Revised phase diagram of Li{sub 2}MoO{sub 4}-ZnMoO{sub 4} system, crystal structure and crystal growth of lithium zinc molybdate

Orthorhombic lithium zinc molybdate was first chosen and explored as a candidate for double beta decay experiments with {sup 100}Mo. The phase equilibria in the system Li{sub 2}MoO{sub 4}-ZnMoO{sub 4} were reinvestigated, the intermediate compound Li{sub 2}Zn{sub 2}(MoO{sub 4}){sub 3} of the alpha-Cu{sub 3}Fe{sub 4}(VO{sub 4}){sub 6} (lyonsite) type was found to be nonstoichiometric: Li{sub 2-2x}Zn{sub 2+x}(MoO{sub 4}){sub 3} (0<=x<=0.28) at 600 deg. C. The eutectic point corresponds to 650 deg. C and 23 mol% ZnMoO{sub 4}, the peritectic point is at 885 deg. C and 67 mol% ZnMoO{sub 4}. Single crystals of the compound were prepared by spontaneous crystallization from the melts and fluxes. In the structures of four Li{sub 2-2x}Zn{sub 2+x}(MoO{sub 4}){sub 3} crystals (x=0; 0.03; 0.21; 0.23), the cationic sites in the face-shared octahedral columns were found to be partially filled and responsible for the compound nonstoichiometry. It was first showed that with increasing the x value and the number of vacancies in M3 site, the average M3-O distance grows and the lithium content in this site decreases almost linearly. Using the low-thermal-gradient Czochralski technique, optically homogeneous large crystals of lithium zinc molybdate were grown and their optical, luminescent and scintillating properties were explored. - Graphical abstract: The phase diagram of the system Li{sub 2}MoO{sub 4}-ZnMoO{sub 4} was revised, Li{sub 2-2x}Zn{sub 2+x}(MoO{sub 4}){sub 3} (0<=x<=0.28 at 600 deg. C) isotypical to alpha-Cu{sub 3}Fe{sub 4}(VO{sub 4}){sub 6} was found. Structural studies for x=0; 0.03; 0.21; 0.23 show consecutive increasing the number of vacancies and atomic displacement anisotropy in the face-shared octahedral columns. Large Li{sub 2}Zn{sub 2}(MoO{sub 4}){sub 3} crystals were grown and their optical, luminescent and scintillating properties were explored.

36 MATERIALS SCIENCE↗

Low temperature molten-salt synthesis of nanocrystalline cubic Sr{sub 2}SbMnO{sub 6}

Sr{sub 2}SbMnO{sub 6} (SSM) powders were successfully synthesized at reasonably low temperatures via molten-salt synthesis (MSS) method using eutectic composition of 0.635 Li{sub 2}SO{sub 4}-0.365 Na{sub 2}SO{sub 4} (flux). High-temperature cubic phase SSM was stabilized at room temperature by calcining the as-synthesized powders at 900 deg. C/10 h. The phase formation and morphology of these powders were characterized via X-ray powder diffraction and scanning electron microscopy, respectively. The SSM phase formation associated with {approx}60 nm sized crystallites was also confirmed by transmission electron microscopy. The activation energy associated with the particle growth was found to be 95+-5 kJ mol{sup -1}. The dielectric constant of the tetragonal phase of the ceramic (fabricated using this cubic phase powder) with and without the flux (sulphates) has been monitored as a function of frequency (100 Hz-1 MHz) at room temperature. Internal barrier layer capacitance (IBLC) model was invoked to rationalize the dielectric properties. - Graphical abstract: The as synthesized powders of Sr{sub 2}SbMnO{sub 6} calcined at 900 deg. C/10 h yielded a cubic phase ({approx}60 nm sized crystallites). Centrosymmetric tetragonal (I4/mcm) phase was obtained by increasing the calcination temperature to 1000 deg. C. Display Omitted

