At least 1,099 records · Page 61

Oxidation effects on the mechanical properties of a SiC-fiber-reinforced reaction-bonded Si3N4 matrix composite

The room-temperature mechanical properties of SiC fiber reinforced reaction bonded silicon nitride composites were measured after 100 hrs exposure at temperatures to 1400 C in nitrogen and oxygen environments. The composites consisted of approx. 30 vol percent uniaxially aligned 142 micron diameter SiC fibers in a reaction bonded Si3N4 matrix. The results indicate that composites heat treated in a nitrogen environment at temperatures to 1400 C showed deformation and fracture behavior equivalent to that of the as-fabricated composites. Also, the composites heat treated in an oxidizing environment beyond 400 C yielded significantly lower tensile strength values. Specifically in the temperature range from 600 to 1000 C, composites retained approx. 40 percent of their as-fabricated strength, and those heat treated in the temperatures from 1200 to 1400 C retained 70 percent. Nonetheless, for all oxygen heat treatment conditions, composite specimens displayed strain capability beyond the matrix fracture stress; a typical behavior of a tough composite.

Bhatt, Ramakrishna T.↗

Strength, toughness and R-curve behaviour of SiC whisker-reinforced composite Si3N4 with reference to monolithic Si3N4

The flexural strength and fracture toughness of 30 vol pct SiC whisker-reinforced Si3N4 material were determined as a function of temperature from 25 to 1400 C in an air environment. It was found that both strength and toughness of the composite material were almost the same as those of the monolithic counterpart. The room-temperature strength was retained up to 1100 C; however, appreciable strength degradation started at 1200 C and reached a maximum at 1400 C due to stable crack growth. In contrast, the fracture toughness of the two materials was independent of temperature with an average value of 5.66 MPa sq rt m. It was also observed that the composite material exhibited no rising R-curve behavior at room temperature, as was the case for the monolithic material. These results indicate that SiC whisker addition to the Si3N4 matrix did not provide any favorable effects on strength, toughness and R-curve behavior.

Choi, S. R.↗

Material properties and device evaluations of ECR-deposited a-Si:H and a-SiC:H films

Device-quality a-Si:H and a-SiC:H films have been deposited using electron cyclotron resonance (ECR) microwave plasmas of SiH4, CH4, and H2 mixtures. Typical material properties of ECR-deposited, photosensitive a-Si:H films are: (1) high photosensitivity up to 2 x 106 with a photoconductivity of 10 exp -5 to 10 exp -4/(Ohm-cm), (2) a Tauc gap of 1.75 to 1.85 eV, (3) an Urbach slope of 50-60 meV determined by the constant photocurrent method, and (4) an integrated defect density of 1-2 x 10 exp 16/cu cm determined by junction capacitance measurements. Highly conductive, p-type a-SiC:H films have been produced by ECR plasmas with a conductivity of 0.2/(Ohm-cm).

Shing, Y. H.↗

Effects of casting conditions and deformation processing on A356 aluminum and A356-20 vol. pct SiC composites

The effects of casting conditions and deformation processing on the mechanical properties of unreinforced A356 aluminum and A356-20 vol pct SiC composite were investigated by tensile properties in these compounds fabricated by either sand casting or squeeze casting techniques followed by hot working to 33, 50, 90, and 95 percent reductions. The evolution of the microstructure and values of tensile properties were evaluated for the cast materials in each of the hot worked conditions. It was found that, while the deformation processing of the sand-cast composite resulted in banding of the Al and SiC particles within the microstructure, such features were not observed in the squeeze-cast microstructure. The tensile strengths of the squeeze cast materials was found to be higher than those of the sand cast materials, for both the unreinforced and composite samples, while increased amounts of deformation were found to improve the ductility of the composite.

