Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Etching”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,099 records · Page 61

LET Spectrum Measurements In CR-39 PNTD With AFM

Energetic protons, neutrons, and heavy ions undergoing collisions with target nuclei of varying Z can produce residual heavy recoil fragments via intra-nuclear cascade/evaporation reactions. The particles produced in these non-elastic collisions generally have such extremely short range ({approx}<10 {mu}m) that they cannot be directly observed by conventional detection methods including CR-39 plastic nuclear track detector (PNTD) that has been chemically etched for analysis by standard visible light microscopy. However, high-LET recoil fragments having range on the order of several cell diameters can be produced in tissue during radiotherapy using proton and carbon beams. We have developed a method to analyze short-range, high-LET tracks in CR-39 plastic nuclear track detector (PNTD) using short duration chemical etching ({approx}<1 {mu}m) following by automated atomic force microscope (AFM) scanning. The post-scan data processing used in this work was based on semi-automated matrix analysis opposed to traditional grey-scale image analysis. This method takes advantage of the 3-D data obtained via AFM to achieve robust discrimination of nuclear tracks from other features inherently present in the post-etch detector surface. Through automation of AFM scanning, sufficient AFM scan frames were obtained to attain an LET spectrum spanning the LET range from 200-1500 keV/{mu}m. In addition to our experiments, simulations were carried out with the Monte Carlo transport code, FLUKA. To demonstrate this method, CR-39 PNTD was exposed to the proton therapy beam at Loma Linda University Medical Center (LLUMC) at 60 and 230 MeV. Additionally, detectors were exposed to 1 GeV protons at the NASA Space Radiation Laboratory (NSRL) at Brookhaven National Laboratory (BNL). For these exposures CR-39 PNTD, Al and Cu target foils were used between detector layers.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Metal-assisted electroless fabrication of nanoporous p-GaN for increasing the light extraction efficiency of light emitting diodes

We report metal-assisted electroless fabrication of nanoporous p-GaN to improve the light extraction efficiency of GaN-based light emitting diodes (LEDs). Although it has long been believed that p-GaN cannot be etched at room temperature, in this study we find that Ag nanocrystals (NCs) on the p-GaN surface enable effective etching of p-GaN in a mixture of HF and K{sub 2}S{sub 2}O{sub 8} under ultraviolet (UV) irradiation. It is further shown that the roughened GaN/air interface enables strong scattering of photons emitted from the multiple quantum wells (MQWs). The light output power measurements indicate that the nanoporous LEDs obtained after 10 min etching show a 32.7% enhancement in light-output relative to the conventional LEDs at an injection current of 20 mA without significant increase of the operating voltage. In contrast, the samples etched for 20 min show performance degradation when compared with those etched for 10 min, this is attributed to the current crowding effect and increased surface recombination rate.

36 MATERIALS SCIENCE↗

Influence of hydrogen patterning gas on electric and magnetic properties of perpendicular magnetic tunnel junctions

To identify the degradation mechanism in magnetic tunnel junctions (MTJs) using hydrogen, the properties of the MTJs were measured by applying an additional hydrogen etch process and a hydrogen plasma process to the patterned MTJs. In these studies, an additional 50 s hydrogen etch process caused the magnetoresistance (MR) to decrease from 103% to 14.7% and the resistance (R) to increase from 6.5 kΩ to 39 kΩ. Moreover, an additional 500 s hydrogen plasma process decreased the MR from 103% to 74% and increased R from 6.5 kΩ to 13.9 kΩ. These results show that MTJs can be damaged by the hydrogen plasma process as well as by the hydrogen etch process, as the atomic bonds in MgO may break and react with the exposed hydrogen gas. Compounds such as MgO hydrate very easily. We also calculated the damaged layer width (DLW) of the patterned MTJs after the hydrogen etching and plasma processes, to evaluate the downscaling limitations of spin-transfer-torque magnetic random-access memory (STT-MRAM) devices. With these calculations, the maximum DLWs at each side of the MTJ, generated by the etching and plasma processes, were 23.8 nm and 12.8 nm, respectively. This result validates that the hydrogen-based MTJ patterning processes cannot be used exclusively in STT-MRAMs beyond 20 nm.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Wet chemical thinning of molybdenum disulfide down to its monolayer

We report on the preparation of mono- and bi-layer molybdenum disulfide (MoS{sub 2}) from a bulk crystal by facile wet chemical etching. We show that concentrated nitric acid (HNO{sub 3}) effectively etches thin MoS{sub 2} crystals from their edges via formation of MoO{sub 3}. Interestingly, etching of thin crystals on a substrate leaves behind unreacted mono- and bilayer sheets. The flakes obtained by chemical etching exhibit electronic quality comparable to that of mechanically exfoliated counterparts. Our findings indicate that the self-limiting chemical etching is a promising top-down route to preparing atomically thin crystals from bulk layer compounds.

