At least 1,135 records · Page 63

Magnetic Properties of MFeCrO{sub 4} (M = Co/Ni) Prepared by Solution Combustion Method

Single phase MFeCrO{sub 4} (M = Co/Ni) nanosized samples are prepared by solution combustion method using glycine as fuel. Lattice parameter obtained after Rietveld refinement of the powder x-ray diffraction pattern of CoCrFeO{sub 4} and NiCrFeO{sub 4} samples are 8.374 and 8.325 Å and corresponding crystallite sizes are 40 and 27 nm, respectively. FTIR spectra of both samples show tetrahedral and octahedral metal oxygen bond stretching peaks at 596 and 488 cm{sup −1}, indicating spinel phase formation. DC magnetisation study indicates that both samples are ferrimagnetic at room temperature, with CoCrFeO{sub 4} having a higher value of saturation magnetisation. Mössbauer spectra indicate the presence of magnetic relaxation in the samples. Also, the strength of interaction with nearest neighbour Fe{sup 3+} cations is higher in NiCrFeO{sub 4}.

36 MATERIALS SCIENCE↗

Influence of the B-site ordering on the magnetic properties of the new La{sub 3}Co{sub 2}MO{sub 9} double perovskites with M = Nb or Ta

Double perovskites La{sub 3}Co{sub 2}NbO{sub 9} and La{sub 3}Co{sub 2}TaO{sub 9} have been prepared by both solid state and sol-gel synthesis. The crystal structures have been studied from X-ray and neutron powder diffraction data. Rietveld refinements show that the crystal structure is monoclinic (P2{sub 1}/n), with different degrees of ordering of B' and B'' cations, with octahedra tilted according to the Glazer notation a{sup -}b{sup -}c{sup +}. Occupancy refinements show that the solid state materials are more B-site ordered than the sol-gel ones. Magnetization measurements show that these perovskites show two magnetic contributions, one with spontaneous magnetization and other with linear behaviour with the magnetic field associated to antiferromagnetic correlations. In the samples synthesized by solid state the spontaneous magnetization is more important than those synthesized by the sol-gel and present T{sub C} of 62 K for Nb and 72 K for Ta. On the other hand, materials prepared by sol-gel have T{sub C} 20 K for Nb and 40 K for Ta, respectively and major presence of the antiferromagnetic contribution. The competition between these magnetic behaviours is interpreted, by a microscopic point of view, as to be due to the different degrees of Co{sup 2+} ions disorder on the B site of the double perovskite structure. This disorder affects the ratio between the antiferromagnetic Co{sup 2+}-O-Co{sup 2+} and the ferromagnetic Co{sup 2+}-O-M{sup 5+}-O-Co{sup 2+} couplings proposed for the system.

36 MATERIALS SCIENCE↗

Nonstoichiometry, point defects and magnetic properties in Sr{sub 2}FeMoO{sub 6-{delta}} double perovskites

The phase stability, nonstoichiometry and point defect chemistry of polycrystalline Sr{sub 2}FeMoO{sub 6-{delta}} (SFMO) was studied by thermogravimety at 1000, 1100, and 1200 Degree-Sign C. Single-phase SFMO exists between -10.2{<=}log pO{sub 2}{<=}-13.7 at 1200 Degree-Sign C. At lower oxygen partial pressure a mass loss signals reductive decomposition. At higher pO{sub 2} a mass gain indicates oxidative decomposition into SrMoO{sub 4} and SrFeO{sub 3-x}. The nonstoichiometry {delta} at 1000, 1100, and 1200 Degree-Sign C was determined as function of pO{sub 2}. SFMO is almost stoichiometric at the upper phase boundary (e.g. {delta}=0.006 at 1200 Degree-Sign C and log pO{sub 2}=-10.2) and becomes more defective with decreasing oxygen partial pressure (e.g. {delta}=0.085 at 1200 Degree-Sign C and log pO{sub 2}=-13.5). Oxygen vacancies are shown to represent majority defects. From the temperature dependence of the oxygen vacancy concentration the defect formation enthalpy was estimated ({Delta}H{sub OV}=253{+-}8 kJ/mol). Samples of different nonstoichiometry {delta} were prepared by quenching from 1200 Degree-Sign C at various pO{sub 2}. An increase of the unit cell volume with increasing defect concentration {delta} was found. The saturation magnetization is reduced with increasing nonstoichiometry {delta}. This demonstrates that in addition to Fe/Mo site disorder, oxygen nonstoichiometry is another source of reduced magnetization values. - Graphical abstract: Nonstoichiometry {delta} of Sr{sub 2}FeMoO{sub 6-{delta}} as function of oxygen partial pressure at 1000, 1100, and 1200 Degree-Sign C. Highlights: Black-Right-Pointing-Pointer Sr{sub 2}FeMoO{sub 6-{delta}} is stable at T=1200 Degree-Sign C at low pO{sub 2} only. Black-Right-Pointing-Pointer Nonstoichiometry {delta} measured at 1200, 1100, and 1000 Degree-Sign C. Black-Right-Pointing-Pointer Increase of oxygen vacancy concentration with lower pO{sub 2}. Black-Right-Pointing-Pointer Reduction of magnetization with increasing nonstoichiometry {delta}.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Preparation and magnetic properties of spindle porous iron nanoparticles

