Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SINTERED MATERIALS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,117 records · Page 62

Multi-scale modeling of the evolution of structure and properties in materials for nuclear energy applications

Nuclear energy is an important component of an overall strategy to address climate change. Idaho National Laboratory (INL) is the U.S. Department of Energy’s primary facility for research and development in nuclear science and technology for energy generation, supporting the improvement and life extension of the existing reactor fleet and the development and licensing of new reactor designs. Computational modeling is an important component of these activities, particularly in the area of materials for nuclear applications, where experimental data can be very challenging and expensive to acquire, and where data is especially scarce for new reactor designs. INL has used multi-scale modeling – linking atomistic, mesoscale, and engineering scales – to improve the ability to predict the performance of materials for nuclear energy applications. These modeling efforts make extensive of MOOSE (Multiphysics Object-Oriented Simulation Environment), a general-purpose open source finite element framework developed at INL. In this talk, I will give an overview of the approach and tools used, and several examples of application, including performance of nuclear fuels, understanding radiation-driven formation of nanoscale void and gas bubble superlattices, and powder densification through electric field assisted sintering.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Porous acicular mullite obtained by controlled oxidation of waste molybdenum disilicide

Highlights: • Waste MoSi{sub 2} heating elements were used as starting material for fabrication of porous acicular mullite. • Calcined MoSi{sub 2} powder was source of SiO{sub 2} and pore former at the same time. • Porous acicular mullite is promising material for filtration of diesel engine exhaust. • Samples with decent mechanical integrity and porosity of more than 60% were fabricated. - Abstract: Porous acicular mullite was fabricated by using waste MoSi{sub 2} heating element and Al{sub 2}O{sub 3}. Careful calcination of the pulverized heating element led to the formation of a mixture of MoO{sub 3} and amorphous SiO{sub 2}. This mixture was employed as both SiO{sub 2} precursor and pore former. The oxidation of MoSi{sub 2} and mullite formation were studied. The effect of fabrication temperature on phase composition, porosity, grain morphology, and compressive strength of sintered mullite was examined. Pure mullite with porosity of more than 60% and compressive strength of ∼20 MPa was obtained at temperature as low as 1300 °C. The microstructure consisted of elongated, rectangular, prism-like grains which are known to be effective in filtration of diesel engine exhaust. The increase in sintering temperature caused the change of grain morphology and reduction in compressive strength.

36 MATERIALS SCIENCE↗

Interfacial characterization in carbon nanotube reinforced aluminum matrix composites

In this work, the effects of the sintering parameters, such as temperature and the techniques used (HP and SPS), on CNT/Al composite interfaces are studied. The major role of the native aluminum oxide (Al{sub 2}O{sub 3}) layer covering the aluminum grains is highlighted. It is shown that, for a sintering temperature below 620 °C, the amorphous Al{sub 2}O{sub 3} layer prevents the reaction between aluminum and carbon. For greater sintering temperatures, the breaking of the oxide layer due to its crystallization leads to the formation of aluminum carbide (Al{sub 4}C{sub 3}) by reaction between aluminum and the CNT. The Al{sub 4}C{sub 3} crystals grow perpendicularly to the matrix grain boundaries by thermally activated diffusion of the carbon atoms coming from the CNT. It is also demonstrated that, by limiting the sintering time, which is the case in SPS, it is possible to limit the growth of the Al{sub 4}C{sub 3} crystals and thus to preserve the CNT. - Highlights: • The high reactivity between CNT and Al matrix, resulting Al{sub 4}C{sub 3} formation during the sintering process is highlighted. • We demonstrate, thanks to in-situ TEM observations, that Al{sub 4}C{sub 3} crystals grow into aluminum grains by carbon diffusion. • The native aluminum oxide around the aluminum particles prevents the diffusion of carbon into the aluminum grains. • We show that the protective layer can be broken because of its crystallization, leading to the formation of Al{sub 4}C{sub 3}. • SPS, by limiting the sintering duration, is an interesting way for preparing CNT/Al composites without carbide formation.

