Magnetic and magnetocaloric properties of La{sub 0.85}(Na{sub 1−x}K{sub x}){sub 0.15}MnO{sub 3} ceramics produced by reactive spark plasma sintering
La{sub 0.85}(Na{sub 1−x}K{sub x}){sub 0.15}MnO{sub 3} (0 ≤ x ≤ 1) ceramics were synthesized from the raw La(OH){sub 3}, NaOH, KOH, and MnO{sub 2} powders using Reactive Spark Plasma Sintering. All the compounds were obtained as pure, dense, and ultrafine grained pellets. The Rietveld refinement of the X-Ray powder diffraction shows that all our synthesized samples are single phase and crystallize in the distorted rhombohedral system with R-3c space group. The thermal variation of their magnetization under a magnetic applied field of 50 mT shows a paramagnetic to ferromagnetic transition at a Curie temperature very close to room temperature. The magnetic entropy change, deduced from magnetization measurements versus magnetic applied field up to 5 T at several temperatures exhibits a maximum |ΔS{sub M}|{sub max} which slightly increases with increasing K content. The relative cooling power values, inferred from the |ΔS{sub M}| vs T peak broadening, vary slightly with the potassium content, reaching, values between 316 and 289 Jkg{sup −1}, in an applied magnetic field of 5 T, when x increases from 0 to 1. Technically, these large values make the prepared materials very promising for domestic magnetic refrigeration.