Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “dissolution”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,117 records · Page 62

Determining the Solubility Behavior of Kogarkoite in Simulated Nuclear Waste

Kogarkoite (Na 3 FSO 4 ) is a sparingly soluble fluoride–sulfate double salt that has been identified in high level nuclear waste sludge at the Hanford Site and, more recently, in sludge batch compilation samples at the Savannah River Site (SRS). Due to its complex dissolution behavior, which exhibits an inverse dependence on sodium ion activity, the presence of this mineral poses significant challenges to waste retrieval and processing. Incomplete dissolution during sludge washing can lead to the retention of fluoride and sulfate in the high-level waste feed, potentially causing the formation of corrosive, immiscible molten salt layers, known as "glass gall,” in vitrification melters. Current efforts to optimize flowsheet parameters and wash-water volumes are hindered by the absence of a commercially available, certified reference material, which prevents the accurate calibration of analytical methods and the verification of dissolution kinetics. To address this critical gap, this research focuses on the laboratory synthesis of pure Kogarkoite to serve as a standard for comprehensive solubility and washing performance testing. A coupled synthesis and simulant campaign was executed using an evaporative crystallization protocol designed to replicate the dynamic concentration effects observed in tank farm operations. Thirteen simulant matrices were prepared by dissolving systematically varied ratios of sodium fluoride (NaF) and sodium sulfate (Na 2 SO 4 ) in deionized water under three distinct caustic regimes: 0.0 g (control), 4.0 g (~1 M), and 12.0 g (~3 M) sodium hydroxide (NaOH). While thermodynamic equilibrium models suggest that high-caustic environments should favor the stability of the double salt7, results from this evaporative study at 25 0 C revealed a distinct kinetic divergence. Simulants with high hydroxide loading predominantly yielded large, blocky crystals of sodium sulfate decahydrate (Na 2 SO 4 .10H 2 O). Successful synthesis of pure Kogarkoite was achieved exclusively in specific NaOH-free compositional windows, where the precipitate manifested as fine, opaque granular aggregates. Ion chromatography (IC) analysis confirmed phase purity through the simultaneous stoichiometric depletion of both fluoride and sulfate from the supernatant. This successful synthesis establishes a reproducible route to generate bulk Kogarkoite, enabling the subsequent phase of quantitative dissolution testing using inhibited water to optimize sludge-batch assembly.

Sarker, Md Sharif [Florida International Univ. (FI↗

Dose and dose rate effects on the microstructural and mechanical stability of long-range ordered precipitates in Inconel 718

Nickel-based alloys offer exceptional mechanical properties and corrosion resistance for various applications in extreme environments such as high neutron flux, temperature, and stress. Precipitates, resulting from thermal treatments, increase the strength and creep resistance of these alloys. Here, heavy ion irradiation is shown to destabilize the γ' and γ" precipitates in Inconel 718 nickel-based alloy by disordering and dissolution processes. Transmission electron microscopy and atom probe tomography reveal that the disordering and dissolution rates of the precipitates are proportional to both irradiation dose and dose rate. Irradiation induced disordering occurs at a higher rate than the dissolution. From analyzing the hardening contributions, microscale mechanical results suggest radiation-induced disordering is responsible for the majority of the softening response at low dose. In addition, low dose radiation-induced disordering results in strain localization and is believed to be the primary cause for the drastic degradation of uniform elongation and toughness in irradiated Inconel 718.

36 MATERIALS SCIENCE↗

Characterization of cation environments in polycrystalline forsterite by Mg-25 MAS, MQMAS, and QCPMG NMR

