SEARCH · Engineering Papers
Results for “STEELS, STAINLESS - WELDING”
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Crack Growth Rate and Fracture Toughness J-R Curve Tests on Irradiated Cast Austenitic Stainless Steels
Explore the source record for details and available documents.
Electrochemical Nitridation of a Stainless Steel for PEMFC Bipolar Plates
Explore the source record for details and available documents.
Effect of Pressurized Water Reactor Environment on Material Parameters of 316 Stainless Steel: A Cyclic Plasticity Based Evolutionary Material Modeling Approach
Explore the source record for details and available documents.
Diffusion bonding of 316L stainless steel for ITER applications.
No abstract prepared.
Effect of crack-tip hydrogen profiles on the embrittled fracture toughness of a stainless steel
No abstract prepared.
Corrosion of a Stainless Steel in High Temperature Phosphoric Acid
Explore the source record for details and available documents.
Multiphase SESAME equation of state 4295 for Stainless Steel AM363
Abstract not provided.
Synergistic Effect of Nitrogen and Refractory Material on TiN Formation and Equiaxed Grain Structure of Ferritic Stainless Steel
The effect of nitrogen content on the formation of an equiaxed solidification structure of Fe-16Cr steel was investigated. Moreover, two different kinds of refractory materials, i.e., alumina and magnesia, were employed to control the type of oxide inclusion. The characteristics of TiN(-oxide) inclusions were quantitatively analyzed in both molten steel and solidified samples. When the melting was carried out in the alumina refractory, the grain size continuously decreased with increasing nitrogen content. However, a minimum grain size was observed at a specific nitrogen content (approx. 150 ppm) when the steel was melted in the magnesia refractory. Most of the single TiN particles had a cuboidal shape and fine irregularly shaped particles were located along the grain boundary due to the microsegregation of Ti at the grain boundary during solidification. The type of TiN-oxide hybrid inclusion was strongly affected by the refractory material where Al{sub 2}O{sub 3}-TiN and MgAl{sub 2}O{sub 4}-TiN hybrid-type inclusions were obtained in the alumina and magnesia refractory experiments, respectively. The formation of oxide inclusions was well predicted by thermochemical computations and it was commonly found that oxide particles were initially formed, followed by the nucleation and growth of TiN. When the nitrogen content increased, the number density of TiN linearly increased in the alumina refractory experiments. However, the number of TiN exhibits a maximum at about [N] = 150 ppm, at which a minimum grain size was obtained in the magnesia refractory experiments. Therefore, the larger the number density of TiN, the smaller the primary grain size after solidification. The number density of TiN in the steel melted in the magnesia refractory was greater than that in the steel melted in the alumina refractory at given Ti and N contents, which was due to the lower planar lattice disregistry of MgAl{sub 2}O{sub 4}-TiN interface rather than that of Al{sub 2}O{sub 3}-TiN interface. When ∆T{sub TiN} (= difference between the TiN precipitation temperature and the liquidus of the steel) was 20 K to 40 K, the number density of effective TiN was maximized and thus, the grain size was minimized after solidification. Finally, although most of the TiN particles were smaller than 1 μm in the molten steel samples irrespective of the nitrogen content, TiN particles larger than 10 μm were observed in the solidified samples when the nitrogen content was greater than 150 ppm. The growth of TiN particles during melting and solidification was well predicted by the combinatorial simulation of the ‘Ostwald ripening model’ based on the Lifshitz–Slyozov–Wagner theory in conjunction with the ‘Diffusion controlled model’ using Ohnaka’s microsegregation equation.
Energetic Condensation Coating Of Cu On Stainless Steel For High Power Couplers, Phase II Final Technical Report
Explore the source record for details and available documents.
Characteristics of Nozzle Clogging and Evolution of Oxide Inclusion for Al-Killed Ti-Stabilized 18Cr Stainless Steel
Characteristics of nozzle clogging and evolution of oxide inclusion were studied by sampling the deposits of submerged entry nozzle (SEN) and the molten steel in tundish during Al-killed Ti-stabilized 18Cr stainless steelmaking process. The deposits found in the clogging of SEN were mainly composed of frozen steel and inclusions. The inclusions in the deposits and tundish were both mainly (MgO-Al{sub 2}O{sub 3}){sub rich}-CaO-TiO{sub x}. The compositions of most inclusions were Liquid+Spinel or Liquid+TiSp phase. The (MgO-Al{sub 2}O{sub 3}){sub rich}-CaO inclusions that were not effectively modified by calcium treatment could be a source of clogging. By combining both the experimental results and thermodynamic calculation, (MgO-Al{sub 2}O{sub 3}){sub rich}-TiO{sub x} inclusions (TiSp inclusions) would be formed with the decreasing temperature in steel during continuous casting, which could be transported and accumulated on the inner wall of the SEN. Increasing the calcium content in the molten steel could decrease the formation of TiSp inclusions. During continuous casting, these inclusions accumulated on the inner wall of the SEN and gradually formed porous network of clog. Molten steel would gradually solidify in the porous space of the clog due to the increased residence time of the molten steel when flowing through it. The clogging gradually increased and caused the shutdown of continuous casting.
Manufacturing characterization of meso-scale parts made from stainless steel.
No abstract prepared.
Solid state bonding of CuCrZr to 316L stainless steel for ITER applications.
No abstract prepared.
Ultra-Low Temperature Testing Requirements for 316L Stainless Steel in ASME B31.3 (Projects 157 and 173)
Explore the source record for details and available documents.
Modifying a Stainless Steel for PEMFC Bipolar Plates via Electrochemical Nitridation
Explore the source record for details and available documents.
The role of strain-induced alpha-martensite on hydrogen-assisted fracture of austenitic stainless steels.
No abstract prepared.
The Influence of Modification on Crystal Lattice Stability of Austenite in Stainless Steel
Using the methods of electron diffraction microscopy and X-ray diffraction analysis, the influence of alloying of the austenitic steel, Grade 110H13, with chromium and vanadium, as well as high-melting, ultrafine-grained TiO{sub 2}, ZrO{sub 2} powders and Na{sub 3}AlF{sub 6} cryolite on its structural-phase state and microstructure is investigated. It is shown that the matrix of non-modified steel is completely austenitic and consists of an iron-based solid solution and the interstitial (C, N, O and other) and substitutional (Cr, V and other) atoms simultaneously. Alloying with chromium and vanadium changes neither its phase composition nor defect structure, while alloy modification results in qualitatively new structural features: γ → ε-transformation, high-intensity microtwinning, defect structure changes, and a sharp increase in the scalar dislocation density. The features of the deformation-induced microtwinning and ε-martensite plates identified in the modified steel promote revealing additional microtwin systems in the matrix γ-phase, which result in structural changes making it possible to classify it as a γ′-phase. It is found out that an introduction of modifying additions gives rise to the following sequence of structural-phase transformations: γ→γ′→(γ′ +ε). The experimental data obtained demonstrate that as a result of modification the crystal lattice transits into a low-stability state. This transition is accompanied by marked structural-phase changes consisting in the formation of several microtwin systems and γ → ε-transformation. These structural-phase changes in the modified steel are due to the crystal-lattice transition into the low-stability state, followed by new structural-phase alterations.