Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ELONGATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,189 records · Page 66

Effect of Final Cooling Temperature on Microstructure and Mechanical Properties of a Cr-Ni-Mo-V Bainite Steel

The microstructural evolution and mechanical properties of a low-carbon high-strength bainitic steel under different final cooling temperatures were studied. The microstructures of the experimental steel at different final cooling temperatures were composed of acicular ferrite and granular bainite. A decrease in final cooling temperature resulted in an increase in volume fraction of granular bainite and a decrease in volume fraction of acicular ferrite. The specimen with the lowest final cooling temperature (459 °C) exhibited the highest yield strength, tensile strength, and yield ratio, and a lower total elongation than the specimens with the highest final cooling temperatures (501 and 535 °C) because of the higher volume fraction of granular bainite and finer bainitic ferrite lath. The specimen with the lowest final cooling temperature had a lower absorbed energy than that of the highest final cooling temperature, because the strip-like martensite–austenite (M-A) constituents that existed between the bainitic ferrite or in prior austenite grain boundaries reduced its toughness. At an intermediate final cooling temperature of 501 °C, the experimental steel exhibited excellent mechanical properties with a yield strength, tensile strength, and absorbed energy of 825 MPa, 1232 MPa, and 102 J, respectively.

36 MATERIALS SCIENCE↗

Microstructure and Strain Rate-Dependent Tensile Deformation Behavior of Fiber Laser-Welded Butt Joints of Dual-Phase Steels

The microstructure and tensile deformation behavior of the fiber laser-welded similar and dissimilar dual-phase (DP) steel joints over a wide range of strain rates from 10{sup −3} to 10{sup 3} s{sup −1} were investigated for the further applications on the lightweight design of vehicles. The high strain rate dynamic tensile deformation process and full-field strain distribution of the base metals and welded joints were examined using the digital image correlation method and high-speed photography. The strain rate effects on the stress–strain responses, tensile properties, deformation, and fracture behavior of the investigated materials were analyzed. The yield stress (YS) and ultimate tensile strength (UTS) of the dissimilar DP780/DP980 welded joints were lying in-between those of the DP780 and DP980 base metals, and all materials exhibited positive strain rate dependence on the YS and UTS. Owing to the microstructure heterogeneity, the welded joints showed relatively lower ductility in terms of total elongation (TE) than those of the corresponding base metals. The strain localization started before the maximum load was reached, and the strain localization occurred earlier during the whole deformation process with increasing strain rate. As for the dissimilar welded joint, the strain localization tended to occur in the vicinity of the lowest hardness value across the welded joint, which was in the subcritical HAZ at the DP780 side. As the strain rate increased, the typical ductile failure characteristic of the investigated materials did not change.

36 MATERIALS SCIENCE↗

Mechanical Behavior of Commercially Pure Titanium Weldments at Lower Temperatures

Commercially pure titanium is used for low-temperature applications due to good toughness attributed to single-phase microstructure (α). Electron beam welding (EBW) and gas tungsten arc welding (GTAW) processes have been used for welding two grades of commercially pure titanium (Grade 2 and Grade 4). Martensitic microstructure is found to be finer in the case of EBW joint as compared to GTAW joint due to faster rate of cooling in the former process. Weldments have been characterized to study the mechanical behavior at ambient (298 K) and cryogenic temperatures (20 and 77 K). Strength of weldments increases with the decrease in temperature, which is found to be more prominent in case of Grade 4 titanium as compared to Grade 2. Weld efficiency of Grade 4 is found to be higher at all the temperatures (ambient, 77 and 20 K). However, ultimate tensile strength/yield strength ratio is higher for Grade 2 as compared to Grade 4. % Elongation is found to increase/retained at cryogenic temperatures for Grade 2, and it is found to decrease for Grade 4. Electron backscattered diffraction analysis and transmission electron microscopy of deformed samples confirmed the presence of extensive twinning in Grade 2 and the presence of finer martensitic structure in Grade 4. Fractography analysis of tested specimens revealed the presence of cleavage facets in Grade 4 and dimples in specimens of Grade 2. Higher strength in Grade 4 is attributed to higher oxygen restricting the twin-assisted slip, which is otherwise prominent in Grade 2 titanium.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Dissimilar Joints of Al-Mg{sub 2}Si and 5052 Aluminum Alloy by Friction Stir Welding