36 MATERIALS SCIENCE↗

U Metal Oxidation with Steam (U)

The Savannah Rive National Laboratory 9SRNL) is evaluating a method to produce uranium oxide (UO 2 ) from uranium metal using steam. The typical methods for making UO 2 yield powders with particle-size ranges of 1 to 50 micron. The goal of the steam oxidation is to produce a depleted uranium (DU) product with a larger particle size that can be used as a surrogate for testing physical and mechanical process techniques to refine uranium and/or plutonium bearing residues. Several studies in the literature indicated that reactions between uranium metal and steam will yield UO 2 as fine powders in the 160 to 500 °C range, but granular materials form above 500°C. Above 880 °C, a hard compact scale forms on the U metal. Furthermore, sintering of UO 2 occurs at about 1300 °C, but it has been stated that the presence of steam enhances the sintering characteristics of UO 2 . Initial studies into the oxidation of DU metal in an atmosphere of argon and steam have been completed. Oxidation of depleted uranium metal in Ar/steam at 600, 710, 700, and 830 °C yielded at UO 2 product with little or no impurity at each temperature. Although not enough sample was available to perform sieve analysis for particle size distribution, SEM images reveal that a significant volume fraction of the products at 710, 770, and 830 °C exceeds 100 microns. The material produced at 600 °C was too fine for programmatic needs. Questions associated with the UO 2 include morphology of product, mechanical strength of the particles, and performance in milling operations. The size of the samples produced in these tests did not allow for quantitative assessment of particle size of mechanical strength. A qualitative assessment of the particles formed at 710, 770, and 830 °C was that the samples produced at 710 and 770 °C were friable, and the sample produced 830 °C had more mechanical strength. Sintering of the samples in Ar/steam at 970 °C appeared to increase the strength of the particles without changing their general particle size characteristics. Due to the small sample sizes, the increase in strength could not be quantified. If the sintering at 970 °C is inadequate, higher sintering temperatures in Ar/steam can be evaluated. Future work will increase scale of the steam oxidation conditions which yield the most-favorable particle-size distributions with sufficient mechanical strength for programming usage. Further consideration will be given to oxidation temperature, steam addition to the reaction vessel, U metal pretreatment, and sintering conditions after oxidation. The UO 2 production could involve a two-step process where particles are formed in steam at lower temperatures (700-850 °C) and then sintered in Ar/steam at elevated temperatures (950-1200 °C). Larger samples (50-100 g each) will provide sufficient UO 2 product for sieve analysis and assessment of mechanical strength relatives to subsequent milling operations.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Cyclic moisture reactivation of calcium sorbents for long duration thermochemical energy storage

The transition to a flexible and reliable energy infrastructure, using electro-thermal energy generation technologies such as geothermal, concentrated solar power, and nuclear, usually demands simultaneous advancement of thermal energy storage (TES) to support on-demand electricity generation and industrial applications while mitigating the inherent intermittency of renewable energy sources and power outages from direct energy generation. Among TES technologies, thermochemical energy storage (TCES) based on calcium looping emerges as a compelling high-power energy storage candidate due to its high reaction enthalpy, compatibility with elevated operating temperatures, and abundance of low-cost materials. However, the long-term durability of calcium-based sorbents for TCES is hindered by surface sintering and particle aggregation, leading to performance degradation over repeated thermal cycles. This study explores a moisture hydration-based strategy to regenerate a degraded calcium sorbent and mitigate performance degradation for long duration TCES. The addition of moisture transforms calcium oxide into calcium hydroxide and produces intercalation water layers, associated with a regenerated surface area and reduced calcium oxide crystallite size. Both these effects are beneficial in restoring the sorbents' reactivity for carbonization. Additionally, an optimized hydration-assisted reactivation protocol balances the recovered energy storage capacity with heating penalty required for moisture removal from hydrated samples, resulting in an enhanced energy storage capacity up to 176% compared to benchmark sorbents that undergo cycling without reactivation after 60 cycles. In conclusion, these results highlight the potential of hydration-assisted reactivation to enhance the long-term performance of TCES, providing an effective pathway to advancing electro-thermal storage technologies.

36 MATERIALS SCIENCE↗

Electrical and thermal properties of Fe substituted double-filled Ba{sub x}Yb{sub y}Fe{sub z}Co{sub 4-z}Sb{sub 12} skutterudites

