Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “fractures”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,189 records · Page 66

The effect of loading direction on the fracture behaviors of cortical bone at a dynamic loading rate

Here, the dynamic cracking processes in porcine cortical bone were visualized in real-time using the high-speed synchrotron X-ray phase-contrast imaging (PCI) technique in three osteon orientations: in-plane transverse, out-of-plane transverse and in-plane longitudinal. The dynamic flexural loading applied on the pre-notched bone specimens was introduced by a modified Kolsky compression bar. High-speed X-ray images of the entire loading events were documented with a high-speed camera. Three-dimensional X-ray micro-computed tomography was conducted to examine the intact microstructures and obtain the basic material properties of the bone material used for mechanical characterizations. The onset location, where crack initiated, and the subsequent direction, along which the incipient crack propagated, were measured quantitatively using the high-speed X-ray images and the latter was found dependent on the osteon direction significantly. The crack propagation velocities were dependent on crack extension over the entire crack path significantly for all the three directions while the initial velocity for in-plane longitudinal direction was lower than the other two directions. Straight-through crack paths were observed for in-plane longitudinal specimens while the cracks were deflected and twisted in the in-plane transverse direction. For out-of-plane transverse direction, the cracks follow paths with tortuosity fall in between the other two directions, showing a mixed mode of fractures of the former two extreme cases. The toughening mechanisms, visualized by the high-speed X-ray images, and the corresponding fracture toughness, evaluated in terms of fracture initiation toughness and crack growth resistance curve (R-curve), were also found significantly different among the three osteon directions, suggesting an overall transition from brittle to ductile-like fracture behaviors at the dynamic displacement rate (5.4 m/s) as the osteon orientation varies from in-plane longitudinal to out-of-plane transverse, and to in-plane transverse eventually.

42 ENGINEERING↗

A fourth-order phase-field fracture model: Formulation and numerical solution using a continuous/discontinuous Galerkin method

Modeling crack initiation and propagation in brittle materials is of great importance to be able to predict sudden loss of load-carrying capacity and prevent catastrophic failure under severe dynamic loading conditions. Second-order phase-field fracture models have gained wide adoption given their ability to capture the formation of complex fracture patterns, e.g. via crack merging and branching, and their suitability for implementation within the context of the conventional finite element method. Higher-order phase-field models have also been proposed to increase the regularity of the exact solution and thus increase the spatial convergence rate of its numerical approximation. However, they require special numerical techniques to enforce the necessary continuity of the phase field solution. In this paper, we derive a fourth-order phase-field model of fracture in two independent ways; namely, from Hamilton’s principle and from a higher-order micromechanics-based approach. The latter approach is novel, and provides a physical interpretation of the higher-order terms in the model. In addition, we propose a continuous/discontinuous Galerkin (C/DG) method for use in computing the approximate phase-field solution. This method employs Lagrange polynomial shape functions to guarantee -continuity of the solution at inter-element boundaries, and enforces the required regularity with the aid of additional variational and interior penalty terms in the weak form. Finally, the phase-field equation is coupled with the momentum balance equation to model dynamic fracture problems in hyper-elastic materials. Two benchmark problems are presented to compare the numerical behavior of the C/DG method with mixed finite element methods.

42 ENGINEERING↗

Visco-inertial gas flow through wellbore cement fractures

Understanding the nature of fluid flow through fractured wellbore cement is fundamental for evaluating the leakage potential and risk assessments of leaky wellbores. In this study, the conditions that require considering visco-inertial flow for describing the gas flow through wellbore cement fractures were investigated. Nitrogen gas flow tests were conducted on fractured cement samples under varying pressure conditions and flow rates, covering both viscous and visco-inertial flow regimes. The data substantially deviated from Darcy's law at higher flowrates and were well-fit to Forchheimer's equation for visco-inertial flow. The inertial coefficient and critical Reynolds number were expressed as a function of the hydraulic aperture. Finally, the empirical function obtained from the experiments was used as an input to numerical simulations which showed the significant role of visco-inertial flow in wellhead pressure build-up and leakage rates, and demonstrated the importance of visco-inertial flow when modeling gas flow through wellbore cement fractures.