36 MATERIALS SCIENCE↗

Study of phase relationships in the Sr{sub 3}(PO{sub 4}){sub 2}–CePO{sub 4} system. Phase diagram and thermal characteristics of phases

A diagram representing phase relationships in the Sr{sub 3}(PO{sub 4}){sub 2}–CePO{sub 4} phosphate system has been developed on the basis of results obtained by thermal analysis (DTA/DSC/TGA) and X-ray diffraction (XRD) methods. One intermediate compound with the formula Sr{sub 3}Ce(PO{sub 4}){sub 3} occurs in the Sr{sub 3}(PO{sub 4}){sub 2}–CePO{sub 4} system at temperatures exceeding 1045 °C. The compound has a eulytite structure with the following structural parameters: a=b=c=10.1655(8) Å, α=β=γ=90.00°, V=1050.46(6) Å{sup 3}. It's melting point exceeds 1950 °C. A limited solid solution exists in the system, which possesses the structure of a low-temperature form of Sr{sub 3}(PO{sub 4}){sub 2}. At 1000 °C the maximal concentration of CePO{sub 4} in the solid solution is below 20 mol%. The solid solution phase field narrows with increased temperature. There is a eutectic point in the (Sr{sub 3}(PO{sub 4}){sub 2}+Sr{sub 3}Ce(PO{sub 4}){sub 3}) phase field at 1765 °C and 15 mol% of CePO{sub 4}. The melting temperature of Sr{sub 3}(PO{sub 4}){sub 2} is 1882±15 °C. - Graphical abstract: The phase diagram of Sr{sub 3}(PO{sub 4}){sub 2}–CePO{sub 4} system showing the stability ranges of limited solid solution and Sr{sub 3}Ce(PO{sub 4}){sub 3} phases. - Highlights: • Sr{sub 3}(PO{sub 4}){sub 2} melts at 1882 °C. • Phase diagram of Sr{sub 3}(PO{sub 4}){sub 2}–CePO{sub 4} system has been proposed. • Limited solid solution of CePO{sub 4} in Sr{sub 3}(PO{sub 4}){sub 2} forms in the system. • The Sr{sub 3}Ce(PO{sub 4}){sub 2} phosphate is stable at temperatures above 1045 °C.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High temperature redox reactions with uranium: Synthesis and characterization of Cs(UO{sub 2})Cl(SeO{sub 3}), Rb{sub 2}(UO{sub 2}){sub 3}O{sub 2}(SeO{sub 3}){sub 2}, and RbNa{sub 5}U{sub 2}(SO{sub 4}){sub 7}

Cs(UO{sub 2})Cl(SeO{sub 3}) (1), Rb{sub 2}(UO{sub 2}){sub 3}O{sub 2}(SeO{sub 3}){sub 3} (2), and RbNa{sub 5}U{sub 2}(SO{sub 4}){sub 7} (3) single crystals were synthesized using CsCl, RbCl, and a CuCl/NaCl eutectic mixture as fluxes, respectively. Their lattice parameters and space groups are as follows: P2{sub 1}/n (a=6.548(1) Å, b=11.052(2) Å, c=10.666(2) Å and β=93.897(3)°), P1{sup ¯} (a=7.051(2) Å, b=7.198(2) Å, c=8.314(2) Å, α=107.897(3)°, β=102.687(3)° and γ=100.564(3)°) and C2/c (a=17.862(4) Å, b=6.931(1) Å, c=20.133(4) Å and β=109.737(6)°. The small anionic building units found in these compounds are SeO{sub 3}{sup 2−} and SO{sub 4}{sup 2−} tetrahedra, oxide, and chloride. The crystal structure of the first compound is composed of [(UO{sub 2}){sub 2}Cl{sub 2}(SeO{sub 3}){sub 2}]{sup 2−} chains separated by Cs{sup +} cations. The structure of (2) is constructed from [(UO{sub 2}){sub 3}O{sub 11}]{sup 16−} chains further connected through selenite units into layers stacked perpendicularly to the [0 1 0] direction, with Rb{sup +} cations intercalating between them. The structure of compound (3) is made of uranyl sulfate layers formed by edge and vertex connections between dimeric [U{sub 2}O{sub 16}] and [SO{sub 4}] polyhedra. These layers contain unusual sulfate–metal connectivity as well as large voids. - Graphical abstract: A new family of uranyl selenites and sulfates has been prepared by high-temperature redox reactions. This compounds display new bonding motifs. Display Omitted - Highlights: • Low-dimensional Uranyl Oxoanion compounds. • Conversion of U(IV) to U(VI) at high temperatures. • Dimensional reduction by both halides and stereochemically active lone-pairs.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A{sub 5}RE{sub 4}X[TO{sub 4}]{sub 4} crystal growth: Fluoride flux synthesis of Na{sub 5}Ln{sub 4}F[GeO{sub 4}]{sub 4} (Ln=Pr, Nd), the first quaternary germanate oxyfluorides