Fe-substituted double-filled Ba{sub x}Yb{sub y}Fe{sub z}Co{sub 4-z}Sb{sub 12} (x=0.1, y=0.2 and z=0.0-0.4 nominal) compounds were synthesized using a melting-annealing-spark plasma sintering (SPS) method. Their thermoelectric properties were assessed by measuring the Seebeck coefficient, electrical conductivity, thermal conductivity and the Hall coefficient. The sign of the Hall coefficient indicates that electrons are the dominant carriers in all compounds except Ba{sub 0.1}Yb{sub 0.2}Fe{sub 0.4}Co{sub 3.6}Sb{sub 12}. The temperature dependence of the electrical conductivity and the carrier concentration reflect the transition from extrinsic to intrinsic behavior depending on the amount of Fe substituted for Co. Jonker and Ioffe analyses are applied to Fe-substituted double-filled Ba{sub x}Yb{sub y}Fe{sub z}Co{sub 4-z}Sb{sub 12} compounds in order to evaluate the range of minimum and maximum power factors achievable in n-type filled skutterudite compounds at room temperature (300 K). The predicted maximum room temperature power factor values in the range of 15-45 {mu}W/K{sup 2} cm are comparable to experimentally reported values of n-type skutterudite compounds. - Graphical abstract: Room temperature Jonker plot of Ba{sub x}Yb{sub y}Fe{sub z}Co{sub 4-z}Sb{sub 12} samples. Highlights: Black-Right-Pointing-Pointer The TE properties of Ba{sub x}Yb{sub y}Fe{sub z}Co{sub 4-z}Sb{sub 12} compounds were investigated. Black-Right-Pointing-Pointer Jonker and Ioffe analysis applied in order to predict the range of power factor achievable at room temperature. Black-Right-Pointing-Pointer The thermal conductivity is strongly suppressed with increasing of Fe substitution on Co site. Black-Right-Pointing-Pointer We see that small quantities of Fe on Co site is beneficial on enhancement ZT value.

36 MATERIALS SCIENCE↗

Embedding of Optical Fibers with Electric Field Assisted Sintering

The Electric Field Assisted Sintering (EFAS) technique was used for embedding the fibers, involving rapid heating via an electric current and pressure, reducing fiber exposure to high temperatures. Stainless steel guide tubes were inserted at the fiber-matrix junctions to prevent fiber breakage during the sintering process. The study varied key EFAS parameters—temperature (800°C to 980°C), pressure (40-50 MPa), and hold time (5-10 minutes)—to assess how they influenced fiber embedding. After embedding, the fibers were inspected using optical frequency domain reflectometry (OFDR) to evaluate optical losses and strain along the fiber length. The OFDR scans confirmed that the fibers remained intact, and subsequent transmission tests demonstrated no macroscopic fractures. The embedded samples were also analyzed using scanning electron microscopy (SEM) and X-ray computed tomography (CT) scans. These tests confirmed good bonding between the fiber and matrix with no cracking, though some porosity was present in samples fabricated at lower temperatures. At higher temperatures (980°C), the fiber-matrix bonding was continuous and defect-free, with metal coatings aiding in the bonding process. Elemental analysis showed interdiffusion between the fiber coatings and matrix materials, particularly between the gold coating and stainless steel. Helium leak tests revealed that lower sintering temperatures resulted in matrix porosity, causing leaks, but samples fabricated at 980°C were leak-tight.

46 - INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AN↗

Sliding Wear Behavior of Spark-Plasma-Sintered Fe-Based Amorphous Alloy Coatings on Cu-Ni Alloy

This paper reports on the processing of Fe{sub 48}Cr{sub 15}Mo{sub 14}Y{sub 2}C{sub 15}B{sub 6} amorphous alloy coatings on Cu-10%Ni (wt.%) alloy using spark plasma sintering. The amorphous alloy coatings were sintered at temperatures ranging from 575 to 675 °C at a pressure of 50 MPa. The development of microstructure, phases, and wear properties with sintering temperature of the coatings is investigated. The sintered coatings were found to be near fully dense with hardness close to that of the sintered bulk amorphous alloy. X-ray analysis indicated increasing degree of devitrification of the amorphous coatings with increasing sintering temperature. The wear behavior of the coatings is significantly influenced by the sintering temperature with volume wear rate first decreasing in the temperature range of 575-650 °C and then increasing above 650 °C. The variation in wear behavior is explained based on relative stability of the protective surface layer and embrittlement of the surface with the sintering temperature.

36 MATERIALS SCIENCE↗

Microwave-assisted synthesis: A fast and efficient route to produce LaMO{sub 3} (M = Al, Cr, Mn, Fe, Co) perovskite materials

Research highlights: {yields} Lanthanum perovskites can be prepared by microwave irradiation in a domestic set-up. {yields} Microwave-assisted synthesis yields well crystallized and pure materials, sometimes nanosized. {yields} Rietveld analysis has been performed to refine the structures. {yields} Magnetic and electric measurements are similar to those previously reported. {yields} Microwave-assisted synthesis is a fast and efficient method for the synthesis of lanthanum perovskites. -- Abstract: A series of lanthanum perovskites, LaMO{sub 3} (M = Al, Cr, Mn, Fe, Co), having important technological applications, have been successfully prepared by a very fast, inexpensive, reproducible, environment-friendly method: the microwave irradiation of the corresponding mixtures of nitrates. Worth to note, the microwave source is a domestic microwave oven. In some cases the reaction takes place in a single step, while sometimes further annealings are necessary. For doped materials the method has to be combined with others such as sol-gel. Usually, nanopowders are produced which yield high density pellets after sintering. Rietveld analysis, oxygen stoichiometry, microstructure and magnetic measurements are presented.

