Effect of Base Metal Misorientation on Single-Crystal Superalloy Transient Liquid-Phase Bonded Joints

In this paper, experiments and theoretical analysis were conducted to elucidate the internal relation between base metal misorientation and the characteristics of DD5 single-crystal superalloy TLP joints. The alloy was bonded at 1513 K for 10 h in vacuum environment. High-temperature creep rupture tests were carried out to determine the joint’s quality. Results revealed that base metal misorientation exerted a remarkable influence on DD5 alloy TLP joints. The joints of base metals with [001] orientation were used in this research. When the misorientation was smaller than 9°-10°, the single crystallization of joints can be realized and joints can achieve excellent mechanical properties. When the misorientation was more than 10°, there would be second-phase particles distributed in grain boundaries, thus resulting in poor mechanical property of joint; moreover, the characteristics of joint did not change with base metal misorientation in this case.

36 MATERIALS SCIENCE↗

Postmastectomy radiation therapy using VMAT technique for breast cancer patients with expander reconstruction

Postmastectomy radiotherapy (PMRT) following immediate breast reconstruction is increasingly adopted in the management of breast cancer patients. We retrospectively evaluate the complication rates of PMRT using VMAT technique to immediate tissue expander-based reconstructions and the possible impact of tissue expander volume on radiotherapy planning. We reviewed the data of patients who underwent immediate expander breast reconstruction and received PMRT with VMAT (50 Gy in 25 fractions) on the reconstructed breast and axillary levels III–IV. Neoadjuvant or adjuvant systemic therapy was administered in most of the patients. Autologous fat grafting was routinely performed at the time of second-stage reconstruction. Between 2015 and 2017, PMRT was delivered to 46 consecutive patients (median age 50 years) with expander reconstruction. Median follow-up was 27 months (range 10–41). Two patients (4.3%) had a reconstruction failure, as expander rupture and infection, following the first- and the second-stage reconstruction, respectively. In most cases expanders were completely inflated before PMRT (65.2%). Median expander volume before PMRT was 425 cm{sup 3} (range 150–700 cm{sup 3}). The amount of expander inflation did not significantly affect dosimetry, except for skin dose, with a surface receiving more than 30 Gy of 36.6 ± 0.9 cm{sup 2} and 47.0 ± 2.5 cm{sup 2} for a volume expander below or above the median, respectively. However, this variable was not predictor for complications. Disease progression was recorded in 15.2% of patients. PMRT using VMAT technique for breast cancer patients with expander reconstruction is associated with a very low complication rate. The expander volume before PMRT does not significantly compromise radiotherapy dose distribution.

62 RADIOLOGY AND NUCLEAR MEDICINE↗

An unmet clinical need: The history of thrombus imaging

Robust thrombus imaging is an unresolved clinical unmet need dating back to the mid 1970s. While early molecular imaging approaches began with nuclear SPECT imaging, contrast agents for virtually all biomedical imaging modalities have been demonstrated in vivo with unique strengths and common weaknesses. Two primary molecular imaging targets have been pursued for thrombus imaging: platelets and fibrin. Some common issues noted over 40 years ago persist today. Acute thrombus is readily imaged with all probes and modalities, but aged thrombus remains a challenge. Similarly, anti-coagulation continues to interfere with and often negate thrombus imaging efficacy, but heparin is clinically required in patients suspected of pulmonary embolism, deep venous thrombosis or coronary ruptured plaque prior to confirmatory diagnostic studies have been executed and interpreted. These fundamental issues can be overcome, but an innovative departure from the prior approaches will be needed.

