Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “FILM”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,135 records · Page 63

Interfacial Strength Evaluation of Oxide Films on Carbon Steel by Using the Laser Shock Adhesion Test

We investigate the adhesion strength (interfacial strength) of the oxide film formed on a carbon steel substrate by using a laser shock adhesion test (LaSAT). A rolled carbon steel (SS400) plate is first heated at high temperature (700 °C) under the atmosphere (heat treatment) to cause the formation of oxide films about 20-50 μm thick on the steel surface. The film consisted of multiple layers, including wustite (FeO), magnetite (Fe{sub 3}O{sub 4}), and hematite (Fe{sub 2}O{sub 3}). Next, the x-ray diffraction method was used to measure the residual stress in the film. We find that compression stress develops in the film because of a mismatch of thermal strain in between the film and substrate after the heat treatment. With LaSAT, strong elastic wave generates by a pulsed laser ablation of the substrate backside, and results in interfacial fractures in the oxide films. To monitor the normal (out-of-plane) displacement of the top surface film, a laser ultrasonic interferometer is simultaneously utilized, such that we detect film delamination and determine the critical laser energy for interfacial fracture to obtain the critical stress (interfacial strength). Furthermore, additional pulsed laser irradiation is conducted against a pre-delaminated specimen in order to examine the growth of delamination area and evaluate the interfacial fracture toughness. Finally, elastic wave propagation in the sample is computed using the finite element method (FEM) in order to evaluate the interfacial stress field, accurately. For the FEM, multiple layers in the oxide film are modeled, and the residual stress due to thermal strain mismatch is introduced. The FEM computations reveal the stress distribution around the interface and evaluate the critical stress and critical stress intensity factor for delamination. We thus quantitatively evaluate the interfacial strength and interfacial fracture toughness of the oxide film formed on carbon steel. The mechanism of interfacial fracture is also discussed on the basis of microstructures in a film with multiple layers. This result may be useful for understanding the adhesion quality of oxide film during the hot-rolling process.

36 MATERIALS SCIENCE↗

Influence of vanadium incorporation on the microstructure, mechanical and tribological properties of Nb–V–Si–N films deposited by reactive magnetron sputtering

Composite Nb–V–Si–N films with various V contents (3.7–13.2 at.%) were deposited by reactive magnetron sputtering and the effects of V content on the microstructure, mechanical and tribological properties of Nb–V–Si–N films were investigated. The results revealed that a three-phase structure, consisting of face-centered cubic (fcc) Nb–V–Si–N, hexagonal close-packed (hcp) Nb–V–Si–N and amorphous Si{sub 3}N{sub 4}, co-exists in the Nb–V–Si–N films and the cubic phase is dominant. The hardness and critical load (L{sub c}) of Nb–V–Si–N films initially increased gradually and reached a summit, then decreased with the increasing V content in the films and the maximum values were 35 GPa and 9.8 N, respectively, at 6.4 at.% V. The combination of V into Nb–Si–N film led to the fracture toughness linearly increasing from 1.11 MPa·m{sup 1/2} at 3.7 at.% V to 1.67 MPa·m{sup 1/2} at 13.2 at.% V. At room temperature (RT), the average friction coefficient decreased from 0.80 at 3.7 at.% V to 0.55 at 13.2 at.% V for the Nb–V–Si–N films. The wear rate of Nb–V–Si–N films initially decreased and then increased after reaching a minimum value of about 6.35 × 10{sup −} {sup 7} mm{sup 3}/N·mm at 6.4 at.% V. As the rise of testing temperature from 200 °C to 600 °C, the average friction coefficient of Nb–V–Si–N films decreased with the increase of the testing temperature regardless of V content. However, the wear rate gradually increased for all films. The average friction coefficient and wear rate at RT and elevated temperatures were mainly influenced by the vanadium oxides with weakly bonded lattice planes. - Highlight: • Fcc-Nb–V–Si–N, hcp-Nb–V–Si–N and amorphous Si{sub 3}N{sub 4} co-existed in the films. • The amount of Si{sub 3}N{sub 4} decreased with increasing V content in the films. • Hardness of Nb–V–Si–N film (6.4 at.%) reached a maximum value of 35 GPa. • Addition of V led to the increase of fracture toughness. • Tribological properties were influenced by lubricant wear debris.

