evolution of Reeled Pipeline Steels during Cyclic Plastic Deformation

API X60 steel used for reeled pipeline was subjected to different amounts of cyclic plastic deformation (CPD) by multiple tension–compression tests in order to study the deformation behavior and microstructural evolution during each stage of reel-lay installation process. It was found that the yield strength was significantly reduced by about 110 MPa during the first CPD cycle due to the Bauschinger effect. However, the yield strength was little affected by the subsequent CPD cycles, and the yield strength difference between tension and compression tended to reach a steady-state value of 23 MPa after multiple CPD cycles. With the increase in CPD cycles, the proportion of low-angle grain boundaries declined from 50.9 to 35.7%, and the CPD contributed to the formation of immovable dislocation walls and cells due to the dislocation rearrangement, causing the stable yield strength. The CPD process with strain level of 3% had no prominent effect on the tensile strength and elongation, because the change in microstructures was not enough to alter the work hardening completely after multiple CPD cycles.

36 MATERIALS SCIENCE↗

Microstructural Characterization and Simulation of High Temperature Inelastic Deformation and Fracture of Al-Li 2070

A combined experimental and simulation investigation is carried out to characterize the high temperature deformation behavior of a recently developed Al-Li alloy, AA2070, over a temperature range including typical forging temperatures. Focus is placed on providing explanations for the temperature-dependent plastic and fracture behavior observed for this material using macroscale tensile tests, microscale imaging and analysis, and physics-based micromechanical modeling. It is shown that AA2070 experiences non-monotonic elongation to failure with a rise in temperature. Detailed fractography and microstructural analysis, including dynamic recrystallization analysis, provide insight into this interesting and practically useful behavior. In addition, a validated crystal plasticity model is called upon to explain the unique texture observed in the necked region of the ductile tensile specimen. The insights provided by this investigation will allow improved design of high temperature forming operations for AA2070 and similar alloys which can extend the application of third generation Al-Li alloys.

36 MATERIALS SCIENCE↗

Significant Contribution to Strength Enhancement from Deformation Twins in Thermomechanically Processed Al{sub 0.1}CoCrFeNi Microstructures

Strengthening mechanisms from thermomechanical processing treatments were explored in single-phase FCC high-entropy alloy Al{sub 0.1}CoCrFeNi. Cold work offers substantial strengthening in this low stacking fault energy material owing to the resultant high work hardening rates. An enormous increase in yield strength of ~ 275% was obtained in 40% rolled material, but was accompanied by a steep drop in ductility. Recovery and recrystallization annealing treatments were investigated for improving elongation and obtaining better balance of strength–ductility combinations. Formation of novel microstructures from the different processing routes was examined. X-ray diffraction peak broadening and mechanical test results were coupled to estimate micro-strain in the different conditions and understand micro-strain’s correlation to strength. Retention of large-scale deformation twins formed during cold rolling is shown to play a key role in elevation of yield strength after heat treatments.

36 MATERIALS SCIENCE↗

Creep and Fatigue Issues for Structural Materials in Demonstration Fusion Energy Systems

in an environment consisting of intense neutron irradiation, high temperatures, and cyclic varying stress. Therefore, thermal creep and creep-fatigue (in addition to radiation effects issues such as irradiation creep) are anticipated to be important issues for the engineering design of structural materials for fusion reactors. The key materials systems under consideration for structures of fusion reactors include 8-9%Cr ferritic/martensitic steels, oxide dispersion strengthened ferritic steels, vanadium alloys, and SiC fiber-reinforced SiC matrix ceramic composites. The current elevated temperature creep-fatigue design rules based on the American Society of Mechanical Engineers (ASME) code are discussed, along with a brief review of creep-fatigue interaction mechanisms. Refinements to current international design codes to include radiation-induced phenomena such as reduction in uniform elongation have been performed in association with the engineering design of the ITER fusion energy device currently under construction in France. Several other creep-fatigue issues of potential importance for fusion energy applications are discussed.

36 MATERIALS SCIENCE↗

Single-strand DNA translation initiation step analyzed by Isothermal Titration Calorimetry

Is single-strand DNA translatable? Since the 60s, the question still remains whether or not DNA could be directly translated into protein. Some discrepancies in the results were reported about functional translation of single-strand DNA but all results converged on a similar behavior of RNA and ssDNA in the initiation step. Isothermal Titration Calorimetry method was used to determine thermodynamic constants of interaction between single-strand DNA and S30 extract of Escherichia coli. Our results showed that the binding was not affected by the nature of the template tested and the dissociation constants were in the same range when ssDNA (K{sub d} = 3.62 {+-} 2.1 x 10{sup -8} M) or the RNA corresponding sequence (K{sub d} = 2.7 {+-} 0.82 x 10{sup -8} M) bearing SD/ATG sequences were used. The binding specificity was confirmed by antibiotic interferences which block the initiation complex formation. These results suggest that the limiting step in translation of ssDNA is the elongation process.

60 APPLIED LIFE SCIENCES↗