Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “DISULFIDES”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,117 records · Page 62

The synergistic effects of slip ring-brush design and materials

The design, fabrication, and testing of four power slip rings for synchronous orbit application are considered. Environmental and instrumentation systems necessary for monitoring electrical noise, friction, and brush wear in air and at less than 5 X 10 to the minus 8th power torr were developed. Composite brushes consisting of silver-molybdenum disulfide-graphite and silver-niobium diselenide-graphite were employed on rings of coin silver and rhodium plate. These four contact combinations were tested during ambient condition run-in at 150 and a humidity sequence at 0.1. The first nine months of a two year vacuum test performed at 0.1 rpm were completed.

Lewis, N. E.↗

Friction, wear and noise of slip ring and brush contacts for synchronous satellite use.

A program is being conducted for testing of slip rings for synchronous orbit application. Instrumentation systems necessary for monitoring electrical noise, friction, and brush wear at atmospheric pressure and at less than 50 ntorr have been developed. A multiplex scheme necessary for the simultaneous recording of brush displacement, friction, and electrical noise has also been developed. Composite brushes consisting of silver-molybdenum disulfide-graphite and silver-niobium diselenide-graphite have been employed on rings of coin silver and rhodium plate. Four contact combinations have been tested during an ambient condition run-in at 150 rpm and a humidity sequence at 0.1 rpm. The first six months of the two year vacuum test at 0.1 rpm have been completed. Electrical noise, friction and brush wear data recorded during these periods have been analyzed.

Lewis, N. E.↗

Evidence of crystal structure in some sputtered MoS2 films.

Electron diffraction patterns and electron micrographs of molybdenum disulfide films sputtered on single-NaCl-crystal and electropolished-aluminum substrates are presented as evidence that crystalline MoS2 films can be sputtered onto various substrates in thicknesses up to 2 microns. Applied to Falex test pins and V-blocks, some of these films exhibited a wear life as long as 65 minutes at 1000 lb jaw load.

Lavik, M. T.↗

Friction, wear, and noise of slip ring and brush contacts for synchronous satellite use.

A program is being conducted for testing of slip rings for synchronous orbit application. Instrumentation systems necessary for monitoring electrical noise, friction, and brush wear at atmospheric pressure and at less than 50 nanotorr have been developed. A multiplex scheme necessary for the simultaneous recording of brush displacement, friction, and electrical noise has also been developed. Composite brushes consisting of silver-molybdenum disulfide-graphite and silver-niobium diselenide-graphite have been employed on rings of coin silver and rhodium plate. Brush property measurements made included measurement of density, electrical resistivity, shear strength, and microstructure.

Lewis, N. E.↗

Effect of strain hardening on friction behavior of iron lubricated with benzyl structures

Sliding friction experiments were conducted with iron, copper, and aluminum in contact with iron in various states of strain. The surfaces were examined in dry sliding and with various benzyl compounds applied as lubricants. Friction experiments were conducted with a hemispherical rider contacting a flat disk at loads of from 50 to 600 grams with a sliding speed of 0.15 cm/min. Results indicate that straining increases friction for dry sliding and for surfaces lubricated with certain benzyl structures such as dibenzyl disulfide. With other benzyl compounds (e.g., benzyl formate), friction coefficients are lower for strained than for annealed iron.

Buckley, D. H.↗

Testing and evaluation of solid lubricants for gas bearings

The testing and results of testing solid film lubricants for gas lubricated bearing applications are reported. The tests simulated operational hazards of tilting pad gas bearings. The presence of a low coefficient of friction and the endurance of the solid film lubricant were the criteria for judging superior performance. All solid lubricants tested were applied to a plasma sprayed chrome oxide surface. Molybdenum disulfide and graphite fluoride were the solid lubricants tested; other test parameters included the method of application of the solid lubricant and the surface finish of the plasma sprayed coating. In general, the application of a solid film lubricant was found to significantly improve the coefficient of friction of the rubbing surfaces.

Albrecht, P. R.↗

Start-stop testing of two self-acting air-lubricated spiral groove thrust bearing coatings

Start-stop tests were conducted on air-lubricated spiral-groove thrust bearings. Application of a matrix-bonded molybdenum disulfide (MoS2) coating over a porous chrome oxide coating resulted in significantly lower friction, compared to bearings coated with chrome oxide only. The MoS2 coated bearing sustained 15,000 start-stop cycles at a maximum of 3600 rpm. Each cycle was 15 seconds on, 30 seconds off. The chrome oxide coated bearing failed by local welding after 2030 cycles. Both types of coatings exhibited early failures under higher thrust loads when operating films were insufficient to sustain the load without overheating.

Dunfee, J. D.↗

Effect of crosslinking density on biaxial relaxation of SBR by using reduced variables

The use of reduced variables to account for the effect of crosslinking density in a styrene-butadiene rubber (SBR) system is demonstrated for general biaxial stress states. Recently published results from stress relaxation tests on five SBR vulcanizates crosslinked to different degrees by tetramethylthiuram disulfide were superposed by using the crosslinking density as a reduction variable. The equilibrium shear modulus calculated from the master relaxation curve at long reduced times was in satisfactory agreement with other results for SBR. The time-axis shifts were related in a linear logarithmic manner to the crosslinking density but had a slope slightly less than values previously reported for elastomer systems.

Arenz, R. J.↗

Simplified explosive-weld evaluation

Weld surfaces, coated with commercially available molybdenum disulfide, allow visual inspection of significant indications of bond quality. Process reduces number of trial welds, making explosive bonding more competitive.