36 MATERIALS SCIENCE↗

Preparation and thermochromic properties of Ce-doped VO{sub 2} films

Graphical abstract: This effect of doping concentration on the phase transition temperature of VO{sub 2} films demonstrates that the phase transition temperature is decreasing along with the increase of the Ce dopant concentrations. After doping Ce, the transition temperature of VO{sub 2} film changes appreciably. Highlights: ► Ce-doped VO{sub 2} films were prepared on muscovite substrate by inorganic sol–gel method for the first time. ► The cerium existing in the VO{sub 2} films in the form of Ce{sup 4+} and Ce{sup 3+} was substituted for part of V atoms in the lattice. ► Ce doping could remarkably reduce the particle size of the Ce-doped films compared with undoped films. ► The phase transition temperature of Ce-doped VO{sub 2} films decreased appreciably with maintaining high-quality phase transition. - Abstract: Mixture of cerium (III) nitrate hexahydrate and vanadium pentaoxide powder were used as precursor to prepare Ce-doped VO{sub 2} films on the muscovite substrate by inorganic sol–gel method. SEM, XRD and XPS were used to investigate the morphologies and structures of VO{sub 2} films. The results show that the VO{sub 2} films grow on the muscovite substrate with preferred orientated (0 1 1) plane and the Ce exists in the form of Ce{sup 4+} and Ce{sup 3+} replacing part of V atoms in the lattice. The infrared transmittance change was measured from room temperature to the temperature above the metal–insulator transition. The films have excellent thermochromic performance. The metal–insulator transition temperature of VO{sub 2} films changes appreciably with Ce doped, which decreases by 4.5 °C per 1 at.% doping. Furthermore, Ce doping could remarkably reduce the particle size of VO{sub 2} films.

36 MATERIALS SCIENCE↗

Non-toxic novel route synthesis and characterization of nanocrystalline ZnS{sub x}Se{sub 1−x} thin films with tunable band gap characteristics

Highlights: • A simple, inexpensive, and non-toxic CBD route is used to deposit ZnS thin films. • The ZnS{sub x}Se{sub 1−x} thin films formation takes place via annealing of ZnS thin films in Se atmosphere. • S/(S + Se) ratio found to be temperature dependent and easy tuning of band gap has been done by Se atom deposition. - Abstract: An environmentally benign chemical bath deposition (CBD) route was employed to deposit zinc sulfide (ZnS) thin films. The CBD-ZnS thin films were further selenized in a furnace at various temperatures viz. 200, 300, 400, and 500 °C and the S/(S + Se) ratio was found to be dependent on the annealing temperature. The effects of S/(S + Se) ratio on the structural, compositional and optical properties of the ZnS{sub x}Se{sub 1−x} (ZnSSe) thin films were investigated. EDS analysis showed that the S/(S + Se) ratio decreased from 0.8 to 0.6 when the film annealing temperature increased from 200 to 500 °C. The field emission scanning electron microscopy and atomic force microscopy studies showed that all the films were uniform, pin hole free, smooth, and adhered well to the glass substrate. The X-ray diffraction study on the ZnSSe thin films showed the formation of the cubic phase, except for the unannealed ZnSSe thin film, which showed an amorphous phase. The X-ray photoelectron spectroscopy revealed Zn-S, Zn-Se, and insignificant Zn-OH bonds formation from the Zn 2p{sub 3/2}, S 2p, Se 3d{sub 5/2}, and O 1s atomic states, respectively. The ultraviolet–visible spectroscopy study showed ∼80% transmittance in the visible region for all the ZnSSe thin films having various absorption edges. The tuning of the band gap energy of the ZnSSe thin films was carried out by selenizing CBD-ZnS thin films, and as the S/(S + Se) ratio decreased from 0.8 to 0.6, the band gap energy decreased from 3.20 to 3.12 eV.