Forsterite (Mg2SiO4) is a silicate mineral frequently studied in the Earth sciences as it has a simple crystal structure and fast dissolution kinetics (elemental release rates under typical conditions on the order of 10-7 mol/m2/s1). During the dissolution process, spectroscopic techniques are often utilized to augment solution chemical analysis and to provide data for determining reaction mechanisms. Nuclear magnetic resonance (NMR) is able to interrogate the local bonding arrangement and coordination of a particular nuclide to obtain in structural information. Although previous NMR studies have focused on the silicon and oxygen environments in forsterite, studies focusing on the two nonequivalent magnesium environments in forsterite are limited to a few single-crystal studies. In this study, we present the results of 25Mg MAS, MQMAS, and static QCMG experiments performed on a powdered sample of pure synthetic forsterite. We also present spectral fits obtained from simulation software packages, which directly provide quadrupolar parameters for 25Mg nuclei occupying each of the two nonequivalent magnesium sites in the forsterite structure. These results are compared to calculations of the electric field gradient tenor conducted in previous ab initio studies to make definitive assignments correlating each peak to their respective magnesium site in the forsterite structure. Although previous NMR investigations of forsterite have focused on single-crystal samples, we have focused on powdered forsterite as the increased surface area of powdered samples makes them more amenable to laboratory-scale dissolution studies and, ultimately, the products from chemical weathering may be monitored an quantified.

36 MATERIALS SCIENCE↗

DOE FG02-03ER63557: Final Technical Report: Reactivity of Primary Soil Minerals and Secondary Precipitates Beneath Leaking Hanford Waste Tanks

The purpose of the project was to investigate rates and mechanisms of reactions between primary sediment minerals and key components of waste tank solutions that leaked into the subsurface at the Hanford Site. Results were expected to enhance understanding of processes that cause (1) changes in porosity and permeability of the sediment and resultant changes in flow paths of the contaminant plumes, (2) formation of secondary precipitates that can take up contaminants in their structures, and (3) release of mineral components that can drive redox reactions affecting dissolved contaminant mobility. Measured rates can also be used directly in reactive transport models. Project tasks included (1) measurement of the dissolution rates of biotite mica from low to high pH and over a range of temperature relevant to the Hanford subsurface, (2) measurement of dissolution rates of quartz at high pH and in the presence of dissolved alumina, (3) measurement of the dissolution rates of plagioclase feldspar in high pH, high nitrate, high Al-bearing solutions characteristic of the BX tank farms, (4) incorporation of perrhenate in iron-oxide minerals as a function of pH, and (5) initiation of experiments to measure the formation of uranium(VI)-silicate phases under ambient conditions. Task 2 was started under a previous grant from the Environmental Management Science Program and Task 4 was partially supported by a grant to the PI from the Geosciences Program, Office of Basic Energy Sciences. Task 5 was continued under a subsequent grant from the Environmental Remediation Sciences Program, Office of Biological and Environmental Research.

54 ENVIRONMENTAL SCIENCES↗

Employing the Dynamics of the Electrochemical Interface in Aqueous Zinc-Ion Battery Cathodes

Intrinsically stable materials are desirable for constructing energy storage devices, which aim to demonstrate durability under the harsh electrochemical conditions that are detrimental to their lifespan. However, in this study it is demonstrated that the intrinsic instability of an electrochemical interface can be converted from an obstacle into an advantage. In aqueous zinc-ion batteries, manganese oxide (MnO 2 ) exhibits considerable dissolution even in electrolyte containing Mn 2+ salt. Balancing with redeposition alleviates the harmful impact of dissolution on performance and alters the trajectory of the active phase. Inclusion of Mn 2+ salt in the electrolyte induces MnO 2 deposition on all conductive surfaces, requiring that distracting side reactions be eliminated to isolate the dynamics of the active phase. Under conditions favoring dissolution, capacity decreases dramatically and a highly crystalline tetragonal ZnMn 2 O 4 phase forms, while redeposition helps maintain capacity and promotes a disordered cubic Zn-rich phase. Ultimately, this work aims to illuminate a path forward to unlock the potential of batteries made with materials that are fundamentally unstable in their operating environment.