Rozak, G. A.↗

Silicon isotopic composition in large meteoritic SiC particles and Na-22 origin of Ne-22

Large SiC particles extracted from acid-insoluble residues of carbonaceous chondrites are isotopically anomalous in both silicon and carbon and contain isotopically extreme noble gases. These particles are thought to have originated in mass outflows from red giant stars and to have existed in the interstellar medium at the time the solar system formed from an interstellar cloud. Calculations show that the silicon isotope correlations in those large SiC particles can be generated only in the most massive carbon stars. Consequently, the almost pure Ne-22 in those particles must be interpreted as the condensation of radioactive Na-22 in the particles as they flowed away from the stars. The Na-22 is produced through proton capture by Ne-21 at the base of the surface convection zone. Ne-22 does not exist abundantly in helium shells hot enough to burn magnesium, which is necessary to establish the measured silicon isotopic composition.

Brown, Lawrence E.↗

Sliding wear of self-mated Al2O3-SiC whisker-reinforced composites at 23-1200 C

Microstructural changes occurring during sliding wear of self-mated Al2O3 SiC whisker-reinforced composites were studied using optical, scanning electron microscopy and transmission electron microscopy. Pin-on-disc specimens were slid in air at 2.7 m/s sliding velocity under a 26.5 N load for 1 h. Wear tests were conducted at 23, 600, 800 and 1200 C. Mild wear with a wear factor of 2.4 x 10 exp -7 - 1.5 x 10 exp -6 cu mm /N per m was experienced at all test temperatures. The composite showed evidence of wear by fatigue mechanisms at 800 C and below. Tribochemical reaction (SiC oxidation and reaction of SiO2 and Al2O3) leads to intergranular failure at 1200 C. Distinct microstructural differences existing at each test temperature are reported.

Farmer, S. C.↗

Effect of process conditions and chemical composition on the microstructure and properties of chemically vapor deposited SiC, Si, ZnSe, ZnS and ZnS(x)Se(1-x)

Subatmospheric pressure CVD processes have been developed to produce theoretically dense, highly pure, void-free and large area bulk materials, SiC, Si, ZnSe, ZnS and ZnS(x)Se(1-x). These materials are used for optical elements, such as mirrors, lenses and windows, over a wide spectral range from the VUV to the IR. We discuss the effect of CVD process conditions on the microstructure and properties of these materials, with emphasis on optical performance. In addition, we discuss the effect of chemical composition on the properties of the composite material ZnS(x)Se(1-x). We first present a general overview of the bulk CVD process and the relationship between process conditions, such as temperature, pressure, reactant gas concentration and growth rate, and the microstructure, morphology and properties of CVD-grown materials. Then we discuss specific results for CVD-grown SiC, Si, ZnSe, ZnS and ZnS(x)Se(1-x).

Pickering, Michael A.↗

Effect of high temperature annealing on the microstructure of SCS-6 SiC fibers

The effect of annealing the SCS-6 SiC fiber for one hour at 2000 C in an argon atmosphere is reported. The SiC grains in the fiber coarsen appreciably and the intergranular carbon films segregate to the grain junctions. It would appear that grain growth in the outer part of the fiber is primarily responsible for the loss in fiber strength and improvement in fiber creep resistance.

Ning, X. J.↗

Electron cyclotron resonance microwave plasma deposition of a-Si:H and a-SiC:H films

The paper reports electron cyclotron resonance (ECR) deposition of a-Si:H and a-SiC:H thin films using SiH4, CH4, and hydrogen mixed gas plasmas. The ECR deposition conditions were investigated in the pressure region of 0.1 to 100 mtorr, and the film properties were characterized by light and dark conductivity measurements, XRD, Raman spectroscopy, optical transmission, and IR spectroscopy. In addition, the hydrogen dilution effect on ECR-deposited a-SiC:H was investigated.

Shing, Y. H.↗

The astrophysical interpretation of isotope anomalies in graphite and SiC grains of chondrites

The C, N, and Mg isotopic compositions in graphite and SiC grains of carbonaceous chondrites can be explained by nuclear processes in massive O,B stars of second generation passed a stage of WR star with intensive stellar wind, where grain condensation had taken place. The interstellar graphite and SiC grains with anomalous isotopic compositions of C, N, Ne, and Si and other elements of nucleosynthetic origin, found in non-equilibrated chondrites, are most suitable for determination of astro-physical objects, where nucleosynthesis had taken place. Two objects were examined: (1) massive O,B stars of second generation passed a stage of WR star with intensive stellar wind (O,B-WR model) and (2) low-mass stars (1 less than or equal to M/solar mass less than or equal to 3) during thermally pulsing asymptotic giant branch phase (TP-AGB model).