36 MATERIALS SCIENCE↗

Growth and Characterization of Epitaxial FeWO 4 Thin Films with Controlled Oxygen Stoichiometry

Here, we report the growth of single-phase epitaxial FeWO 4 thin films, using plasma-assisted molecular beam epitaxy, and investigate structural, optical, and electronic properties. The FeWO 4 films grow in (100) orientation on c-plane sapphire (0001) substrates and exhibit 3 rotational twin variants where FeWO 4 [001] is aligned to sapphire [100] equivalent in-plane directions. X-ray diffraction measurements indicate that the epitaxial FeWO 4 (100) structure is optimized when 80-100 W of rf power is applied to an atomic oxygen source during growth, yielding films with minimal strain and impurity phases or other orientations. In films grown with 120 W of rf power, FeWO 4 crystallites develop inhomogeneous and homogeneous strains and are potentially contaminated with Fe 3+ oxide phase impurities. In films grown with 60 W of rf power, FeWO 4 crystallites do not form fully epitaxial layers. X-ray photoelectron spectroscopy indicates that the structural changes are correlated with the Fe 3+ /Fe 2+ oxidation state ratio increasing from 0.6-1.4 with rf power from 60-120 W. X-ray fluorescence spectroscopy indicates that the Fe/W composition ratio is also increasing from 1.1-1.8 with rf power from 60-120 W. Ultraviolet and visible optical absorption spectra indicate a 1.8 ± 0.1 eV band gap with an additional interband absorption feature at 3.1 ± 0.1 eV in the 80-100 W films, with similar onsets observed in the 60 W films. In the 120 W films, the higher lying transition is shifted to 2.7 ± 0.1 eV due to the Fe 3+ enrichment. Electrical resistivity decreases over 2 orders of magnitude with oxidation from 10 4 -10 5 Ω cm in 60 W films to 120 ± 10 Ω cm in 120 W films. Thermopower measurements show p-type to n-type conductivity conversion when oxidation states shift from Fe 2+ majority in the 100 W films to Fe 3+ majority in the 120 W films. We conclude that electron polaron hopping driven by Fe 3+ is a dominant transport mechanism and a source of n-type conductivity in overoxidized FeWO 4 films.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Characteristics of ultra low-k nanoporous and fluorinated silica based films prepared by plasma enhanced chemical vapor deposition

Low dielectric constant (low-k) silica based films were deposited on p-type silicon and polycarbonate substrates by radio frequency (RF) plasma enhanced chemical vapor deposition method at low temperature. A mixture of tetraethoxysilane vapor, oxygen, and tetrafluoromethane (CF{sub 4}) was used for the deposition of the films in forms of two structures called as SiO{sub x}C{sub y} and SiO{sub x}C{sub y}F{sub z}. Properties of the films were controlled by amount of porosity and fluorine content in the film matrix. The influence of RF power and CF{sub 4} flow on the elemental composition, deposition rate, surface roughness, leakage current, refractive index, and dielectric constant of the films were characterized. Moreover, optical emission spectroscopy was applied to monitor the plasma process at the different parameters. Electrical characteristics of SiO{sub x}C{sub y} and SiO{sub x}C{sub y}F{sub z} films with metal-oxide-semiconductor structure were investigated using current-voltage analysis to measure the leakage current and breakdown field, as well as capacitance-voltage analysis to obtain the film's dielectric constant. The results revealed that SiO{sub x}C{sub y} films, which are deposited at lower RF power produce more leakage current, meanwhile the dielectric constant and refractive index of these films decreased mainly due to the more porosity in the film structure. By adding CF{sub 4} in the deposition process, fluorine, the most electronegative and the least polarized atom, doped into the silica film and led to decrease in the refractive index and the dielectric constant. In addition, no breakdown field was observed in the electrical characteristics of SiO{sub x}C{sub y}F{sub z} films and the leakage current of these films reduced by increment of the CF{sub 4} flow.

36 MATERIALS SCIENCE↗

Additive to regulate the perovskite crystal film growth in planar heterojunction solar cells