62 RADIOLOGY AND NUCLEAR MEDICINE↗

Membrane binding mode of intrinsically disordered cytoplasmic domains of T cell receptor signaling subunits depends on lipid composition

Intrinsically disordered cytoplasmic domains of T cell receptor (TCR) signaling subunits including {zeta}{sub cyt} and CD3{epsilon}{sub cyt} all contain one or more copies of an immunoreceptor tyrosine-based activation motif (ITAM), tyrosine residues of which are phosphorylated upon receptor triggering. Membrane binding-induced helical folding of {zeta}{sub cyt} and CD3{epsilon}{sub cyt} ITAMs is thought to control TCR activation. However, the question whether or not lipid binding of {zeta}{sub cyt} and CD3{epsilon}{sub cyt} is necessarily accompanied by a folding transition of ITAMs remains open. In this study, we investigate whether the membrane binding mechanisms of {zeta}{sub cyt} and CD3{epsilon}{sub cyt} depend on the membrane model used. Circular dichroic and fluorescence data indicate that binding of {zeta}{sub cyt} and CD3{epsilon}{sub cyt} to detergent micelles and unstable vesicles is accompanied by a disorder-to-order transition, whereas upon binding to stable vesicles these proteins remain unfolded. Using electron microscopy and dynamic light scattering, we show that upon protein binding, unstable vesicles fuse and rupture. In contrast, stable vesicles remain intact under these conditions. This suggests different membrane binding modes for {zeta}{sub cyt} and CD3{epsilon}{sub cyt} depending on the bilayer stability: (1) coupled binding and folding, and (2) binding without folding. These findings explain the long-standing puzzle in the literature and highlight the importance of the choice of an appropriate membrane model for protein-lipid interactions studies.

60 APPLIED LIFE SCIENCES↗

Neuraminidase inhibitor R-125489 - A promising drug for treating influenza virus: Steered molecular dynamics approach

Highlights: {yields} We study binding affinity of R-125489 and its prodrug CS-8958 to neuraminidase of pathogenic influenza viruses by molecular dynamics simulations. {yields} It is shown that, in agreement with experiments, R-125489 binds to neuraminidase more tightly than CS-8958. {yields} We predict that R-125489 can be used to treat not only wild-type but also tamiflu-resistant N294S, H274Y variants of A/H5N1 virus. {yields} The high correlation between theoretical and experimental data implies that SMD is a very promising tool for drug design. -- Abstract: Two neuraminidase inhibitors, oseltamivir and zanamivir, are important drug treatments for influenza. Oseltamivir-resistant mutants of the influenza virus A/H1N1 and A/H5N1 have emerged, necessitating the development of new long-acting antiviral agents. One such agent is a new neuraminidase inhibitor R-125489 and its prodrug CS-8958. An atomic level understanding of the nature of this antiviral agents binding is still missing. We address this gap in our knowledge by applying steered molecular dynamics (SMD) simulations to different subtypes of seasonal and highly pathogenic influenza viruses. We show that, in agreement with experiments, R-125489 binds to neuraminidase more tightly than CS-8958. Based on results obtained by SMD and the molecular mechanics-Poisson-Boltzmann surface area method, we predict that R-125489 can be used to treat not only wild-type but also tamiflu-resistant N294S, H274Y variants of A/H5N1 virus as its binding affinity does not vary much across these systems. The high correlation level between theoretically determined rupture forces and experimental data on binding energies for the large number of systems studied here implies that SMD is a promising tool for drug design.

60 APPLIED LIFE SCIENCES↗

Ischemic preconditioning enhances integrity of coronary endothelial tight junctions