Lavrukhina, A. K.↗

Fingerprints of carbon, nitrogen, and silicon isotopes in small interstellar SiC grains from the Murchison meteorite

We report ion microprobe determinations of the carbon, nitrogen, and silicon isotopic compositions of small SiC grains from the Murchison CM2 chondrite. Analyses were made on samples containing variable numbers of grains and on 14 individual grains. In some cases the multiple-grain sample compositions were probably dominated by only one or two grains. Total ranges observed are given. Only a few grains show values near the range limits. Both the total ranges of carbon and nitrogen isotopic compositions, and even the narrower ranges typical for the majority of the grains, are similar to those observed for larger SiC grains. Two rare components appear to be present in the smaller-size fraction, one characterized by C-12/C-13 about 12-16 and the other by very heavy nitrogen. The carbon and nitrogen isotopic compositions qualitatively may reflect hydrostatic H-burning via the CNO cycle and He-burning in red giants, as well as explosive H-burning in novae. The silicon isotopic compositions of most grains qualitatively show what is the signature of He-burning. The silicon isotopic composition of one grain, however, suggests a different process.

Hoppe, Peter↗

An investigation on the rheological behavior of metallic semi-solid slurries of Al-6.5 pct Si and semi-solid composite slurries of SiC particulates in an Al-6.5 pct Si alloy matrix

The rheology of SiC particulate/Al-6.5 pct Si composite slurries was explored. The rheological behavior of the composite slurries shows both thixotropic and pseudoplastic behaviors. Isostructural experiments on the composite slurries revealed a Newtonian behavior beyond a high shear rate limit. The rheology of fully molten composite slurries over the low to high shear rate range indicates the existence of a low shear rate Newtonian region, an intermediate pseudoplastic region and a high shear rate Newtonian region. The isostructural studies indicate that the viscosity of a composite slurry depends upon the shearing history of a given volume of material. An unexpected shear thinning was noted for SiC particulate + alpha slurries as compared to semi-solid metallic slurries at the same fraction solid. The implications of these findings for the processing of slurries into cast components is discussed.

Moon, H.-K.↗

Effects of Thermal Cycling on Thermal Expansion and Mechanical Properties of Sic Fiber-reinforced Reaction-bonded Si3n4 Composites

Thermal expansion curves for SiC fiber-reinforced reaction-bonded Si3N4 matrix composites (SiC/RBSN) and unreinforced RBSN were measured from 25 to 1400 C in nitrogen and in oxygen. The effects of fiber/matrix bonding and cycling on the thermal expansion curves and room-temperature tensile properties of unidirectional composites were determined. The measured thermal expansion curves were compared with those predicted from composite theory. Predicted thermal expansion curves parallel to the fiber direction for both bonding cases were similar to that of the weakly bonded composites, but those normal to the fiber direction for both bonding cases resulted in no net dimensional changes at room temperature, and no loss in tensile properties from the as-fabricated condition. In contrast, thermal cycling in oxygen for both composites caused volume expansion primarily due to internal oxidation of RBSN. Cyclic oxidation affected the mechanical properties of the weakly bonded SiC/RBSN composites the most, resulting in loss of strain capability beyond matrix fracture and catastrophic, brittle fracture. Increased bonding between the SiC fiber and RBSN matrix due to oxidation of the carbon-rich fiber surface coating and an altered residual stress pattern in the composite due to internal oxidation of the matrix are the main reasons for the poor mechanical performance of these composites.

Bhatt, R. T.↗

Photoconductive and photovoltaic response of high-dark-resistivity 6H-SiC devices

The optoelectronic properties of high-resistivity p-type hexagonal silicon carbide (6H-SiC) have been investigated using lateral photoconductive switches. Both photovoltaic and photoconductive effects are reported, measured at 337 nm, which is above the 6H-SiC absorption edge. These photoconductive switches have been fabricated with dark resistances of up to 1 M omega; photoconductive switching efficiencies of more than 80% have been achieved. In addition, these devices displayed a high-speed photovoltaic response to nanosecond laser excitations in the ultraviolet spectral region; in particular, the observed photovoltaic response pulse width can be shorter than the exciting laser pulse width. This subnanosecond photovoltaic response has been modeled and good qualitative agreement with experiment has been obtained.