Al-Mg{sub 2}Si alloy and 5052 Al alloy were welded successfully by friction stir welding (FSW) in this study. The results show that the alloy consists of three distinct zones after FSW: the base material zone (BMZ), the transitional zone, and the weld nugget (WN). The morphologies of the primary Mg{sub 2}Si phases are identified as coarse equiaxed crystals for Al-Mg{sub 2}Si alloys in the BMZ. The WN is a mixture of rich Al-Mg{sub 2}Si and rich 5052 alloy, and a banded structure is formed in the zone. Interestingly, in the WN, the equiaxed crystals changed to polygonal particles with substantially reduced sizes in the rich Al-Mg{sub 2}Si zone. However, in addition to the white rich Mg phase appearing in the rich 5052 zone near the interface, the 5052 alloy does not show obvious changes. The hardness gradually increases from the BMZ of the 5052 to the welded joint to the Al-Mg{sub 2}Si BMZ. In addition, the ultimate tensile strength (UTS) of the welded joint is higher than that of the base material of the Al-Mg{sub 2}Si, whereas it is lower than that of the 5052 base alloy. The results of the elongation are similar to the UTS results. The fracture mechanism is also investigated.

36 MATERIALS SCIENCE↗

Effect of Heat Treatment on the Properties of CoCrMo Alloy Manufactured by Selective Laser Melting

To obtain medical implants with better mechanical properties, it is necessary to conduct studies on the heat treatment process of the selective laser melting (SLM) manufacturing parts. The differential scanning calorimetry method was used to study the heat treatment process of the phase transition of SLM CoCrMo alloy parts. The tensile properties were tested with a tensile test machine, the quantity of carbide precipitated after heat treatment was measured by energy-dispersive x-ray spectroscopy, and the tensile fracture morphology of the parts was investigated using SEM. The obtained results were: Mechanical properties in terms of elongation and tensile strength of CoCrMo alloy manufactured by SLM that had been heat-treated at 1200 °C for 2 h followed by cooling with water were not only higher than the national standard but also higher than the experimental results of the same batch of castings. The mechanism of fracture of parts manufactured by SLM without heat treatment was brittle fracture, whereas parts which had been heat-treated at 1200 °C for 2 h combined with water cooling and at 1200 °C for 1 h with furnace cooling suffered ductile fracture. This study provides the basis for defining the applications for which CoCrMo alloys manufactured by SLM are suitable within the field of medical implants.

36 MATERIALS SCIENCE↗

Effect of Al on Grain Refinement and Mechanical Properties of Mg-3Nd Casting Alloy

The effect of Al on the grain refinement and mechanical properties of as-cast Mg-3Nd alloy was investigated systematically by a series of microstructural analysis, solidification analysis and tensile tests. The results show that Al has an obvious refining effect on the as-cast Mg-3Nd alloy. With increasing Al content, the grain size of the as-cast Mg-3Nd alloy decreases firstly, then increases slightly after the Al content reaching 3 wt.%, and the minimum grain size of the Mg-3Nd alloy is 48 ± 4.0 μm. The refining mechanism can be attributed to the formation of Al{sub 2}Nd particles, which play an important role in the heterogeneous nucleation. The strength and elongation of the Mg-3Nd alloy refined by Al also increase with increasing Al content and slightly decrease when the Al content is more than 3 wt.%, and the strengthening mechanism is attributed to the grain refinement as well as dispersed intermetallic particles. Furthermore, the microstructural thermal stability of the Mg-3Nd-3Al alloy is higher than that of the Mg-3Nd-0.5Zr alloy. Overall, the Mg-3Nd alloy with Al addition is a novel alloy with wide and potential application prospects.

36 MATERIALS SCIENCE↗

Effects of Controlled Cooling-Induced Ferrite–Pearlite Microstructure on the Cold Forgeability of XC45 Steel

The combination of hot/warm and cold forging with an intermediate controlled cooling process is a promising approach to saving costs in the manufacture of automobile parts. In this work, the effects of the ferrite–pearlite microstructure, which formed after controlled cooling, on the cold forgeability of a medium-carbon steel were investigated. Different specimens for both normal and notched tensile tests were directly heated to high temperature and then cooled down at different cooling rates, producing different ferrite volume fractions, ranging from 6.69 to 40.53%, in the ferrite–pearlite microstructure. The yield strength, ultimate tensile strength, elongation rate, percentage reduction of area, and fracture strain were measured by tensile testing. The yield strength, indicating deformation resistance, and fracture strain, indicating formability, were used to evaluate the cold forgeability. As the ferrite volume fraction increased, the cold forgeability of the dual-phase ferritic–pearlitic steel improved. A quantitatively relationship between the ferrite volume fraction and the evaluation indexes of cold forgeability for XC45 steel was obtained from the test data. To validate the mathematical relationship, different tensile specimens machined from real hot-forged workpieces were tested. There was good agreement between the predicted and measured values. Our predictions from the relationship for cold forgeability had an absolute error less than 5%, which is acceptable for industrial applications and will help to guide the design of combined forging processes.

