Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Direct Conversion”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,189 records · Page 66

Prediction of the Effective Coefficient of Thermal Expansion of Heterogeneous Media using Two-point Correlation Functions

Statistical continuum mechanics is used to predict the coefficient of thermal expansion (CTE) for solid oxide fuel cell glass-ceramic seal materials with different morphology and crystallinity. Two-point correlation functions are utilized to represent the microstructure morphology and phase distribution. The model uses two-point correlation function representing microstructure, along with local properties, to predict the effective CTE. Prediction results agree well with experimental results. The advantage of the statistical continuum mechanics model in predicting the effective properties of anisotropic media is to take into consideration of microstructure.

30 DIRECT ENERGY CONVERSION↗

Factors Affecting Limiting Current in Solid Oxide Fuel Cells or Debunking the Myth of Anode Diffusion Polarization

Limiting current densities for solid oxide fuel cells were measured using both button cells and a flow-through cell. The cell anodes were supplied mixtures of humidified hydrogen and various inert gasses. It was demonstrated that the true limiting current in flow-through cells is reached when either: the hydrogen is nearly or completely depleted at the anode-electrolyte interface near the outlet; or when the concentration of steam at that interface becomes high enough to interfere with adsorption or transport of the remaining hydrogen near the triple-phase boundaries. Choice of inert gas had no effect on limiting currents in the flow-through tests, indicating that diffusion within the porous anode had no significant effect on cell performance at high currents. In the button cells, the apparent limiting currents were significantly changed by the choice of inert gas, indicating that they were determined by diffusion through the bulk gas within the support tube. It was concluded that the apparent limiting currents measured in button cells are influenced more by parameters of the experimental setup, such as the proximity of the fuel tube outlet, than by the physical properties of the anode.

08 HYDROGEN↗

Performance and cost of automotive fuel cell systems with ultra-low platinum loadings.

An automotive polymer-electrolyte fuel cell (PEFC) system with ultra-low platinum loading (0.15 mg-Pt cm{sup -2}) has been analyzed to determine the relationship between its design-point efficiency and the system efficiency at part loads, efficiency over drive cycles, stack and system costs, and heat rejection. The membrane electrode assemblies in the reference PEFC stack use nanostructured, thin-film ternary catalysts supported on organic whiskers and a modified perfluorosulfonic acid membrane. The analyses show that the stack Pt content can be reduced by 50% and the projected high-volume manufacturing cost by >45% for the stack and by 25% for the system, if the design-point system efficiency is lowered from 50% to 40%. The resulting penalties in performance are a <1% reduction in the system peak efficiency; a 2-4% decrease in the system efficiency on the urban, highway, and LA92 drive cycles; and a 6.3% decrease in the fuel economy of the modeled hybrid fuel-cell vehicle on the combined cycle used by EPA for emission and fuel economy certification. The stack heat load, however, increases by 50% at full power (80 kW{sub e}) but by only 23% at the continuous power (61.5 kW{sub e}) needed to propel the vehicle on a 6.5% grade at 55 mph. The reduced platinum and system cost advantages of further lowering the design-point efficiency from 40% to 35% are marginal. The analyses indicate that thermal management in the lower efficiency systems is very challenging and that the radiator becomes bulky if the stack temperature cannot be allowed to increase to 90-95 C under driving conditions where heat rejection is difficult.

30 DIRECT ENERGY CONVERSION↗

Electrochemical, Structural and Surface Characterization of Nickel/Zirconia Solid Oxide Fuel Cell Anodes in Coal Gas Containing Antimony

The interaction of antimony with the nickel-zirconia solid oxide fuel cell (SOFC) anode has been investigated. Tests with both anode-supported and electrolyte-supported button cells were performed at 700 and 800oC in synthetic coal gas containing 10 ppb to 9 ppm antimony. Minor performance loss was observed immediately after Sb introduction to coal gas resulting in ca. 5 % power output drop. While no further degradation was observed during the following several hundred hours of testing, cells abruptly and irreversibly failed after 800-1500 hours depending on Sb concentration and test temperature. Antimony was found to interact strongly with nickel and result in extensive alteration phase formation, consistent with expectations based on thermodynamic properties. Nickel antimonide phases, NiSb and Ni5Sb2, were partially coalesced into large grains and eventually affected electronic percolation through the anode support. Initial degradation was attributed to diffusion of antimony to the active anode/electrolyte interface to form an adsorption layer.