03 NATURAL GAS↗

Numerical study of the effect of propped surface area and fracture conductivity on shale gas production: Application for multi-size proppant pumping schedule design

Hydraulic fracturing is a technique extensively used in the oil and gas industry, where water, proppant (sand) and additives are injected into unconventional reservoirs to enhance the recovery of shale hydrocarbon. Although some previous studies have developed pumping schedules that maximize gas production for a single-size proppant, there are very few studies that consider the effect of varying proppant diameters across pumping stages on shale gas production. Motivated by this, we carried out an extensive sensitivity analysis to determine the effect of different proppant diameters on the average fracture conductivity (FC), average propped surface area (PSA) and cumulative shale gas production volume. We found out that the cumulative shale gas production volume depends on both the average PSA and average FC. We also found out that small-diameter proppant resulted in higher average PSA and lower average FC, whereas large-diameter proppant resulted in lower average PSA and higher average FC. Hence, we designed a multi-size proppant pumping schedule considering both of these parameters into account for simultaneously propagating multiple fractures to maximize shale gas production from unconventional reservoirs. Since the size of injected proppant particles determines the average PSA and average FC for the propped hydraulic fractures, we developed a novel framework called Sequentially Interlinked Modeling Structure (SIMS) to predict the average PSA, average FC and cumulative shale gas production volume at the end of 10 years for a given pumping schedule. Then, we used this SIMS framework to obtain a multi-size proppant pumping schedule that maximizes shale gas production. In closing, we demonstrated that the obtained pumping schedule gives a cumulative shale gas production volume greater than the values obtained from the existing pumping schedules.

03 NATURAL GAS↗

A phase-field approach to model multi-axial and microstructure dependent fracture in nuclear grade graphite

The fracture behavior of nuclear grade graphites is strongly influenced by underlying microstructural features such as the character of filler particles, and the distribution of pores and voids. These microstructural features influence the crack nucleation and propagation behavior, resulting in quasi-brittle fracture with a tortuous crack path and significant scatter in measured bulk strength. This paper uses a phase-field method to model the microstructural and multi-axial fracture in H-451, a historic variant of nuclear graphite that provides the basis for an idealized study on a legacy grade. The representative volume elements are constructed from randomly located pores with random size obtained from experimentally determined log-normal distribution. The representative volume elements are then subjected to simulated multi-axial loading, and a reasonable agreement of the resulting fracture stress with experiments is obtained. Finally, quasi-brittle stress-strain evolution with a tortuous crack path is also observed from the simulations and is consistent with experimental results.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Fracture mechanics approach to TRISO fuel particle failure analysis

Weibull stress-based methods for failure probability assessment have been developed and analyzed to assess the integrity of tristructural isotropic (TRISO) fuel particles during fuel life cycles and accident operating conditions. While simple, these methods entail a number of drawbacks when stress concentrates near crack tips, including finite element mesh size dependency when the Weibull stress is averaged over the finite element domain. Fracture mechanics approaches involving the use of interaction integrals eliminate this lack of mesh convergence and produce consistent fracture predictions. In this work, we use an interaction integral approach to computing stress intensity factors for a crack in the inner pyrolytic carbon layer perpendicular to the silicon carbide layer, which is simplified representation of a failure mode in TRISO particles. Further, the interface between these two TRISO layers has been shown to become porous, which we simulate by considering a transition of mechanical properties over such porous length, i.e. the layers are modeled as a functionally graded material. Aspects such as porosity and thermal and irradiation eigenstrains are considered in computing the stress intensity factor from a fracture mechanics approach and compared with the known Weibull stress failure approach. The methodology introduced in this paper enables a more general fracture probability assessment in TRISO particles and eliminates the need to identify best suited parameters when using local or averaged stress-based failure criterion. Finally, the numerical sensitivity studies show how parameters such as the porous transition zone length, the material stiffness, and creep affect the probability of TRISO fuel particle failure.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Tensile deformation and fracture behavior of spray-deposition 7075/15SiC{sub p} aluminum matrix composite sheet at elevated temperatures

The tensile deformation and fracture behavior of spray-deposition 7075/15SiC{sub p} (15 vol.% SiC particle) aluminum matrix composite sheet were studied by uniaxial tension tests at temperatures ranging from 300 deg. C to 450 deg. C and strain rates of 0.001-0.1 s{sup -1}, and the fracture surfaces were examined by using a scanning electron microscopy. The results show that strain softening is present up to the point of failure and the flow stress level increases with increasing strain rate but decreases with increasing temperature. The total elongation to fracture increases with increasing temperature and with decreasing strain rate. The maximum strain rate sensitivity exponent is 0.24 which is much lower than that of typical superplastic materials. The apparent activation energy is calculated to be approximately 379 kJ/mol which is much higher than its unreinforced counterpart. The fracture surface morphology shows a large amount of localized plastic deformation in the aluminum matrix and numerous large cavities around the reinforcement. The absence of strain accommodation by interface sliding might have caused premature failure at the reinforcement/matrix interface.