Spindle porous iron nanoparticles were firstly synthesized by reducing the pre-synthesized hematite ({alpha}-Fe{sub 2}O{sub 3}) spindle particles with hydrogen gas. The products were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), X-ray photoelectron spectroscopy (XPS), nitrogen adsorption/desorption isotherms and vibrating sample magnetometry (VSM). A lattice shrinkage mechanism was employed to explain the formation process of the porous structure, and the adsorbed phosphate was proposed as a protective shell in the reduction process. N{sub 2} adsorption/desorption result showed a Brunauer-Emmett-Teller (BET) surface area of 29.7 m{sup 2}/g and a continuous pore size distribution from 2 nm to 100 nm. The magnetic hysteresis loop of the synthesized iron particles showed a saturation magnetization of 84.65 emu/g and a coercivity of 442.36 Oe at room temperature.

36 MATERIALS SCIENCE↗

Structural, Optical and Magnetic Properties of PANI/Se{sub 0.95}Fe{sub 0.05} Nanocomposites

Polyaniline (PANI) coupled with Se{sub 0.95}Fe{sub 0.05} in various weight percentage (5 and 10 wt%) were formed by in situ polymerization method of PANI in the presence of Se{sub 0.95}Fe{sub 0.05}. The functionality of the investigated nanocomposites was investigated by X-ray diffraction (XRD), Fourier transform infrared (FTIR), vibrating sample magnetometer (VSM), and photoluminescence (PL) analyses. The structural characteristics of PANI and the existence of Se{sub 0.95}Fe{sub 0.05} together with PANI were confirmed using XRD. The different functional groups of nanocomposite were studied using FTIR. PANI/Se{sub 0.95}Fe{sub 0.05} nanocomposites exhibited a weak ferromagnetic behavior. Law of Approach to saturation was used to determine the saturation magnetization of nanocomposites samples. The PL of PANI and nanocomposites emitted five emissions in violet and blue ranges. The PL intensity of the emission peaks is significantly reduced when Se{sub 0.95}Fe{sub 0.05} is introduced to PANI matrix.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Crystal structure and magnetic properties of Li,Cr-containing molybdates Li{sub 3}Cr(MoO{sub 4}){sub 3}, LiCr(MoO{sub 4}){sub 2} and Li{sub 1.8}Cr{sub 1.2}(MoO{sub 4}){sub 3}