01 COAL, LIGNITE, AND PEAT↗

Mechanical properties of solid oxide fuel cell glass-ceramic seal at high temperatures

Mechanical properties of solid oxide fuel cell glass-ceramic seal material, G18, are studied at high temperatures. Samples of G18 are aged for either 4h or 100h, resulting in samples with different crystallinity. Reduced modulus, hardness, and time-dependent behavior are measured by nanoindentation. The nanoindentation is performed at room temperature, 550, 650, and 750°C, using loading rates of 5 mN/s and 25 mN/s. Results show a decrease in reduced modulus with increasing temperature, with significant decrease above the glass transition temperature (Tg). Hardness generally decreases with increasing temperature, with a slight increase before Tg for the 4h aged sample. Dwell tests show that creep increases with increasing temperature, but decrease with further aging.

30 DIRECT ENERGY CONVERSION↗

Effects of Tungsten Oxide Addition on the Electrochemical Performance of Nanoscale Tantalum Oxide-Based Electrocatalysts for Proton Exchange Membrane PEM Fuel Cells

In the present study, the properties of a series of non-platinum based nanoscale tantalum oxide/tungsten oxide-carbon composite catalysts was investigated for potential use in catalyzing the oxygen reduction reaction (ORR) on the cathode side of a PEM fuel cell membrane electrode assembly. Electrochemical performance was measured using a half-cell test set up with a rotating disc electrode and compared with a commercial platinum-on-carbon (Pt/C) catalyst. Overall, all of the oxide-based composite catalysts exhibit high ORR on-set potentials, comparable to that of the baseline Pt/C catalyst. The addition of tungsten oxide as a dopant to tantalum oxide greatly improved mass specific current density. Maximum performance was achieved with a catalyst containing 32 mol% of tungsten oxide, which exhibited a mass specific current density ~8% that of the Pt/C catalyst at 0.6 V vs. the normal hydrogen electrode (NHE) and ~35% that of the Pt/C catalyst at 0.2 V vs. NHE. Results from X-ray photoelectron spectroscopy analysis indicated that the tungsten cations in the composite catalysts exist in the +6 oxidation state, while the tantalum displays an average valence of +5, suggesting that the addition of tungsten likely creates an oxygen excess in the tantalum oxide structure that influences its oxygen absorption kinetics. When the 32mol% tungsten doped catalyst loading on the working electrode was increased to five times that of the original loading (which was equivalent to that of the baseline Pt/C catalyst), the area specific current density improved four fold, achieving an area specific current density ~35% that of the Pt/C catalyst at 0.6 V vs. NHE.

08 HYDROGEN↗

Phase Stability and Electrical Conductivity of Ca-doped LaNb1-xTaxO4- high temperature proton conductors

The electrical conductivity, phase structure and stability of La0.99Ca0.01Nb1-xTaxO4- (x=0, 0.1, 0.2, 0.3, 0.4 and 0.5, =0.005) a potential candidate for proton conductor for Solid Oxide Fuel Cells (SOFCs) have been investigated using AC impedance technique and in-situ X-ray powder diffraction. Partially substituting Nb with Ta elevates the phase transition temperature (from monoclinic to a tetragonal structure at high temperature) from ~520 C for x=0 to near 800 C for x=0.4. AC conductivity of the La0.99Ca0.01Nb1-xTaxO4- both in dry and wet air decreased slightly with increase of Ta content above 750 C, while below 500 C, it decreased one order of magnitude. It was also found that the activation energy for the total conductivity increases with increasing Ta content from 0.50 eV (x=0) to 0.58 eV (x=0.3) for the tetragonal phase, however, it decreases with increasing Ta content from 1.18 eV (x=0) to 1.08 eV (x=0.4) for the monoclinic phase. By removing the detrimental high temperature phase transition out of intermediate temperature range, partial substitution of Nb with Ta brings this class of material closer to its application in intermediate-temperature SOFCs.

