Effect of Thermal Aging and Test Temperatures on Fracture Toughness of SS 316(N) Welds

The effect of thermal aging and test temperatures on fracture toughness (J{sub 0.2}) of SS 316(N) weld material has been studied based on J-R curve evaluations. The aging of the welds was carried out at temperatures 370, 475 and 550 °C and for durations varying from 1000 to 20,000 h. The fracture toughness (J-R curve) tests were carried out at 380 and 550 °C for specimens after all aging conditions, including as-weld condition. The initiation fracture toughness (J{sub 0.2}) of the SS 316(N) weld material has shown degradation after 20,000-h aging durations and is reflected in all the test temperatures and aging temperatures. The fracture toughness after different aging conditions and test temperatures, including as-weld condition, was higher than the minimum specified value for this class of welds.

36 MATERIALS SCIENCE↗

Experimental results of conductive inserts to reduce nuclear fuel temperature during nuclear volumetric heating

Advanced fuel designs that incorporate thinner fuel UO2 pellets interspaced by high thermal conductivity inserts have been proposed, with the primary goals of reducing peak centerline temperatures and temperature gradients across fuel pellets and enhancing heat transfer from the fuel to the coolant. An initial series of experiments has been performed on this design, including laboratory experiments and a series of experiments using the Idaho National Laboratory (INL) Transient Reactor Test (TREAT) Facility, the latter of which compared thermal gradient driven fracture of standard pellet designs with that in the proposed advanced fuel design. Although reducing fracture is not the primary objective of the new fuel design, the lower thermal gradients are expected to reduce fracture, so it can serve as an indicator of the thermal behavior of this fuel in the reactor. The in-reactor tests were conducted at multiple linear heat generation rates and confirm the expected result that fracture in both the standard and advanced fuel pellets occurs during the first ramp to power in standard light-water reactor conditions. Post-irradiation examination of the experiment material was performed and included quantification of the extent of fracture in the fuel pellets. It was found that the advanced-design pellets reduce the extent of fracture in a statistically significant way. This confirms the expected behavior predicted by two-dimensional axisymmetric models of this experiment. Here in this study is an important first experimental confirmation of the efficacy of the proposed inserts for achieving their desired effect on the thermal behavior of the fuel.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Mechanical behavior of La0.8Sr0.2Ga0.8Mg0.2O3 perovskites

Mechanical properties such as Young's modulus, fracture toughness and slow crack growth have been measured for phase pure and highly dense (<5% porosity) La0.8Sr0.2Ga0.8Mg0.2O3 perovskites. The Young's modulus was measured to be ~175 GPa, while strength and fracture toughness both exhibited low values confirming the poor mechanical properties of the material. LSGM was also proved to be highly susceptible to slow crack growth in humid air at room temperature where in order to survive a one year period the static stresses in the material should be as low as 50 MPa for a 50% failure probability.

36 MATERIALS SCIENCE↗

Lattice Reinforced Cermet Materials

This project developed ceramic-metal (cermet) composite materials reinforced with embedded metal lattices. The goal of the project was to develop materials that have a higher tensile and compressive strength as well as greater fracture toughness than conventional boron carbide-aluminum cermets. These materials have applications in structural applications as well as advanced vehicle and personnel armors.

36 MATERIALS SCIENCE↗

Crack propagation, arrest and statistics in heterogeneous materials.

We investigate theoretically statistics and thermally activated dynamics of crack nucleation and propagation in a two-dimensional heterogeneous material containing quenched randomly distributed defects. We consider a crack tip dynamics accounting for dissipation, thermal noise and the random forces arising from the elastic interactions of the crack opening with the defects. The equation of motion is based on the generalized Griffith criterion and the dynamic energy release rate and gives rise to Langevin-type stochastic dynamics in a quenched disordered potential. For different types of quenched random forces, which are characterized (a) by the range of elastic interactions with the crack tip and (b) the range of correlations between defects, we derive a number of static and dynamic quantities characterizing crack propagation in heterogeneous materials both at zero temperature and in the presence of thermal activation. In the absence of thermal fluctuations we obtain the nucleation and propagation probabilities, typical arrest lengths, the distribution of crack lengths and of critical forces. For thermally activated crack propagation we calculate the mean time to fracture. Depending on the range of elastic interactions between crack tip and frozen defects, heterogeneous material exhibits brittle or ductile fracture. We find that aggregations of defects generating long-range interaction forces (e.g. clouds of dislocations) lead to anomalously slow creep of the crack tip or even to its complete arrest. We demonstrate that heterogeneous materials with frozen defects contain a large number of arrested microcracks and that their fracture toughness is enhanced to the experimentally accessible timescales.