36 MATERIALS SCIENCE↗

Manufacturing of Thermoset Polyimide Composites by Laser Sintering

Selective Laser Sintering (SLS) is an additive manufacturing technique that builds 3D models layer by layer using a laser to selectively melt cross sections in powdered polymeric materials, following sequential slices of the computer-aided design (CAD) model. SLS generally uses thermoplastic polymeric powders such as polyamides. The resultant 3D-printed objects are often weaker in their strength compared to traditionally processed materials, due to their higher porosity. This paper described the process development of using melt-processable imide oligomers terminated with reactive 4-phenylethynylphthalic anhydride (4-PEPA) to conduct laser sintering (LS). The first successful 3D-printing of high temperature RTM370 thermoset polyimide carbon fiber composites were further post-cured to promote additional crosslinking for achieving higher temperature (T g = 370°C) capability. Another novel imide oligomer, RTM385-SLS, formulated with a complex melt viscosity [ƞ*] of ~104-105 poise is also suitable for LS. RTM385-SLS resin powder was mixed with 20-25% of hexagonal boron nitride (h-BN) and subjected to LS to print out “Green” specimens which could be further post-cured to afford a thermally conductive but electrically insulating composites with high T g of 385 °C. The cured composite specimens were then subjected to mechanical testing, thermal conductivity and porosity measurements as well as SEM characterization.

additive Manufacturing↗

Self-propagating high-temperature synthesis of Lu{sub 2}O{sub 3} powders for optical ceramics

A technique has been developed for the self-propagating high-temperature synthesis of lutetium oxide (Lu{sub 2}O{sub 3}) powders using citric acid, glycine, and lutetium acetate as fuels. We have carried out thermodynamic analysis of synthesis conditions and examined the effect of the nature of the fuel on the properties of the resultant powders. Using vacuum sintering at a temperature of 1780°C and powders prepared with glycine as a fuel and containing 25 mol % yttrium oxide and 5 mol % lanthanum oxide as sintering aids, we have obtained transparent lutetium oxide-based ceramics.

36 MATERIALS SCIENCE↗

Enhancement of thermal shock resistance of reaction sintered mullite–zirconia composites in the presence of lanthanum oxide

Mullite–zirconia composites containing 20 wt.% zirconia were prepared by reaction sintering of zircon flour, sillimanite beach sand and calcined alumina. 0 to 8 mol% of La{sub 2}O{sub 3} with respect to zirconia was used as sintering aid. The effect of additive on the various physical, microstructures, mechanical and thermo-mechanical properties was studied. Quantitative phase analysis shows the change in tetragonal zirconia content with incorporation of lanthanum oxide. La{sub 2}O{sub 3} addition has significantly improved the thermal shock resistance of the samples. Samples without additive retained only 20% of initial flexural strength after 5 cycles, whereas samples containing 5 mol% La{sub 2}O{sub 3} retained almost 78% of its initial flexural strength even after 15 thermal shock cycles. - Highlights: • Mullite–zirconia composites were prepared by reaction sintering route utilizing zircon and sillimanite beach sand. • Lanthanum oxide was used as sintering aid. • The presence of lanthanum oxide decreased the densification temperature. • Lanthanum oxide significantly improved the thermal shock resistance of the composites.

36 MATERIALS SCIENCE↗

Complex shaped boron carbides from negative additive manufacturing

In this paper, complex shaped boron carbide with carbon (B 4 C/C) at near-full densities were achieved for the first time using negative additive manufacturing techniques via gelcasting. Negative additive manufacturing involves 3D printing of sacrificial molds used for casting negative copies. B 4 C powder distributions and rheology of suspensions were optimized to successfully cast complex shapes. In addition to demonstrating scalability of these complex geometries, hierarchically meso-porous structures were also shown to be possible from this technique. Resorcinol-Formaldehyde (RF) polymer was selected as the gelling agent and can also pyrolyze into a carbon aerogel network to act as the sintering aid for B 4 C. Finally, due to the highly effective distribution of in situ carbon for the B 4 C matrix, near-full sintered density of 97–98% of theoretical maximum density was achieved.