36 MATERIALS SCIENCE↗

Interfacial Microstructure and Mechanical Properties of Friction Stir Welded Joints of Commercially Pure Aluminum and 304 Stainless Steel

In the present investigation, friction stir welding of commercially pure aluminum and 304 stainless steel was carried out at varying tool rotational speeds from 200 to 1000 rpm in steps of 200 rpm using 60 mm/min traverse speed at 2 (degree) tool tilt angle. Microstructural characterization of the interfacial zone was carried out using optical microscope and scanning electron microscope. Energy-dispersive spectroscopy indicated the presence of FeAl{sub 3} intermetallic phase. Thickness of the intermetallic layer increased with the increase in tool rotational speed. X-ray diffraction studies indicated the formation of intermetallic phases like FeAl{sub 2}, Fe{sub 4}Al{sub 13}, Fe{sub 2}Al{sub 5}, and FeAl{sub 3}. A maximum tensile strength of ~ 90% that of aluminum along with ~ 4.5% elongation was achieved with the welded sample at tool rotational speed of 400 rpm. The stir zone showed higher hardness as compared to base metals, heat affected zone, and thermo-mechanically affected zone due to the presence of intermetallics. The maximum hardness value at the stir zone was achieved at 1000 rpm tool rotational speed.

36 MATERIALS SCIENCE↗

Effect of Cold Rolling and Heat Treatment on Microstructure and Mechanical Properties of Ti-4Al-1Mn Titanium Alloy

Mechanical behavior of Ti-4Al-1Mn titanium alloy has been studied in annealed, cold-rolled and heat-treated conditions. Room temperature tensile strength as well as % elongation has been found to be low with increasing amount of cold rolling. Lowering of strength in cold worked condition is attributed to premature failure. However, the same has been mitigated after heat treatment. Significant effect of cooling media (air and water) from heat treatment temperature on microstructure was not found except for the degree of fineness of α plates. Optimum properties (strength as well as ductility) were exhibited by samples subjected to 15% cold rolling and heat treatment below β transus temperature, which can be attributed to presence of recrystallized microstructure. In cold worked condition, the microstructure shows fine fragmented α plates/Widmanstätten morphology with high dislocation density along with a large amount of strain fields and twinning, which gets transformed to recrystallized equiaxed microstructure and with plate-like morphology after near β heat treatment. Prior cold work is found to have a significant effect on mechanical properties supported by evolution of microstructure. Twinning is found to be assisting in deformation as well as in recrystallization through the formation of deformation and annealing twins during cold working and heat treatment. Fracture analysis of the tested sample with prior cold work and heat-treated condition revealed quasi-ductile failure as compared to only ductile failure features seen for samples heat treated without prior cold work.

36 MATERIALS SCIENCE↗

Integrating GLL-Weibull Distribution Within a Bayesian Framework for Life Prediction of Shape Memory Alloy Spring Undergoing Thermo-mechanical Fatigue

The present paper tackles an important but unmapped problem of the reliability estimations of smart materials. First, an experimental setup is developed for accelerated life testing of the shape memory alloy (SMA) springs. Generalized log-linear Weibull (GLL-Weibull) distribution-based novel approach is then developed for SMA spring life estimation. Applied stimulus (voltage), elongation and cycles of operation are used as inputs for the life prediction model. The values of the parameter coefficients of the model provide better interpretability compared to artificial intelligence based life prediction approaches. In addition, the model also considers the effect of operating conditions, making it generic for a range of the operating conditions. Moreover, a Bayesian framework is used to continuously update the prediction with the actual degradation value of the springs, thereby reducing the uncertainty in the data and improving the prediction accuracy. In addition, the deterioration of material with number of cycles is also investigated using thermogravimetric analysis and scanning electron microscopy.

36 MATERIALS SCIENCE↗

Mechanical Properties and Microstructural Evolution of Yb-Modified Al-20%Si Alloy

In the study, the mechanical properties and microstructural evolution of hypereutectic Al-20%Si-xYb alloys (x = 0, 0.1, 0.3, 0.5 and 0.7 wt.%) were studied. The as-prepared samples were characterized by scanning electron microscopy, optical microscope, x-ray diffraction (XRD) and electron probe microanalysis. The characterization results showed with the addition amount of Yb increasing to 0.5%, the eutectic Si structure was gradually modified from coarse needle-like/platelet-like structure into fine coral-like fibrous structure and the primary Si phases were gradually converted from coarse platelet-like/star-like/polygonal shape into fine blocky shape. In particular, according to the results of WDS and XRD analyses, the Yb-rich intermetallic phase in the Al-20%Si alloy is Al{sub 3}Yb. Tensile test was carried out to study the mechanical properties of Al-20%Si-x%Yb alloys, and results showed that the elongation and ultimate tensile strength increased by 73.6% and 64.5%, respectively.