Cho, Pak S.↗

Thermal Stability of Hi-Nicalon SiC Fiber in Nitrogen and Silicon Environments

The room temperature tensile strength of uncoated and two types of pyrolytic boron nitride coated (PBN and Si-rich PBN) Hi-Nicalon SiC fibers was determined after 1 to 400 hr heat treatments to 1800 C under N2 pressures of 0.1, 2, and 4 MPa, and under 0.1 Mpa argon and vacuum environments. In addition, strength stability of both uncoated and coated fibers embedded in silicon powder and exposed to 0.1 MPa N2 for 24 hrs at temperatures to 1400 C was investigated. The uncoated and both types of BN coated fibers exposed to N2 for 1 hr showed noticeable strength degradation above 1400 C and 1600 C, respectively. The strength degradation appeared independent of nitrogen pressure, time of heat treatment, and surface coatings. TEM microstructural analysis suggests that flaws created due to SiC grain growth are responsible for the strength degradation. In contact with silicon powder, the uncoated and both types of PBN coated fibers degrade rapidly above 1350 C.

Bhatt, R. T.↗

System for the growth of bulk SiC crystals by modified CVD techniques

The goal of this program was the development of a SiC CVD growth of films thick enough to be useful as pseudo-substrates. The cold-walled CVD system was designed, assembled, and tested. Extrapolating from preliminary evaluation of SiC films grown in the system at relatively low temperatures indicates that the growth rate at the final temperatures will be high enough to make our approach practical. Modifications of the system to allow high temperature growth and cleaner growth conditions are in progress. This program was jointly funded by Wright Laboratory, Materials Directorate and NASA LeRC and monitored by NASA.

Steckl, Andrew J.↗

Bend stress relaxation and tensile primary creep of a polycrystalline alpha-SiC fiber

Understanding the thermomechanical behavior (creep and stress relaxation) of ceramic fibers is of both practical and basic interest. On the practical level, ceramic fibers are the reinforcement for ceramic matrix composites which are being developed for use in high temperature applications. It is important to understand and model the total creep of fibers at low strain levels where creep is predominantly in the primary stage. In addition, there are many applications where the component will only be subjected to thermal strains. Therefore, the stress relaxation of composite consituents in such circumstances will be an important factor in composite design and performance. The objective of this paper is to compare and analyze bend stress relaxation and tensile creep data for alpha-SiC fibers produced by the Carborundum Co. (Niagara Falls, NY). This fiber is of current technical interest and is similar in composition to bulk alpha-SiC which has been studied under compressive creep conditions. The temperature, time, and stress dependences will be discussed for the stress relaxation and creep results. In addition, some creep and relaxation recovery experiments were performed in order to understand the complete viscoelastic behavior, i.e. both recoverable and nonrecoverable creep components of these materials. The data will be presented in order to model the deformation behavior and compare relaxation and/or creep behavior for relatively low deformation strain conditions of practical concern. Where applicable, the tensile creep results will be compared to bend stress relaxation data.

Hee Man, Yun↗

High-Field Fast-Risetime Pulse Failures in 4H- and 6H-SiC pn Junction Diodes

We report the observation of anomalous reverse breakdown behavior in moderately doped (2-3 x 10(exp 17 cm(exp -3)) small-area micropipe-free 4H- and 6H-SiC pn junction diodes. When measured with a curve tracer, the diodes consistently exhibited very low reverse leakage currents and sharp repeatable breakdown knees in the range of 140-150 V. However, when subjected to single-shot reverse bias pulses (200 ns pulsewidth, 1 ns risetime), the diodes failed catastrophically at pulse voltages of less than 100 V. We propose a possible mechanism for this anomalous reduction in pulsed breakdown voltage relative to dc breakdown voltage. This instability must be removed so that SiC high-field devices can operate with the same high reliability as silicon power devices.

Neudeck, Philip G.↗