36 MATERIALS SCIENCE↗

Uncladded sensing fiber for refractive index measurement

The formation of chemically etched optical fiber for use in refractive index sensor is addressed. This presented design of a refractive index (RI) sensor is based on recording the power loss exhibited by radiation propagating through an etched multimode fiber (MMF) immersed in the liquid under study. The decreasing diameters of fibers are found to be strongly dependent on the temperature and etchant composition. This experiment was performed for different unclad etched fibers for same sensing length and the RI changes from 1.33 RIU to 1.38 RIU. When the multimode fiber (MMF) is etched for 12 hours the sensitivity of the sensor is approximately 204.25dBm/RIU, which is larger than without etched fiber having sensitivity 127.2dBm/RIU.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Design criteria for XeF{sub 2} enabled deterministic transformation of bulk silicon (100) into flexible silicon layer

Isotropic etching of bulk silicon (100) using Xenon Difluoride (XeF{sub 2}) gas presents a unique opportunity to undercut and release ultra-thin flexible silicon layers with pre-fabricated state-of-the-art Complementary Metal Oxide Semiconductor (CMOS) electronics. In this work, we present design criteria and mechanism with a comprehensive mathematical model for this method. We consider various trench geometries and parametrize important metrics such as etch time, number of cycles and area efficiency in terms of the trench diameter and spacing so that optimization can be done for specific applications. From our theoretical analysis, we conclude that a honeycomb-inspired hexagonal distribution of trenches can produce the most efficient release of ultra-thin flexible silicon layers in terms of the number of etch cycles, while a rectangular distribution of circular trenches provides the most area efficient design. The theoretical results are verified by fabricating and releasing (varying sizes) flexible silicon layers. We observe uniform translation of design criteria into practice for etch distances and number of etch cycles, using reaction efficiency as a fitting parameter.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Distribution of Tritium in the Near Surface of Type 316 Stainless Steel

The distribution of tritium in the near surface of stainless steel, type 316, has been measured using a combination of a ZnCl 2 wash and acid etching with diluted aqua regia. This method improves upon etching measurements reported in the literature: results show depth resolutions of ~10 nm using the diluted aqua regia. The ZnCl 2 wash results show very high surface concentrations (~1.5 x10 13 Bq/cm 3 ), which decreases by a factor of 10 6 after etching to a depth of ~10 um. Further, the tritium concentrations in the near surface (<10 um) of unmodified stainless-steel samples do not change significantly over the course of 233 days, which indicates a quasi-equilibrium state has been reached. Tritium migration to the surface from the subsurface region was measured by etching a sample, then storing it in air for 2 to 4 days. After storing in air, the surface concentrations increased a thousandfold and rapidly decreased to base levels after etching an additional ~2 um. Finally, these measurements indicate that perturbing the quasi-equilibrium concentration profile results in tritium migration to the surface in order to reestablish the prior equilibrium state.

36 MATERIALS SCIENCE↗

Surface roughening of silicon, thermal silicon dioxide, and low-k dielectric coral films in argon plasma

The surface roughness evolutions of single crystal silicon, thermal silicon dioxide (SiO{sub 2}), and low dielectric constant film coral in argon plasma have been measured by atomic force microscopy as a function of ion bombardment energy, ion impingement angle, and etching time in an inductively coupled plasma beam chamber, in which the plasma chemistry, ion energy, ion flux, and ion incident angle can be adjusted independently. The sputtering yield (or etching rate) scales linearly with the square root of ion energy at normal impingement angle; additionally, the angular dependence of the etching yield of all films in argon plasma followed the typical sputtering yield curve, with a maximum around 60 deg. -70 deg. off-normal angle. All films stayed smooth after etching at normal angle but typically became rougher at grazing angles. In particular, at grazing angles the rms roughness level of all films increased if more material was removed; additionally, the striation structure formed at grazing angles can be either parallel or transverse to the beam impingement direction, which depends on the off-normal angle. More interestingly, the sputtering caused roughness evolution at different off-normal angles can be qualitatively explained by the corresponding angular dependent etching yield curve. In addition, the roughening at grazing angles is a strong function of the type of surface; specifically, coral suffers greater roughening compared to thermal silicon dioxide.

