Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “INTERMETALLICS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,153 records · Page 64

Effect of aqueous‐based cathode slurry pH and immersion time on corrosion of aluminum current collector in lithium‐ion batteries

Corrosion of aluminum can occur during the manufacturing of lithium‐ion batteries when using aqueous‐based cathode slurries. In exposure tests, the alkaline pH value of aqueous‐based cathode slurries and immersing time were revealed as the principle factors that control the corrosion of aluminum during the cathode manufacturing process. The nickel manganese cobalt oxide active material used in the slurry does not have a direct impact on corrosion of the aluminum current collector. The initiation and evolution of localized corrosion on aluminum are closely related to the formation of galvanic cells between aluminum matrix and intermetallic particles. X‐ray photoelectron spectroscopy results confirmed that the pH of cathode slurry was the only factor that alters aluminum surface composition, during which the oxide passive film was gradually degraded into hydroxide. Electrochemical characterizations showed that aluminum electrodes gave remarkably different response to the different pH of test solutions. The time‐pH‐variant electrochemical response was ascribed to the change of passive film and electric double layer properties.

Li, S. Y.↗

Composition-Mediated Order-Disorder Transformation in FePt Nanoparticles

Thumbnail image of graphical abstract Heat-treated alloy FePt nanoparticles transform into L10 FePt and mixed L10/L12 FePt3 intermetallic phases. Enrichment in Pt in some nanoparticles, rather than intrinsic thermodynamic effects, drives phase segregation. FePt nanoparticles of uniform, equimolar composition are expected to transform into phase-pure, highly ordered L10 FePt nanoparticles.

Johnston-Peck, Aaron C.↗

The Zintl Concept Applied to Intergrowth Structures: Electron‐Hole Matching, Stacking Preferences, and Chemical Pressures in Pd 5 InAs

Abstract Enumerating the potential stacking sequences of layers is a fundamental way to account for the structure diversity of solid state compounds. In many cases, these stacking variations represent polymorphs with only small energetic differences. Here, we examine a compound for which the preferred stacking pattern instead reveals key aspects about its chemical bonding: Pd 5 InAs. Its structure is based on the intergrowth of slabs of the AuCu 3 and PtHg 2 (or alternatively, fluorite) structure types. Two basic stacking arrangements are available to this compound, represented by the Pd 5 TlAs and HoCoGa 5 structure types. DFT total energy calculations reveal that the former outcompetes the latter by a staggering 0.65 eV/formula unit. Through a combination of DFT‐reversed approximation Molecular Orbital (DFT‐raMO) and DFT‐Chemical Pressure (DFT‐CP) analysis we trace this preference to two factors. First, with DFT‐raMO analysis, we derive a Zintl‐like bonding scheme of Pd 5 InAs. This scheme, along with the inspection of selected crystal orbitals, is then connected to preferred stacking through the coordination environments of the Pd atoms at the interface between the Pd−In and Pd−As layers. In the hypothetical HoCoGa 5 ‐type and observed Pd 5 InAs‐type structures, different Pd coordination environments arise at the interfaces. The hypothetical structure features square planar PdIn 2 As 2 units, in each of which the same 4d‐orbital serves in the Pd sublattice's role as both Lewis acid (for interactions with the As) and Lewis base (for interactions with the In). In the observed structure, tetrahedral PdIn 2 As 2 units occur instead, so that these contradictory roles are distributed to separate 4d‐orbitals, leading to more effective bonding. DFT‐CP analysis illustrates that this driving force for the Pd 5 TlAs‐type arrangement is supplemented by a favorable alignment of the packing tensions in the parent structures. Altogether, the resulting picture demonstrates how the reaction of simple intermetallic structures to form intergrowths can be guided by recognizable chemical interactions.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Joining AA7099 to Ni-Cr-Mo Steel using Friction Stir Dovetailing

Friction stir dovetailing (FSD) was used to join 0.5 inch (12.7 mm) AA7099 to 0.5 inch (12.7 mm) Ni-Cr-Mo steel in a lap configuration. Two new FSD approaches are reported that significantly reduce zinc embrittlement of Fe-Al intermetallic compounds (IMCs) which form during conventional friction stir welding (FSW). The first method uses the general FSD approach where a custom designed tool is employed to extrude the AA7099 into the pre-machined dovetail groove of underlying steel by forming mechanical interlocking and metallurgical bonding simultaneously. The second method uses a two-step approach where FSD of AA6061 is first used to form a silicon-rich Fe-Al IMC within the dovetail groove. AA7099 plate is then joined to the AA6061 within the dovetail using conventional FSW. A discussion of the new FSD technique, joint configurations, and process parameters are provided along with joint microstructural analyses and mechanical performance.