25 ENERGY STORAGE↗

Mitigating Cyclable Li‐Ion Inventory Loss in Full Cells with Mn‐Rich Disordered Rocksalt Cathodes

Lithium (Li)- and manganese (Mn)-rich disordered rock salt (DRX) materials are promising cathode materials for next-generation Li-ion batteries. Although these cathode materials are Li-ions rich in their pristine state, their incorporation into full cells results in challenges with maintaining Li-ion inventory during cycling. Herein, the degradation mechanisms of DRX materials in different DRX||Graphite full cells are reported. It is found that DRX electrodes contain Li impurities, primarily due to the environmental sensitivity of mechanochemically synthesized DRX materials during sample transfer and storage. In addition, the structural instability of DRX triggers Mn dissolution. Dissolved Mn ions react with exposed Li x C y compounds and induce electrolyte decomposition on the anode, further depleting Li-ion inventory. Control experiments involving the pre-addition of Mn 2+ provide clear evidence of the impact of Mn dissolution on Li-ion inventory. The electrochemical activation process can stabilize DRX, alleviate Mn dissolution and thus mitigate the loss of Li-ion inventory. These mechanistic insights inform the development of chemical pre-lithiation and electrolyte additive strategies to collectively passivate interfaces, mitigate the effects of trace dissolved Mn ions, and preserve Li-ion inventory. Ultimately, the DRX||Graphite full cell achieves highly reversible electrochemical reactions with a high capacity retention. This study fills a research gap in DRX-based full cells and provides insights into degradation mechanisms and optimization strategies for their practical use.

36 MATERIALS SCIENCE↗

Computational Approach for Rapidly Predicting Temperature–Dependent Polymer Solubilities Using Molecular–Scale Models

One promising approach to recycle multicomponent plastic waste (e. g., multilayer plastic films) is selective dissolution. Selective dissolution is a solvent-mediated process in which differences in polymer solubility in a carefully chosen solvent system are exploited to recover a target polymer. Here, a computational approach was developed that rapidly predicts temperature-dependent polymer solubilities to guide the design of solvent systems for solvent-mediated polymer recycling. Polymer conformations were obtained from molecular dynamics simulations by modeling the polymer as a short oligomer and then used as input to the conductor-like screening model for real solvents (COSMO-RS) for solubility predictions. Using polyethylene (PE) and ethylene vinyl alcohol (EVOH) as representative polymers, the effect of simulation parameters was systematically studied, and predicted solubilities were found to be in good agreement with experimental measurements. Furthermore, the applicability of the approach was demonstrated by identifying selective solvents for PE and EVOH dissolution from a library of 524 solvents.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Secondary structure and dynamics study of the intrinsically disordered silica-mineralizing peptide P 5 S 3 during silicic acid condensation and silica decondensation

The silica forming repeat R5 of sil1 from Cylindrotheca fusiformis was the blueprint for the design of P5S3, a 50-residue peptide which can be produced in large amounts by recombinant bacterial expression. It contains five protein kinase A target sites and is highly cationic due to 10 lysine and 10 arginine residues. In the presence of supersaturated ortho silicic acid P5S3 strongly enhances silica-formation whereas it retards the dissolution of amorphous silica (SiO2) at globally undersaturated concentrations. The secondary structure of P5S3 during these different functions was studied by circular dichroism (CD), complemented by nuclear magnetic resonance (NMR) studies of the peptide in the absence of silicate. The NMR studies of dual-labeled (13C, 15N) P5S3 revealed a disordered structure at pH 2.8 and 4.5. Within the pH range of 4.5 to 9.5, the CD data verified the disordered secondary structure but also suggested the presence of some polyproline II character in the absence of silicic acid. Upon silicic acid polymerization and during dissolution of preformed silica, the CD spectrum of P5S3 indicated partial transition into an α-helical conformation which was transient during silica-dissolution. Consequently, the secondary structural changes observed for P5S3 correlate with the presence of oli-gomeric/polymeric silicic acid, presumably due to P5S3-silicic acid interactions. These interactions appear, at least in part, ionic in nature since dodecylsulfate micelles, which are negatively charged, cause similar conformational shifts to P5S3 in the absence of silica while ß-D-dodecyl maltoside micelles, which are neutral, do not. Thus, P5S3 influences both the condensation of silicic acid into silica and its decondensation back to silicic acid. Moreover, the dynamics of these pro-cesses may be indirectly monitored by following structural changes to P5S3 with CD spectroscopy.