Single crystals of LiCr(MoO{sub 4}){sub 2}, Li{sub 3}Cr(MoO{sub 4}){sub 3} and Li{sub 1.8}Cr{sub 1.2}(MoO{sub 4}){sub 3} were grown by a flux method during the phase study of the Li{sub 2}MoO{sub 4}-Cr{sub 2}(MoO{sub 4}){sub 3} system at 1023 K. LiCr(MoO{sub 4}){sub 2} and Li{sub 3}Cr(MoO{sub 4}){sub 3} single phases were synthesized by solid-state reactions. Li{sub 3}Cr(MoO{sub 4}){sub 3} adopts the same structure type as Li{sub 3}In(MoO{sub 4}){sub 3} despite the difference in ionic radii of Cr{sup 3+} and In{sup 3+} for octahedral coordination. Li{sub 3}Cr(MoO{sub 4}){sub 3} is paramagnetic down to 7 K and shows a weak ferromagnetic component below this temperature. LiCr(MoO{sub 4}){sub 2} is isostructural with LiAl(MoO{sub 4}){sub 2} and orders antiferromagnetically below 20 K. The magnetic structure of LiCr(MoO{sub 4}){sub 2} was determined from low-temperature neutron diffraction and is based on the propagation vektor k{sup -}>=(1/2 ,1/2 ,0). The ordered magnetic moments were refined to 2.3(1) mu{sub B} per Cr-ion with an easy axis close to the [1 1 1-bar] direction. A magnetic moment of 4.37(3) mu{sub B} per Cr-ion was calculated from the Curie constant for the paramagnetic region. The crystal structures of the hitherto unknown Li{sub 1.8}Cr{sub 1.2}(MoO{sub 4}){sub 3} and LiCr(MoO{sub 4}){sub 2} are compared and reveal a high degree of similarity: In both structures MoO{sub 4}-tetrahedra are isolated from each other and connected with CrO{sub 6} and LiO{sub 5} via corners. In both modifications there are Cr{sub 2}O{sub 10} fragments of edge-sharing CrO{sub 6}-octahedra. - Graphical abstract: Magnetic structure of LiCr(MoO{sub 4}){sub 2}. The orientation of the magnetic moments of Cr{sup 3+} are shown by arrows.

36 MATERIALS SCIENCE↗

Aurivillius phases of PbBi{sub 4}Ti{sub 4}O{sub 15} doped with Mn{sup 3+} synthesized by molten salt technique: Structure, dielectric, and magnetic properties

Doping of manganese (Mn{sup 3+}/Mn{sup 4+}) into the Aurivillius phase Pb{sub 1-x}Bi{sub 4+x}Ti{sub 4-x}Mn{sub x}O{sub 15} was carried out using the molten salt technique for various Mn concentrations (x=0, 0.2, 0.4, 0.6, 0.8, and 1). Single phase samples could be obtained in the composition range with x up to 0.6 as confirmed by X-ray and neutron diffraction analysis. Dielectric measurements show a peak at 801, 803, 813 and 850 K for samples with x=0, 0.2, 0.4, and 0.6, respectively, related to the ferroelectric transition temperature (T{sub c}). The main contribution of the in-plane polarization for x{<=}0.2 which was calculated from the atomic positions obtained by the structure analysis is the dipole moment in the Ti(1)O{sub 6} layer; however, for x{>=}0.4 the polarization originates from the dipole moment in the Ti(2)O{sub 6} layer. Mn doping in the Pb{sub 1-x}Bi{sub 4+x}Ti{sub 4-x}Mn{sub x}O{sub 15} does not show any long range magnetic ordering. -- Graphical abstract: The dipole moment of TiO{sub 6} dependence of x in Pb{sub 1-x}Bi{sub 4+x}Ti{sub 4-x}Mn{sub x}O{sub 15} (0{<=}x{<=}0.6): (a) along a-axis and (b) on the ab plane. This figure indicated that polarization in the ab-plane contribute to the total polarization. Display Omitted Highlights: {yields} We have prepared Pb{sub 1-x}Bi{sub 4+x}Ti{sub 4-x}Mn{sub x}O{sub 15}, 0{<=}x{<=}1 by the molten-salt method. {yields} The oxides adopted A2{sub 1}am space group. {yields} Dipole moments of the inner Ti(1)O{sub 6} are the main polarization contributor for x{<=}0.2. {yields} Dipole moments of the outer Ti(2)O{sub 6} are the main polarization contributor for x>0.2. {yields} Ferromagnetic interactions show the contribution of mixed valence of Mn{sup 3+}/Mn{sup 4+}.