36 MATERIALS SCIENCE↗

Tailoring ductile-phase toughened tungsten hierarchical microstructures for plasma-facing materials

Biological materials, such as bones, nacre, etc., have been found to show attractive and unique combinations of stiffness, strength and fracture toughness. Research has been conducted in various engineering areas to mimic the naturally hierarchical microstructures or nanostructures of these materials to produce materials with optimum stiffness, high strength and fracture toughness for their intended structural applications. In the same objective, this work applies a multiscale microstructural approach recently developed to investigate the deformation and fracture behavior of ductile phase toughened tungsten (W) materials such as tungsten-nickel/iron (W-Ni/Fe) composites that possess lamellar-like and hierarchical “brick-and-mortar” (BAM) microstructures. First, the approach is used to simulate tensile loading of W-Ni/Fe specimens cut out from hot-rolled W-Ni/Fe plates which possess lamellar-like microstructures. The finite element model of the gage section of the specimen consists of a W-Ni/Fe dual-phase microstructural domain in which the constitutive behaviors of W and Ni/Fe phases are described by an elastic-plastic damage model. The predicted material stress-strain response and crack pattern development as a function of loading are then compared to the corresponding experimental results to determine the constitutive model parameters for W and Ni/Fe. Subsequently, the model parameters are used to analyze W-Ni/Fe BAM microstructures that are artificially created to investigate the effects of microstructural features and morphologies on the composite stress-strain response, damage, and fracture patterns. The modeling shows that regular BAM microstructures that experience bridging mechanism combined with crack penetration across W-phase regions exhibit significantly higher strengths than the rather random lamellar-like microstructures. More significantly, however adjusting the brick’s length-to-height ratio, the BAM microstructure can be designed to allow a more distributed damage zone which leads to increased strength, ductility and fracture energy.

36 MATERIALS SCIENCE↗

Plastic Stress-strain Relations for 75S-T6 Aluminum Alloy Subjected to Biaxial Tensile Stresses

In this investigation, the material tested was a 75S-T6 aluminum alloy and the stresses were essentially biaxial and tensile. The biaxial tensile stresses were produced in a specially designed testing machine by subjecting a thin-walled tubular specimen to axial tension and internal pressure. Plastic stress-strain relations for various biaxial stress conditions were obtained using a clip-type SR-4 strain gage. Three types of tests were made: Constant-stress-ratio tests, variable-stress-ratio tests, and special tests. The constant-stress-ratio test results gave control data and showed the influence of biaxial stresses on the yield, fracture, and ultimate strength of the material. By means of the variable-stress-ratio tests, it is possible to determine whether there is any significant difference between the flow and deformation type of theory. Finally, special tests were conducted to check specific assumptions made in the theories of plastic flow. The constant-stress-ratio tests show that the deformation theory based on the octahedral, effective; or significant stress-strain relations is in approximate agreement with the test results. The variable-stress-ratio tests show that both the deformation and flow theory are in equally good agreement with the test results.

Marin, Joseph↗

Forced Cooling Friction Stir Welding of 2060-T8 Al-Li Alloy

Friction stir welding of 2060-T8 Al-Li alloy was experimentally investigated. Forced cooling process was realized by placing two copper pressure plates with a waterway on both sides of weld top surface. The relations between joint formation, microstructures and mechanical properties were mainly discussed. Compared with conventional joint by natural cooling, the welding joint with smaller flashes by forced cooling has the smaller well-distributed grains and higher microhardness in the stir zone (SZ). The tensile strength and elongation of forced cooling joint, respectively, reach 445.7 MPa and 6.7%, which are obviously higher than those of the conventional joint. The fracture locations of the conventional and forced cooling joints are located in the SZ, and the fracture surface morphologies show a typical ductile fracture mode.

36 MATERIALS SCIENCE↗

Characterization of modified calcium-silicate cements exposed to acidic environment

Portland cement which is used as a binder in concrete in the construction industry has been developed into a biomaterial. It is marketed as mineral trioxide aggregate and is used in dentistry. This material has been reported to be very biocompatible and thus its use has diversified. The extended use of this material has led to developments of newer versions with improved physical properties. The aim of this study was to evaluate the effect of acidic environments found in the oral cavity on fast setting calcium silicate cements with improved physical properties using a combination of techniques. Two fast setting calcium silicate cements (CSA and CFA) and two cement composites (CSAG and CFAG) were assessed by subjecting the materials to lactic acid/sodium lactate buffer gel for a period of 28 days. At weekly intervals the materials were viewed under the tandem scanning confocal microscope (TSM), and scanning electron microscope (SEM). The two prototype cements exhibited changes in their internal chemistry with no changes in surface characteristics. Since the changes observed were mostly sub-surface evaluation of surface characteristics of cement may not be sufficient in the determination of chemical changes occurring. - Research Highlights: {yields} An acidic environment affects modified fast setting calcium silicate-based cements. {yields} No surface changes are observed in acidic environment. {yields} An acidic environment causes sub-surface changes in the material chemistry which are only visible in fractured specimens. {yields} A combination of techniques is necessary in order to evaluate the chemical changes occurring.