Friction stir dovetailing, FSD, AA7099, AA6061, ro↗

Joining Dissimilar Materials via Rotational Hammer Riveting Technique

A mechanically robust joining method for Mg/Al and Mg/CFRP could enable multi-material assemblies that decrease vehicle weight while offering more flexibility for designers. However, certain challenges exist for joining Mg/Al and Mg/CFRP. Mechanical joining, such as conventional riveting, clinching and bolting do not form a metallurgical bond between the fastener and metal sheet being fastened. Large differences in physical and mechanical properties of metals and polymers make joining Al or Mg to CFRP challenging via various welding techniques. With solid-state and fusion based welding, rapid formation of brittle intermetallic compounds at the Mg/Al interface lead to interfacial fracture under mechanical loading. In this study, a Rotational Hammer Rivet (RHR) technique was developed to fabricate Mg/CFRP and Mg/Al joints. With RHR technique, direct joining between Mg/Al and Mg/CFRP were replaced by joining Mg rivet head and top Mg sheet. Through heat generated by plastic deformation of an Mg rivet, RHR creates a metallurgical bond between rivet head and Mg sheet which seals corrosive electrolyte from penetrating around the rivet head.

riveting, magnesium alloys, CFRP, Dissimilar Joini↗

Anodization Compatibility of Eutectic Aluminum–Cerium Alloys

Anodizing is the most common method for producing corrosion resistant layer coatings for aluminum alloys. It is possible to use anodizing with most commercial aluminum alloys to increase material corrosion resistance, but often the brittle, passive oxide layer formed during anodization does not adhere well to the material, reducing effectiveness, and overall compatibility. Therefore, it is important for the compatibility and effect of anodization to be studied for any newly developed alloys. Recently developed eutectic Al–Ce alloys offer advantages like high castability, limited or no heat treatment requirements, and high-temperature strength retention. In this work, Al–Ce alloys are shown to have good compatibility with current processes and may exhibit improved adhesion of passivated layer because intermetallic phases anchor the anodized product to unconverted bulk. The source of these phenomena and their effect on material corrosion and layer adhesion properties of Al–Ce alloys will be discussed and compared with results from common commercial aluminum alloys.

Sims, Zachary↗

Shear Assisted Processing and Extrusion of Unhomogenized Aluminum Alloy 6063 Castings with High Iron Content

Shear Assisted Processing and Extrusion (ShAPE) was used to fabricate aluminum 6063 tubing directly from secondary scrap. Trimmings from an automotive manufacturing facility were cast into billets spiked with iron (0.3 wt% Fe) to explore the tolerance of ShAPE to Fe contamination. Billets were extruded in the unhomogenized condition to form tubing with an outer diameter of 12 mm and wall thickness of 2 mm. Tensile properties reached 0.2% YS = 206 MPa, UTS = 238 MPa, and U.E. = 16.3% in the T6 temper. Performance exceeds the ASTM minimum standard and is on par with ASM typical values for conventional extrusion of primary aluminum billets in the fully homogenized condition. Microstructural characterization shows extensive refinement of grain size along with dispersion and refinement of Fe-Al-Si intermetallic phases. This study suggests that ShAPE extrusion may offer a lower carbon manufacturing pathway through direct recycling of secondary aluminum scrap and elimination of the billet homogenization step.

solid phase processing, AA 6063, extrusion, Shear ↗

Solutionization via Severe Plastic Deformation: Effect on Natural Aging in an Al-Mg-Si-(Mn) Alloy

Shear Assisted Processing and Extrusion (ShAPE), a severe plastic deformation technique that is fast and scalable, was used to produce thin-wall tubing from alloy 6082 (Al-0.8Mg-0.9Si-0.7Mn) with in-situ solutionization during processing quickly followed by quenching. Quench medium and input material heat treatment were varied and natural aging behavior (T1 heat treatment) was evaluated using tensile testing. As-cast input material was found to have higher strength early in post-ShAPE natural aging and homogenized input material was found to have strengthening during natural aging. Compared to air quenching, water quenching gave greater strength both early in and after natural aging. These observations along with microscopy suggest that: 1. air quenching was too slow; 2. as-cast material was not fully solutionized but plastic deformation broke up the coarse intermetallic particles, which provided strengthening; and 3. homogenized material was solutionized well, which led to good natural aging behavior.