Crystals of Na{sub 5}Pr{sub 4}F[GeO{sub 4}]{sub 4} and Na{sub 5}Nd{sub 4}F[GeO{sub 4}]{sub 4} were synthesized using a eutectic sodium fluoride, sodium chloride flux. Both compounds crystallize in the tetragonal space group I-4 with lattice parameters of a=12.1173(4) Å and c=5.6795(2) Å (Pr) and of a=12.0642(17) Å and c=5.6674(11) Å (Nd). The structure of the reported compounds is three-dimensional with face and corner sharing lanthanide polyhedra which edge and corner share with isolated germanium tetrahedra. These novel compositions represent the first example of quaternary germanium containing oxyfluorides. - Graphical abstract: Structural image of the first examples of quaternary germanate oxyfluorides. Display Omitted - Highlights: • Molten flux growth of crystals of two lanthanide germanate oxyfluorides. • Expansion of the A{sub 5}RE{sub 4}X[TO{sub 4}]{sub 4} family into germanate oxyfluorides. • Synthesis of Na{sub 5}Nd{sub 4}F[GeO{sub 4}]{sub 4} and Na{sub 5}Pr{sub 4}F[GeO{sub 4}]{sub 4}.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Characterization of novel borides in Ti-Nb-Zr-Ta + 2B metal-matrix composites

Metal-matrix composites consisting of a complex quaternary Ti-35Nb-7Zr-5Ta alloy reinforced by borides have been successfully deposited from a powder feedstock consisting of a blend of elemental titanium, niobium, zirconium, tantalum, and, titanium diboride (TiB{sub 2}) powders, using the laser engineered net-shaping (LENS{sup TM}) process. The microstructures of the as-deposited composites have been characterized using scanning electron microscopy, orientation microscopy, and, transmission electron microscopy. Both primary and eutectic boride precipitates, exhibiting the orthorhombic B27 structure, are observed in these as-deposited composites. The complex primary borides exhibit an unusual compositional variation within the same precipitate, which has been investigated in detail using site-specific characterization with a transmission electron microscope. The ability to form near-net shape components using the Laser Engineered Net Shaping process makes these laser-deposited composites promising candidates for wear-resistant applications in biomedical implants.

36 MATERIALS SCIENCE↗

Research on microstructures of sub-rapidly solidified AZ61 Magnesium Alloy

AZ61 magnesium alloy foils of 0.5-3.0 mm thick were successfully produced by using sub-rapid solidification technique. Microstructures of conventionally solidified (CS) and sub-rapidly solidified (sub-RS) alloys were examined by optical microscope (OM) and scanning electron microscope (SEM). The results showed that the cellular grain of 1.8-13.5 {mu}m can be obtained during sub-rapid solidification process. Phase compositions and microdistribution of the alloying elements in the foils were analyzed by X-ray diffraction (XRD) and electron probe microanalyzer (EPMA), respectively. The eutectic transformation L {yields} {alpha}-Mg + {beta}-Mg{sub 17}Al{sub 12} and microsegregation in conventionally solidified AZ61 alloy were remarkably suppressed in sub-rapid solidification process. As a consequence, the alloying elements Al, Zn, Mn showed much higher solid solubility and the sub-rapid solidification microstructures dominantly consisted of supersaturated {alpha}-Mg solid solution. Meanwhile, the {beta}-Mg{sub 17}Al{sub 12} phases located in the {alpha}-Mg grain boundaries are largely decreased due to high solidification cooling rate.