36 MATERIALS SCIENCE↗

Influence of Boron on Austenite to Ferrite Transformation Behavior of Low Carbon Steel Under Continuous Cooling

In the current work, the influence of boron on austenite to ferrite transformation behavior under continuous cooling condition and its associated features, e.g., final microstructure, mechanical properties, etc., in low carbon steel has been studied. The steels (C 0.04 wt.%, B 10-100 ppm) prepared in an open air laboratory furnace showed identical microstructures having ferrite grains of 20-25 µm. However, tensile test data indicate variation of yield strength and ultimate tensile strength with boron content. The yield point elongation and strain aging index both were found to decrease with increase in boron content or boron-to-nitrogen ratio. As the boron nitride precipitates stimulate the nucleation of ferrite phase, the dilation curves show an increase in austenite to ferrite transformation start temperature with boron content. The resulting microstructure and hardness value also corroborate the finding. Transmission electron microscopy findings revealed the presence of ultra-fine boron nitride (BN) precipitates in both grain boundary and grain body of the steel having boron concentration of 30 ppm and beyond. The presence of these precipitates also increased with boron content. Based on austenite decomposition behavior, related microstructure and hardness values it is conjectured that these BN precipitates may act as nucleating agent for polygonal ferrite during austenite decomposition, thereby softening the steel during fast cooling.

36 MATERIALS SCIENCE↗

Experimental Investigation of Mechanical Performance and Printability of Gamma-Irradiated Additively Manufactured ABS

The work presented in this paper investigates the effects of gamma radiation on ABS in forms of irradiated 3D-printed parts, and irradiated filament used to later 3D-printed parts, using a cobalt-60 gamma irradiator. Tensile and flexural test samples were fabricated using off-the-shelf FDM 3D printers and irradiated at different dosages. Mechanical properties including elastic and flexure moduli, ultimate and flexural strength, % elongation at break, and surface hardness were evaluated, and results were compared to a control group. Evidence of cross-linking and chain scission and signs of possible oxidation of polymer caused by irradiation were found in both test groups which led to changes in mechanical properties. Moreover, it was found that ABS filament retains its printability after absorbing 15 kGy of gamma radiation and that its mechanical performance is very similar to those of irradiated samples at the same dose. Obtained results show promise for using ABS to fabricate sterile surgical instruments.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Processing Parameter Effects on Residual Stress and Mechanical Properties of Selective Laser Melted Ti6Al4V

Selective laser melting (SLM) process is characterized by large temperature gradients resulting in high levels of residual stress within the additively manufactured metallic structure. SLM-processed Ti6Al4V yields a martensitic microstructure due to the rapid solidification and results in a ductility generally lower than a hot working equivalent. Post-process heat treatments can be applied to SLM components to remove in-built residual stress and improve ductility. Residual stress buildup and the mechanical properties of SLM parts can be controlled by varying the SLM process parameters. This investigation studies the effect of layer thickness on residual stress and mechanical properties of SLM Ti6Al4V parts. This is the first-of-its kind study on the effect of varying power and exposure in conjunction with keeping the energy density constant on residual stress and mechanical properties of SLM Ti6Al4V components. It was found that decreasing power and increasing exposure for the same energy density lowered the residual stress and improved the % elongation of SLM Ti6Al4V parts. Increasing layer thickness resulted in lowering the residual stress at the detriment of mechanical properties. The study is based on detailed experimental analysis along with finite element simulation of the process using ABAQUS to understand the underlying physics of the process.

36 MATERIALS SCIENCE↗

Effects of Rolling Temperature on the Microstructure and Properties of 2Cr13/316L/9Cr18MoV Stainless Steel Composite Plate Fabricated by Hot-Rolling Bonding Process

A 15-layer composite plate was developed. The microstructure and mechanical properties were characterized by scanning electron microscopy, Vickers microhardness, tensile, and bending tests. Particularly, the effects of hot-rolling at different rolling temperatures of 1130, 1180, 1250, and 1300 °C on the microstructure and mechanical properties of the 2Cr13/316L/9Cr18MoV composite plates were investigated in detail. The results indicated that, with the increase in the rolling temperature, the tensile strength was first decreased and then slightly increased by the coarsening of grains and the increase in the ferrite content in the 2Cr13 layers. The highest tensile elongation of 12.5% and tensile strength of 958.1 MPa were obtained for the composite plate manufactured with the rolling temperature of 1180 °C. The 2Cr13/316L/9Cr18MoV composite plates with rolling temperatures of 1130 and 1180 °C obtained by hot-rolling processes withstood larger bending deformations, showing only local cracks after the bending process because of their strong combined interfaces. However, during the bending to 130° of specimens fabricated with the rolling temperature of 1250 and 1300 °C, the specimens experienced direct fracture at very low bending displacements.

