Aging behavior of polymeric solar absorber materials - Part 1: Engineering plastics

In this series of two papers, various polymeric materials are investigated as to their potential applicability as absorber materials for solar thermal collectors. The focus of the investigation is to study the aging behavior of these materials under maximum operating conditions (80 C in water up to 16,000 h) and stagnation conditions (140 C in air up to 500 h) typical for northern climate. The materials supplied or produced as polymer films were first characterized in the unaged state and then for different states of aging by differential scanning calorimetry (DSC), by size exclusion chromatography (SEC) and by mechanical tensile tests. Physical aging phenomena were studied by DSC, SEC analysis provided information on chemical degradation of the materials. In addition, physical and chemical aging were both analyzed via the small and large strain mechanical behavior. While the present Part 1 of this paper series deals with the aging behavior of engineering plastics, including two amorphous polymers (a polyphenylene ether polystyrene blend (PPE + PS) and polycarbonate (PC)) and two semi-crystalline polymers (two types of polyamide 12 (PA12)), the aging behavior of so-called ''commodity'' plastics (PE and PP) is the subject of Part 2. Comparing the two aging conditions, the amorphous materials (PPE + PS and PC) turned out to be more prone to physical and chemical aging at 140 C in air. In contrast, the semi-crystalline PA12 materials were more strongly affected by exposure to water at 80 C, although to different degrees, depending on the modification. (author)

14 SOLAR ENERGY↗

Mechanical characterization of fine-grain dispersion-strengthened tungsten as a plasma facing material

Field-Assisted Sintering Technology (FAST) was used to produce fine-grained, dispersion-strengthened tungsten (W) materials. Investigated materials 4138, 4353, and 4355 composed of 3 wt% ZrC sintered at 1800 °C, 5 wt% ZrC sintered at 1800 °C, and 3 wt% ZrC sintered at 2000 °C, respectively. They were compared against ITER-grade W. A series of mechanical and thermal property testing and microstructure studies were conducted to study them as a potential plasma facing material (PFM) for fusion reactors. Hardness testing showed that manufacturing conditions substantially altered hardness. Material 4355 had an average HV10 value of 497.2 ± 16.8, slightly higher than ITER-grade at 378.5 ± 40.3. However, material 4353 was substantially higher with an HV10 value of 738.9 ± 31.7 over the investigated temperature range. Electron Backscatter Diffraction (EBSD) analysis showed that FAST produced substantially smaller grains than the hot-rolled ITER-grade W material, offering notable control over grain size. Materials 4353 and 4355 had grain sizes of 0.44 ± 0.20 µm and 3.67 ± 0.89 µm, respectively, whereas ITER-grade 27.14 ± 19.76 µm at room temperature. The fine grain structures showed no net coarsening after 1 hr. anneals up to 1800 °C, several hundred degrees above the 1100 – 1500 °C recrystallization range reported for conventional W. Inverse application of the Zener pinning relationship to the measured grain sizes indicates that these two FAST sintering conditions produce markedly different effective dispersoid populations, with effective particle diameters of approximately 90 nm at a peak sintering temperature of 1800 °C and approximately 460 nm at 2000 °C, respectively. This result demonstrates that the FAST thermal condition itself, and not the nominal ZrC content alone, governs the pinning effectiveness of the dispersion. Thermal diffusivity measurements support this finding independently. Materials of identical composition sintered at different temperatures differ by approximately 19% in measured thermal diffusivity with statistically indistinguishable density, while materials of different composition and sintering temperature converge to within approximately 2%. At a representative divertor heat flux of 10 MW/m², the lower thermal conductivity of the fine-grained materials corresponds to approximately 28 to 33 °C per millimeter of armor thickness relative to ITER-grade W, traded against a substantially larger margin to recrystallization-driven degradation. While high temperature tensile testing revealed likely contamination that motivates refinement of the manufacturing process, FAST-produced, fine-grained, dispersion-strengthened W offers process-controlled microstructural stability well above the operating temperatures of conventional W and supports its continued development as a PFM for economically viable commercial fusion power.