36 MATERIALS SCIENCE↗

Influence of constitutional liquation on corrosion behaviour of aluminium alloy 2017A

The purpose of this work was to investigate microstructural aspects of constitutional liquation in the aluminium alloy 2017A and to determine its effect on corrosion behaviour of this alloy. Non-equilibrium melting of the alloy in the naturally aged condition was provoked by rapid heating above the eutectic temperature and immediate cooling in air. Corrosion testing was performed by exposure to a marine onshore atmosphere. The microstructure examinations were carried out using light microscopy, scanning electron microscopy, X-ray energy dispersion and X-ray diffraction analysis. It was found that, due to rapid heating rate, coarse {theta} (Al{sub 2}Cu) particles were melted by constitutional liquation and this way introduced strong susceptibility of 2017A alloy to intergranular corrosion.

36 MATERIALS SCIENCE↗

Sr effect on the microstructure and tensile properties of A357 aluminum alloy and Al{sub 2}O{sub 3}/SiC-A357 cast composites

The effect of strontium as a modifier on the microstructures and tensile properties of two castable particulate metal matrix composites has been studied. The particulate metal matrix composites had similar matrix alloy (A357) but different reinforcing fine particles (silicon carbide and alumina). Results showed that the addition of 0.03% strontium makes a modest improvement to the yield strength, ultimate tensile strength and elongation percentage values, and the scatter of these properties, but makes a significant improvement to minimum strength and elongation results. Microstructural examinations by scanning electron microscope and energy dispersive spectroscopy analysis of metal matrix composites showed segregation of strontium on both the silicon carbide and alumina particles. Further results showed that the addition of higher strontium levels contributes to the over-modification of the eutectic silicon and promotes the formation of an Al-Si-Sr intermetallic compound on the particle/matrix interface.

36 MATERIALS SCIENCE↗

Observation of high-temperature phase transformation in the Si-modified aluminide coating on mild steel using EBSD

Mild steel was coated by hot-dipping in a molten bath containing Al-10 wt.% Si. The phase transformation in the aluminide layer during diffusion at 750 deg. C in static air was analyzed by Electron Backscatter Diffraction. The results showed that the aluminide layer of the as-coated specimen consisted of an outer Al-Si eutectic topcoat and the inner Fe-Al-Si and Fe-Al intermetallic layers. The formation of {tau}{sub 5}-Al{sub 7}Fe{sub 2}Si and {tau}{sub 6}-Al{sub 4}FeSi was observed with increasing exposure time at 750 deg. C, while the {tau}{sub 1}-(Al,Si){sub 5}Fe{sub 3} phase precipitated into the Fe{sub 2}Al{sub 5} phase. After 60 min of exposure, the {tau}{sub 5}-Al{sub 7}Fe{sub 2}Si and {tau}{sub 6}-Al{sub 4}FeSi phases disappeared. The FeAl phase not only formed at the interface between Fe{sub 2}Al{sub 5} and the steel substrate, but also transformed from {tau}{sub 1}-(Al,Si){sub 5}Fe{sub 3} after diffusion for 10 h. With prolonged exposure, the growing FeAl phase decreased the thickness of Fe{sub 2}Al{sub 5} and forced the formation of FeAl{sub 2} phase. Finally, the aluminide layer comprised only FeAl{sub 2} and FeAl.

