A facile pathway to prepare VO{sub 2} and V{sub 2}O{sub 3} powders via a carbothermal reduction process
The development of a highly efficient and low cost production process is instrumental for the wide application of VO{sub 2} and V{sub 2}O{sub 3}. In this paper, VO{sub 2} and V{sub 2}O{sub 3} powders are successfully prepared via carbothermal reduction of V{sub 2}O{sub 5} in a flowing Ar atmosphere at 973 K and 1423 K, respectively. Compared with the traditional methods, graphite is used as a reductant, which resulted in a low cost. The experimental results show that a high temperature assists in improving the kinetic rate. The phase transformation during the low-temperature reduction process between 948 K and 973 K occurs in the following sequential order: V{sub 2}O{sub 5}→V{sub 6}O{sub 13}→VO{sub 2}. When the temperature is 1423 K or 1473 K, the phase transformation can be described as follows: V{sub 2}O{sub 5}→V{sub 3}O{sub 5}→V{sub 2}O{sub 3}. Owing to the shrink of the volume, the as-prepared VO{sub 2} and V{sub 2}O{sub 3} particles could not maintain the original micro-morphology of V{sub 2}O{sub 5}. Relative to VO{sub 2}, the as-prepared V{sub 2}O{sub 3} particles are porous. It is also concluded that the V{sub 2}O{sub 3} can be easily oxidized to VO{sub 2}, when the partial pressure of O{sub 2} is in the range of 10{sup −8} atm to 10{sup −1} atm. Therefore, a reasonable reaction temperature and reaction time are important to prepare high purity V{sub 2}O{sub 3}.