Parker, Gabe [ORNL] (ORCID:0000000190394100)↗

Mechanical Properties of Permanent Foaming Fixatives for Deactivation and Decommissioning Activities

DOE-EM have identified an operational requirement for a fixative that can immobilize and/or encapsulate residual contamination in 3D void volumes (pipes, gloveboxes, waste containers, etc.) during D and D activities. Failure to safely and effectively immobilize residual contamination can: Put workers at risk, Contaminate the public and environment, Drive up operational costs. Commercial-off-the-shelf (COTS) polyurethane (PU) foams is one possible solution and is currently being investigated in collaboration with Savannah River National Lab (SRNL). Mechanical property testing will dictate how well PU foams can withstand physical stressors outlined in safety documents while immobilizing residual contamination. Results can provide a performance criteria for Section 5 of ASTM E3191: Standard Specification for Permanent Foaming Fixatives Used to Mitigate Spread of Radioactive Contamination. Polyurethanes consists of repeating units of urethanes which are produced from an exothermic reaction between a polyol (an alcohol with two or more hydroxyl groups in a molecule) and an isocyanate [2]. PUs consists of 3D cells that are formed by a blowing agent which is normally water. Water interacting with the isocyanate creates carbon dioxide and urea which contributes to cells' growth and expansion. The cross-linking between the polyol and isocyanate solidify the cell faces and walls. Micro scale properties that can influence mechanical properties include: Relative density (ratio between density of cellular material and density of the solid of which the cell walls are made of). Cells connectivity between edges and faces, and number of cells contact neighbors [3]. Whether a foam is open-celled or closed-celled. Closed-celled foams have a thin membrane that encloses each cell which can contribute to the stiffness of the foam. Incorporating fillers in the PU matrix like carbon-based nanoparticles in the form of expandable graphite (EG) can increase the thermal and mechanical performance [4]. When exposed to heat, EG produces a char layer that prevents heat and oxygen transfer which is known as intumescing. Mechanical performance is dependent on amount of EG loading since the cell sizes are linearly dependent on it. Overall, the rigid foams (I-R2) proved superior. SEM Analysis: I-R2 had the most consistent spherical sizes (average cell diameter: 489 μm), which enhance the relative density the most [5]. Tensile Testing Results: I-R2 experienced the largest breaking load (103.65 lbf) and stress (289.42 psi). I-R2 also had a higher Young's Modulus compared to R1 (2.99 ksi to 2.09 ksi). Compression Testing Results: I-R2 had the highest stress at 80% deflection (360.67 psi), load (1387.48 lbf) and modulus (3.92 ksi)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Diffusion bonding titanium to stainless steel using Nb/Cu/Ni multi-interlayer

By using Nb/Cu/Ni structure as multi-interlayer, diffusion bonding titanium to austenitic stainless steel has been conducted. The effects of bonding temperature and bonding time on the interfacial microstructure were analyzed by scanning electron microscope equipped with energy dispersive spectroscope, and the joint strength was evaluated by tensile test. The results showed that Ni atoms aggregated at the Cu-Nb interface, which promoted Cu solution in Nb. This phenomenon forms a Cu-Nb solution strengthening effect. However, such effect would decay by using long bonding time that dilutes Ni atom aggregation, or be suppressed by using high bonding temperature that embrittles the Cu-Nb interface due to the formation of large grown intermetallic compounds. The sound joint was obtained by promoted parameters as 850 Degree-Sign C for 30-45 min, under which a bonding strength around 300 MPa could be obtained. - Highlights: Black-Right-Pointing-Pointer Titanium was diffusion bonded to stainless steel using Nb/Cu/Ni multi-interlayer. Black-Right-Pointing-Pointer The effects of bonding parameters on microstructure and joint strength were studied. Black-Right-Pointing-Pointer Nickel aggregation promotes Cu solution in Nb which can strengthen the joint. Black-Right-Pointing-Pointer The sound joint with strength of around 300 MPa was obtained by promoted parameters.