36 MATERIALS SCIENCE↗

Mechanical behavior and fracture characterization of a monocrystalline Cu-Al-Ni subjected to thermal cycling treatments under load

The mechanical behavior and fracture characteristics resulting from thermal cycling treatments under different applied loads were investigated in a monocrystalline Cu-13.5 wt.%Al-4.0 wt.%Ni alloy. The treatments consisted of 300 cycles in the temperature interval between 0 deg. C (close to M{sub f}) and 100 deg. C (above A{sub f}), under applied load conditions of 0.2 and 0.5 kg corresponding, respectively, to stresses of 11 x 10{sup -2} and 28 x 10{sup -2} MPa. Following each treatment, the specimens were tested in compression until fracture at room temperature. In addition to the compression results, the mechanical behavior was also evaluated by microhardness tests. Structural changes related to phase transformations were characterized by X-ray diffraction and the fracture characteristics were analyzed by scanning electron microscopy. It was found that the thermal cycling treatments promote significant changes in the structure due to a reversible martensitic transformation. An increase in the applied load results in a decrease in both the pseudo-yield and the total strain. It also results in a lower fracture resistance owing to additional deformation accumulated during the cycling treatment, which provokes the reversible martensitic transformation.

36 MATERIALS SCIENCE↗

Evaluation of a nanoporous lyotropic liquid crystal polymer membrane for the treatment of hydraulic fracturing produced water via cross-flow filtration

Current commercial nanofiltration and reverse osmosis membranes are limited in scope and performance due to their physicochemical properties. Desalination of hydraulic fracturing wastewater poses a particular challenge to membrane filtration given the high concentrations of both organic compounds and salts present in these waters. The recently-developed nanoporous, bicontinuous cubic, lyotropic liquid crystal, thin-film-composite polymer membrane (TFC Q I membrane), having unique physicochemical properties, enables an alternative treatment of hydraulic fracturing wastewater. Specifically, the TFC Q I membrane recovers the organic compounds from this high-salinity wastewater, enabling biodegradation to occur after desalination. However, other performance criteria must be demonstrated for a membrane to reach application. The work presented herein demonstrates the stable performance of the TFC Q I membrane during 66 h of cross-flow filtration of hydraulic fracturing produced water. Compared to the commercial NF90 membrane, the TFC Q I membrane recovered a larger portion of the organic compounds, had a higher thickness-normalized water flux, and fouled less. Finally, the combination of the TFC Q I membrane's selectivity with its reduced fouling propensity makes possible a treatment for hydraulic fracturing wastewater and other complex aqueous streams inaccessible by most commercial membranes, motivating the further study and development of the TFC Q I membrane.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Improvement of the fracture toughness of hydroxyapatite (HAp) by incorporation of carboxyl functionalized single walled carbon nanotubes (CfSWCNTs) and nylon

The potential of improving the fracture toughness of synthetic hydroxyapatite (HAp) by incorporating carboxyl functionalized single walled carbon nanotubes (CfSWCNTs) and polymerized ε-caprolactam (nylon) was researched. A series of HAp samples with CfSWCNTs concentrations varying from 0 to 1.5 wt.%, without, and with nylon addition was prepared. X-ray diffraction (XRD), Scanning Electron Microscopy (SEM), and Transmission Electron Microscopy (TEM) were used to characterize the samples. The three point bending test was applied to measure the fracture toughness of the composites. A reproducible value of 3.6 ± 0.3 MPa.√m was found for samples containing 1 wt.% CfSWCNTs and nylon. This value is in the range of the cortical bone fracture toughness. Lastly, the increase of the CfSWCNTs content results to decrease of the fracture toughness, and formation of secondary phases.

36 MATERIALS SCIENCE↗

Influence of fatigue precracking and specimen size on Master Curve fracture toughness measurements of EUROFER97 and F82H steels

EUROFER97 and F82H steels are two leading reduced-activation ferritic-martensitic (RAFM) steels for fusion first wall and blanket applications. Exposure to the harsh environment of fusion reactors can result in severe degradation of fracture toughness. Thus, the post-irradiation evaluation of fracture toughness is critical for understanding the material behavior. Due to the space constraints of irradiation facilities and challenges in controlling a uniform irradiation condition for large size specimens, the development of small specimen test techniques (SSTT) is indispensable to evaluate the performance of irradiated materials. In this study, we evaluated specimen size effects on the Master Curve fracture toughness of EUROFER97 and F82H steels. A wide variety of specimens, including 0.5 T compact tension (C(T)) specimens, 0.16 T mini-compact tension (miniC(T)) specimens, and 1.65 mm miniature bend bar specimens, were tested. The testing methodology was based on the Master Curve method in the ASTM E1921 standard. No specimen size effect was observed in 0.5 T C(T) and 0.16 T miniC(T) specimens on the Master Curve reference temperature T0, while 1.65 mm miniature bend bar specimens yielded a higher T 0Q . A strong effect of fatigue precracking on T 0 for 0.5 T C(T) and 0.16 T miniC(T) specimens was observed, such that testing on specimens with skewed fatigue precrack fronts resulted in lower T 0 than for specimens with ASTM standard qualified straight fatigue precrack fronts. The results highlight the importance of experimental quality control in developing SSTT for Master Curve fracture toughness testing. Lastly, we also evaluated and provided recommendations on the minimum number of specimens needed for each specimen type for yielding reliable T 0Q values.