Highlights: Black-Right-Pointing-Pointer Cardiac tight junctions are present between coronary endothelial cells. Black-Right-Pointing-Pointer Ischemic preconditioning preserves the structural and functional integrity of tight junctions. Black-Right-Pointing-Pointer Myocardial edema is prevented in hearts subjected to ischemic preconditioning. Black-Right-Pointing-Pointer Ischemic preconditioning enhances translocation of ZO-2 from cytosol to cytoskeleton. -- Abstract: Ischemic preconditioning (IPC) is one of the most effective procedures known to protect hearts against ischemia/reperfusion (IR) injury. Tight junction (TJ) barriers occur between coronary endothelial cells. TJs provide barrier function to maintain the homeostasis of the inner environment of tissues. However, the effect of IPC on the structure and function of cardiac TJs remains unknown. We tested the hypothesis that myocardial IR injury ruptures the structure of TJs and impairs endothelial permeability whereas IPC preserves the structural and functional integrity of TJs in the blood-heart barrier. Langendorff hearts from C57BL/6J mice were prepared and perfused with Krebs-Henseleit buffer. Cardiac function, creatine kinase release, and myocardial edema were measured. Cardiac TJ function was evaluated by measuring Evans blue-conjugated albumin (EBA) content in the extravascular compartment of hearts. Expression and translocation of zonula occludens (ZO)-2 in IR and IPC hearts were detected with Western blot. A subset of hearts was processed for the observation of ultra-structure of cardiac TJs with transmission electron microscopy. There were clear TJs between coronary endothelial cells of mouse hearts. IR caused the collapse of TJs whereas IPC sustained the structure of TJs. IR increased extravascular EBA content in the heart and myocardial edema but decreased the expression of ZO-2 in the cytoskeleton. IPC maintained the structure of TJs. Cardiac EBA content and edema were reduced in IPC hearts. IPC enhanced the translocation of ZO-2 from cytosol to cytoskeleton. In conclusion, TJs occur in normal mouse heart. IPC preserves the integrity of TJ structure and function that are vulnerable to IR injury.

60 APPLIED LIFE SCIENCES↗

Oxaliplatin triggers necrosis as well as apoptosis in gastric cancer SGC-7901 cells

Intrinsic apoptotic pathway is considered to be responsible for cell death induced by platinum anticancer drugs. While in this study, we found that, necrosis is an indispensable pathway besides apoptosis in oxaliplatin-treated gastric cancer SGC-7901 cells. Upon exposure to oxaliplatin, both apoptotic and necrotic features were observed. The majority of dead cells were double positive for Annexin V and propidium iodide (PI). Moreover, mitochondrial membrane potential collapsed and caspase cascades were activated. However, ultrastructural changes under transmission electron microscope, coupled with the release of cellular contents, demonstrated the rupture of the plasma membrane. Oxaliplatin administration did not stimulate reactive oxygen species (ROS) production and autophagy, but elevated the protein level of Bmf. In addition, receptor interacting protein 1 (RIP1), but not receptor interacting protein 3 (RIP3) and its downstream components participated in this death process. Necrostatin-1 (Nec-1) blocked oxaliplatin-induced cell death nearly completely, whereas z-VAD-fmk could partially suppress cell death. Oxaliplatin treatment resulted in poly(ADP-ribose) polymerase-1 (PARP-1) overactivation, as indicated by the increase of poly(ADP-ribose) (PAR), which led to NAD{sup +} and ATP depletion. PARP-1 inhibitor, olaparib, could significantly block oxaliplatin-induced cell death, thus confirming that PARP-1 activation is mainly responsible for the cytotoxicity of oxaliplatin. Phosphorylation of H2AX at Ser139 and translocalization of apoptosis-inducing factor (AIF) are critical for this death process. Taken together, these results indicate that oxaliplatin can bypass canonical cell death pathways to kill gastric cancer cells, which may be of therapeutic advantage in the treatment of gastric cancer. - Highlights: • Oxaliplatin induces apoptotic and necrotic cell death. • Nec-1 can inhibit oxaliplatin-induced cell death nearly completely. • RIP3 and its downstream components are not involved in this process. • PARP-1 overactivation-mediated energy depletion, H2AX phosphorylation and AIF translocation are crucial for this cell death.

60 APPLIED LIFE SCIENCES↗

Acoustic emission for characterising the crack propagation in strain-hardening cement-based composites (SHCC)

This paper presents the analysis of crack propagation in strain-hardening cement-based composite (SHCC) under tensile and flexural load by using acoustic emission (AE). AE is a non-destructive technique to monitor the development of structural damage due to external forces. The main objective of this research was to characterise the cracking behaviour in SHCC in direct tensile and flexural tests by using AE. A better understanding of the development of microcracks in SHCC will lead to a better understanding of pseudo strain-hardening behaviour of SHCC and its general performance. ARAMIS optical deformation analysis was also used in direct tensile tests to observe crack propagation in SHCC materials. For the direct tensile tests, SHCC specimens were prepared with polyvinyl alcohol (PVA) fibre with three different volume percentages (1%, 1.85% and 2.5%). For the flexural test beam specimens, only a fibre dosage of 1.85% was applied. It was found that the application of AE in SHCC can be a good option to analyse the crack growth in the specimens under increasing load, the location of the cracks and most importantly the identification of matrix cracking and fibre rupture or slippage.