36 MATERIALS SCIENCE↗

Effect of Strengthening Mechanism on Strain-Rate Related Tensile Properties of Low-Carbon Sheet Steels for Automotive Application

In order to ensure crash resistance of the steels used in automotive components, the ensile deformation behavior needs to be studied and predicted not only under quasi-static condition, but also under dynamic loading rates. In the present study, tensile tests have been performed on four different automobile grade sheet steels, namely interstitial free steel, dual-phase 600 and 800, and a carbon manganese steel over the strain rate regime of 0.001-800/s. Apart from the variation in strength (which always increased with strain rate), the effect of strengthening mechanism on strain rate sensitivity and strain hardening behavior has been evaluated. Strain rate sensitivity was found to increase at high-strain rate regime for all the steels. Contribution of solid solution hardening on strain rate sensitivity at lower plastic strains was found to be higher compared to dislocation strengthening and second-phase hardening. However, precipitation hardening coupled with solid solution hardening produced the highest strain rate sensitivity, in C-Mn-440 steel at high strain rates. Different strain-rate-sensitive models which take into account the change in yield stress and strain hardening behavior with strain rate for ductile materials were used to predict the flow behavior of these sheet steels at strain rates up to 800/s.

36 MATERIALS SCIENCE↗

Modelling the graphite fracture mechanisms

In order to define a design criterion for graphite components, it is important to identify the physical phenomena responsible for the graphite fracture, to include them in a more effective modelling. In a first step, a large panel of experiments have been realised in order to build up an important database; results of tensile tests, 3 and 4 point bending tests on smooth and notched specimens have been analysed and have demonstrated an important geometry related effects on the behavior up to fracture. Then, first simulations with an elastic or an elastoplastic bilinear constitutive law have not made it possible to simulate the experimental fracture stress variations with the specimen geometry, the fracture mechanisms of the graphite being at the microstructural scale. That is the reason why a specific F.E. model of the graphite structure has been developed in which every graphite grain has been meshed independently, the crack initiation along the basal plane of the particles as well as the crack propagation and coalescence have been modelled too. This specific model has been used to test two different approaches for fracture initiation: a critical stress criterion and two criteria of fracture mechanic type. They are all based on crystallographic considerations as a global critical stress criterion gave unsatisfactory results. The criteria of fracture mechanic type being extremely unstable and unable to represent the graphite global behaviour up to the final collapse, the critical stress criterion has been preferred to predict the results of the large range of available experiments, on both smooth and notched specimens. In so doing, the experimental observations have been correctly simulated: the geometry related effects on the experimental fracture stress dispersion, the specimen volume effects on the macroscopic fracture stress and the crack propagation at a constant stress intensity factor. In addition, the parameters of the criterion have been related to experimental observations: the local crack initiation stress of 8 MPa corresponds to the non-linearity apparition on the global behavior observed experimentally and the the maximal critical stress defined for the particle of 30 MPa is equivalent to the fracture stress of notched specimens. This innovative combination of crack modelling and a local crystallographic critical stress criterion made it possible to understand that cleavage initiation and propagation in the graphite microstructure was driven by a mean critical stress criterion. (authors)

36 MATERIALS SCIENCE↗

Load partitioning between ferrite/martensite and dispersed nanoparticles of a 9Cr ferritic/martensitic (F/M) ODS steel at high temperatures