36 MATERIALS SCIENCE↗

Microstructure and corrosion behavior of cast Fe-B alloys dipped into liquid zinc bath

The corrosion behavior of cast Fe-B alloys in a liquid zinc bath was examined. As a result, the as-cast Fe-3.5B alloy displays the best corrosion resistance in all tested specimens owing to its netlike structure of eutectic Fe{sub 2}B against the liquid zinc. XRD and EDS results indicate that the main phases in the corrosion layer are determined to be {delta}, {zeta} and {eta} from the matrix to the zinc zone, respectively. The corrosion process is controlled by the diffusion of zinc atoms and the dissolution mechanism. According to the observations, only three steps occur in the whole dissolution process: the preferential dissolution of {alpha}-Fe, the formation of intermetallic compounds, and the spalling of Fe{sub 2}B caused by cracks that mainly result from the internal stress produced by Fe/Zn phase transformation. The continuous netlike Fe{sub 2}B phase delays the further reaction of Fe/Zn and hinders the diffusion of zinc atoms between the substrate and liquid zinc effectively, improving corrosion resistance of Fe-B alloy in comparison with 1Cr18Ni9Ti stainless steel.

36 MATERIALS SCIENCE↗

Effects of Sc content on the microstructure of As-Cast Al-7 wt.% Si alloys

The effects of Sc content on the microstructure of as-cast Al-Si alloys were investigated by adding 0.05, 0.1, 0.15, 0.2, 0.25, 0.3, and 0.4 wt.% Sc to hypoeutectic Al-7 wt.% Si alloys. The results show that there are significant changes in the microstructure when the Sc content is increased to 0.15%. The volume fraction of the primary {alpha}-Al phase increased nearly monotonically with increasing Sc content in the as-cast state. As the Sc content increased, the average length of the eutectic Si in the as-cast Al-7Si-xSc alloy decreased sharply from 150 {mu}m (without Sc content) to 20 {mu}m (0.4 wt.% Sc content). The Sc atoms are concentrated in the interdendritic regions. A fish-bone structure composed of Al, Si, Sc, and Fe, which might be the Fe-rich phase precipitated on the AlSc{sub 2}Si{sub 2} (V-phase) was detected adjacent to the grain boundary by scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS). - Highlights: Black-Right-Pointing-Pointer Significant changes in the microstructure when the Sc content is increased to 0.15%. Black-Right-Pointing-Pointer Volume fraction of the primary a-Al phase increased with increasing Sc content. Black-Right-Pointing-Pointer Average length of Si decreased sharply from 150 to 20 {mu}m with increasing Sc content. Black-Right-Pointing-Pointer The Sc atoms are concentrated in the interdendritic regions.

36 MATERIALS SCIENCE↗

Non-destructive characterisation of polymers and Al-alloys by polychromatic cone-beam phase contrast tomography

X-ray computed tomography (XCT) has become a very important tool for the non-destructive characterisation of materials. Continuous improvements in the quality and performance of X-ray tubes and detectors have led to cone-beam XCT systems that can now achieve spatial resolutions down to 1 {mu}m and even below. Since not only the amplitude but also the phase of an X-ray beam is altered while passing through an object, phase contrast effects can occur even for polychromatic sources when the spatial coherence due to a small focal spot size is high enough. This can lead to significant improvements over conventional attenuation-based X-ray computed tomography. Phase contrast can increase by edge enhancement the visibility of small structures and of features which are only slightly different in attenuation. We report on the possibilities of polychromatic cone-beam phase contrast tomography for non-destructive characterisation of materials. A carbon fibre-reinforced polymer and the Al-alloys AlMg5Si7 and AlSi18 were investigated with high resolution cone-beam X-ray computed tomography with a polychromatic tube source. Under certain conditions strong phase contrast resulting in an upward and downward overshooting of the grey values across edges was observed. The phase effects are much stronger for the polymer than for the Al-alloys. The influence on the phase contrast of the parameters, including source-detector distance, focal spot size and tube acceleration voltage is presented. Maximum phase contrast was observed for a maximum distance between the source and the detector, for a low voltage and a minimum focal spot size at the X-ray source. The detectability of the different phases is improved by the edge enhancement and the resulting improvement of sharpness. Thus, a better segmentation of the carbon fibres in the fibre-reinforced polymer and of the Mg{sub 2}Si-phase in the AlMg5Si7-alloy is achieved. Primary and eutectic Si cannot be detected by attenuation-based X-ray computed tomography due to the small difference in X-ray attenuation between the Si and the Al-matrix in AlSi18. However, phase contrast effects lead to a significant detectability and the large primary Si particles become clearly visible in the tomograms of AlSi18. - Highlights: Black-Right-Pointing-Pointer Phase contrast increases with increasing distance object-detector and with decreasing U, X-ray spot. Black-Right-Pointing-Pointer The detectability of details is improved by the phase contrast. Black-Right-Pointing-Pointer For the carbon fibre-reinforced polymer the visibility of the carbon fibres is improved. Black-Right-Pointing-Pointer For AlMg5Si7 the detectability of the phases Fe-aluminides and Mg{sub 2}Si particles is improved. Black-Right-Pointing-Pointer For AlSi18 primary Si particles with a size > 50 {mu}m become detectable because of the phase contrast.