36 MATERIALS SCIENCE↗

Assessment of irradiation embrittlement effect on fatigue life of a pressurized-water reactor pressure vessel using the fracture toughness master curve approach

The reactor pressure vessel (RPV) is a critical structural component in pressurized-water reactors, and it is designed to withstand extreme conditions, such as high pressures, elevated temperatures, and prolonged radiation exposure. Ensuring RPV integrity is essential for the safe and reliable long-term operation of nuclear power plants, especially as aging mechanisms such as fatigue and irradiation embrittlement pose increased risks. Fatigue, caused by cyclic thermal and mechanical loading, can lead to crack initiation in localized high-stress regions. Simultaneously, neutron irradiation, particularly in the beltline region, progressively reduces fracture toughness, increasing susceptibility to brittle fracture. These combined effects of fatigue and irradiation embrittlement potentially impact the RPV structural integrity, necessitating fitness-for-service assessments. This study applies the fracture toughness master curve approach to evaluate the impact of irradiation embrittlement on RPV fatigue life. A coupled thermo-mechanical stress analysis identifies critical stress locations under normal service transients, pinpointing regions most vulnerable to fatigue crack initiation and growth. Stress intensity factors for postulated flaws at these locations are calculated, enabling an assessment of fatigue life under irradiated and unirradiated conditions. The results indicate that neutron irradiation embrittlement accelerates the conditions in which a critical crack can form and lead to failure, particularly at lower temperatures. The failure occurs where reduced fracture toughness limits the material’s resistance to crack growth. Axial cracks at nozzle corners are the most life limiting without irradiation, while circumferential cracks demonstrate longer fatigue lives. The findings highlight the importance of incorporating irradiation effects into fatigue life predictions to ensure the long-term structural integrity of RPVs.

22 - GENERAL STUDIES OF NUCLEAR REACTORS↗

Finite domain solution of a hydraulic fracture in a permeable rock

In this work, we present a domain-based algorithm to simulate the propagation of a plane-strain hydraulic fracture in a zero-toughness permeable elastic medium. The algorithm utilizes a domain-based method to solve the elasticity equation and integrates a multi-scale tip asymptote, which is particular to hydraulic fractures, into this framework. This integration is key to accurately model the energy dissipation and the fluid leak-off in the fracture tip region. The algorithm combines a 2D finite volume method (FVM) for solving the elasticity equation with a 1D FVM for solving the nonlinear lubrication equation. Incorporating the far-field asymptotics and using a moving-mesh scheme reduces the computational burden while improving the accuracy of the scheme. The paper concludes with an analysis of the numerical results. This study demonstrates the potential of this domain-based approach for modeling hydraulic fractures in poroelastic media.

Domain-based method↗

High temperature fracture toughness of single-layer CrAlN and CrAlSiN hard coatings

Hardness and toughness are among of the most important physical properties of hard coatings and it is important to analyze them at temperatures present during coating applications. CrAlN and CrAlSiN are hard coating materials frequently used in high temperature applications. Here, while both possess high oxidation resistance and thermal stability, they differ in their microstructure. In this work, the fracture toughness of magnetron-sputtered single-layer CrAlN and CrAlSiN hard coatings was determined up to 700 °C by in-situ scanning electron microscopy micro-cantilever deflection tests. The results show a decreasing trend of the fracture toughness with increasing temperature. While both coatings' fracture toughness trends are similar up to 400 °C, they diverge at higher temperatures. In general, the evolution of the fracture toughness with increasing temperature shows similarities to the observed changes in hardness in the same temperature range.