36 MATERIALS SCIENCE↗

Structural and ambient/sub-ambient temperature magnetic properties of Er-substituted cobalt-ferrites synthesized by sol-gel assisted auto-combustion method

Er-substituted cobalt-ferrites CoFe{sub 2−x}Er{sub x}O{sub 4} (0 ≤ x ≤ 0.04) were synthesized by sol-gel assisted auto-combustion method. The precursor powders were calcined at 673–873 K for 4 h, subsequently pressed into pellets and sintered at 1273 K for 4 h. X-ray diffraction (XRD) confirmed the presence of the spinel phase for all the compositions and, additional orthoferrite phase for higher compositions (x = 0.03 and 0.04). The XRD spectra and the Transmission Electron Microscopy micrographs indicate that the nanocrystalline particulates of the Er-substituted cobalt ferrites have crystallite size of ∼120–200 nm. The magnetization curves show an increase in saturation magnetization (M{sub S}) and coercivity (H{sub C}) for Er-substituted cobalt-ferrites at sub-ambient temperatures. M{sub S} for CoFe{sub 2}O{sub 4}, CoFe{sub 0.99}Er{sub 0.01}O{sub 4}, CoFe{sub 0.98}Er{sub 0.02}O{sub 4}, and CoFe{sub 0.97}Er{sub 0.03}O{sub 4} peak at 89.7 Am{sup 2}/kg, 89.3 Am{sup 2}/kg, 88.8 Am{sup 2}/kg, and 87.1 Am{sup 2}/kg, respectively, at a sub-ambient temperature of ∼150 K. H{sub C} substantially increases with decrease in temperature for all the compositions, while it peaks at x = 0.01−0.02 at all temperatures. The combination of Er content—x ∼ 0.02 and the temperature—∼5 K provides the maximum H{sub C} ∼ 984 kA/m. Er-substituted cobalt-ferrites have higher cubic anisotropy constant, K{sub 1}, compared to pure cobalt-ferrite at ambient/sub-ambient temperatures. K{sub 1} gradually increases for all compositions in the temperature decreasing from 300 to 100 K. While K{sub 1} peaks at ∼150 K for pure cobalt-ferrite, it peaks at ∼50 K for CoFe{sub 0.99}Er{sub 0.01}O{sub 4}, CoFe{sub 0.98}Er{sub 0.02}O{sub 4}, and CoFe{sub 0.96}Er{sub 0.04}O{sub 4}. The M{sub S} (∼88.7 Am{sup 2}/kg), at 5 K, for Er substituted cobalt-ferrite is close to the highest values reported for Sm and Gd substituted cobalt-ferrites. The M{sub S} (∼83.5 Am{sup 2}/kg) at 300 K for Er-substituted cobalt-ferrite is the highest among the lanthanide series element substituted cobalt-ferrites. The H{sub C} (at 5 K) for Er substituted cobalt-ferrite is close to the highest values observed for La, Ce, Nd, Sm, and Gd substituted cobalt-ferrites.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Crystal structure and magnetic properties of the Cr-doped spiral antiferromagnet BiMnFe{sub 2}O{sub 6}

Graphical abstract: - Highlights: • The substitution of Cr for Mn in BiMnFe{sub 2}O{sub 6} is possible by the solution–gel method. • The BiCr{sub x}Mn{sub 1−x}Fe{sub 2}O{sub 6} solid solution is obtained for the x values up to 0.3. • Increasing Cr content lowers the temperature of the antiferromagnetic ordering. - Abstract: We report the Cr{sup 3+} for Mn{sup 3+} substitution in the BiMnFe{sub 2}O{sub 6} structure. The BiCr{sub x}Mn{sub 1−x}Fe{sub 2}O{sub 6} solid solution is obtained by the solution–gel synthesis technique for the x values up to 0.3. The crystal structure investigation using a combination of X-ray powder diffraction and transmission electron microscopy demonstrates that the compounds retain the parent BiMnFe{sub 2}O{sub 6} structure (for x = 0.3, a = 5.02010(6)Å, b = 7.06594(7)Å, c = 12.6174(1)Å, S.G. Pbcm, R{sub I} = 0.036, R{sub P} = 0.011) with only a slight decrease in the cell parameters associated with the Cr{sup 3+} for Mn{sup 3+} substitution. Magnetic susceptibility measurements suggest strong similarities in the magnetic behavior of BiCr{sub x}Mn{sub 1−x}Fe{sub 2}O{sub 6} (x = 0.2; 0.3) and parent BiMnFe{sub 2}O{sub 6}. Only T{sub N} slightly decreases upon Cr doping that indicates a very subtle influence of Cr{sup 3+} cations on the magnetic properties at the available substitution rates.