36 MATERIALS SCIENCE↗

Influence of fiber inclination angle on bond-slip behavior of different alkali-activated composites under dynamic and quasi-static loadings

This study investigates the influence of inclination angle (0° and 45°) on the interfacial bond-slip behavior of macro steel fibers (straight, hooked end-deformed and length-deformed) and length-deformed polypropylene fibers reinforced in fly-ash and metakaolin based alkali-activated composites (AACs) under quasi-static and dynamic loadings. AACs demonstrate superior peak bond strength and toughness compared to cement composites regardless of fiber type and loading rate. Results also show that straight steel fiber exhibits a complete pullout in AACs. The amount of deformation of the fibers (deformation ratio) determined the failure type at different inclination angle and loading rate, thus governing the peak load and energy absorption. Depending on the fiber orientation, premature fiber rupture or matrix cracking is observed under dynamic loading in AACs due to matrix brittleness. The fiber failure modes in dynamic pullout are no different from those observed in the quasi-static pullout in AACs.

36 MATERIALS SCIENCE↗

Combustion characteristics of fuel droplets with addition of nano and micron-sized aluminum particles

The burning characteristics of fuel droplets containing nano and micron-sized aluminum particles were investigated. Particle size, surfactant concentration, and the type of base fluid were varied. In general, nanosuspensions can last much longer than micron suspensions, and ethanol-based fuels were found to achieve much better suspension than n-decane-based fuels. Five distinctive stages (preheating and ignition, classical combustion, microexplosion, surfactant flame, and aluminum droplet flame) were identified for an n-decane/nano-Al droplet, while only the first three stages occurred for an n-decane/micron-Al droplet. For the same solid loading rate and surfactant concentration, the disruption and microexplosion behavior of the micron suspension occurred later with much stronger intensity. The intense droplet fragmentation was accompanied by shell rupture, which caused a massive explosion of particles, and most of them were burned during this event. On the contrary, for the nanosuspension, combustion of the large agglomerate at the later stage requires a longer time and is less complete because of formation of an oxide shell on the surface. This difference is mainly due to the different structure and characteristics of particle agglomerates formed during the early stage, which is a spherical, porous, and more-uniformly distributed aggregate for the nanosuspension, but it is a densely packed and impermeable shell for the micron suspension. A theoretical analysis was then conducted to understand the effect of particle size on particle collision mechanism and aggregation rate. The results show that for nanosuspensions, particle collision and aggregation are dominated by the random Brownian motion. For micron suspensions, however, they are dominated by fluid motion such as droplet surface regression, droplet expansion resulting from bubble formation, and internal circulation. And the Brownian motion is the least important. This theoretical analysis explains the different characteristics of the particle agglomerates, which are responsible for the different microexplosion behaviors that were observed in the experiments. (author)

33 ADVANCED PROPULSION SYSTEMS↗

Experimental Determination of the Effect of the Ratio of B/Al on Glass Dissolution along the Nepheline (NaAlSiO 4 ) – Malinkoite (NaBSiO 4 ) Join