In this study, a high-energy synchrotron radiation X-ray technique was used to investigate the tensile deformation processes of a 9Cr-ODS ferritic/martensitic (F/M) steel at different temperatures. Two minor phases within the 9Cr-ODS F/M steel matrix were identified as Y2Ti2O7 and TiN by the high-energy X-ray diffraction, and confirmed by the analysis using energy dispersive X-ray spectroscopy (EDS) of scanning transmission electron microscope (STEM). The lattice strains of the matrix and particles were measured through the entire tensile deformation process. During the tensile tests, the lattice strains of the ferrite/martensite and the particles (TiN and Y2Ti2O7) showed a strong temperature dependence, decreasing with increasing temperature. Analysis of the internal stress at three temperatures showed that the load partitioning between the ferrite/martensite and the particles (TiN and Y2Ti2O7) was initiated during sample yielding and reached to a peak during sample necking. At three studied temperatures, the internal stress of minor phases (Y2Ti2O7 and TiN) was about 2 times that of F/M matrix at yielding position, while the internal stress of Y2Ti2O7 and TiN reached about 4.5-6 times and 3-3.5 times that of the F/M matrix at necking position, respectively. It indicates that the strengthening of the matrix is due to minor phases (Y2Ti2O7 and TiN), especially Y2Ti2O7 particles. Although the internal stresses of all phases decreased with increasing temperature from RT to 600 degrees C, the ratio of internal stresses of each phase at necking position stayed in a stable range (internal stresses of Y2Ti2O7 and TiN were about 4.5-6 times and 3-3.5 times of that of F/M matrix, respectively). The difference between internal stress of the F/M matrix and the applied stress at 600 degrees C is slightly lower than those at RI and 300 degrees C, indicating that the nanoparticles still have good strengthening effect at 600 degrees C. (C) 2015 Elsevier B.V. All rights reserved.

Microstructure↗

Effect of Si impurities on microstructure and tensile properties of a cast Al-Mg-Fe alloy

Al-Mg alloys are attractive for structural castings owing to their superior strength and ductility in the as-cast state. However, given the tight tolerance for impurities, Al-Mg alloys produced from secondary sources still face multiple challenges. Here, we report the effect of increased Si impurity (0.05–1.6 wt%), which is commonly found in secondary Al sources, on microstructure and tensile properties of a cast Al-4.3Mg-1.6Fe (wt%) alloy, commercially referred to as Castaduct-42 alloy. Microstructural characterization revealed that Si addition increased the volume fraction, size, and aspect ratio of primary Al13Fe4 intermetallic particles as well as the volume fraction of other binary and ternary eutectic phases. Tensile testing results demonstrated that increasing Si impurities from 0.05 to 1.6 wt% reduced ductility from 14.3 ± 1.4 % to 2.2 ± 1.0 %. A particle cracking damage accumulation model coupled with failure analysis indicated primary Al13Fe4 intermetallic particles to be the major contributing factor to the deterioration in ductility with increasing Si content. Additionally, the stabilizing effect of Si on primary Al 13 Fe 4 was inconsistent with the CALPHAD calculation results based on existing CALPHAD databases which predict a slightly decreasing primary Al13Fe4 phase fraction with increasing Si concentration. This work provides new insights into the phase stability and mechanical behavior of the lesser studied Al-Mg-Fe-Si alloy system that will contribute to the development of sustainable cast Al-Mg based alloys.

36 MATERIALS SCIENCE↗

In Situ Study on Fracture Behavior of Thick-Section Friction Stir-Welded AA 5083 Alloy

Friction stir welding (FSW) produces a gradient microstructure with distinct metallurgical zones. Here, the present study focuses on characterizing the fracture behavior during uniaxial loading across thick-section FSW joint in nonheat-treatable 5083 aluminum alloy. The hardness variation is linked to microstructural features across the weld zones through correlative microscopy. Notably, the heat-affected zone (HAZ) exhibits a lower hardness of 75 HV, while the thermomechanically affected zone (TMAZ) and stir zones (SZ) display a hardness of around 79HV. A marginal difference in hardness in HAZ prompts strain localization in HAZ on the advancing side of the weld, resulting in offset in fracture from the SZ, which is captured through in situ monitoring of the tensile test. Further, the postdeformation analysis reveals crack propagation along the maximum shear stress plane due to the coalescence of microvoids resulting from the fracturing and debonding of second-phase particles. Overall, this study provides valuable insight for optimizing the FSW process of AA 5083 alloy for thick-section applications.