59 BASIC BIOLOGICAL SCIENCES↗

Direct Observation of Pure Cu and Cu-Ag Anode Passivation in H{sub 2}SO{sub 4}-CuSO{sub 4} Aqueous Solution by Channel Flow Double Electrode and Optical Microscopy

The dissolution and passivation of pure Cu and Cu-5 wt pct Ag anodes in H{sub 2}SO{sub 4}-CuSO{sub 4} electrolyte were investigated by a direct observation method that combined the techniques of optical microscopy and channel flow double electrode. Linear sweep voltammetry of the anodes showed that the dissolution of Cu transited from the charge transfer-controlled reaction to the mass transfer-controlled reaction, followed by the passivation of the electrodes. The direct observation of the pure Cu anode revealed that Cu particles were generated on the surface and the particles fell away during passivation. On the other hand, a slime layer of Ag particles that adhered to the surface was generated during the dissolution of the Cu-5 wt pct Ag anode. The Cu-5 wt pct Ag anode was passivated with a lower current density than the pure Cu anode, which suggested that the morphology and adhesive characteristics of the slime on the anode affected the passivation. The direct observation method described herein is useful for understanding reactions on electrodes that undergo drastic changes in their surface morphology. Information obtained from this method can help with the development of new processes for the effective utilization of limited natural resources and energy, such as the recycling of Cu by electrorefining.

36 MATERIALS SCIENCE↗

Thermo-chemical Fluid Flow Simulation in Hot-Dip Galvanizing: The Evaluation of Dross Build-Up Formation

This paper presents a new computational framework to investigate the driving force for the formation of intermetallic dross particles in the zinc bath and dross build-up on the bath hardware. This is a major problem in continuous hot-dip galvanizing lines. The Computational Fluid Dynamics (CFD) model calculates the turbulent thermo-chemical flow conditions within the liquid melt. A detailed modeling of the steel strip–liquid interface enhances this approach, by means of a conjugated heat transfer calculation and a spatially resolved, temperature- and concentration-dependent iron dissolution and aluminum uptake. The heart of the computational framework is a thermodynamic model, which assesses the driving force for the formation or dissolution of dross particles in the bath and dross build-up on stationary and rotating equipment. The simulation results are validated with temperature and species depth profile measurements. The applicability of the CFD model is shown by investigating the locally resolved aluminum uptake and iron dissolution at the steel-strip surface, and the multi-physics conditions in the region near the roll. The novel approach of evaluating the thermodynamic driving force enables the assessment of the formation of dross build-up at the roll surface.

36 MATERIALS SCIENCE↗

Influence of citric acid on the hydration of Portland cement

Citric acid can be used to retard the hydration of cement. Experiments were carried out to investigate the influence of citric acid on the composition of solid and liquid phases during cement hydration. Analyses of the solid phases showed that dissolution of alite and aluminate slowed down while analyses of the pore solution showed that citric acid was removed almost completely from the pore solution within the first hours of hydration. The complexation of the ions by citrate was weak, which could also be confirmed by thermodynamic calculations. Only 2% of the dissolved Ca and 0.001% of the dissolved K formed complexes with citrate during the first hours. Thus, citric acid retards cement hydration not by complex formation, but by slowing down the dissolution of the clinker grains. Thermodynamic calculations did not indicate precipitation of a crystalline citrate species. Thus, it is suggested that citrate sorbed onto the clinker surface and formed a protective layer around the clinker grains retarding their dissolution.

36 MATERIALS SCIENCE↗

Modeling the degradation of Portland cement pastes by biogenic organic acids

Reactive transport models can be used to assess the long-term performance of cement-based materials subjected to biodegradation. A bioleaching test (with Aspergillus niger fungi) applied to ordinary Portland cement pastes during 15 months is modeled with HYTEC. Modeling indicates that the biogenic organic acids (acetic, butyric, lactic and oxalic) strongly accelerate hydrate dissolution by acidic hydrolysis whilst their complexation of aluminum has an effect on the secondary gel stability only. The deepest degradation front corresponds to portlandite dissolution and decalcification of calcium silicate hydrates. A complex pattern of sulfate phases dissolution and precipitation takes place in an intermediate zone. The outermost degraded zone consists of alumina and silica gels. The modeling accurateness of calcium leaching, pH evolution and degradation thickness is consistently enhanced whilst considering increase of diffusivity in the degraded zones. Precipitation of calcium oxalate is predicted by modeling but was hindered in the bioleaching reactor.