36 MATERIALS SCIENCE↗

EuTZn (T=Pd, Pt, Au) with TiNiSi-type structure-Magnetic properties and {sup 151}Eu Moessbauer spectroscopy

The europium compounds EuTZn (T=Pd, Pt, Au) were synthesized from the elements in sealed tantalum tubes in an induction furnace. These intermetallics crystallize with the orthorhombic TiNiSi-type structure, space group Pnma. The structures were investigated by X-ray diffraction on powders and single crystals: a=732.3(2), b=448.5(2), c=787.7(2) pm, R{sub 1}/wR{sub 2}=0.0400/0.0594, 565 F{sup 2} values for EuPdZn, a=727.8(3), b=443.7(1), c=781.7(3) pm, R{sub 1}/wR{sub 2}=0.0605/0.0866, 573 F{sup 2} values for EuPtZn, and a=747.4(2), b=465.8(2), c=789.1(4) pm, R{sub 1}/wR{sub 2}=0.0351/0.0590, 658 F{sup 2} values for EuAuZn, with 20 variables per refinement. Together the T and zinc atoms build up three-dimensional [TZn] networks with short T-Zn distances. The EuTZn compounds show Curie-Weiss behavior in the temperature range from 75 to 300 K with mu{sub eff}=7.97(1), 7.70(1), and 7.94(1) mu{sub B}/Eu atom and theta{sub P}=18.6(1), 34.9(1), and 55.5(1) K for T=Pd, Pt, and Au, respectively, indicating divalent europium. Antiferromagntic ordering was detected at 15.1(3) K for EuPdZn and canted ferromagnetic ordering at 21.2(3) and 51.1(3) K for EuPtZn and EuAuZn. {sup 151}Eu Moessbauer spectroscopic measurements confirm the divalent nature of the europium atoms by isomer shift values ranging from -8.22(8) (EuPtZn) to -9.23(2) mm/s (EuAuZn). At 4.2 K full magnetic hyperfine field splitting is observed in all three compounds due to magnetic ordering of the europium magnetic moments. - Graphical abstract: Europium coordination in EuPdZn, EuPtZn, and EuAuZn.

36 MATERIALS SCIENCE↗

Pure dipolar-interacted CoFe{sub 2}O{sub 4} nanoparticles and their magnetic properties

Graphical abstract: The mono-dispersed CoFe{sub 2}O{sub 4} nanoparticles with the uniform size of 10.5 ± 2 nm were first synthesized and then they were embedded in amorphous SiO{sub 2} matrix with different CoFe{sub 2}O{sub 4} nanoparticles’ concentrations. The large coercivity (3056 Oe) and the remanence ratio (0.63) were obtained by suitably diluting CoFe{sub 2}O{sub 4} nanoparticles into the SiO{sub 2} matrix. The reciprocal of the absolute maximum of δm and the M{sub r}/M{sub s} ratio behave in the same trend (as shown in (e)), indicating that the M{sub r}/M{sub s} ratio was dominated by the interparticle dipolar interaction. The present work is meaningful for revealing the underlying mechanism in nano-scaled magnetic system and improving the magnetic performance. - Highlights: • The mono-dispersed CoFe{sub 2}O{sub 4} nanoparticles with the uniform size of 10.5 ± 2 nm were synthesized by the thermal decomposition of metals acetylacetonates in solvents with high boiling point. • The large coercivity (3056 Oe) and the remanence ratio (0.63) were obtained by diluting CoFe{sub 2}O{sub 4} nanoparticles into the SiO{sub 2} matrix with a suitable concentration. • The surface anisotropy and interparticle dipolar interaction affect the magnetic performance and magnetic ordering state. • It was observed that the M{sub r}/M{sub s} ratio was dominated by the interparticle dipolar interaction. - Abstract: The mono-dispersed and uniform CoFe{sub 2}O{sub 4} nanoparticles were synthesized by the thermal decomposition of Fe(acac){sub 3} and Co(acac){sub 2}. Then the CoFe{sub 2}O{sub 4} nanoparticles were diluted in amorphous SiO{sub 2} matrix with different CoFe{sub 2}O{sub 4} nanoparticles’ concentrations. All samples show the positive or negative exchange bias behavior, indicating the presence of canted spin layer at the CoFe{sub 2}O{sub 4} nanoparticles’ surface. The large effective anisotropy constant (3.38 × 10{sup 6} erg/cm{sup 3}) was observed, which can be attributed to the induced surface anisotropy by the canted surface spins. The reduced magnetization (M{sub r}/M{sub s}) was dominated by the interparticle dipolar interaction while the coercivity (H{sub c}) was determined by the synergistic effects of the surface anisotropy, interparticle dipolar interaction and interface effect. By suitably diluting CoFe{sub 2}O{sub 4} in the SiO{sub 2} matrix, the high H{sub c} (3056 Oe) and the M{sub r}/M{sub s} (0.63) can be obtained, which is larger than most of those reported before. The present work is meaningful for revealing the underlying mechanism in nano-scaled magnetic system and improving the magnetic performance.