36 MATERIALS SCIENCE↗

Research on Resistance Heating Behavior of High-Strength Steel and its Hot-Stamping Forming

A hot-stamping process of high-strength steel sheet using resistance heating (RH) was developed to improve springback and formability. The RH curves of S355J2W steel and the microstructure and mechanical properties after RH were explored to control and guide the RH time and the selected current density for the subsequent RH hot-stamping forming. Moreover, scanning electron microscopy observations revealed the microstructure evolution in RH and the improvement of mechanical properties at a current density of 0-6.67 A mm{sup −2}, showing the advantage of the application of RH to these materials. The results showed that steel strength can be increased by up to 3.2% and the elongation can be improved by up to 33% after RH. In addition, the forming height increased and the forming angle is closer to the desired angle with the increased current density in cap-shaped RH hot-stamping forming experiment, which means that the forming accuracy is improved. A comparison of the forming accuracy of cap-shaped parts formed by RH under different current densities with those heated to the same temperature by furnace heating (FH) shows that there is no obvious difference between them. The heating time of RH is much shorter than that of the FH, and the surface quality of the parts formed by RH hot-stamping is better than that of the parts formed by FH hot-stamping. These results demonstrate that the RH method has the advantages of efficiency, safety, energy saving and the improvement of surface quality as well as a clear understanding of the benefits of RH hot-stamping forming for materials properties and forming accuracy; this work also develops and applies fundamental theory to practical engineering of bogie cover plate manufacturing.

36 MATERIALS SCIENCE↗

Optimization of Hot Deformation Parameters and Constitutive Analysis for As-Cast Mg-5Li-3Zn-0.3Y Alloy Using Processing Maps

Hot deformation behavior of as-cast Mg-5Li-3Zn-0.3Y (wt.%) alloy has been studied by establishing processing maps covering the range of 200-450 °C in temperature and 0.001-10 s{sup −1} in strain rate. The map corresponding to the strain of 0.7 reveals that a domain of dynamic recrystallization occurred at 340-400 °C/0.01-0.158 s{sup −1} with its peak efficiency of approximately 31%. Analysis of the flow behaviors and microstructural observations indicated that dynamic recrystallization occurred in the domain, in which fine microstructure can be achieved. The above conditions represent the optimum processing parameters, and the flow instability regimes are also recognized from the maps. The average deformation in the deformed range was 136.414 kJ/mol which is close to that for lattice self-diffusion in magnesium and far smaller than that for as-cast Mg-5.75Zn-0.73Y-0.36Zr (wt.%) alloy. It is believed that a lower activation energy for Mg-5Li-3Zn-0.3Y alloy can partly result from both the weak particle pinning effects and adding Li into the Mg-Zn-Y-Zr alloy. Results of extrusion experiments conducted at 350 °C show that the alloy can be easily extruded with good mechanical properties of the yield strength of 132 MPa, the fracture strength of 215 MPa and the elongation of 20.9%, and the grains can be well refined.

36 MATERIALS SCIENCE↗

Effect of Tool Temperature on Microstructure and Properties of Tailored Hot Stamping Components

Traditional boron steel hot stamping technology can achieve components with full martensite and tensile strength of 1500 MPa. However, fully martensitic hot stamped components exhibit very low level of ductility and are rarely used in energy absorbing structures. Hot stamping with segmented heating and cooling tool can obtain multiphase quenched structures and the tailored mechanical properties. Hot stamping experiment of U-shape component was performed with segmented heating and cooling tool. Mechanical properties of the formed component were measured, and scanning electron microscope and color tint etching were used to quantify the quenched phases achieved under different tool temperatures. The results showed that hardness value decreased from 470 to 230 HV and tensile strength reduced about 50% from 1406 to 730 MPa and elongation increased from 4.19 to 10.20% as tool temperatures increased from 25 to 500 °C. Meanwhile, martensite decreased from 85 to 30% and bainite increased from 12 to 55%, and there was also a small increase in ferrite. In order to get the influence of quenched phases on the strength and hardness of tailored hot stamped component, linear fitting optimization was used to establish mathematical models for area fraction of quenched phases and strength and hardness.

36 MATERIALS SCIENCE↗