36 MATERIALS SCIENCE↗

In-situ early-age hydration study of sulfobelite cements by synchrotron powder diffraction

Eco-friendly belite calcium sulfoaluminate (BCSA) cement hydration behavior is not yet well understood. Here, we report an in-situ synchrotron X-ray powder diffraction study for the first hours of hydration of BCSA cements. Rietveld quantitative phase analysis has been used to establish the degree of reaction (α). The hydration of a mixture of ye'elimite and gypsum revealed that ettringite formation (α ∼ 70% at 50 h) is limited by ye'elimite dissolution. Two laboratory-prepared BCSA cements were also studied: non-active-BCSA and active-BCSA cements, with β- and α′{sub H}-belite as main phases, respectively. Ye'elimite, in the non-active-BCSA system, dissolves at higher pace (α ∼ 25% at 1 h) than in the active-BCSA one (α ∼ 10% at 1 h), with differences in the crystallization of ettringite (α ∼ 30% and α ∼ 5%, respectively). This behavior has strongly affected subsequent belite and ferrite reactivities, yielding stratlingite and other layered phases in non-active-BCSA. The dissolution and crystallization processes are reported and discussed in detail. -- Highlights: •Belite calcium sulfoaluminate cements early hydration mechanism has been determined. •Belite hydration strongly depends on availability of aluminum hydroxide. •Orthorhombic ye’elimite dissolved at a higher pace than cubic one. •Ye’elimite larger reaction degree yields stratlingite formation by belite reaction. •Rietveld method quantified gypsum, anhydrite and bassanite dissolution rates.

36 MATERIALS SCIENCE↗

Effect of retarders on the early hydration of calcium-sulpho-aluminate (CSA) type cements

The retardation of calcium-sulpho-aluminate (CSA) type cements by three common retarders—sodium gluconate, sodium–potassium tartrate and borax is investigated at a 2% addition rate. Each of the retarders has a different effect on the early-age hydrate assemblage, as shown by quantitative X-ray diffraction, thermogravimetric analysis, scanning electron microscopy and pore solution analysis. Regardless of the retarder used, the hydration starts with mainly the dissolution of ready soluble (calcium) alkali sulphates and ye'elimite, followed by the formation of ettringite and aluminium hydroxide, whereby the specific clinker mineral dissolution as well as ettringite-forming reaction is delayed in different ways depending on the retarder used. The results showed that the retardation is mainly caused by preventing hydrates formation in the case of tartrate and gluconate. Contrary, borax retards the hydration by preventing to a certain extent the dissolution of ye'elimite and lowers the initial pH. Furthermore, the morphology of ettringite is altered depending on the type of the retarder used.

36 MATERIALS SCIENCE↗

Modelling of the sulfuric acid attack on different types of cementitious materials

A chemical-reactive transport model is used to simulate the sulfuric acid attack of cement pastes based on ordinary Portland cement (CEM I), blended Portland cements (CEM III, CEM IV, and CEM V), and calcium aluminate cement (CAC). This model accounts for the dissolution of cement hydrates (portlandite, C-S-H, hydrogarnet), and the precipitation of deterioration products (ettringite and gypsum). Moreover, diffusion of the aqueous species in the pore space of the material is considered. With this model, the hydrate contents, the porosity, and the deterioration phase contents throughout a sulfuric acid attack are determined. Two indicators are defined to predict the service life of the cementitious materials: the deterioration depth and the dissolved calcium content. These two indicators show that calcium aluminate cement has a better resistance to sulfuric acid attack than that of Portland cements. This better resistance is mainly due to the partial dissolution of CAC hydrate as opposed to the total dissolutions of CH and C-S-H.