36 MATERIALS SCIENCE↗

Processing of GaN/Si(111) Epitaxial Structures for MEMS Applications

Two different approaches for the etching of the gallium nitride epitaxial layers grown on Si(111) substrates by plasma-assisted molecular beam epitaxy have been elaborated. It is demonstrated that anisotropic etch profiles can be achieved by both photoenhanced wet chemical etching and reactive plasma-chemical etching methods. Moreover, it is shown, that the photoenhanced wet chemical etching allows to remove GaN layer without damaging silicon substrate.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Plasma Treatment of Niobium SRF Cavity Surfaces

Plasma based surface modification provides an excellent opportunity to eliminate non- superconductive pollutants in the penetration depth region of the SRF cavity surface and to remove mechanically damaged surface layer improving surface roughness. We have demonstrated on flat samples that plasma etching in Ar / Cl2 of bulk Nb is a viable alternative surface preparation technique to BCP and EP methods, with comparable etching rates. The geometry of SRF cavities made of bulk Nb defines the use of asymmetric RF discharge configuration for plasma etching. In a specially designed single cell cavity with sample holders, discharge parameters are combined with etched surface diagnostics to obtain optimum combination of etching rates, roughness and homogeneity in a variety of discharge types, conditions, and sequences. The optimized experimental conditions will ultimately be applied to single cell SRF cavities.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Understanding the mechanism of base development of hydrogen silsesquioxane

There have been numerous studies of electron beam exposed hydrogen silsesquioxane (HSQ) development conditions in order to improve the developer contrast. For TMAH based development, improvements were made by going to higher TMAH normalities and heating the developer. Yang and Berggren showed development of electron beam exposed (HSQ) by NaOH with added Na salts (various anions) significantly improves the contrast. Here, we study the contrast and etching rates of 100 keV exposed HSQ in NaOH in the presence of LiCl, NaCl, and KCl salts and use this as a segway to understand the mechanisms governing contrast during development HSQ development. The basic mechanism of development of HSQ can be understood by comparing to etching of quartz in basic solutions. Hydroxide ions act as nucleophiles which attack silicon. When a silicon-oxygen bond of the Si-O-Si matrix is broken, Si-O{sup -} and Si-OH are formed which can reversibly react to form the original structure. When a Si-H bond is broken via reaction with hydroxide, Si-O{sup -} and H{sub 2} gas are formed. Salts can change the etching rates as a function of dose in a non-linear fashion to increase etch contrast. Figs. 1, 2, and 3 show contrast curves for HSQ developed in 0.25 N sodium hydroxide and with the addition of NaCl, LiCl and KCl salts at several concentrations. NaCl addition resulted in the highest contrast. Contrast improves with additional salt concentration while sensitivity decreases. Interestingly enough, addition of salt decreases the removal of material of NaOH alone at higher doses while increasing the rate at lower concentrations. Addition of LiCl salts improves contrast over NaOH alone. Furthermore, the sensitivity at all doses increases as the LiCl concentration increases, a salting out effect. Similar to NaCl salt behavior, the addition of KCl salts, improves contrast at the expense of sensitivity. However, unlike NaCl, even at very high doses, KCl addition increases removal rate of HSQ. We propose explanations for these results by considering the change of nucleophilic strength of the OH{sup -} as a function of cation size and concentration, the ability for salts to block the surface etching, competition between bond breakage and recombination, and the density of the HSQ as a function of dose. Furthermore, we will discuss evolution of contrast as a function of development time in the context of our models.

36 MATERIALS SCIENCE↗

17.1%-Efficient Multi-Scale-Textured Black Silicon Solar Cells without Dielectric Antireflection Coating: Preprint

In this work we present 17.1%-efficient p-type single crystal Si solar cells with a multi-scale-textured surface and no dielectric antireflection coating. Multi-scale texturing is achieved by a gold-nanoparticle-assisted nanoporous etch after conventional micron scale KOH-based pyramid texturing (pyramid black etching). By incorporating geometric enhancement of antireflection, this multi-scaletexturing reduces the nanoporosity depth required to make silicon 'black' compared to nanoporous planar surfaces. As a result, it improves short-wavelength spectral response (blue response), previously one of the major limiting factors in 'black-Si' solar cells. With multi-scale texturing, the spectrum-weighted average reflectance from 350- to 1000-nm wavelength is below 2% with a 100-nm deepnanoporous layer. In comparison, roughly 250-nm deep nanopores are needed to achieve similar reflectance on planar surface. Here, we characterize surface morphology, reflectivity and solar cell performance of the multi-scale textured solar cells.