36 MATERIALS SCIENCE↗

Fracture toughness evaluation for thin-shell stainless steel weldment

Integrity of spent nuclear fuel (SNF) interim storage canisters are very important to the safety of the back-end nuclear fuel cycle. Stress corrosion cracking (SCC) potential of interim storage canister has been considered as a high priority. Because no post-weld heat treatment was required for forming these canisters, the high tensile residual stress existed within these canister welds. This can change the fracture resistance capacity significantly as well as increase SCC potential. Due to relative thin shell thickness of a canister weldment, the spiral notch torsion test (SNTT) method of small specimen approach was used to estimate the canister weldment fracture toughness. Most SNTT weldment samples fracture initiation sites are at heat-affected zone (HAZ) regions. The estimated fracture toughness $J_Q'$ for the baseline SS304 steel is at 283 kJ/m 2 . The estimated $J_Q'$ for the SS304/308 weld from HAZ and weld specimens are 126 kJ/m 2 and 148.9 kJ/m 2 , respectively.

36 MATERIALS SCIENCE↗

Integrated Experimental and Modeling Study of Geochemical Reactions of Simple Fracturing Fluids with Caney Shale

Interactions between rock minerals and hydraulic fluids directly impact the geochemical and geomechanical properties of shale formations. However, the mechanisms of geochemical reactions in shale unconventional reservoirs remain poorly understood. Here, to investigate the geochemical reactions between shale and hydraulic fracturing fluids, a series of batch reactor experiments were undertaken. Three rock samples with different mineralogical compositions and three fluid samples of different compositions (deionized water, deionized water + 2% potassium chloride (KCl), and deionized water + 0.5% choline chloride (C 5 H 14 ClNO) were used. Experiments were undertaken at reservoir temperature and atmospheric pressure. Elemental compositions of effluents after 1, 3, 7, 14, 28 days were analyzed using Inductively Couple Plasma Mass Spectrometry (ICP-MS). Medical Computed Tomography (CT) scan and X-ray Fluorescence (XRF) were conducted on the entire core run to help upscale results obtained from rock-fluid interaction experiments. Geochemical modeling using a reactive simulator, TOUGHREACT, was undertaken to corroborate experimental results. Results show that lower pH triggered high dissolution rates in the rock samples, especially the carbonate components. As pH increased, the rate of dissolution declined significantly, though for most cases dissolution still continued. Observed dissolved silica concentrations were much higher than the quartz solubility, suggesting that much of the silica originates from more soluble silica polymorphs and possibly desorption from clay mineral exchange sites. Concentration of most elemental species in solution increased but aluminium and magnesium concentrations declined rapidly following initial entry into solution. Geochemical modeling corroborated the conclusions regarding mineral dissolution and precipitation observed from experiments, notably; the dissolution of calcite and oxidation of pyrite in reacted shale samples, the likely presence of silica polymorphs such as opal, chalcedony or amorphous silica in these samples, and the reduction of Al and Mg concentrations in solution by precipitation of secondary aluminosilicate phases. The de-flocculation of clay minerals during reaction implies fines migration after hydraulic fracturing. This is detrimental to reservoir productivity as clay fines are displaces and lodged within the micro and nano-fractures created during fracturing. The immediate consumption of aluminium and magnesium also has implications on blockage of hydrocarbon pathways due to precipitation of new minerals in these locations.

04 OIL SHALES AND TAR SANDS↗

Ductile to brittle transition in dynamic fracture of brittle bulk metallic glass

We report an unusual transition from a locally ductile to a pure brittle fracture in the dynamic fracture of brittle Mg{sub 65}Cu{sub 20}Gd{sub 10} bulk metallic glass. The fractographic evolution from a dimple structure to a periodic corrugation pattern and then to the mirror zone along the crack propagation direction during the dynamic fracture process is discussed within the framework of the meniscus instability of the fracture process zone. This work might provide an important clue in understanding of the energy dissipation mechanism for dynamic crack propagation in brittle glassy materials.

36 MATERIALS SCIENCE↗

Time-resolved measurement of photon emission during fast crack propagation in three-point bending fracture of silica glass and soda lime glass

Simultaneous time-resolved measurements of photon emission (PE) and fast crack propagation upon bending fracture were conducted in silica glass and soda lime glass. Observation of fracture surfaces revealed that macroscopic crack propagation behavior was similar between the silica glass and soda lime glass when fracture loads for these specimens were comparable and cracks propagated without branching. However, a large difference in the PE characteristics was found between the two glasses. In silica glass, PE (645–655 nm) was observed during the entire crack propagation process, whereas intense PE (430–490 nm and 500–600 nm) was observed during the initial stages of propagation. In contrast, only weak PE was detected in soda lime glass. These results show that there is a large difference in the atomic processes involved in fast crack propagation between these glasses, and that PE can be used to study brittle fracture on the atomic scale.

36 MATERIALS SCIENCE↗