The electronic states and electron-lattice interaction in the silver halides - Photoemission studies
Examining photoemission from silver halides from room to liquid nitrogen temperatures to determine electron energy states
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Examining photoemission from silver halides from room to liquid nitrogen temperatures to determine electron energy states
Scattering distributions for argon incident on fresh epitaxial silver films
Optical luminescence in reaction detection at rear of porous electrodes and comparison of interface reaction resistance and electrolyte ohmic resistance in zinc-silver oxide batteries
Elimination of microbial and viral agents from spacecraft water systems by silver ions from electrolytic ion generator
Development of heat-sterilizable 40-Ah sealed, nonmagnetic silver zinc cell for use on Viking spacecraft
Anomalous temperature dependent silver halides photoemission related to lattice vibrationally dependent hybridization of valence states
Cellulose application as zinc silver oxide battery separator, considering chemical stability, cellophane properties, polymerization and crystallinity
Service performance and tests of zinc silver oxide batteries on Explorers 17 and 32
Electric field effect of epitaxial thin silver films on mica in vacuum as function of temperature, thickness and surface specularity
Fuel cell regenerated by photochemical reduction enables novel slurry system to transport particles of reduced silver between regenerator section and anode. Fundamental reactions which provide electrical power from the fuel cell are given.
A method of detecting radiation damage tracks due to heavy particles in large single crystals of the silver halides is described. The tracks, when made visible with a simple electrical apparatus, appear similar to tracks in emulsions. The properties of the crystals, the technique of printing out the tracks, and evidence concerning the threshold energy for registering particles indicates that this method may find application in heavy ion dosimetry. The method has been found to be sensitive to stopping He nuclei and relativistic M group cosmic rays. Some impurities strongly influence the printout of the tracks, and the effects of these impurities are discussed.
A new kind of silver-zinc cell was developed and tested under NASA support which can withstand severe heat sterilization requirements and does not display the traditional life limiting aspect of sinc electrodes i.e. shape change. These cells could be used on planetary lander mission which require wet-stand periods of over a year, a modest number of cycles (400 to 500) and may require dry heat sterilization. The weight advantage of these cells over the traditional nickel cadmium batteries also makes it an attractive alternative for synchronous orbit service where 400 to 500 cycles would be required over a 5 year period.
The development of an inorganic separator material for use in construction of 40 ampere-hour silver zinc cells is discussed. Acceptance tests were conducted to determine real quality, physical defects and ampere-hour capacity. All acceptance tests were performed at an ambient temperature of 23 to 27 C at existing relative humidity and atmospheric pressure. Of the 63 cells tested, only one failed to meet the equipment specifications.
Study of the solid electrolyte ZnCl2-2NH3 rechargeable silver zinc electrochemical cell by X-ray diffraction analysis of the reaction products led to the conclusion that some water is consumed when the cell is discharged. Replacement of ZnCl2-2NH3 by ZnCl2-4Zn(OH)2 gave cells with high internal resistance and limited capacity. The salt formed by exposing a fibrous membrane saturated with ZnCl2 solution to fumes from ammonium carbonate in a dry desiccator comprised ZnCl2-4Zn(OH)2, ZnCl2,3NH4Cl and a third unidentified component. The temperature coefficient of open circuit EMF was nearly zero over the range from -25 C to 50 C. The internal resistance and polarization increased substantially below -25 C. There is some indication that exposure to 50 C for 29 hours causes some deterioration.
A prototype silver zinc cell is reported for which the electrolyte is being stored in a separate tank; the cell is being activated when additional power is required by collapsing the neoprene bellows container and thus forcing the electrolyte into cell through a plastic connection. A solar array is proposed as main power source for the flow actuator.
The lifetime of separator membranes currently employed in the electrolyte environment of silver-zinc batteries was estimated at 3 to 5 years. The separator membranes are crosslinked polyethylene film containing grafted poly (potassium acrylate)(PKA), the latter being the hydrophilic agent which promotes electrolyte ion transport. The lifetime was estimated by monitoring the rate of loss of PKA from the separators, caused by chemical attack of the electrolyte, and relating this loss rate to a known relationship between battery performance and PKA concentration in the separators.
The trajectory of the particle is made visible under a microscope by the accumulation of metallic silver at regions of the lattice damaged by the particle. This decoration of the particle track is accomplished by exposure of the crystal to light. The decoration of normally present lattice imperfections such as dislocations can be suppressed by the addition to the crystal of less than ten parts per million of a suitable polyvalent metal impurity. An account of some preliminary attempts to grow thin single crystals of AgCl is given also, and suggestions for a more refined technique are offered.
A new kind of silver-zinc cell has been developed and tested under NASA support which can withstand severe heat sterilization requirements. These cells could be used on planetary lander mission which require wet-stand periods of over a year, a modest number of cycles (400 to 500) and may require dry heat sterilization. The weight advantage of these cells over the traditional nickel-cadmium batteries also makes it an attractive alternative for synchronous orbit service where 400 to 500 cycles would be required over a 5 year period.