We reported a planar heterojunction perovskite solar cell fabricated from MAPbI{sub 3−x}Cl{sub x} perovskite precursor solution containing 1-chloronaphthalene (CN) additive. The MAPbI{sub 3−x}Cl{sub x} perovskite films have been characterized by UV-vis, SEM, XRD, and steady-state photoluminescence (PL). UV-vis absorption spectra measurement shows that the absorbance of the film with CN additive is significantly higher than the pristine film and the absorption peak is red shift by 30 nm, indicating the perovskite film with additive possessing better crystal structures. In-situ XRD study of the perovskite films with additive demonstrated intense diffraction peaks from MAPbI{sub 3−x}Cl{sub x} perovskite crystal planes of (110), (220), and (330). SEM images of the films with additive indicated the films were more smooth and homogenous with fewer pin-holes and voids and better surface coverage than the pristine films. These results implied that the additive CN is beneficial to regulate the crystallization transformation kinetics of perovskite to form high quality crystal films. The steady-state PL measurement suggested that the films with additive contained less charge traps and defects. The planar heterojunction perovskite solar cells fabricated from perovskite precursor solution containing CN additive demonstrated 30% enhancement in performance compared to the devices with pristine films. The improvement in device efficiency is mainly attributed to the good crystal structures, more homogenous film morphology, and also fewer trap centers and defects in the films with the additive.

36 MATERIALS SCIENCE↗

Growth and microstructure of columnar Y-doped SrZrO{sub 3} films deposited on Pt-coated MgO by pulsed laser deposition

Direct integration of proton conductor films on Pt-coated substrates opens the way to film-based proton transport devices. Columnar SrZr{sub 0.95}Y{sub 0.05}O{sub 3−δ} (SZY) films with dense microstructure were deposited on Pt-coated MgO(100) substrates at 830 °C by pulsed laser deposition. The optimal window of ambient O{sub 2} pressure for good crystallinity of SZY films is from 400 to 600 mTorr. The ambient O{sub 2} compresses the plasma plume of SZY and increases the deposition rate. The 10 nm thick Ti adhesion layer on MgO(100) greatly affects the orientation of the sputtered Pt layers. Pt deposited directly on MgO shows a highly (111)-preferred orientation and leads to preferentially oriented SZY films while the addition of a Ti adhesion layer makes Pt show a less preferential orientation that leads to randomly oriented SZY films. The RMS surface roughness of preferentially oriented SZY films is larger than that of randomly oriented SZY films deposited under the same ambient O{sub 2} pressure. As the O{sub 2} pressure increased, the RMS surface roughness of preferentially oriented SZY films increased, reaching 45.7 nm (2.61% of film thickness) at 600 mTorr. This study revealed the ambient O{sub 2} pressure and orientation dependent surface roughness of SZY films grown on Pt-coated MgO substrates, which provides the potential to control the surface microstructure of SZY films for electrochemical applications in film-based hydrogen devices.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Microstructure and temperature coefficient of resistance of thin cermet resistor films deposited from CrSi{sub 2}-Cr-SiC targets by S-gun magnetron

Technological solutions for producing nanoscale cermet resistor films with sheet resistances above 1000 {Omega}/{open_square} and low temperature coefficients of resistance (TCR) have been investigated. 2-40 nm thick cermet films were sputter deposited from CrSi{sub 2}-Cr-SiC targets by a dual cathode dc S-gun magnetron. In addition to studying film resistance versus temperature, the nanofilm structural features and composition were analyzed using scanning electron microscopy, atomic force microscopy, high-resolution transmission electron microscopy, energy-dispersive x-ray spectroscopy, and electron energy loss spectroscopy. This study has revealed that all cermet resistor films deposited at ambient and elevated temperatures were amorphous. The atomic ratio of Si to Cr in these films was about 2 to 1. The film TCR displayed a significant increase when the deposited film thickness was reduced below 2.5 nm. An optimized sputter process consisting of wafer degassing, cermet film deposition at elevated temperature with rf substrate bias, and a double annealing in vacuum, consisting of in situ annealing following the film sputtering and an additional annealing following the exposure of the wafers to air, has been found to be very effective for the film thermal stabilization and for fine tuning the film TCR. Cermet films with thicknesses in the range of 2.5-4 nm deposited using this technique had sheet resistances ranging from 1800 to 1200 {Omega}/{open_square} and TCR values from -50 ppm/ deg. C to near zero, respectively. A possible mechanism responsible for the high efficiency of annealing the cermet films in vacuum (after preliminary exposure to air), resulting in resistance stabilization and TCR reduction, is also discussed.

