An Approach to Improve the Retention of the Fission Product Ag in TRISO Fuel Particles - 18596
The silicon carbide (SiC) coating included in TRISO particles acts as the main barrier against the radioactive fission products release into the coolant circuit. However, radioactive silver (Ag{sup 110m}) was identified outside the intact particles with a very high release fraction, which could be problematic in the licensing process for modern HTR fuel. Our previous work proposed that dissolution/recrystallization of SiC by Ag could help Ag migrate at 1800 deg. C. The aim of this work is to study whether dissolution of SiC by Ag could take place and contribute to the Ag migration at operation temperature (from 1000 to 1300 deg. C). Both, experiment and thermodynamic analysis, showed that SiC dissolution by Ag was possible above 890 deg. C. But the dissolution from 1000 to 1300 deg. C is far less effective in moving Ag due to the insufficient driving force for activating self-penetration into the grain boundaries, compared with the previous work conducted at 1800 deg. C. Compared with silver alone, the silver-palladium mixture was more permeable in SiC and showed a diffusive behavior. The diffusion front was Ag rich while most palladium remained in reaction zone rather than in the diffusion front. Furthermore, thermodynamic analysis suggested that non-stoichiometric SiC with additional free silicon could impede such a reaction. Hence it is conceivable that a sacrificial layer of SiC+Si on the inner side of the main SiC coating could improve fission product retention overall without a significant increase in cost. (authors)