36 MATERIALS SCIENCE↗

Microstructural analysis of laser weld fusion zone in Haynes 282 superalloy

Analytical electron microscopy and spectroscopy analyses of the fusion zone (FZ) microstructure in autogenous laser beam welded Haynes 282 (HY 282) superalloy were performed. The micro-segregation patterns observed in the FZ indicate that Co, Cr and Al exhibited a nearly uniform distribution between the dendrite core and interdendritic regions while Ti and Mo were rejected into the interdendritic liquid during the weld solidification. Transmission electron diffraction analysis and energy dispersive X-ray microanalysis revealed the second phase particles formed along the FZ interdendritic region to be Ti-Mo rich MC-type carbide particles. Weld FZ solidification cracking, which is sometimes associated with the formation of {gamma}-{gamma}' eutectic in {gamma}' precipitation strengthened nickel-base superalloys, was not observed in the HY 282 superalloy. Modified primary solidification path due to carbon addition in the newly developed superalloy is used to explain preclusion of weld FZ solidification cracking in the material. - Highlights: Black-Right-Pointing-Pointer A newly developed superalloy was welded by CO{sub 2} laser beam joining technique. Black-Right-Pointing-Pointer Electron microscopy characterization of the weld microstructure was performed. Black-Right-Pointing-Pointer Identified interdendritic microconstituents consist of MC-type carbides. Black-Right-Pointing-Pointer Modification of primary solidification path is used to explain cracking resistance.

36 MATERIALS SCIENCE↗

Microstructural characterization of ferrotitanium and ferroniobium

Ferroniobium and ferrotitanium, which are added during the steel-making process, may contain phases that do not melt or dissolve in molten steel. This can lead to the presence of coarse Ti- and Nb-rich particles in the resultant steel, which may have an adverse effect on the mechanical properties. In the present study, detailed microstructural characterization, using electron microscopy (both SEM and TEM) and X-ray diffraction (XRD), of commercial grades of ferrotitanium and ferroniobium alloys is carried out to identify the various phases. The ferrotitanium alloy was composed of mainly β-Ti solid solution and a Fe–Ti–Al ternary intermetallic. There were minor amounts of α-Ti solid solution, Ti(C{sub x}N{sub 1−x}) and FeTi. For the ferroniobium alloy, two main phases were present, a Nb-rich solid solution and μ-Fe{sub 7}Nb{sub 6}. The Fe{sub 7}Nb{sub 6} intermetallic phase exhibited two different morphologies, a proeutectic form that was slightly Fe-rich and a eutectic form that was slightly Nb-rich. - Highlights: ► Ferrotitanium has five phases — β-Ti and Ti–Fe–Al ternary are the main phases. ► Ferroniobium has two phases — Nb solid solution and μ-Fe{sub 7}Nb{sub 6} phases. ► The μ-Fe{sub 7}Nb{sub 6} phase has two morphologies — one heavily faulted.