36 MATERIALS SCIENCE↗

Effect of Zn-doping on structural and magnetic properties of copper ferrite nanoparticles

The nanoparticles of CuFe{sub 2}O{sub 4} (CF) and Cu{sub 0.8}Zn{sub 0.2}Fe{sub 2}O{sub 4} (CZF) were synthesized using co-precipitation method to study the effect of Zn doping in Cu-ferrite. The X-ray diffraction (XRD) patterns were well fitted with two-phase structure using Rietveld analysis as Fd-3 m space group (spinel system) and C12/c1 space group (monoclinic system CuO-phase). The average crystallite size of the CF and CZF nanoparticles for spinel structure are 6 and 7 nm respectively. The spinel phase fraction is increased from 56% to 71% with Zn-doping of 20% in CF. The transmission electron micrograph analysis showed the narrow size distribution for CZF nanoparticles. The magnetization plots as a function of magnetic field (M (H)) of CF and CZF nanoparticles indicate superparamagnetic behavior. The magnetization is increased with Zn-doping in CF. The stable spinel Cu-ferrite can be obtained with Zn-doping in CF.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Crystal structure and magnetic properties of novel Hf{sub 3}Ni{sub 2}Si{sub 3}-type R{sub 3}Co{sub 2}Ge{sub 3} compounds (R=Y, Sm, Tb-Tm)

The novel R{sub 3}Co{sub 2}Ge{sub 3} compounds with R=Y, Sm, Tb-Tm adopt the Hf{sub 3}Ni{sub 2}Si{sub 3}-type structure (ordered variant of the Ca{sub 3}Ga{sub 5}-type one, space group Cmcm). Sm{sub 3}Co{sub 2}Ge{sub 3}, Tb{sub 3}Co{sub 2}Ge{sub 3}, Ho{sub 3}Co{sub 2}Ge{sub 3} and Er{sub 3}Co{sub 2}Ge{sub 3} undergo an antiferromagnetic-type ordering and Tb{sub 3}Co{sub 2}Ge{sub 3} demonstrates a field-sensitive magnetic behavior. Tm{sub 3}Co{sub 2}Ge{sub 3} is a pure paramagnet down to 5 K, whereas Y{sub 3}Co{sub 2}Ge{sub 3} demonstrates Pauli paramagnetism down to {approx}120 K. In zero applied field and between {approx}50 and {approx}15 K Tb{sub 3}Co{sub 2}Ge{sub 3} shows a non-collinear antiferromagnetic ordering with wave vectors K{sub 0}=[0, 0, 0] and K{sub 1}=[{+-}1/3, 0, 0] and a magnetic unit cell 3a{sub Tb{sub 3Co{sub 2Ge{sub 2}}}} Multiplication-Sign b{sub Tb{sub 3Co{sub 2Ge{sub 3}}}} Multiplication-Sign c{sub Tb{sub 3Co{sub 2Ge{sub 3}}}} , whereas below {approx}15 K it exhibits a complex antiferromagnetic ordering with K{sub 0}=[0, 0, 0], K{sub 1}=[{+-}1/3, 0, 0] and K{sub 2}=[1/2, 0, 0] wave vectors and magnetic unit cell 6a{sub Tb{sub 3Co{sub 2Ge{sub 2}}}} Multiplication-Sign b{sub Tb{sub 3Co{sub 2Ge{sub 2}}}} Multiplication-Sign c{sub Tb{sub 3Co{sub 2Ge{sub 2}}}}. - Graphical abstract: The Hf{sub 3}Ni{sub 2}Si{sub 3}-type {l_brace}Y, Sm, Gd-Tm{r_brace}{sub 3}Co{sub 2}Ge{sub 3} (space group Cmcm) demonstrate complex field sensitive antiferromagnetic ordering. The rare earth sublattice of 4d site plays crucial role in the magnetisation of R{sub 3}Co{sub 2}Ge{sub 3} compounds. Highlights: Black-Right-Pointing-Pointer The {l_brace}Y, Sm, Gd-Tm{r_brace}{sub 3}Co{sub 2}Ge{sub 3} adopts the Hf{sub 3}Ni{sub 2}Si{sub 3}-type structure (space group Cmcm). Black-Right-Pointing-Pointer They demonstrate complex field sensitive antiferromagnetic ordering. Black-Right-Pointing-Pointer The 4d site rare earth sublattice plays crucial role in the magnetism of R{sub 3}Co{sub 2}Ge{sub 3}.