30 DIRECT ENERGY CONVERSION↗

Tungsten Carbide Modified High Surface Area Carbon as Fuel Cell Catalyst Support

Phase pure WC nanoparticles were synthesized on high surface area carbon black (800 m{sup 2} g{sup -1}) by a temperature programmed reaction (TPR) method. The particle size of WC can be controlled under 30 nm with a relatively high coverage on the carbon surface. The electrochemical testing results demonstrated that the corrosion resistance of carbon black was improved by 2-fold with a surface modification by phase pure WC particles. However, the WC itself showed some dissolution under potential cycling. Based on the X-ray diffraction (XRD) and inductively coupled plasma (ICP) analysis, most of the WC on the surface was lost or transformed to oxides after 5000 potential cycles in the potential range of 0.65-1.2 V. The Pt catalyst supported on WC/C showed a slightly better ORR activity than that of Pt/C, with the Pt activity loss rate for Pt/WC/C being slightly slower compared to that of Pt/C. The performance and decay rate of Pt/WC/C were also evaluated in a fuel cell.

30 DIRECT ENERGY CONVERSION↗

High Performance Ceramic Interconnect Material for Solid Oxide Fuel Cells (SOFCs): Ca- and Transition Metal-doped Yttrium Chromite

The effect of transition metal substitution on thermal and electrical properties of Ca-doped yttrium chromite was investigated in relation to use as a ceramic interconnect in high temperature solid oxide fuel cells (SOFCs). 10 at% Co, 4 at% Ni, and 1 at% Cu substitution on B-site of 20 at% Ca-doped yttrium chromite led to a close match of thermal expansion coefficient (TEC) with that of 8 mol% yttria-stabilized zirconia (YSZ), and a single phase Y0.8Ca0.2Cr0.85Co0.1Ni0.04Cu0.01O3 remained stable between 25 and 1100 degree C over a wide oxygen partial pressure range. Doping with Cu significantly facilitated densification of yttrium chromite. Ni dopant improved both electrical conductivity and dimensional stability in reducing environments, likely through diminishing the oxygen vacancy formation. Substitution with Co substantially enhanced electrical conductivity in oxidizing atmosphere, which was attributed to an increase in charge carrier density and hopping mobility. Electrical conductivity of Y0.8Ca0.2Cr0.85Co0.1Ni0.04Cu0.01O3 at 900 degree C is 57 S/cm in air and 11 S/cm in fuel (pO2=5×10^-17 atm) environments. Chemical compatibility of doped yttrium chromite with other cell components was verified at the processing temperatures. Based on the chemical and dimensional stability, sinterability, and thermal and electrical properties, Y0.8Ca0.2Cr0.85Co0.1Ni0.04Cu0.01O3 is suggested as a promising SOFC ceramic interconnect to potentially overcome technical limitations of conventional acceptor-doped lanthanum chromites.

30 DIRECT ENERGY CONVERSION↗

Extended reaction zone of La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3 cathode for solid oxide fuel cell