36 MATERIALS SCIENCE↗

Physical and mechanical metallurgy of NiAl

Considerable research has been performed on NiAl over the last decade, with an exponential increase in effort occurring over the last few years. This is due to interest in this material for electronic, catalytic, coating and especially high-temperature structural applications. This report uses this wealth of new information to develop a complete description of the properties and processing of NiAl and NiAl-based materials. Emphasis is placed on the controlling fracture and deformation mechanisms of single and polycrystalline NiAl and its alloys over the entire range of temperatures for which data are available. Creep, fatigue, and environmental resistance of this material are discussed. In addition, issues surrounding alloy design, development of NiAl-based composites, and materials processing are addressed.

Noebe, Ronald D.↗

In-service Inspection Ultrasonic Testing of Reactor Pressure Vessel Welds for Assessing Flaw Density and Size Distribution per 10 CFR 50.61a, Alternate Fracture Toughness Requirements

Pressurized thermal shock (PTS) events are system transients in a pressurized water reactor (PWR) in which there is a rapid operating temperature cool-down that results in cold vessel temperatures with or without repressurization of the vessel. The rapid cooling of the inside surface of the reactor pressure vessel (RPV) causes thermal stresses that can combine with stresses caused by high pressure. The aggregate effect of these stresses is an increase in the potential for fracture if a pre-existing flaw is present in a material susceptible to brittle failure. The ferritic, low alloy steel of the reactor vessel beltline adjacent to the core, where neutron radiation gradually embrittles the material over the lifetime of the plant, can be susceptible to brittle fracture. The PTS rule, described in the Code of Federal Regulations, Title 10, Section 50.61 (§50.61), “Fracture Toughness Requirements for Protection against Pressurized Thermal Shock Events,” adopted on July 23, 1985, establishes screening criteria to ensure that the potential for a reactor vessel to fail due to a PTS event is deemed to be acceptably low. The U.S. Nuclear Regulatory Commission (NRC) completed a research program that concluded that the risk of through-wall cracking due to a PTS event is much lower than previously estimated. The NRC subsequently developed a rule, §50.61a, published on January 4, 2010, entitled “Alternate Fracture Toughness Requirements for Protection Against Pressurized Thermal Shock Events” (75 FR 13). Use of the new rule by licensees is optional. The §50.61a rule differs from §50.61 in that it requires licensees who choose to follow this alternate method to analyze the results from periodic volumetric examinations required by the ASME Code, Section XI, Rules for Inservice Inspection (ISI) of Nuclear Power Plants. These analyses are intended to determine if the actual flaw density and size distribution in the licensee’s reactor vessel beltline welds are bounded by the flaw density and size distribution values used in the PTS technical basis. Under a contract with the NRC, Pacific Northwest National Laboratory (PNNL) has been working on a program to assess the ability of current inservice inspection (ISI)-ultrasonic testing (UT) techniques, as qualified through ASME Code, Appendix VIII, Supplements 4 and 6, to detect small fabrication or inservice-induced flaws located in RPV welds and adjacent base materials. As part of this effort, the investigators have pursued an evaluation, based on the available information, of the capability of UT to provide flaw density/distribution inputs for making RPV weld assessments in accordance with §50.61a. This paper presents the results of an evaluation of data from the 1993 Browns Ferry Nuclear Plant, Unit 3, Spirit of Appendix VIII reactor vessel examination, a comparison of the flaw density/distribution from this data with the distribution in §50.61a, possible reasons for differences, and plans and recommendations for further work in this area.

alloy 82/182↗

A hexagonal close-packed high-entropy alloy: The effect of entropy

The formation of disordered solid solution in the hexagonal close-packed (hcp) structure in the GdHoLaTbY alloy and its mechanical properties were investigated in this study. The single hcp phase of the alloy in the as-cast state was confirmed by X-ray diffraction and scanning electron microscopy analyses. The compressive yield strength, fracture strength, and plastic strain of the alloy are 108 MPa, 880 MPa, and 21.8 %, respectively, and the Vickers hardness is 96 HV. The results show that the yield strength, fracture strength, and hardness of the alloy obey the rule of mixture, which indicates that there is no hardening effect from entropy. Although the high entropy of mixing stabilizes the solid solution against intermetallic compounds, lack of severe lattice distortion from elastic strain or electronic interactions between principal elements impacts little on the mechanical properties.