Milligan, Brian K.↗

Enhanced Tensile and Tear Toughness Properties of Thin-Wall Vacuum-Assisted High-Pressure Die-Cast Aural-5 Alloy by Friction Stir Processing

Steadily rising demand for glider weight reduction has driven the development of vacuum-assisted high-pressure die-cast (HPDC) Al-alloys for automotive structural components. Aural-5 is a strontium-modified HPDC alloy utilizing manganese (Mn) to reduce die soldering, eliminating detrimental needle-shaped Fe-bearing ß-phase intermetallic and improving ductility. HPDC Aural-5 contains shrinkage porosity, dendrites with Al-Si eutectic colonies, externally solidified crystals (ESCs), shear-band structure, and large second-phase particulates. Porosity, ESCs and large second-phase particles work as crack initiation sites, negatively impacting tensile properties. In this study, friction stir processing (FSP) is employed for microstructural modification of a thin-walled HPDC Aural-5 by eliminating porosity and breaking down dendrites, second-phase particles, eutectic colonies, ESCs and shear-band structures to create wrought microstructure with homogenized particle distribution. Mechanical property characterization indicates ~30% and ~35% enhancement in yield strength and ductility and associated marked effects on ~69% improvement in tear toughness according to the ASTM B871 test.

Friction stir processing, Aural-5, Strength, Tear ↗

Microstructure and Magnetic Properties of Electrodeposited Cobalt Film

Cobalt films were electrodeposited onto both iron and copper substrates from an aqueous solution containing a mixture of cobalt sulfate, boric acid, sodium citrate, and vanadyl sulfate. The structural, intermetallic diffusion and magnetic properties of the electrodeposited films were studied. Cobalt electrodeposition was carried out in a passively divided cell aided by addition of vanadyl sulfate to keep the counter electrode clean. The divided electrolytic cell with very negative current densities cause the electrodeposited Co to adopt a face-centered cubic (fcc) structure, which is more magnetically reversible than the hexagonally close-packed (hcp) structured Co. The coercive field is also significantly less in the fcc-electrodeposited cobalt than in the hcp. SEM images show dense, uniform Co films without any cracks or porosity. Beside the deposition current, thickness of the film was also found to affect the crystal orientation particularly on iron substrates. Diffusion of cobalt film into the iron substrate was studied under reduced environment and a fast process was observed.

36 MATERIALS SCIENCE↗

Shear localization and size-dependent strength of YCd 6 quasicrystal approximant at the micrometer length scale

Mechanical properties of materials are strongly dependent of their atomic arrangement as well as the sample dimension, particularly at the micrometer length scale. Here in this study, we investigated the small-scale mechanical properties of single-crystalline YCd 6 , which is a rational approximant of the icosahedral Y-Cd quasicrystal. In situ microcompression tests revealed that shear localization always occurs on {101} planes, but the shear direction is not constrained to any particular crystallographic directions. Furthermore, the yield strengths show the size dependence with a power law exponent of 0.4. Shear localization on {101} planes and size-dependent yield strength are explained in terms of a large interplanar spacing between {101} planes and the energetics of shear localization process, respectively. The mechanical behavior of the icosahedral Y-Cd quasicrystal is also compared to understand the influence of translational symmetry on the shear localization process in both YCd 6 and Y-Cd quasicrystal micropillars. Finally, the results of this study will provide an important insight in a fundamental understanding of shear localization process in novel complex intermetallic compounds.

36 MATERIALS SCIENCE↗

Thermodynamics and kinetics of precipitation and austenite reversion during aging of Ti-free grade 300 maraging steel manufactured by laser powder bed fusion (LPBF)

Austenite reversion and intermetallic precipitation are two key phase transformations in maraging steels which determine the strength and ductility. Usually, an optimum aging temperature/time is determined using trial and error approach with inputs from thermodynamic databases and a-posteriori microscopy/hardness evaluations. In this study, a thermo-kinetic model is developed to predict the precipitation and austenite reversion kinetics during various post-fabrication heat treatments in a Ti-free variant of grade 300 maraging steel manufactured using laser powder bed fusion. The thermo-kinetic model was based on the principles of Scheil solidification and the classical nucleation theory. The predictions from the thermo-kinetic model were verified using suitable microscopy techniques, and the results from the thermo-kinetic model agree well with the experimental measurements. Overall, results highlight the fact that an Integrated Computational Materials Engineering approach can be used to predict the precipitation and austenite reversion kinetics, and be used as an input for an efficient design of heat treatments for achieving optimum mechanical properties.