The oxygen reduction reaction at the cathode of solid oxide fuel cell (SOFC) is a complicated process which involves the interaction of oxygen molecules, electrons, and oxygen ions. Therefore, it can only proceed at locations where gas, electronic conductor, and an oxygen ion conductor meet. Although the extension of the reaction zone beyond the traditional so-called triple-phase-boundary (TPB) is widely accepted for a mixed ionically and electronically conductive cathode, work in this area has yet to reach a consensus on how far the reaction zone can be extended. In this study, anode-supported fuel cells with a variety of LSCF cathode thicknesses were fabricated and tested in two cathode environments, flowing oxygen and flowing air. In flowing oxygen, the cell performance increased with LSCF cathode thickness over the entire range investigated (from 5 to 33 μm). In flowing air, the cell performance also increased with the LSCF cathode thickness from 5 to 13 μm, but then remained almost constant with further increase in cathode thickness. In flowing oxygen, since there was no concentration polarization related to oxygen diffusion, the polarization resistance of oxygen reduction decreased with the LSCF cathode thickness because of the increased number of reaction sites. A linear relationship was established between the reciprocal of the polarization resistance and the cathode thickness, which was explained by a model developed for aqueous gas diffusion electrodes.

30 DIRECT ENERGY CONVERSION↗

Compliant alkali silicate sealing glass for solid oxide fuel cell applications: Combined stability in isothermal ageing and thermal cycling with YSZ coated ferritic stainless steels

An alkali-containing silicate glass (SCN-1) is currently being evaluated as a candidate sealing glass for solid oxide fuel cell (SOFC) applications. The glass contains about 17 mole% alkalis (K+Na) and has low glass transition and softening temperatures. It remains vitreous and compliant around 750-800oC after sealing without substantial crystallization, as contrary to conventional glass-ceramic sealants, which experience rapid crystallization after the sealing process. The glassy nature and low characteristic temperatures can reduce residual stresses and result in the potential for crack healing. In a previous study, the glass was found to have good thermal cycle stability and was chemically compatible with YSZ coating during short term testing. In the current study, the compliant glass was further evaluated in a more realistic way in that the sealed glass couples were first isothermally aged for 1000h followed by thermal cycling. High temperature leakage was measured. The chemical compatibility was also investigated with powder mixtures at 700 and 800oC to enhance potential interfacial reaction. In addition, interfacial microstructure was examined with scanning electron microscopy and evaluated with regard to the leakage and chemical compatibility results.

30 DIRECT ENERGY CONVERSION↗

Effects of Operating Conditions on Internal Resistances in Enzyme Fuel Cells Studied via Electrochemical Impedance Spectroscopy

Enzyme fuel cells (EFCs) offer some advantages over traditional precious-metal-catalyzed fuel cells, such as polymer electrolyte membrane fuel cells (PEMFCs). However, EFCs exhibit far less power output than PEMFCs and have relatively short life spans before materials must be replaced. In this work, electrochemical impedance spectroscopy (EIS) is used to analyze the internal resistances throughout the EFC at a variety of operating conditions. EIS analysis is focused primarily on the resistances of the anode, solution/membrane, and cathode. Increased enzyme loading results in improved power output and reductions in internal resistance. Conditions are identified for which enzyme loading does not limit the EFC performance. EIS experiments are also reported for EFCs operated continuously for 2 days; power output declines sharply over time, while all internal resistances increase. Drying of the cathode and enzyme/mediator degradation are believed to have contributed to this behavior. Finally, experiments are performed at varying air-humidification temperatures. Little effect on internal resistances or power output is observed. However, it is anticipated that increased air humidification can improve longevity by delivering more water to the cathode. Improvements to the enzymatic cathode are needed for EFC development. These improvements need to focus on improving transport rather than increasing enzyme loading.

30 DIRECT ENERGY CONVERSION↗

Performance of Ni-Fe/gadolinium-doped CeO{sub2} anode supported tubular solid oxide fuel cells using steam reforming of methane

Iron nanoparticles (Fe{sub 2}O{sub 3}) were added to NiO/gadolinium-doped CeO{sub 2} (GDC) anode supported solid oxide fuel cell (SOFC) for the direct methane-water fuel operation. The cell was co-sintered at 1400 C, and the anode porosity is 31.8%. The main size corresponding to peak volume is around 1.5 {mu}m. When steam and methane directly fed to the cell, the power density is about 0.57 W cm{sup -2} at 650 C. It is the familiar performance for H{sub 2} operation (4 times of flow rate) with same fuel utilization. Compare with the testing temperature of 600 and 650 C, there is almost no carbon fiber deposition at 700 C with steam/methane (S/C) of 5. At the same time, fuel operation of high value of S/C (=3.3) resulted in fiber-like deposition and degradation of power performance based on loading test results.