The dissolution kinetics of five glasses along the NaAlSiO 4 -NaBSiO 4 join were used to evaluate how the structural variations associated with boron-aluminum substitution affect the rate of dissolution. The composition of each glass varied inversely in mol% of Al 2 O 3 (5 to 25 mol%) and B 2 O 3 (20 to 0 mol%) with Na 2 O (25 mol%) and SiO 2 (50 mol%) making up the remaining amount, in every case Na/(Al+B) = 1.0. Single-pass flow-through experiments (SPFT) were conducted under dilute conditions as a function of solution pH (from 7.0 to 12.0) and temperature (from 23° to 90°C). Analysis by 27 Al and 29 Si MAS-NMR suggests Al (~98% [4] Al) and Si atoms (~100% [4] Si) occupy a tetrahedral coordination whereas, B atoms occupy both tetrahedral ([4]B) and trigonal ( [3] B) coordination. The distribution of [3]B fractionated between [3] B(ring) and [3] B(non-ring) moieties, with the [3] B(ring)/ [3] B(non-ring) ratio increases with the B/Al ratio. The MAS-NMR results also indicated an increase in the fraction of [4] B with an increase in the B/Al ratio. But despite the changes in the B/Al ratio and B coordination, the 29 Si spectra maintain a chemical shift between -88 to -84 ppm for each glass. Unlike the 29 Si spectra, the 27 Al resonances shift to more positive values with an increase in the B/Al ratio which suggests mixing between the [4] Al and [3] B sites, assuming avoidance between tetrahedral trivalent cations ( [4] Al-O- [4] B avoidance). Raman spectroscopy was use to augment the results collected from MAS-NMR and demonstrated that NeB4 (glass sample with the highest B content) was glass-glass phase separated (e.g., heterogeneous glass). Results from SPFT experiments suggest a forward rate of reaction and pH power law coefficients,η, that are independent of B/Al under these neutral to alkaline test conditions for all homogeneous glasses. The temperature dependence shows an order of magnitude increase in the dissolution rate with a 67°C increase in temperature and suggests dissolution is controlled by a surface-mediated reaction, evident by the activation energy, E a , being between 44±8 and 48±7 kJ/mol. Forward dissolution rates, based on Na and Si release, for homogeneous glasses are independent of the B/Al ratio, whereas dissolution rates based on Al and B release are not. Dissolution rates based on B release increase with an increase in the fraction of [3] B(ring). Finally in accord with previous studies, the data discussed in this manuscript suggest rupture of the Al-O and Si-O bond as the rate-limiting step controlling the dissolution of these glasses.

58 GEOSCIENCES↗

A predictive modeling tool for damage analysis and design of hydrogen storage composite pressure vessels

In this study, a predictive modeling tool is developed for damage analysis and design of hydrogen (H 2 ) storage composite pressure vessels. It integrates micromechanics of matrix cracking into a continuum damage mechanics (CDM) description for damage evolution, and three-dimensional (3D) finite element (FE) modeling of the vessel structural response. At the scale of the composite layer (mesoscale), the temperature-dependent stiffness reduction law in terms of the damage variable for transverse matrix cracking is computed using an Eshelby-Mori-Tanaka approach for the initial composite thermoelastic properties and a self-consistent model for the stiffness reduction as a function of the damage variable. While transverse matrix cracking obeying a damage evolution relation can progressively evolve from an initiation to a saturation state, fiber failure is predicted by a micromechanical fiber rupture criterion that accounts for the fiber strength and matrix stress. The implementation of this integrated multiscale modeling model into a 3D FE formulation enables damage analysis and design of H 2 storage composite pressure vessels. The developed tool is illustrated through 3D damage analyses of a cryogenically compressed H 2 storage vessel model subjected to thermomechanical loadings to investigate effects of the helical layer fiber orientation and loading scenario on damage development, vessel integrity and burst pressure.

08 HYDROGEN↗

Ionizing Radiation Shifts the PAI-1/ID-1 Balance and Activates Notch Signaling in Endothelial Cells

Purpose: Transforming growth factor-{beta} (TGF-{beta}) and Notch signaling pathways are important regulators of vascular homeostasis and vessel remodeling; mutations in these pathways can lead to vascular disorders. Similar vascular phenotypes develop in the normal tissues of cancer patients as a long-term effect of radiotherapy. Irradiation most severely affects the capillaries, which become leaky and dilated and might eventually rupture. To investigate the mechanism of such capillary damage, we studied the effect of TGF-{beta} and Notch signaling in microvascular endothelial cells. Methods and Materials: Human microvascular endothelial cells were irradiated with 5 or 10 Gy and activation of TGF-{beta} and Notch signaling pathways was assessed by biochemical methods and a cell migration assay. Results: Ionizing radiation induced Smad2 phosphorylation and nuclear translocation and increased mRNA and protein expression of the activin-like kinase 5 (ALK5) target gene plasminogen activator inhibitor-1 (PAI-1). At the same time, we observed diminished Smad1/5/8 activation and downregulation of the ALK1 downstream target, inhibitor of DNA binding-1 (ID-1). We also measured an upregulation of the Notch ligand Jagged-1 and the target gene Hey1. Decreased inhibitor of DNA binding-1 levels coincided with a reduced ability of the cells to migrate. Conclusion: Ionizing radiation shifts the balance from ALK1 to ALK5 signaling and activates the Notch pathway in endothelial cells. This combination of anti-angiogenic signals contributes to reduced cell migration after irradiation.