36 MATERIALS SCIENCE↗

Modeling of Thermodynamic Properties and Phase Equilibria for the Al-Sm Binary System

The thermodynamic properties and associated phase equilibria for the Al-Sm binary system are examined, and experimental results regarding the stability of the Al{sub 3}Sm, Al{sub 11}Sm{sub 3}, and Al{sub 4}Sm intermetallics are incorporated. In the analysis presented, the liquid phase is described using a three-species association model, the intermediate phases are treated as stoichiometric compounds, and the terminal phases are treated as solid solutions with a single sublattice model. In addition to the stable phases, thermodynamic descriptions of the metastable Al{sub 11}Sm{sub 3}-{alpha} and Al{sub 4}Sm-{gamma} phases are employed, and both stable and metastable phase equilibria are presented over the full composition range, providing a general model, which is consistent with available experimental data. Metastable liquidus curves are examined with respect to the observed crystallization behavior of amorphous Al-Sm alloys.

36 MATERIALS SCIENCE↗

MICROSTRUCTURE OF LONG-TERM AGED IN617 NI-BASE SUPERALLOY

The microstructure of the Ni-base superalloy IN617 that had undergone prolonged aging (approximately 65,000 hours) at a series of temperatures from 482 C to 871 C has been characterized by microhardness measurements, optical microscopy, scanning electron microscopy (SEM), and transmission electron microscopy (TEM). Cr23C6, Mo-rich eta-M6C, and Ti(C,N) constitute the major primary coarse precipitates both within the grains and along the grain boundaries. The secondary carbides were mostly fine Cr23C6, which had a cube-on-cube orientation relationship (OR) with the fcc matrix, and at long times were present in cuboidal and plate-shape forms within the grains and as films along the grain boundaries. Fine, eta-M6C carbides were also observed at low to intermediate temperatures with an OR given by [011] carbide//[011] matrix, carbide// matrix. The coarse eta-M6C carbides increased in extent at 871 C, whereas the counterpart fine carbides were absent. The phase was found to be present at all aging temperatures up to 871 C, with a volume fraction ranging from very low to approximately 5 pct at 593 C, where the peak in microhardness occurs. The observations have also suggested that the presence of a very small amount of at temperatures as high as 871 C at long times may be associated with a reaction between the fine eta-carbides and the matrix. Ultrafine precipitates of the intermetallic phase Ni2(Cr,Mo) with the Pt2Mo-type structure was observed in addition to in samples aged for 28,300 hours at the lowest aging temperature of 482 C. These precipitates were absent in samples aged at higher temperatures. The various observations made have suggested that the long-term thermal stability of the IN617 alloy is reasonably good over a wide temperature range of 538 C to 704 C, whereas at higher temperatures (871 C), the substantial decrease in the volume fraction of and coarsening and clustering of the carbides lead to a large drop in the microhardness. A modified time-temperature-transformation (TTT) diagram was constructed based on the results of this study and comparison with previous reports.

36 MATERIALS SCIENCE↗

Overview of strategies for high-temperature creep and oxidation resistance of alumina-forming austenitic stainless steels

A family of creep-resistant, alumina-forming austenitic (AFA) stainless steel alloys is under development for structural use in fossil energy conversion and combustion system applications. The AFA alloys developed to date exhibit comparable creep-rupture lives to state-of-the-art advanced austenitic alloys, and superior oxidation resistance in the {approx}923 K to 1173 K (650 C to 900 C) temperature range due to the formation of a protective Al{sub 2}O{sub 3} scale rather than the Cr{sub 2}O{sub 3} scales that form on conventional stainless steel alloys. This article overviews the alloy design approaches used to obtain high-temperature creep strength in AFA alloys via considerations of phase equilibrium from thermodynamic calculations as well as microstructure characterization. Strengthening precipitates under evaluation include MC-type carbides or intermetallic phases such as NiAl-B2, Fe{sub 2}(Mo,Nb)-Laves, Ni{sub 3}Al-L1{sub 2}, etc. in the austenitic single-phase matrix. Creep, tensile, and oxidation properties of the AFA alloys are discussed relative to compositional and microstructural factors.