03 NATURAL GAS↗

Demonstration of a Highly Efficient Solid Oxide Fuel Cell Power System Using Adiabatic Steam Reforming and Anode Gas Recirculation

Solid oxide fuel cells (SOFC) are currently being developed for a wide variety of applications because of their high efficiency at multiple power levels. Applications for SOFCs encompass a large range of power levels including 1-2 kW residential combined heat and power applications, 100-250 kW sized systems for distributed generation and grid extension, and MW-scale power plants utilizing coal. This paper reports on the development of a highly efficient, small-scale SOFC power system operating on methane. The system uses adiabatic steam reforming of methane and anode gas recirculation to achieve high net electrical efficiency. The anode exit gas is recirculated and all of the heat and water required for the endothermic reforming reaction are provided by the anode gas emerging from the SOFC stack. Although the single-pass fuel utilization is only about 55%, because of the anode gas recirculation the overall fuel utilization is up to 93%. The demonstrated system achieved gross power output of 1650 to 2150 watts with a maximum net LHV efficiency of 56.7% at 1720 watts. Overall system efficiency could be further improved to over 60% with use of properly sized blowers.

01 COAL, LIGNITE, AND PEAT↗

A Damage Model for Degradation in the Electrodes of solid oxide fuel cells: Modeling the effects of sulfur and antimony in the anode

Over their designed lifetime, high temperature electrochemical devices, such as solid oxide fuel cells (SOFCs), can experience degradation in their electrochemical performance due to environmental conditions, operating conditions, contaminants, and other factors. Understanding the different degradation mechanisms in SOFCs and other electrochemical devices is essential to reducing performance degradation and increasing the lifetime of these devices. In this paper SOFC degradation mechanisms are discussed and a damage model is presented which describes performance degradation in SOFCs due to damage or degradation in the electrodes of the SOFC. A degradation classification scheme is presented that divides the various SOFC electrode degradation mechanisms into categories based on their physical effects on the SOFC. The application of the damage model and the classification method is applied to sulfur poisoning and antimony poisoning which occur in the anode of SOFCs. For sulfur poisoning the model is able to predict the degradation in SOFC performance based on the operating temperature and voltage of the fuel cell and the concentration of gaseous sulfur species in the anode. For antimony poisoning the effects of nickel removal from the anode matrix is investigated.

30 DIRECT ENERGY CONVERSION↗

Performance of Anode-Supported Solid Oxide Fuel Cell with Thin Bi-Layer Electrolyte by Pulsed Laser Deposition

Anode-supported yttria stabilized zirconia (YSZ)/samaria doped ceria (SDC) bi-layer electrolytes with uniform thickness and high density were fabricated by pulsed laser deposition at 1000 degrees C. Fuel cells with such bi-layer electrolytes were fabricated and tested, yielding open circuit voltages from 0.94 to 1.0 V at 600-700 degrees C. Power densities from 0.4 to 1.0 W cm{sup -2} at 0.7 V were achieved in air at temperatures of 600-700 degrees C. Cell performance was improved in flowing oxygen, with an estimated peak power density of over 2 W cm{sup -2} at 650 degrees C, assuming the same overall resistance over the entire range of current density. The high cell performance was attributed to the very low ohmic resistance of the fuel cell, owing to the small thickness of the electrolyte. Stable performance was also demonstrated in that the voltage of the fuel cell showed very little change at a constant current density of 1 A cm{sup -2} during more than 400 hours of operation at 650 degrees C in flowing oxygen. SEM analysis of the fuel cell after testing showed that the bi-layer electrolyte had retained its chemical and mechanical integrity.

30 DIRECT ENERGY CONVERSION↗