62 RADIOLOGY AND NUCLEAR MEDICINE↗

A novel Lagrangian approach for the stable numerical simulation of fault and fracture mechanics

The simulation of the mechanics of geological faults and fractures is of paramount importance in several applications, such as ensuring the safety of the underground storage of wastes and hydrocarbons or predicting the possible seismicity triggered by the production and injection of subsurface fluids. However, the stable numerical modeling of ground ruptures is still an open issue. The present work introduces a novel formulation based on the use of the Lagrange multipliers to prescribe the constraints on the contact surfaces. The variational formulation is modified in order to take into account the frictional work along the activated fault portion according to the principle of maximum plastic dissipation. The numerical model, developed in the framework of the Finite Element method, provides stable solutions with a fast convergence of the non-linear problem. The stabilizing properties of the proposed model are emphasized with the aid of a realistic numerical example dealing with the generation of ground fractures due to groundwater withdrawal in arid regions. - Highlights: • A numerical model is developed for the simulation of fault and fracture mechanics. • The model is implemented in the framework of the Finite Element method and with the aid of Lagrange multipliers. • The proposed formulation introduces a new contribution due to the frictional work on the portion of activated fault. • The resulting algorithm is highly non-linear as the portion of activated fault is itself unknown. • The numerical solution is validated against analytical results and proves to be stable also in realistic applications.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Equibiaxial flexural strength determination of UO 2 using a ball-on-ring test

To increase nuclear fuel performance and reliability, their mechanical properties require an accurate and statistically relevant assessment. Biaxial flexural strength tests provide an alternative to bend bar techniques for assessing mechanical behavior; namely, the transverse rupture strength (TRS) of ceramic samples. Biaxial test samples require simple geometries and minimal surface preparation, reducing fabrication costs and handling hazards. This study investigated the TRS of polycrystalline UO 2 fuel forms at room temperature using a ball-on-ring test fixture. Here, pellets were fabricated from UO 2 powder using conventional powder processing and sintering techniques. The TRS and Weibull parameters were obtained through Weibull statistics on over 60 UO 2 samples tested under equibiaxial flexure. The larger sample size in this study enabled a more robust Weibull statistical analysis than alternative test methods, which may not capture the stochastic failure of typical ceramics. Furthermore, two different loading ball diameters were employed to assess the impact of contact damage on fracture strength. While Hertzian contact damage was observed with the smaller loading ball, the fracture strength remained unaffected. A fracture analysis of the tested UO 2 samples indicated a mixture of intergranular and transgranular fracture that transitions to transgranular fracture with increasing distance from the fracture origin. The characteristic strength of the combined data sets was determined to be 148 MPa, and the Weibull modulus was determined to be 9.1. The TRS values and Weibull parameters were close to values found in the literature for alternative testing techniques using samples with similar microstructure and density. The findings in this study validate the ball-on-ring method used to obtain the TRS of UO 2 with a sample geometry more representative of nuclear fuels. Additionally, experimental TRS results from this study can be implemented in modeling codes to predict fuel performance, which is critical to fuel burnup extension and advanced nuclear fuel technologies.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Statistical fracture behavior of doped UO 2 using a ball-on-ring equibiaxial flexure test method