36 MATERIALS SCIENCE↗

The homogenous alternative to biomineralization: Zn- and Mn-rich materials enable sharp organismal “tools” that reduce force requirements

We measured hardness, modulus of elasticity, and, for the first time, loss tangent, energy of fracture, abrasion resistance, and impact resistance of zinc- and manganese-enriched materials from fangs, stings and other “tools” of an ant, spider, scorpion and nereid worm. The mechanical properties of the Zn- and Mn-materials tended to cluster together between plain and biomineralized “tool” materials, with the hardness reaching, and most abrasion resistance values exceeding, those of calcified salmon teeth and crab claws. Atom probe tomography indicated that Zn was distributed homogeneously on a nanometer scale and likely bound as individual atoms to more than ¼ of the protein residues in ant mandibular teeth. This homogeneity appears to enable sharper, more precisely sculpted “tools” than materials with biomineral inclusions do, and also eliminates interfaces with the inclusions that could be susceptible to fracture. Based on contact mechanics and simplified models, we hypothesize that, relative to plain materials, the higher elastic modulus, hardness and abrasion resistance minimize temporary or permanent tool blunting, resulting in a roughly 2/3 reduction in the force, energy, and muscle mass required to initiate puncture of stiff materials, and even greater force reductions when the cumulative effects of abrasion are considered. We suggest that the sharpness-related force reductions lead to significant energy savings, and can also enable organisms, especially smaller ones, to puncture, cut, and grasp objects that would not be accessible with plain or biomineralized “tools”.

59 BASIC BIOLOGICAL SCIENCES↗

Mechanical and Tribological Behavior of ZrB{sub 2}-TiB{sub 2} System Prepared by Mechanical Activation Spark Plasma Sintering Technique

ZrB{sub 2}-TiB{sub 2} system among varying amount of TiB{sub 2} loading (5, 10, 15, 20 and 30 wt.%) was prepared by mechanical activation spark plasma sintering at 2100 °C for 15-min dwell time under 50 MPa uniaxial pressure in argon atmosphere. The effect of the TiB{sub 2} loading on properties like physical, mechanical and tribological of the prepared samples was studied and evaluated with monolithic ZrB{sub 2} ceramic. Finally, almost fully dense samples (> 96% of theoretical density) were fabricated. Microstructural observation and XRD phase analysis of sintered compact revealed that TiB{sub 2} completely went into the ZrB{sub 2} structure by formation of solid solution with ZrB{sub 2} phase. ZrB{sub 2}-TiB{sub 2} (30 wt.%) showed the highest Vickers micro-hardness (H{sub V}) of 20.64 GPa at 10 N load. On addition of TiB{sub 2}, the fracture toughness of the ZrB{sub 2}-TiB{sub 2} improved up to 4.69 ± 0.43 MPa m{sup 1/2} over monolithic ZrB{sub 2} at 10 N load. At 10 N load, the scratch resistance coefficient, wear rate and wear resistance coefficient of ZrB{sub 2}-TiB{sub 2} (30 wt.%) reached a lowest value of 0.32, 0.35 mm{sup 3}/N m and 0.008, respectively, at 10 N load than other ZrB{sub 2} compositions.

36 MATERIALS SCIENCE↗

Evaluating Fracture Behavior of Bioinspired Alumina-YSZ Composites through Static and Dynamic Mechanical Testing

Ceramic materials are known for their high hardness and strength but are limited by low toughness and sudden failure. Inspired by the microstructure of dental enamel, which features undulating rods that promote crack deflection and energy absorption, architected specimens were designed and manufactured. A bespoke ball-on-ring (BoR) testing apparatus measured the static biaxial rupture strength of these bioinspired materials. Additionally, impact testing with spherical steel projectiles assessed their behavior under dynamic conditions. Monolithic alumina specimens were compared to architected alumina reinforced with yttria-stabilized zirconia (YSZ) rods produced via direct ink write 3D printing. BoR tests revealed that monolithic alumina had a Weibull modulus of 10.53 and a characteristic strength of 372.3 MPa, while the composite specimens showed a Weibull modulus of 5.46 and a characteristic strength of 213.3 MPa. Although the composite failed at lower stresses and projectile velocities, it exhibited notable crack deflection and fracture resistance, with cracks being effectively interrupted by the rod inclusions. The composite specimens also resulted in fewer and larger fragments upon impact. Finite element simulations confirmed the effectiveness of the rod structures in enhancing fracture resistance.