36 MATERIALS SCIENCE↗

Synthesis, crystal and electronic structures and magnetic properties of Li{sub 2}SnMo{sub 3}O{sub 8}: A novel reduced molybdenum oxide containing Mo{sub 3}O{sub 13} cluster units

Powder samples and single crystals of the quaternary oxide Li{sub 2}SnMo{sub 3}O{sub 8} were obtained by solid state reaction. The structure was determined by single-crystal X-ray diffraction. Li{sub 2}SnMo{sub 3}O{sub 8} crystallizes in the hexagonal space group P6{sub 3}mc with unit-cell parameters a=5.7720 (2) Å, c=10.3941 (3) Å and Z=2. Full-matrix least-squares refinement on F{sup 2} using 930 independent reflections for 31 refinable parameters results in R{sub 1}=0.0354 and wR{sub 2}=0.0643. The crystal structure consists of distorted hexagonal-close-packed oxygen layers with stacking sequence abac along [0 0 1] and that are held together by alternating lithium-tin and molybdenum layers. The Li{sup +} and Sn{sup 4+} ions occupy, respectively, tetrahedral and octahedral sites in the ratio 2:1. The Mo atoms occupy octahedral sites and form strongly bonded triangular clusters involving three MoO{sub 6} octahedra that are each shared along two edges, constituting a Mo{sub 3}O{sub 13} unit. Magnetic susceptibility measurements are in agreement with a spin-pairing of the eight d electrons per Mo{sub 3} cluster. The electronic structure of Li{sub 2}SnMo{sub 3}O{sub 8} is analyzed using periodic density functional calculations. - Graphical abstract: We present here the synthesis, the crystal and electronic structures, and the magnetic properties of the new quaternary compound containing Mo{sub 3}O{sub 13} units, Li{sub 2}SnMo{sub 3}O{sub 8}. - Highlights: • The new quaternary reduced molybdenum oxide containing Mo{sub 3} clusters, Li{sub 2}SnMo{sub 3}O{sub 8}, was synthesized by solid state reaction. • Eight electrons per Mo{sub 3} cluster. • Single-crystal X-ray study. • Magnetic susceptibility measurements. • Periodic density functional calculations.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Impedance Spectroscopy and Magnetic Property of Y{sub 3}Fe{sub 5}O{sub 12}

A high-temperature solid-state reaction technique was used for the preparation of the polycrystalline sample of Y{sub 3}Fe{sub 5}O{sub 12} Structural and microstructural analyses exhibited a single-phase formation of the compound with a uniform distribution of grains throughout the surface of the sample. Detailed study on impedance spectroscopy was carried out in a wide range of frequency (10{sup 2}-10{sup 6} Hz) and temperatures (30-500 deg. C). A dielectric anomaly observed at 282 deg. C assumed to be related to the magnetoelectric response of the material. The grain and grain boundary contributions are observed from complex impedance spectrum at high temperatures ({>=}150 deg. C) by the appearance of two semicircular arcs. Study of magnetization using VSM shows that the saturation magnetization of sample at room temperature is found to be 22.8 emu/gm at room temperature.