14 SOLAR ENERGY↗

Interaction between dissolution and precipitation during olivine carbonation: Implications for CO 2 mineralization

Large-scale carbonation of olivine is considered a promising approach for in situ mineral carbonation, offering a permanent and stable method for CO 2 storage. A critical aspect of this process is understanding how dissolution and precipitation interact, as this could drive fracturing and enhance further reactions. In this study, we conducted carbonation experiments on olivine using CO 2 -saturated aqueous solutions of NaHCO 3 and NaCl. Two experimental setups were used: one representing an open geochemical system and the other a closed system, corresponding to reaction-limited and flow-limited scenarios, respectively. Further, post-reaction textural analysis using scanning electron microscopy (SEM) revealed surface coatings of reaction products in the closed system, while etch pits and etch channels were prevalent in the open system. Although no direct evidence of reaction-driven fracturing was observed, etch pits and etch channels may serve as initiation points for subcritical crack formation and growth, potentially maintaining permeability and exposing new unreacted surfaces. Using linear elastic fracture mechanics (LEFM) model, we estimate that microcracks could propagate under a pressure of 0.1 GPa if reaction products accumulate within the etch pits. Our findings offer new insights into the mechanisms governing olivine carbonation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

One-step synthesis of lightly doped porous silicon nanowires in HF/AgNO{sub 3}/H{sub 2}O{sub 2} solution at room temperature

One-step synthesis of lightly doped porous silicon nanowire arrays was achieved by etching the silicon wafer in HF/AgNO{sub 3}/H{sub 2}O{sub 2} solution at room temperature. The lightly doped porous silicon nanowires (pNWs) have circular nanopores on the sidewall, which can emit strong green fluorescence. The surface morphologies of these nanowires could be controlled by simply adjusting the concentration of H{sub 2}O{sub 2}, which influences the distribution of silver nanoparticles (Ag NPs) along the nanowire axis. A mechanism based on Ag NPs-induced lateral etching of nanowires was proposed to explain the formation of pNWs. The controllable and widely applicable synthesis of pNWs will open their potential application to nanoscale photoluminescence devices. - Graphical abstract: The one-step synthesis of porous silicon nanowire arrays is achieved by chemical etching of the lightly doped p-type Si (100) wafer at room temperature. These nanowires exhibit strong green photoluminescence. SEM, TEM, HRTEM and photoluminescence images of pNWs. The scale bars of SEM, TEM HRTEM and photoluminescence are 10 {mu}m, 20 nm, 10 nm, and 1 {mu}m, respectively. Highlights: Black-Right-Pointing-Pointer Simple one-step synthesis of lightly doped porous silicon nanowire arrays is achieved at RT. Black-Right-Pointing-Pointer Etching process and mechanism are illustrated with etching model from a novel standpoint. Black-Right-Pointing-Pointer As-prepared porous silicon nanowire emits strong green fluorescence, proving unique property.

36 MATERIALS SCIENCE↗

Enhanced stability of silicon for photoelectrochemical water oxidation through self-healing enabled by an alkaline protective electrolyte

Alkaline electrolytes impede the corrosion of Si photoanodes under positive potentials and/or illumination, due to the formation of a SiO x layer that etches 2–3 orders of magnitude more slowly than Si. Hence during water oxidation under illumination, pinholes in protection layers on Si photoanodes result in the local formation of a protective, stabilizing passive oxide on the Si surface. However, operation under natural diurnal insolation cycles additionally requires protection strategies that minimize the dark corrosive etching rate of Si at pinholes. We show herein that addition of [Fe(CN) 6 ] 3- to 1.0 M KOH(aq) results in a self-healing process that extends the lifetime to >280 h of an np + -Si(100) photoanode patterned with an array of Ni catalyst islands operated under simulated day/night cycles. The self-healing [Fe(CN) 6 ] 3- additive caused the exposed Si(100) surface to etch >180 times slower than the Si etch rate in 1.0 M KOH(aq) alone. No appreciable difference in etch rate or facet preference was observed between Si(100) and Si(111) surfaces in 1.0 M KOH(aq) with [Fe(CN) 6 ] 3- , indicating that the surface conformally oxidized before Si dissolved. The presence of [Fe(CN) 6 ] 3- minimally impacted the faradaic efficiency or overpotential of p + -Si/Ni electrodes for the oxygen-evolution reaction.