36 MATERIALS SCIENCE↗

Dielectric and magnetic properties of CoFe2O4 prepared by sol-gel auto-combustion method

Cobalt ferrite powders were successfully synthesized by sol-gel auto-combustion method. Influence of sintering temperature on structural, magnetic and dielectric properties was studied. All the obtained samples are spinel ferrite with a cubic symmetry. As the sintering temperature increased from 900 °C to 1300 °C, the average grain size increased from 0.26 μm to 0.83 μm. The dielectric constant and loss tangent measurement showed strong temperature dependence at all frequencies. The maximum magnetization increased while the coercivity and remanent magnetization decreased with the increasing sintering temperature. The non-saturation at high fields may be related to the surface effects in CoFe{sub 2}O{sub 4} samples. When sintered at 1300 °C, the sample showed a maximum magnetization value of ∼87.32 emu/g at room temperature. The highest value of coercivity of all the samples was 1368.33 Oe for the sample sintered at 900 °C.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Evolution of Gold Structure During Thermal Treatment of Au/FeOx Catalysts Revealed by Aberration-Corrected Electron Microscopy

High-resolution aberration-corrected electron microscopy was performed on a series of catalysts derived from a parent material, 2 at.% Au/Fe{sub 2}O{sub 3} (WGC ref. no. 60C), prepared by co-precipitation and calcined in air at 400 C, and a catalyst prepared by leaching surface gold from the parent catalyst and exposed to various treatments, including use in the water-gas shift reaction at 250 C. Aberration-corrected JEOL 2200FS (JEOL USA, Peabody, MA) and Vacuum Generators HB-603U STEM instruments were used to image fresh, reduced, leached, used and re-oxidized catalyst samples. A new in situ heating technology (Protochips Inc., Raleigh, NC, USA), which permits full sub-Angstrom imaging resolution in the JEOL 2200FS was used to study the effects of temperature on the behavior of gold species. A remarkable stability of gold to redox treatments up to 400 C, with atomic gold decorating step surfaces of iron oxide was identified. On heating the samples in vacuum to 700 C, it was found that monodispersed gold began to sinter to form nanoparticles above 500 C. Gold species internal to the iron oxide support material was shown to diffuse to the surface at elevated temperature, coalescing into discrete nanocrystals. The results demonstrate the value of in situ heating for understanding morphological changes in the catalyst with elevated temperature treatments.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Ceramics from self-sustained reactions: Recent advances

Specific applications of self-sustained reactions to fabricate advanced ceramics, along with details such as synthesis conditions, mechanism of microstructure formation, and material properties, are overviewed. The latest achievements in the field include analysis of three such synthetic routes: reactive spark plasma sintering, combustion synthesis with mechanical stimulation, and solution combustion synthesis. Examples of fabrication of high-temperature nanostructured ceramics and composites, as well as non-equilibrium ceramic phases are also discussed.

36 MATERIALS SCIENCE↗

Performance of Nd-Fe-B Magnets Fabricated by Hot Isostatic Pressing and Low-Temperature Sintering

Magnetic properties and microstructure of Nd-Fe-B sintered magnets fabricated by hot isostatic pressing (HIP) were studied. For comparison, magnets were also fabricated by vacuum sintering. The density reached 7.58 g/cm{sup 3} for the magnets HIP-sintered at 1123 K. The density of the magnets vacuum-sintered at 1123 K was much lower, which is of about 6.92 g/cm{sup 3}. While the density of magnets vacuum-sintered at 1318 K was the same as the HIP-sintered magnets, the sintering temperature was significantly decreased to 1123 K. In addition, the average grain size decreased from 9 to 6 μm, which has enhanced coercivity. Therefore, the coercivity increased from 1067.7 to 1238.5 kA/m, which is 16% higher than the vacuum-sintered magnets. HIP is a promising method to obtain high density and high coercivity Nd-Fe-B sintered magnets.

36 MATERIALS SCIENCE↗

Deformation and Tensile Cyclic Fatigue of Plasma-Sprayed ZrO2-8wt% Y2O3 Thermal Barrier Coatings

Deformation (constitutive relations) of free-standing, thick thermal barrier coatings of sprayed ZrO2-8Wt% Y2O3 was determined at ambient temperature in both pure tension and pure compression using cylindrical bar test specimens. The material exhibited both significant nonlinearity and hysteresis in its load-strain curves, The load-strain relations in four-point uniaxial flexure were determined from tension and compression sides and were compared with individual pure tension and compression constitutive data. Effect of sintering on deformation behavior was significant, resulting in a dramatic change in constitutive relation. Cyclic fatigue testing of the coating material in tension-tension at room temperature showed an insignificant susceptibility to fatigue, similar to the slow crack growth behavior of the material in flexure in 800 C air.

Choi, Sung R.↗