Metal oxide dopants, such as titanium and chromium oxides, have garnered considerable attention for their potential to increase grain size (≥ 30 µm) in UO 2 fuel, purportedly enhancing fission gas retention during reactor operation. Fuel performance is significantly impacted by fuel fracture behavior, so it is important to understand the effects of enhanced grain size and dopant content on UO 2 fuel fracture. UO 2 pellets were doped with 0.1 wt% TiO 2 and 0.3 wt% Cr 2 O 3 to alter density and grain size. Inductively coupled plasma mass spectroscopy measured dopant levels pre- and post-sintering. X-ray diffraction revealed lattice changes and microstrain via Rietveld refinement. Field emission scanning electron microscopy determined grain sizes of approximately 30 µm for TiO 2 doping and 7 µm for Cr 2 O 3 doping. Transverse rupture strength tests were performed on over 30 samples per dataset to obtain characteristic strength and Weibull modulus. Results indicate no statistical difference in fracture strength between 0.1 wt% TiO 2 doped UO 2 and undoped UO 2 , while 0.3 wt% Cr 2 O 3 doped UO 2 exhibited a 20% decrease in fracture strength. Doped UO 2 samples also showed reduced Weibull modulus compared to undoped UO 2 , suggesting increased scatter in fracture strength. This study's findings suggest that titanium and chromium oxide doping in UO 2 , regardless of grain size, induce residual stresses, decreasing fracture strength and increasing variability in fracture behavior.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Reassessing early-age strength development of high-volume fly ash concretes for precast buildings

Increasing beneficial use of fresh or landfilled fly ash as a replacement for Portland cement can be more challenging for the construction of precast buildings or similar applications requiring rapid strength development. Therefore, the framework presented in this paper aims to reassess high-volume fly ash concretes but in the context of facilitating more sustainable precast buildings. More specifically, the framework was used to characterize strength development of concrete mixes with a target minimum 24-hour compressive strength of 24.1 MPa (3500 psi), selected as an example strength development metric to demonstrate the framework, and comprised of 40% Class C, Class F, and landfilled (harvested) fly ash – as a high-volume replacement of Type III or Type IL cement. High-early strength was driven by optimized dosages of commercial grade gypsum and accelerating admixtures, in addition to optimal aggregate packing and mix proportioning strategies. Early-age mechanical properties including compressive strength, modulus of rupture, and modulus of elasticity were reevaluated within 24 hours of batching with respect to common precast production demands. Simple data analyses were then used to highlight cases where currently accepted design provisions for the aforementioned properties are either overly-conservative or unconservative with respect to test data. Furthermore, the framework and demonstration of example mixes presented herein aim to promote confidence for using larger fractions of fresh or landfilled fly ashes for precast buildings to further enhance environmental benefits without sacrificing pertinent early-age structural performance.

42 ENGINEERING↗

Multi-faceted framework for extrapolating early age flexural strength to facilitate rapid lifting/handling of high-volume fly ash precast members

Maintaining adequate early-age structural performance for precast concrete components has grown in importance as more sustainable mix designs become more widespread. Achieving high-early flexural strength is particularly crucial to facilitate rapid removal of hardened concrete components from formwork, often within 24 h after fresh concrete placement. Limited research has assessed the effectiveness of traditional design methods in correlating flexural strength with compressive strength for next-generation mix designs, or demonstrated extrapolation of such material performance to larger-scale structural tests. This paper presents a multi-faceted framework to reassess early-age flexural strength for concretes made with relatively high proportions of fly ash from both fresh and harvested sources. Here, the framework provides several pathways, from which the user can select based upon available resources and the specific application, to improve accuracy of early-age cracking moment calculations. Furthermore, the scope includes evaluation of strength performance under curing conditions emulative of those in a precast facility, recommending modulus of rupture equations which are more performance-driven than current design provisions, and experimental tests on prefabricated concrete beams to validate the proposed methodologies. Correlations of early-age strength with both concrete age and maturity measurements compare the effectiveness of utilizing in-situ data to further enhance the prediction methods. Ultimately, the proposed framework helped reduce errors when calculating cracking moment capacity at early ages by tailoring calculations to reflect mix-dependent behavior. Furthermore, most estimates of cracking moment were within 25 % of their corresponding experimental test results, thus promoting confidence for using these strategies with high-volume fly ash precast structures.

42 ENGINEERING↗