Bioinspired materials↗

Brittle-ductile transitions in a metallic glass

Recent computational and laboratory experiments have shown that brittle-ductile transitions in the notch toughnesses of metallic glasses such as Vitreloy 1 are strongly sensitive to the initial effective disorder (or “fictive”) temperature. Glasses with lower effective temperatures are weak and brittle; those with higher effective temperatures are strong and ductile. The analysis of this phenomenon presented here examines the onset of fracture at the tip of a notch as predicted by the shear-transformation-zone theory of spatially varying plastic deformation. The central ingredient of this analysis is an approximation for the dynamics of the plastic zone formed by stress concentration at the notch tip. As a result, this zone first shields the tip but then, with increasing stress, expands suddenly, producing a discontinuous transition between brittle and ductile failure in satisfactory agreement with the numerical and experimental observations.

36 MATERIALS SCIENCE↗

Mechanical Design Guidelines to Inhibit Fracture in Perovskite Solar Cells

Perovskite (PVSK) solar cells offer significant benefits over conventional silicon cells including low-cost solution processibility, minimal materials usage related to strong photon absorption in thin-film cell architectures, and a tunable bandgap. However, PVSK films are mechanically fragile, and fracture of PVSK layers and adjacent interfaces are a significant concern during fabrication, encapsulation, and operation. Herein, a thin-film mechanics fracture analysis tailored for p–i–n and n–i–p PVSK solar cells on both soda lime glass and polyimide substrates fabricated with three PVSK crystallization methods is presented. Here, the role of thermal processing of each cell layer is explored to determine the maximum allowable temperature below which fracture is inhibited. In the analysis, the mechanics basis for processing and materials selection guidelines for preventing fracture in PVSK solar cells is provided.

adhesion↗

Simulating Dynamic Fracture in Oxide Fuel Pellets Using Cohesive Zone Models

It is well known that oxide fuels crack during the first rise to power, with continued fracture occurring during steady operation and especially during power ramps or accidental transients. Fractures have a very strong influence on the stress state in the fuel which, in turn, drives critical phenomena such as fission gas release, fuel creep, and eventual fuel/clad mechanical interaction. Recently, interest has been expressed in discrete fracture methods, such as the cohesive zone approach. Such models are attractive from a mechanistic and physical standpoint, since they reflect the localized nature of cracking. The precise locations where fractures initiate, as well as the crack evolution characteristics, are determined as part of the solution. This paper explores the use of finite element cohesive zone concepts to predict dynamic crack behavior in oxide fuel pellets during power-up, steady operation, and power ramping. The aim of this work is first to provide an assessment of cohesive zone models for application to fuel cracking and explore important numerical issues associated with this fracture approach. A further objective is to provide basic insight into where and when cracks form, how they interact, and how cracking effects the stress field in a fuel pellet. The ABAQUS commercial finite element code, which includes powerful cohesive zone capabilities, was used for this study. Fully-coupled thermo-mechanical behavior is employed, including the effects of thermal expansion, swelling due to solid and gaseous fission products, and thermal creep. Crack initiation is determined by a temperature-dependent maximum stress criterion, based on measured fracture strengths for UO2. Damage evolution is governed by a traction-separation relation, calibrated to data from temperature and burn-up dependent fracture toughness measurements. Numerical models are first developed in 2D based on both axisymmetric (to explore axial cracking) and plane strain (to explore radial cracking) assumptions. A 3D model is then developed, permitting simultaneous radial and axial fractures. Although fuel cracking is clearly three-dimensional, 2D models are of interest since they are simpler to implement, are much less computationally intensive, and have potential application to existing 2D fuel performance codes. Numerical issues related to cohesive zone models, such as mesh dependency and viscous stabilization, are addressed. Model results indicate that for typical oxide fuel properties, both axial and radial cracking occurs during initial heat-up, well before steady-state thermal gradients are established in the pellet. Cracking results in local stress relief and a shift in peak stress locations, leading to the initiation of new cracks. Continued growth of existing cracks, plus the initiation and growth of additional fractures, is observed during steady operation and power ramping. 3D models provide considerable insight into the progressive interactions between radial and axial cracking. Parametric studies demonstrate the effects of temperature dependent material properties on crack initiation and progression. Increasing fracture strength and toughness with temperature, leads to crack arrest in high temperature regions near the pellet’s symmetry axis.