36 MATERIALS SCIENCE↗

Magnetic properties of CuFe{sub 1−x}Cr{sub x}O{sub 2} nanoparticles surrounded by amorphous SiO{sub 2}

CuFe{sub 1−x}Cr{sub x}O{sub 2} (0 ≤ x ≤ 1.0) nanoparticles surrounded by amorphous SiO{sub 2} with an average diameter of 30–50 nm were synthesized using a wet chemical method. The annealing temperatures were controlled to yield various sizes of single-phase CuFe{sub 1−x}Cr{sub x}O{sub 2} nanoparticles. CuFeO{sub 2} bulk crystal is known to have a multiferroic delafossite structure with two Néel temperatures of 11 and 14 K; however, the transition temperature shifted higher as the Cr–ion doping level increased. In addition, the lattice constants decreased in accordance with increased Cr-ion doping, which was confirmed by X-ray diffraction measurements. The magnetization curves showed weak ferromagnetic behavior and no coercivity was observed. Hence, frustration in the triangular lattice of the delafossite structure can be released by Cr–ion doping and higher magnetization can be expected. A fine structure analysis through X-ray absorption fine structure measurements was also conducted. It was found that the structure of the Cu ion is similar to that of Cu{sub 2}O, and the c axis of the CuFe{sub 1−x}Cr{sub x}O{sub 2} should be shortened by the Cr–ion doping.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structural and magnetic properties of La{sub 1−x}Ce{sub x}Fe{sub 1−x}Cr{sub x}O{sub 3} orthoferrite prepared by co-precipitation method

Graphical abstract: TEM micrographs of La{sub 1−x}Ce{sub x}Fe{sub 1−x}Cr{sub x}O{sub 3} for x = 0.0. - Highlights: • The composition of La{sub 1−x}Ce{sub x}Fe{sub 1−x} Cr{sub x}O{sub 3} was prepared by co-precipitation method. • X-ray diffraction showed orthorhombic structure with space group Pnma. • With increasing Ce and Cr content, a decrease of the unit cell volume. • Enhancement in the coercivity (H{sub c}) with increasing Ce and Cr content. • Reduction of M{sub s} and M{sub r} up to x = 0.15 and increases with further increases of x. - Abstract: Nanocrystalline orthoferrites with the composition of La{sub 1−x}Ce{sub x}Fe{sub 1−x} Cr{sub x}O{sub 3} where (x = 0, 0.1, 0.15 and 0.2) were prepared by co-precipitation method. The structural and magnetic properties of the La{sub 1−x}Ce{sub x}Fe{sub 1−x}Cr{sub x}O{sub 3} system have been investigated. X-ray diffraction showed the formation of orthorhombic structure with space group Pnma for different compositions. With increasing Ce and Cr content, lattice parameters a and c were found to decrease while b increases, resulting in a decrease of the unit cell volume. The crystallite size was calculated from XRD data and compared with that obtained from TEM micrographs. Vibrating sample magnetometer measurements reveal an enhancement in the coercivity (H{sub c}) with increasing Ce and Cr content and reduction of saturation magnetization (M{sub s}) and remnant magnetization (M{sub r}) up to x = 0.15 and increases with further increases of x. The magnetic susceptibility measurements vs. temperature showed canted-antiferromagnetic (AFM) in which the Neel temperature is increasing with Ce and Cr content.

36 MATERIALS SCIENCE↗

Influence of europium doping on magnetic properties of 3D topological semimetal Cd{sub 3}As{sub 2} from ESR data

Influence of weak doping by rare-earth elements on magnetic and transport properties of a 3D topological semimetal Cd{sub 3}As{sub 2} was studied experimentally. In particular, the doping by europium causes to change of the magnetoresistance sign from positive to negative. First measurements of electron spin resonance and magnetic susceptibility have shown that there are two types of Eu{sup 2+} magnetic ions that occupy the positions of cadmium ions and tetrahedral vacancies and form the ferromagnetic and antiferromagnetic phases, respectively. These facts give an evidence of small-scaled phase separation and a transformation of the Dirac semimetal to a Weyl semimetal induced by magnetic impurities.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