36 MATERIALS SCIENCE↗

Formation and characterization of microstructure of as-cast Mg–6Gd–4Y–xZn–0.5Zr (x = 0.3, 0.5 and 0.7 wt.%) alloys

Mg–6Gd–4Y–xZn–0.5Zr (x = 0.3, 0.5 and 0.7 wt.%) alloys were prepared via conventional ingot metallurgy (I/M) in this study. The as-cast microstructures of these alloys were established by X-ray diffraction (XRD) analyses, optical microscope (OM), scanning electron microscope (SEM) and transmission electron microscope (TEM) observations. Lamellar stacking order (SF) and 14H-type long period stacking order (LPSO) structure within α-Mg matrix are formed in the three as-cast alloys. The eutectic secondary phase is (Mg,Zn){sub 24}(Gd,Y){sub 5} for the alloy containing 0.3 wt.% Zn, while, it is (Mg,Zn){sub 3}(Gd,Y) for the alloys containing 0.5 wt.% Zn and 0.7 wt.% Zn. Moreover, X phase-(Mg,Zn){sub 12}(Gd,Y) is formed in the latter two as-cast alloys. - Highlights: • LPSO structure has first been found in as-cast Mg–6Gd–4Y–xZn–0.5Zr. • X-phase exists in as-cast Mg–6Gd–4Y–0.3(0.5)Zn–0.5Zr. • Zn content results in different β-phase in the studied alloys.

36 MATERIALS SCIENCE↗

Understanding the solidification and microstructure evolution during CSC-MIG welding of Fe–Cr–B-based alloy

The present is a study of the solidification and microstructure of Fe–28.2%Cr–3.8%B–1.5%Si–1.5%Mn (wt.%) alloy deposited onto a 1020 plain carbon steel substrate using the controlled short-circuit metal inert gas welding process. The as-solidified alloy was a metal matrix composite with a hypereutectic microstructure. Thermodynamic calculation based on the Scheil–Gulliver model showed that a primary (Cr,Fe){sub 2}B phase formed first during solidification, followed by an eutectic formation of the (Cr,Fe){sub 2}B phase and a body-centered cubic Fe-based solid solution matrix, which contained Cr, Mn and Si. Microstructure analysis confirmed the formation of these phases and showed that the shape of the (Cr,Fe){sub 2}B phase was irregular plate. As the welding heat input increased, the weld dilution increased and thus the volume fraction of the (Cr,Fe){sub 2}B plates decreased while other microstructural characteristics were similar. - Highlights: • We deposit Fe–Cr–B-based alloy onto plain carbon steel using the CSC-MIG process. • We model the solidification behavior using thermodynamic calculation. • As deposited alloy consists of (Cr,Fe){sub 2}B plates embedded in Fe-based matrix. • We study the effect of the welding heat input on the microstructure.

36 MATERIALS SCIENCE↗

Study of microstructure and silicon segregation in cast iron using color etching and electron microprobe analysis

An investigation on silicon segregation of lamellar, compacted and nodular graphite iron was carried out by applying a selective, immersion color etching and a modified electron microprobe to study the microstructure. The color etched micrographs of the investigated cast irons by revealing the austenite phase have provided data about the chronology and mechanism of microstructure formation. Moreover, electron microprobe has provided two dimensional segregation maps of silicon. A good agreement was found between the segregation profile of silicon in the color etched microstructure and the silicon maps achieved by electron microprobe analysis. However, quantitative silicon investigation was found to be more accurate than color etching results to study the size of the eutectic colonies. - Highlights: • Sensitivity of a color etchant to silicon segregation is quantitatively demonstrated. • Si segregation measurement by EMPA approved the results achieved by color etching. • Color etched micrographs provided data about solidification mechanism in cast irons. • Austenite grain boundaries were identified by measuring the local Si concentration.

36 MATERIALS SCIENCE↗