36 MATERIALS SCIENCE↗

Deposition of aluminum-doped zinc oxide thin films for optical applications using rf and dc magnetron sputter deposition

Aluminum-doped zinc oxide films were deposited by dc and rf magnetron sputtering from ZnO(98%)Al{sub 2}O{sub 3}(2%) target at room temperature on silicon and glass substrates under a variety of process conditions with the goal of attaining the highest transmittance and lowest resistivity for photovoltaic applications. The magnetron power and pressure were varied. For many dielectric deposition systems, added oxygen is necessary to achieve the appropriate stoichiometry. The effect of oxygen on film properties was then studied by varying the oxygen partial pressure from 1.5x10{sup -5} to 4.0x10{sup -5} T at a constant Ar pressure, with the result that any added oxygen was deleterious. Films deposited under power, pressure, and low-oxygen conditions were then characterized for electrical and optical properties. Following this, the dc and rf sputtered films were annealed at up to 400 deg. C seconds using rapid thermal annealing (RTA), and the influence of annealing on resistivity, transmittance, band gap, as well as grain growth and stress was studied. The effect of RTA was immediate and quite significant on dc films while the effect on rf films was not as profound. As-deposited rf films had a higher average transmittance (87%) and lower resistivity (5.5x10{sup -4} {Omega} cm) compared to as-deposited dc films (84.2% and 8.9x10{sup -4} {Omega} cm). On the other hand, after RTA at 400 deg. C for 60 s, dc films exhibited better average transmittance (92.3%) and resistivity (2.9x10{sup -4} {Omega} cm) than rf films (90.7% and 4.0x10{sup -4} {Omega} cm). The band gap of dc films increased from 3.55 to 3.80 eV while that of rf films increased from 3.76 to 3.85 eV. Finally, dc and rf films were textured in 0.1% HCl and compared to U-type Asahi glass for resistivity and transmittance.

36 MATERIALS SCIENCE↗

Phase, grain structure, stress, and resistivity of sputter-deposited tungsten films

Sputter-deposited W films with nominal thicknesses between 5 and 180 nm were prepared by varying the base pressure prior to film deposition and by including or not including sputtered SiO{sub 2} encapsulation layers. X-ray and electron diffraction studies showed that single phase, polycrystalline {alpha}-W could be achieved in as-deposited films as thin as 5 nm. The stress state in the as-deposited films was found to be inhomogeneous. Annealing resulted in stress relaxation and reduction of resistivity for all films, except the thinnest, unencapsulated film, which agglomerated. In-plane film grain sizes measured for a subset of the annealed films with thicknesses between 5 and 180 nm surprisingly showed a near constant value (101-116 nm), independent of film thickness. Thick-film ({>=}120 nm) resistivity values as low as 8.6 {mu}{Omega} cm at 301 K were obtained after annealing at 850 deg. C for 2 h. Film resistivities were found to increase with decreasing film thicknesses below 120 nm, even for films which are fully A2 {alpha}-W with no metastable, A15 {beta}-W evident.

36 MATERIALS SCIENCE↗

Reactive sputtering of δ-ZrH{sub 2} thin films by high power impulse magnetron sputtering and direct current magnetron sputtering

Reactive sputtering by high power impulse magnetron sputtering (HiPIMS) and direct current magnetron sputtering (DCMS) of a Zr target in Ar/H{sub 2} plasmas was employed to deposit Zr-H films on Si(100) substrates, and with H content up to 61 at. % and O contents typically below 0.2 at. % as determined by elastic recoil detection analysis. X-ray photoelectron spectroscopy reveals a chemical shift of ∼0.7 eV to higher binding energies for the Zr-H films compared to pure Zr films, consistent with a charge transfer from Zr to H in a zirconium hydride. X-ray diffraction shows that the films are single-phase δ-ZrH{sub 2} (CaF{sub 2} type structure) at H content >∼55 at. % and pole figure measurements give a 111 preferred orientation for these films. Scanning electron microscopy cross-section images show a glasslike microstructure for the HiPIMS films, while the DCMS films are columnar. Nanoindentation yield hardness values of 5.5–7 GPa for the δ-ZrH{sub 2} films that is slightly harder than the ∼5 GPa determined for Zr films and with coefficients of friction in the range of 0.12–0.18 to compare with the range of 0.4–0.6 obtained for Zr films. Wear resistance testing show that phase-pure δ-ZrH{sub 2} films deposited by HiPIMS exhibit up to 50 times lower wear rate compared to those containing a secondary Zr phase. Four-point probe measurements give resistivity values in the range of ∼100–120 μΩ cm for the δ-ZrH{sub 2} films, which is slightly higher compared to Zr films with values in the range 70–80 μΩ cm.