Mclarty, D. M.↗

Selected fretting-wear-resistant coatings for titanium - 6-percent-aluminum - 4-percent-vanadium alloy

A titanium - 6-percent-aluminum - 4-percent-vanadium alloy (Ti-6Al-4V) was subjected to fretting-wear exposures against uncoated Ti-6Al-4V as a baseline and against various coatings and surface treatments applied to Ti-6Al-4V. The coatings evaluated included plasma-sprayed tungsten carbide with 12 percent cobalt, aluminum oxide with 13 percent titanium oxide, chromium oxide, and aluminum bronze with 10 percent aromatic polyester; polymer-bonded polyimide, polyimide with graphite fluoride, polyimide with molybdenum disulfide (MoS2), and methyl phenyl silicone bonded MoS2, preoxidation surface treatment, a nitride surface treatment, and a sputtered MoS2 coating. Results of wear measurements on both the coated and uncoated surfaces after 300,000 fretting cycles indicated that the polyimide coating was the most wear resistant and caused the least wear to the uncoated mating surface.

Bill, R. C.↗

Scanning electron microscope investigation of the structural growth in thick sputtered coatings

Sputtered S-Monel, silver, and 304 stainless steel coatings and molybdenum disulfide coatings were deposited on mica and metal substrates with various surface finishes to investigate the structural growth of the coating by scanning electron microscopy. The geometry and the surface morphology of the nodules are characterized. Compositional changes within the coating were analyzed by energy dispersive X-ray analysis. Defects in the surface finish act as preferential nucleation sites and form isolated overlapping and complex nodules and various unusual surface overgrowths on the coating. The nodule boundaries are very vulnerable to chemical etching and these nodules do not disappear after full annealing. Further, they have undesirable effects on mechanical properties; cracks are initiated at the nodules when the coating is stressed by mechanical forces.

Spalvins, T.↗

Atomic hydrogen storage method and apparatus

Atomic hydrogen, for use as a fuel or as an explosive, is stored in the presence of a strong magnetic field in exfoliated layered compounds such as molybdenum disulfide or an elemental layer material such as graphite. The compound is maintained at liquid helium temperatures and the atomic hydrogen is collected on the surfaces of the layered compound which are exposed during delamination (exfoliation). The strong magnetic field and the low temperature combine to prevent the atoms of hydrogen from recombining to form molecules.

Woollam, J. A.↗

Graphite-fiber-reinforced polyimide liners of various compositions in plain spherical bearings

A plain spherical bearing design with a ball diameter of 28.6 mm, a race length of 12.7 mm, and a 1.7-mm-thick, molded composite liner was evaluated. The liner material is a self-lubricating composite of graphite-fiber-reinforced polyimide resin (GFRPI). The liner is prepared by transfer molding a mixture of one part chopped graphite fiber and one part partially polymerized resin into the space between the bearing ball and the outer race and then completing the polymerization under heat and pressure. Several liner compositions were evaluated: two types of polyimide, condensation and addition; two types of graphite fiber, low and high modulus; and four powder additives - cadmium oxide, cadmium iodide, graphite fluoride, and molybdenum disulfide. The bearings were oscillated + or - 15 deg at 1 Hz for 20 kilocycles under a radial unit load of 29 MN sq m (4200 psi) in dry air at 25, 200, or 315 C. Both types of fiber and polyimide gave low friction and wear. A simple equation was developed to fit the wear-time data and adequately predicted wear to 100 kilocycles.

Sliney, H. E.↗

CS2 - Candidate for the 3150-A Venus band

The 3150-A absorption on Venus, found by Barker et al. (1975), may be due to carbon disulfide. The stability and thermodynamics of the carbon chalcogenides are briefly discussed.

Young, A. T.↗

Atomic hydrogen storage

Atomic hydrogen, for use as a fuel or as an explosive, is stored in the presence of a strong magnetic field in exfoliated layered compounds such as molybdenum disulfide or an elemental layer material such as graphite. The compound is maintained at liquid temperatures and the atomic hydrogen is collected on the surfaces of the layered compound which are exposed during delamination (exfoliation). The strong magnetic field and the low temperature combine to prevent the atoms of hydrogen from recombining to form molecules.

Woollam, J. A.↗

The Exxon rechargeable cells

The design and performance of ambient temperature secondary cells based on the titanium disulfide cathode are discussed. These limited performance products were developed for microelectronic applications such as solar rechargeable watches and clocks which require low drain rate and do not require many deep cycles.

Malachesky, P. A.↗

Atomic hydrogen storage method and apparatus

Atomic hydrogen, for use as a fuel or as an explosive, is stored in the presence of a strong magnetic field in exfoliated layered compounds such as molybdenum disulfide or an elemental layer material such as graphite. The compounds maintained at liquid helium temperatures and the atomic hydrogen is collected on the surfaces of the layered compound which are exposed during delamination (exfoliation). The strong magnetic field and the low temperature combine to prevent the atoms of hydrogen from recombining to form molecules.

Woollam, J. A.↗

Gaseous constituents in the plume from eruptions of Mount St. Helens

Measurements in the stratosphere of gaseous constituents in the plume of Mount St. Helens were obtained during five flights of the NASA U-2 aircraft between 19 May and 17 June 1980. Mixing ratios from gas chromatographic measurements on samples acquired about 24 hours after the initial eruption show considerable enhancement over nonvolcanic concentrations for sulfur dioxide (more than 1000 times), methyl chloride (about 10 times), and carbon disulfide (more than 3 times). The mixing ratio of carbonyl sulfide was comparable to nonvolcanic mixing ratios although 3 days later it was enhanced two to three times. Ion chromatography measurements on water-soluble constituents are also reported. Very large concentrations of chloride, nitrate, and sulfate ions were measured, implying large mixing ratios for the water-soluble gaseous constituents from which the anions are derived. Measurements of radon-222 present in the plume are also reported.

Inn, E. C. Y.↗