36 MATERIALS SCIENCE↗

Novel Defense Mechanisms in the Armor of the Scales of the “Living Fossil” Coelacanth Fish

In this work, experiments and analysis revealing the unique defense mechanisms of the coelacanth, a lobe-finned fish termed a “living fossil”, are reported, as it was considered to be extinct until 1938, but extant for 400 million years. Additionally, this defense is provided by primitive elasmoid scales having a rare double-twisted Bouligand structure of lamellae which provides extraordinary resistance to deformation without failure. Distinct from other elasmoid scales, the collagen fibrils in the coelacanth fish scales form bundles which are embedded in a matrix comprising fibers arranged perpendicular to the layered (double-twisted Bouligand) structure that provide added rigidity and resistance to deformation. Using in situ synchrotron small-angle X-ray scattering during uniaxial tensile testing, the deformation mechanisms of the collagen are identified in terms of fibril stretching, reorientation, sliding, bending, and delamination. The unique structure of the coelacanth scales, distinct from modern elasmoid scales such as the carp, provides a variety of mechanisms to arrest cracking, making it an outstanding damage-tolerant material to resist predator attacks.

36 MATERIALS SCIENCE↗

How Water Can Affect Keratin: Hydration‐Driven Recovery of Bighorn Sheep ( Ovis Canadensis ) Horns

Abstract Keratin is one of the most common structural biopolymers exhibiting high strength, toughness, and low density. It is found in various tissues such as hairs, feathers, horns, and hooves with various functionalities. For instance, horn keratin absorbs a large amount of energy during intraspecific fights. Keratinized tissues are permanent tissues because of their basic composition consisting of dead keratinized cells that are not able to remodel or regrow once broken or damaged. The lack of a self‐healing mechanism presents a problem for horns, as they are under continued high risk from mechanical damage. In the present work, it is shown for the first time that a combination of material architecture and a water‐assisted recovery mechanism, in the horn of bighorn sheep, endows them with shape and mechanical property recoverability after being subjected to severe compressive loading. Moreover, the effect of hydration is unraveled, on the material molecular structure and mechanical behavior, by means of synchrotron wide angle X‐ray diffraction, Fourier transform infrared spectroscopy, nanoindentation, and in situ and ex situ tensile tests. The recovery and remodeling mechanism is anisotropic and quite distinct to the self‐healing of living tissue such as bones.

Huang, Wei↗

Synthesis and characterization of polyethylene/oxidized polyethylene miscible blends and role of OPE as a viscosity control

Polymer blending allows for new materials to be designed with unique properties. Here, blends of linear low density polyethylene (PE) and oxidized polyethylene (OPE) have been prepared. PE/OPE blends are characterized for their molten state properties by thermal analysis and rheology; the solid state properties are studied by scattering, diffraction, and tensile testing. Melt miscibility was confirmed by a negative Flory-Huggins interaction parameter (χ ~ -2.3) from Hoffman-Weeks plots. Additionally, a continuous decrease in melting temperature (from 123 to 119 °C) and thermal stability of blends (25% weight loss from 454 to 416 °C) was observed with increasing OPE loading from 0 to 50 wt %. Time-temperature master curves revealed the shifting of the glassy region to higher frequencies and formation of relaxed polymer chains in the glassy region. A plasticization effect was observed with zero shear viscosity of the blends decreasing with increasing OPE loading. In the end, a decrease in lamellar thickness of PE (from 180 to 140 Å) with increasing OPE resulted in increasing the blends' brittleness.