36 MATERIALS SCIENCE↗

Effect of AC target power on AlN film quality

The influence of alternating current (AC) target power on film stress, roughness, and x-ray diffraction rocking curve full width half maximum (FWHM) was examined for AlN films deposited using S-gun magnetron sputtering on insulative substrates consisting of Si wafers with 575 nm thermal oxide. As the AC target power was increased from 5 to 8 kW, the deposition rate increased from 9.3 to 15.9 A/s, film stress decreased from 81 to −170 MPa, and the rocking curve FWHM increased from 0.98 to 1.03°. AlN film behavior is observed to change with target life; films deposited at 200 kWh target life were approximately 40 MPa more compressive and had 0.02° degree higher rocking curve FWHM values than films deposited at 130 kWh. AlN films deposited in two depositions were compared with films deposited in a single deposition, in order to better characterize the growth behavior and properties of AlN films deposited on an existing AlN film, which is not well understood. Two deposition films, when compared with single deposition films, showed no variation in residual stress trends or grain size behavior, but the average film roughness increased from 0.7 to 1.4 nm and rocking curve FWHM values increased by more than 0.25°.

36 MATERIALS SCIENCE↗

Production and characterization of thin film group IIIB, IVB and rare earth hydrides by reactive evaporation

A recent short history of reactive evaporation by D. M. Mattox [History Corner—A Short History of Reactive Evaporation, SVC Bulletin (Society of Vacuum Coaters, Spring 2014), p. 50–51] describes various methods for producing oxides, nitrides, carbides, and some compounds, but hydrides were not mentioned. A study was performed in the mid-1970s at the General Electric Company Neutron Devices Department in Largo, FL, by the author to study preparation of thin film hydrides using reactive evaporation and to determine their unique characteristics and properties. Films were produced of scandium (Sc), yttrium (Y), titanium (Ti), zirconium (Zr), and the rare earth praseodymium (Pr), neodymium (Nd), gadolinium (Gd), dysprosium (Dy), and erbium (Er) hydrides by hot crucible filament and electron beam evaporation in atmospheres of deuterium and tritium gases. All-metal vacuum systems were used and those used with tritium were dedicated for this processing. Thin film test samples 1000 nm thick were prepared on 1.27 cm diameter molybdenum disk substrates for each occluder (i.e., an element that can react with hydrogen to form a hydride) material. Loading characteristics as determined by gas-to-metal atomic ratios, oxidation characteristics as determined by argon–sputter Auger analysis, film structure as determined by scanning electron microscope analysis, and film stress properties as determined by a double resonator technique were used to define properties of interest. Results showed hydrogen-to-metal atomic ratios varied from 1.5 to 2.0 with near maximum loading for all but Pr and Nd occluders which correlated with the oxidation levels observed, with all occluder oxidation levels being variable due to vacuum system internal processing conditions and the materials used. Surface oxide levels varied from ∼80 Å to over 1000 Å. For most films studied, results showed that a maximum loading ratio of near 2.0 and a minimum surface oxide level of ∼80 Å could be obtained with a bulk film oxygen level of ∼0.54 oxygen as determined by microprobe analysis when an evaporation rate of ∼0.313 mg/cm{sup 2} min was used in an atmosphere of D{sub 2} or T{sub 2} gas at a system deposition pressure of 1 × 10{sup −3 }Torr (1.33 × 10{sup −1 }Pa) in an evaporation time of ∼2 min. Platelet type (i.e., a film microstructure showing an overlay of flat plates with large grain sizes) film structures were observed for most films with some film mechanical properties determined (i.e., grain size and Vickers μ-hardness), and reduced stress levels were seen with initial normalized differential (tensile) stress levels being (1.0–4.0) × 10{sup 8 }dyne/cm{sup 2} for tritium loaded samples and (1.5 ± 0.5) × 10{sup 9 }dyne/cm{sup 2} for deuterium loaded samples. Also, stress aging characteristics were determined for some hydride films prepared in a radioactive tritium gas atmosphere. Tritium loading, however, had the undesirable characteristic of having to dispose of the internal processing system fixtures, which can be minimized, but the reactive evaporation technique produced desirable thin films.