36 MATERIALS SCIENCE↗

Synchrotron X-ray nanotomographic and spectromicroscopic study of the tricalcium aluminate hydration in the presence of gypsum

The rheology of modern Portland cement (PC) concrete critically depends on the correct dosage of gypsum (calcium sulfate hydrate) to control the hydration of the most reactive phase - tricalcium aluminate (C{sub 3}A). The underlying physio-chemical mechanism, however, remains unsolved mainly due to the lack of high-spatial-resolved and chemistry-sensitive characterization of the C{sub 3}A dissolution frontier. Here, we fill this gap by integrating synchrotron-radiation based crystallographic, photon-energy-dependent spectroscopic and high-resolution morphological studies of the C{sub 3}A hydration product layer. We propose that ettringite (6CaO·Al{sub 2}O{sub 3}·SO{sub 3}·32H{sub 2}O) is the only hydration product after the initial reaction period and before complete gypsum dissolution. We quantify the 2D and 3D morphology of the ettringite network, e.g. the packing density of ettringite at various surface locations and the surface dissolution heterogeneity. Our results show no trace of a rate-controlling diffusion barrier. We expect our work to have significant impact on modeling the kinetics and morphological evolution of PC hydration.

36 MATERIALS SCIENCE↗

Corrosion of 316 L stainless steel under the natural circulation of molten NaCl-MgCl 2 salt

The corrosion behavior of 316 L stainless steel (SS) was studied via the natural circulation of molten eutectic NaCl-MgCl 2 salt through a microloop. The post-corrosion tested 316 L SS microloop sections were characterized with microscopy techniques to determine the microstructural and microchemical changes that occurred at the alloy/salt interface. It was found that 316 L SS showed heterogeneous dissolution at the hot-leg, whereas deposition of corrosion products occurred at the cold-leg. For the first time, experimentally obtained molten salt flow-induced corrosion of 316 L SS results were combined with computational thermodynamic-kinetic models to validate the dissolution and deposition in terms of elemental compositional changes at the alloy/salt interface. The thermodynamic-kinetic modeling predicted that the heterogeneous dissolution of Cr and Fe from the hot-leg section of 316 L SS persisted throughout the salt circulation. The model also estimated that, despite Cr deposition starting earlier than Fe, the total redeposition of Fe is expected to be significantly greater than that of Cr over the circulation of salt. Furthermore, the modeling accurately predicted the subsurface enrichment of Mo which is attributed to the reduced Cr activity and the relatively higher diffusion rate of Mo within the alloy matrix. Here, the agreement between modeling and experimental results confirms that Fe chlorides dissolve at the hot-leg and subsequently deposit at the cold-leg due to activity changes driven by the thermal gradient. By contrast, Cr was not detected in the cold-leg deposits, which is attributed to its weaker temperature dependence on activity, limiting its redeposition under these conditions.

36 - MATERIALS SCIENCE↗

3.5 billion years of glass bioalteration: Volcanic rocks as a basis for microbial life?

Alteration textures in volcanic glass from the seafloor fall into two classes, one suggestive of abiotic/diffusive hydration and chemical exchange, and another likely to be caused by microbial, cavity-forming, congruent dissolution. Glass bioalteration is common in submarine lavas throughout the world's ocean, dominant in the upper 300 m of the oceanic crust, and found in all well-preserved ophiolites and greenstone belts dating back to 3.5 Ga. It may yield a significant fraction of the global biomass and geochemical fluxes and is relevant to the development of the earliest life on Earth. We present a critical review concerning these glass bioalteration textures and present new data on their microchemical environment. We explore arguments for their biogenicity and further develop the prevalent model for their formation by relating corrosion morphology to the mechanism of microbial dissolution. Biological alteration produces conspicuous micron-scale granular and tubular textures. Granular glass alteration is well explained by colonizing microbes that selectively dissolve the glass in their contact area, forming a sponge-like interconnected network of micron-sized cavities along glass surfaces. Tubular alteration meanwhile, is more likely to be caused by filamentous cell extensions in a process similar to fungal tunneling of soil feldspars and marine carbonates. While we see clear functional similarities to fungal dissolution behavior, we do not know whether fungal or prokaryotic organisms are involved. However, this functional constraint may eventually help to identify potential microbes responsible for these features, potentially including eukaryotic or prokaryotic organisms. Yet, we caution that these organisms may be difficult to identify and to study, because they are likely to be sparsely distributed, slow growing, and difficult to cultivate.

09 BIOMASS FUELS↗