36 MATERIALS SCIENCE↗

Interdiffusion and Intrinsic Diffusion in the Mg-Al System

Solid-to-solid diffusion couples were assembled and annealed to examine the diffusion between pure Mg (99.96%) and Al (99.999%). Diffusion anneals were carried out at 300 , 350 , and 400 C for 720, 360, and 240 hours, respectively. Optical and scanning electron microscopes were utilized to identify the formation of the intermetallic phases, -Al12Mg17 and -Al3Mg2 and absence of the -phase in the diffusion couples. Thicknesses of the -Al12Mg17 and -Al3Mg2 phases were measured and the parabolic growth constants were calculated to determine the activation energies for the growth, 165 and 86 KJ/mole, respectively. Concentration profiles were determined with electron microprobe analysis using pure elemental standards. Composition-dependent interdiffusion coefficients in Mg-solid solution, -Al12Mg17 and - Al3Mg2 and Al-solid solutions were calculated based on the Boltzmann-Matano analysis. Average effective interdiffusion coefficients for each phase were also calculated, and the magnitude was the highest for the -Al3Mg2 phase, followed by -Al12Mg17, Al-solid solution and Mg-solid solution. Intrinsic diffusion coefficients based on Huemann s analysis (e.g., marker plane) were determined for the ~38 at.% Mg in the -Al3Mg2 phase. Activation energies and the pre-exponential factors for the inter- and intrinsic diffusion coefficients were calculated for the temperature range examined. The -Al3Mg2 phase was found to have the lowest activation energies for growth and interdiffusion among all four phases studied. At the marker location in the -Al3Mg2 phase, the intrinsic diffusion of Al was found to be faster than that of Mg. Extrapolations of the impurity diffusion coefficients in the terminal solid solutions were made and compared to the available self- and impurity diffusion data from literature. Thermodynamic factor, tracer diffusion coefficients and atomic mobilities at the marker plane composition were approximated using available literature values of Mg activity in the -Al3Mg2 phase.

Boltzmann-Matano↗

Comparative evaluation of cast aluminum alloys for automotive cylinder heads: Part I Microstructure evolution

The present study stages a comparative evaluation of microstructure and associated mechanical and thermal response for common cast aluminum alloys that are used for manufacturing automotive cylinder heads. The systems considered are Al-Cu (206-T6), Al-Si-Cu (319-T7), and Al-Si (356-T6, A356-T6, and A356 + 0.5Cu-T6). The focus of the present manuscript is on the evaluation of microstructure at various length scales after aging, while the second manuscript will deal with the mechanical and thermal response of these alloys due to short-term (aging) and long-term (pre-conditioning) heat treatments. At the grain-scale, the Al-Cu alloy possessed an equiaxed microstructure as opposed to the dendritic structure for the Al-Si-Cu or Al-Si alloys which is related to the individual solidification conditions for these alloy systems. The composition and morphology of intermetallic precipitates within the grain and at the grain/dendritic boundary are dictated by the alloy chemistry, solidification, and heat treatment conditions. At the nanoscale, these alloys contain various metastable strengthening precipitates (GPI and θ''θ'' in Al-Cu alloy, θ'θ' in Al-Si-Cu alloy, and β'β' in Al-Si alloys) with varying size, morphology, coherency, and thermal stability.

36 MATERIALS SCIENCE↗

Phase Stability in the Fe-Rich Fe-Cr-Ni-Zr Alloys

Knowledge on phase stability in Fe-rich Fe-Cr-Ni-Zr alloys is needed for the development of Laves-phase strengthened Fe-Cr-Ni-Zr ferritic alloys which have shown promising applications as new cladding materials of nuclear reactors due to enhanced high temperature strength, and resistance to creep and irradiation hardening. Phase stability in four Fe-rich Fe-Cr-Ni-Zr alloys was carefully investigated using scanning electron microscopy, transmission electron microscopy, energy-dispersive X-ray spectroscopy and X-ray diffraction techniques. The samples were arc-melted and heat treated at 700 °C for 336 hours and 1000 °C for 1275 hours. The experimental results showed extensive solubility of Ni in the intermetallic phases Fe 23 Zr 6 and Fe 2 Zr_C15. Nickel stabilizes the Laves Fe 2 Zr_C15 structure more than the C36 and C14 structures. In addition to Fe 23 Zr 6 and Fe 2 Zr_C15, Ni 7 Zr 2 was found to be stable in samples with higher Ni content and lower annealing temperature. The body-centered-cubic, Fe 2 Zr_C15 and Fe 23 Z 6 coexist in all samples regardless of composition and temperature. Detailed analysis suggested that the coexistence of these three phases is not a result of thermodynamic equilibrium, but a result of the competing formation kinetics of Fe 2 Zr_C15 and Fe 23 Z 6 .

36 MATERIALS SCIENCE↗