36 MATERIALS SCIENCE↗

The effects of incidence angle on film dosimetry and their consequences in IMRT dose verification

Purpose: The dosimetric accuracy of EDR2 radiographic film has been rigorously assessed in regular and intensity modulated beams for various incidence angles, including the parallel and perpendicular orientation. There clearly exists confusion in literature regarding the effect of film orientation. The primary aim is to clarify potential sources of the confusion and to gain physical insight into the film orientation effect with a link to radiochromic film as well. Methods: An inverse pyramid IMRT field, consisting of six regular and elongated 3 Multiplication-Sign 20 cm{sup 2} field segments, was studied in perpendicular and parallel orientation. Assessment of film self-perturbation and intrinsic directional sensitivity were also included in the experiments. Finally, the authors investigated the orientational effect in composite beams in the two extreme orientations, i.e., perpendicular and parallel. Results: The study of an inverse pyramid dose profile revealed good agreement between the perpendicular film and the diamond detector within 0.5% in the low-scatter regions for both 6 and 18 MV. The parallel oriented film demonstrated a 3% under-response at 5-cm (6 MV) depth against the perpendicular orientation, but both orientations over responded equally in the central region, which received only scattered dose, at both 5- and 20-cm depths. In a regular 6-MV 5 Multiplication-Sign 5 cm{sup 2} field, a 4.1% lower film response was observed in the parallel orientation compared to perpendicular orientation. The under response gradually increased to 6% when reducing the field size to 0.5 Multiplication-Sign 5 cm{sup 2}. On the other hand, the film showed a 1.7% lower response in parallel orientation for the large field size of 20 Multiplication-Sign 20 cm{sup 2} at 5-cm depth but the difference disappeared at 10 cm. At 18 MV, similar but somewhat lower differences were found between the two orientations. The directional sensitivity of the film diminishes with increasing field size and depth. Surprisingly a composite IMRT beam consisting of 20 adjacent strip segments also produced a significant orientational dependence of film response, notwithstanding the large total field size of 20 Multiplication-Sign 20 cm{sup 2}. Conclusions: This analysis allowed the development of a hypothesis about the physics behind the orientational dependence of film response in general and to formulate precautions when using film dosimetry in the dosimetric verification of multibeam treatments.

60 APPLIED LIFE SCIENCES↗

Effect of Ag in CdSe thin films prepared using thermal evaporation

It has been a general practice to dope thin films with suitable dopants to modify the properties of the films to make them more suitable for potential applications. When the dopant concentrations are low, they do not normally affect the structure and morphology of the films. However, it may lead to drastic changes in electronic properties of the films. This might result from the dopant getting incorporated into the lattice of the material of the films. Cadmium selenide is an important compound semiconductor material with an attractive energy band gap. The present work relates to an attempt made to dope CdSe thin films with silver. CdSe:Ag (1–5%) thin films were deposited on glass substrates at an optimized substrate temperature of 453 K using thermal evaporation technique. The grown films were analyzed using X-ray diffraction, scanning electron microscopy (SEM), energy dispersive analysis of X-ray (EDX) techniques. It is observed that undoped CdSe thin films and CdSe:Ag films have hexagonal structure. The grain size was found to increase marginally with an increase in the Ag concentration. The optical band gap of the films determined by optical transmission measurements agree with that of CdSe. Electrical conductivity is observed to increase from 10{sup –4} to 3.66 (Ω cm){sup –1} on addition of silver. The variation of resistance with temperature indicates that the prepared films consist of CdSe and Ag existing as two separate phases coexisting and contributing individually to the resistivity of the films.