42 ENGINEERING↗

Investigation of porous polydimethylsiloxane structures with tunable properties induced by the phase separation technique

This article reports the fabrication and characterization of porous polydimethylsiloxane (PDMS) structures developed by the solvent evaporationinduced phase separation technique. Here, ternary systems containing water/ tetrahydrofuran (THF)/PDMS with various concentrations are produced to form a stable solution. The porous PDMS structures are formed by removing the solvent (THF) and nonsolvent (water) phases during the stepping heat treatment procedure. The analytical ternary phase diagram is constructed based on the thermodynamic equilibrium state in the polymer solution to explain the stable/unstable formulations and the possible composition change path. The results show that the isolated pores with the adjustable pore size ranging from 330 to 1900 μm are obtained by tuning the water to the THF ratio. The mechanical properties of the porous PDMS structures are determined by conducting the tensile tests on the prepared dog bone-shaped specimens. A wide range of elastic modulus ranging between 0.49 and 1.05 MPa was achieved without affecting the density of the porous sample by adjusting the solvent and non-solvent content in the solution. It is shown that the flexibility of the porous structures can be improved by reducing the ratio of water to THF and decreasing the PDMS content. The porosity measurements reveal that the PDMS concentration is the major phase controlling the porosity of the structure, while the effect of water/THF is negligible.

42 ENGINEERING↗

Interlaminar improvement of carbon fiber/epoxy composites via fluorine‐containing high‐epoxy‐value sizing agent

Abstract To improve the interfacial bonding effect of carbon fibers (CFs) and epoxy resins, we prepared a fluorine‐containing high‐epoxy‐value sizing agent (named TS) in this article. It is an emulsion with a more uniform particle size distribution and higher stability better than a commercial Takemoto sizing agent. In addition, sulfonic acid groups can improve the hydrophilicity of the TS, and the presence of epoxy groups enhances the wettability between CFs and the matrix. The properties of the sizing agents were examined by Fourier transform infrared spectroscopy, dynamic light scattering, and thermogravimetric analysis. The sized CFs were evaluated by scanning electron microscopy, x‐ray photoelectron spectroscopy, monofilament tensile test, and dynamic contact angle. Afterward, CF/epoxy composites were prepared, and their fracture morphology and interlaminar shear strength (ILSS) were examined. Results indicated that the TS sizing significantly increased the content of activated carbon on the surface of the CFs and improved the bonding effect between the fiber and the matrix. After TS was sized, the ILSS increased from 49.64 to 58.74 MPa, 18.34% higher than unsized CF/epoxy composites, showing the prominent interfacial reinforcement better than commercial Takemoto.

Qiu, Zhijie↗

Bio‐based glycerol plasticizers for flexible poly(vinyl chloride) blends

Abstract A series of glycerol‐based compounds were investigated for their application as plasticizers for flexible poly(vinyl chloride) (PVC) blends. The effect of plasticizer chemical structure on the performance, migration behavior, and blend morphology were evaluated and compared to blends produced using the commercial plasticizer dioctyl terephthalate (DOTP). Blends containing 40 phr (parts per hundred rubber) of glycerol‐based plasticizer showed a considerable reduction (between 54 to 86°C) in glass transition temperature ( T g ) relative to neat PVC ( T g ~ 80°C). Tensile testing of samples prepared with the glycerol analogs demonstrated higher ductility (elongation at break values of up to 97%) than DOTP (elongation at break value of 75%) at identical plasticizer loadings. The surface morphologies showed excellent incorporation of the glycerol plasticizers functionalized with alkyl chains longer than four carbons in length into the PVC matrix, whereas droplet formation was observed in blends with shorter chain glycerol derivatives. Leaching behavior of the plasticized samples were evaluated into different media and showed that plasticizers comprised of branched, or longer alkyl chains produced 2‐ to 4‐fold lower migration rates compared to those with shorter alkyl chains into polar solutions.