25 ENERGY STORAGE↗

Carbon nanospike coated nanoelectrodes for measurements of neurotransmitters

Here, carbon nanoelectrodes enable the detection of neurotransmitters at the level of single cells, vesicles, synapses and small brain structures. Previously, the etching of carbon fibers and 3D printing based on direct laser writing have been used to fabricate carbon nanoelectrodes, but these methods lack the ability of mass manufacturing. In this paper, we mass fabricate carbon nanoelectrodes by growing carbon nanospikes (CNSs) on metal wires. CNSs have a short, dense and defect-rich surface that produces remarkable electrochemical properties, and they can be mass fabricated on almost any substrate without using catalysts. Tungsten wires and niobium wires were electrochemically etched in batch to form sub micrometer sized tips, and a layer of CNSs was grown on the metal wires using plasma-enhanced chemical vapor deposition (PE-CVD). The thickness of the CNS layer was controlled by the deposition time, and a thin layer of CNSs can effectively cover the entire metal surface while maintaining the tip size within the sub micrometer scale. The etched tungsten wires produced tapered conical nanotips, while the etched niobium wires were long and thin. Both showed excellent sensitivity for the detection of outer sphere ruthenium hexamine and the inner sphere test compound ferricyanide. The CNS nanosensors were used for the measurement of dopamine, serotonin, ascorbic acid and DOPAC with fast-scan cyclic voltammetry. The CNS nanoelectrodes had a large surface area and numerous defect sites, which improved the sensitivity, electron transfer kinetics and adsorption. Finally, the CNS nanoelectrodes were compared with other nanoelectrode fabrication methods, including flame etching, 3D printing, and nanopipettes, which are slower to make and more difficult for mass fabrication. Thus, CNS nanoelectrodes are a promising strategy for the mass fabrication of nanoelectrode sensors for neurotransmitters.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Off state breakdown behavior of AlGaAs / InGaAs field plate pHEMTs

Off-state breakdown voltage, V{sub br}, is an important parameter determining the maximum power output of microwave Field Effect Transistors (FETs). In recent years, the use of field plates has been widely adopted to significantly increase V{sub br}. This important technological development has extended FET technologies into new areas requiring these higher voltages and power levels. Keeping with this goal, field plates were added to an existing AlGaAs / InGaAs pseudomorphic High Electron Mobility Transistor (pHEMT) process with the aim of determining the off-state breakdown mechanism and the dependency of V{sub br} on the field plate design. To find the mechanism responsible for breakdown, temperature dependent off-state breakdown measurements were conducted. It was found that at low current levels, the temperature dependence indicates thermionic field emission at the Schottky gate and at higher current levels, impact ionization is indicated. The combined results imply that impact ionization is ultimately the mechanism that is responsible for the breakdown in the tested transistors, but that it is preceded by thermionic field emission from the gate. To test the dependence of V{sub br} upon the field plate design, the field plate length and the etch depth through the highly-doped cap layer under the field plate were varied. Also, non-field plate devices were tested along side field plate transistors. It was found that the length of the etched region under the field plate is the dominant factor in determining the off-state breakdown of the more deeply etched devices. For less deeply etched devices, the length of the field plate is more influential. The influence of surface states between the highly doped cap layer and the passivation layer along the recess are believed to have a significant influence in the case of the more deeply etched examples. It is believed that these traps spread the electric field, thus raising the breakdown voltage. Three terminal breakdown voltages approaching 60V for the most deeply recessed devices are seen.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Suppression of low-frequency charge noise in gates-defined GaAs quantum dots

To reduce the charge noise of a modulation-doped GaAs/AlGaAs quantum dot, we have fabricated shallow-etched GaAs/AlGaAs quantum dots using the wet-etching method to study the effects of two-dimensional electron gas (2DEG) underneath the metallic gates. The low-frequency 1/f noise in the Coulomb blockade region of the shallow-etched quantum dot is compared with a non-etched quantum dot on the same wafer. The average values of the gate noise are approximately 0.5 μeV in the shallow-etched quantum dot and 3 μeV in the regular quantum dot. Our results show the quantum dot low-frequency charge noise can be suppressed by the removal of the 2DEG underneath the metallic gates, which provides an architecture for noise reduction.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