36 MATERIALS SCIENCE↗

Thin Film Packaging Solutions for High Efficiency OLED Lighting Products

The objective of the 'Thin Film Packaging Solutions for High Efficiency OLED Lighting Products' project is to demonstrate thin film packaging solutions based on SiC hermetic coatings that, when applied to glass and plastic substrates, support OLED lighting devices by providing longer life with greater efficiency at lower cost than is currently available. Phase I Objective: Demonstrate thin film encapsulated working phosphorescent OLED devices on optical glass with lifetime of 1,000 hour life, CRI greater than 75, and 15 lm/W. Phase II Objective: Demonstrate thin film encapsulated working phosphorescent OLED devices on plastic or glass composite with 25 lm/W, 5,000 hours life, and CRI greater than 80. Phase III Objective: Demonstrate 2 x 2 ft{sup 2} thin film encapsulated working phosphorescent OLED with 40 lm/W, 10,000 hour life, and CRI greater than 85. This report details the efforts of Phase III (Budget Period Three), a fourteen month collaborative effort that focused on optimization of high-efficiency phosphorescent OLED devices and thin-film encapsulation of said devices. The report further details the conclusions and recommendations of the project team that have foundation in all three budget periods for the program. During the conduct of the Thin Film Packaging Solutions for High Efficiency OLED Lighting Products program, including budget period three, the project team completed and delivered the following achievements: (1) a three-year marketing effort that characterized the near-term and longer-term OLED market, identified customer and consumer lighting needs, and suggested prototype product concepts and niche OLED applications lighting that will give rise to broader market acceptance as a source for wide area illumination and energy conservation; (2) a thin film encapsulation technology with a lifetime of nearly 15,000 hours, tested by calcium coupons, while stored at 16 C and 40% relative humidity ('RH'). This encapsulation technology was characterized as having less than 10% change in transmission during the 15,000 hour test period; (3) demonstrated thin film encapsulation of a phosphorescent OLED device with 1,500 hours of lifetime at 60 C and 80% RH; (4) demonstrated that a thin film laminate encapsulation, in addition to the direct thin film deposition process, of a polymer OLED device was another feasible packaging strategy for OLED lighting. The thin film laminate strategy was developed to mitigate defects, demonstrate roll-to-roll process capability for high volume throughput (reduce costs) and to support a potential commercial pathway that is less dependent upon integrated manufacturing since the laminate could be sold as a rolled good; (5) demonstrated that low cost 'blue' glass substrates could be coated with a siloxane barrier layer for planarization and ion-protection and used in the fabrication of a polymer OLED lighting device. This study further demonstrated that the substrate cost has potential for huge cost reductions from the white borosilicate glass substrate currently used by the OLED lighting industry; (6) delivered four-square feet of white phosphorescent OLED technology, including novel high efficiency devices with 82 CRI, greater than 50 lm/W efficiency, and more than 1,000 hours lifetime in a product concept model shelf; (7) presented and or published more than twenty internal studies (for private use), three external presentations (OLED workshop-for public use), and five technology-related external presentations (industry conferences-for public use); and (8) issued five patent applications, which are in various maturity stages at time of publication. Delivery of thin film encapsulated white phosphorescent OLED lighting technology remains a challenging technical achievement, and it seems that commercial availability of thin, bright, white OLED light that meets market requirements will continue to require research and development effort. However, there will be glass encapsulated white OLED lighting products commercialized in niche markets during the 2008 calendar year. This commercialization effort, the project team believes, will lead to increasing market attention and broader demand for more efficient, wide area general purpose white OLED lighting in the coming years.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Real-Time Monitoring of Strain Accumulation and Relief during Epitaxy of Ultrathin Co Ferrite Films with Varied Co Content

Ultrathin Co x Fe 3-x O 4 films of high structural quality and with different Co content (x = 0.6–1.2) were prepared by reactive molecular beam epitaxy on MgO(001) substrates. Epitaxy of these ferrite films is extensively monitored by means of time-resolved (operando) X-ray diffraction recorded in out-of-plane geometry to characterize the temporal evolution of the film structure. The Co ferrite films show high crystalline ordering and smooth film interfaces independent of their Co content. All Co x Fe 3-x O 4 films exhibit enhanced compressive out-of-plane strain during the early stages of growth, which partly releases with increasing film thickness. When the Co content of the ferrite films increases, the vertical-layer distances increase, accompanied by slightly increasing film roughnesses. The latter result is supported by surface-sensitive low-energy electron diffraction as well as X-ray reflectivity measurements on the final films. In contrast, the substrate–film interface roughness decreases with increasing Co content, which is confirmed with X-ray reflectivity measurements. In addition, the composition and electronic structure of the ferrite films is characterized by means of hard X-ray photoelectron spectroscopy performed after film growth. The experiments reveal the expected increasing Fe 3+ /Fe 2+ cation ratios for a higher Co content.

36 MATERIALS SCIENCE↗