Halloran, Matthew W.↗

Extrusion‐Based Printing of Nanostructured Fatty Acid Gels Incorporated in Hydrogels

Soft materials with unique nanostructures such as lamellar, hexagonal, and cubic morphologies can replicate complex structures that have potential in various fields, including biomedical and industrial applications. However, a key challenge in advancing the broader applications of 3D printing for these nanostructured soft materials is insufficient mechanical properties that hinder their printability and compromise structural stability in the final product. In this study, the suitability of a fatty acid‐based lamellar gel is evaluated for direct extrusion‐based 3D printing. Here, the lamellar gel with varying water content is integrated with a photocurable hydrogel to preserve the shape and stability of the final prints. Complex 2D and 3D design patterns are used to assess extrusion behavior, structural stability, and print precision under varying pressures. Small‐angle X‐ray Scattering (SAXS) measurements reveal the formation of lamellar nanostructures and confirm their retention after photocuring in various gels. Rheological analysis confirms that these gels exhibit key properties suitable for extrusion‐based 3D printing, such as shear‐thinning behavior. Additionally, tensile testing is conducted to evaluate the mechanical properties across cured print samples. This study underscores the potential of nanostructured gels as a robust and versatile platform, facilitating the development of materials engineered for various applications.

36 MATERIALS SCIENCE↗

Influence of Air and Ethanol Dehydration on Structure, Behavior, and Function of Type I Collagen Scaffolds

Ethanol dehydration is a common step in both scaffold manufacturing and tissue processing, yet the influence of ethanol on collagen is not well understood. This study examined the effects of dehydration, via ethanol treatment and air drying, on collagen structure, behavior, mechanics, and rehydration capacity. Multiple material characterization methods were used including Fourier Transform infrared spectroscopy (FTIR), Raman spectroscopy, scanning electron microscopy, thermogravimetric analysis, small/medium angle x‐ray scattering, volumetric swelling analysis, and tensile testing. Ethanol dehydration removed bulk water from scaffolds, making them stronger and stiffer, but also showed loss of molecular water. This molecular water appears to act as a collagen stabilizer, resulting in less thermally stable scaffolds. The loss of molecular water is also evident in the molecular d‐spacing. Secondary structure of scaffolds was also altered by ethanol, resulting in significantly enhanced rehydration capacity. Bulk water, both before and after rehydration, largely determined mechanical properties, which did not correlate with other structural measures such as FTIR. While rehydration largely returned collagen spacing to pre‐ethanol treated state, structural alterations seen in FTIR cannot be recovered. These results have implications for not only collagen scaffolds, but in many tissue engineering and processing applications.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Dimorphic Mechanisms of Fragility in Diabetes Mellitus: the Role of Reduced Collagen Fibril Deformation

ABSTRACT Diabetes mellitus (DM) is an emerging metabolic disease, and the management of diabetic bone disease poses a serious challenge worldwide. Understanding the underlying mechanisms leading to high fracture risk in DM is hence of particular interest and urgently needed to allow for diagnosis and treatment optimization. In a case–control postmortem study, the whole 12th thoracic vertebra and cortical bone from the mid-diaphysis of the femur from male individuals with type 1 diabetes mellitus (T1DM) (n = 6; 61.3 ± 14.6 years), type 2 diabetes mellitus (T2DM) (n = 11; 74.3 ± 7.9 years), and nondiabetic controls (n = 18; 69.3 ± 11.5) were analyzed with clinical and ex situ imaging techniques to explore various bone quality indices. Cortical collagen fibril deformation was measured in a synchrotron setup to assess changes at the nanoscale during tensile testing until failure. In addition, matrix composition was analyzed including determination of cross-linking and non-crosslinking advanced glycation end-products like pentosidine and carboxymethyl-lysine. In T1DM, lower fibril deformation was accompanied by lower mineralization and more mature crystalline apatite. In T2DM, lower fibril deformation concurred with a lower elastic modulus and tendency to higher accumulation of non-crosslinking advanced glycation end-products. The observed lower collagen fibril deformation in diabetic bone may be linked to altered patterns mineral characteristics in T1DM and higher advanced glycation end-product accumulation in T2DM. © 2022 The Authors. Journal of Bone and Mineral Research published by Wiley Periodicals LLC on behalf of American Society for Bone and Mineral Research (ASBMR).

59 BASIC BIOLOGICAL SCIENCES↗