Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Deposit”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,099 records · Page 61

The Impact of Deposition Temperature on Sodium Fluoride Recrystallization in Cu(In,Ga)Se 2 Solar Cells

Deposited CIGS layers typically undergo a NaF post deposition treatment (PDT) to improve the electrical properties of the deposited films. Here, these NaF annealing processes can also be used to recrystallize CIGS films. To determine the effect of NaF as a fluxing agent, CIGS was deposited at varying substrate temperatures. In-situ annealing with NaF was then done to determine how the initial grain structure energy impacts recrystallization. Gallium appears to be a significant deterrent to recrystallization; the most crystallized film experienced a phase segregation between CIS and gallium containing compounds. By investigating these phase separations more, it might be feasible that a process of rapidly depositing CIGS at extremely low temperatures could create films of sufficient quality to be economically viable.

14 SOLAR ENERGY↗

Shifts in bacterial traits under chronic nitrogen deposition align with soil processes in arbuscular, but not ectomycorrhizal-associated trees

Nitrogen (N) deposition increases soil carbon (C) storage by reducing microbial activity. These effects vary in soil beneath trees that associate with arbuscular (AM) and ectomycorrhizal (ECM) fungi. Variation in carbon C and N uptake traits among microbes may explain differences in soil nutrient cycling between mycorrhizal associations in response to high N loads, a mechanism not previously examined due to methodological limitations. Here, we used quantitative Stable Isotope Probing (qSIP) to measure bacterial C and N assimilation rates from an added organic compound, which we conceptualize as functional traits. As such, we applied a trait-based approach to explore whether variation in assimilation rates of bacterial taxa can inform shifts in soil function under chronic N deposition. We show taxon-specific and community-wide declines of bacterial C and N uptake under chronic N deposition in both AM and ECM soils. N deposition-induced reductions in microbial activity were mirrored by declines in soil organic matter mineralization rates in AM but not ECM soils. Our findings suggest C and N uptake traits of bacterial communities can predict C cycling feedbacks to N deposition in AM soils, but additional data, for instance on the traits of fungi, may be needed to connect microbial traits with soil C and N cycling in ECM systems. In conclusion, our study also highlights the potential of employing qSIP in conjunction with trait-based analytical approaches to inform how ecological processes of microbial communities influence soil functioning.

59 BASIC BIOLOGICAL SCIENCES↗

High rate deposition of photocatalytic TiO{sub 2} films with high activity by hollow cathode gas-flow sputtering method

Photocatalytic TiO{sub 2} films were deposited by a hollow cathode gas-flow sputtering method using two Ti metal targets mounted parallel to each other. The Ar and O{sub 2} flow rates were 3000 and 0-50 SCCM (SCCM denotes cubic centimeter per minute at STP), respectively, and total gas pressure during the deposition was maintained at 45 Pa. The highest deposition rate for the photocatalytic TiO{sub 2} films was 162 nm/min at 30 SCCM of O{sub 2} flow. The as-deposited films and postannealed films, annealed in air at 300 deg. C for 1 h, were used to carry out photocatalytic decomposition of acetaldehyde (CH{sub 3}CHO). In particular, the postannealed films showed extremely high photocatalytic activity compared to the photocatalytic activity of films deposited by conventional reactive sputtering.

36 MATERIALS SCIENCE↗

Role of chamber dimension in fluorocarbon based deposition and etching of SiO{sub 2} and its effects on gas and surface-phase chemistry

It is well understood that chamber geometry is an influential factor governing plasma processing of materials. Simple models suggest that a large fraction of this influence is due to changes in basic plasma properties, namely, density, temperature, and potential. However, while such factors do play an important role, they only partly describe the observed differences in process results. Therefore, to better elucidate the role of chamber geometry in this work, the authors explore the influence of plasma chemistry and its symbiotic effect on plasma processing by decoupling the plasma density, temperature, and potential from the plasma-surface (wall) interactions. Specifically, a plasma system is used with which the authors can vary the chamber dimension so as to vary the plasma-surface interaction directly. By varying chamber wall diameter, 20-66 cm, and source-platen distance, 4-6 cm, the etch behavior of SiO{sub 2} (or the deposition behavior of fluorocarbon polymer) and the resulting gas-phase chemistry change significantly. Results from in situ spectroscopic ellipsometry show significant differences in etch characteristics, with etch rates as high as 350 nm/min and as low as 75 nm/min for the same self-bias voltage. Fluorocarbon deposition rates are also highly dependent on chamber dimension and vary from no net deposition to deposition rates as high as 225 nm/min. Etch yields, however, remain unaffected by the chamber size variations. From Langmuir probe measurements, it is clear that chamber geometry results in significant shifts in plasma properties such as electron and ion densities. Indeed, such measurements show that on-wafer processes are limited at least in part by ion flux for high energy reactive ion etch. However, in situ multipass Fourier transform infrared spectroscopy reveals that the line-averaged COF{sub 2}, SiF{sub 4}, CF{sub 2}, and CF{sub 3} gas-phase densities are also dependent on chamber dimension at high self-bias voltage and also correlate well to the CF{sub x} overlayer stoichiometry under deposition conditions.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Studies on hard TaN thin film deposition by R C-Mag technique

The physical and mechanical properties of pulsed rotating cylindrical magnetron sputter-grown tantalum nitride (TaN) thin films were studied. Initially, films were grown at ambient substrate temperature by varying the reactive (N{sub 2}) to sputter (Ar) gas ratio (R) at a constant pulsing frequency of the target power (100 kHz). The results were compared with planar magnetron-grown TaN samples. The R C-Mag. grown thin films have properties nearly similar to the high temperature (300 degree sign C) dc planar magnetron sputter deposited samples. In comparison to the planar magnetron deposition, the progression of the phase composition occurs over a wider range of R in the pulsed R C-Mag. deposition. These observed differences for R C-Mag. deposition are attributed to the increased glancing angle deposition of adatoms and pulsing of the target power. To study the effect of pulsing frequency of the target power in R C-Mag., the films were also grown at different frequencies at a fixed R (0.1). With the increase in frequency, the mechanical hardness increased up to 50 kHz and started decreasing beyond 50 kHz. The observed changes in the mechanical hardness are attributed to the increase in stress and to the formation of increased polycrystalline understoichiometric TaN phases.

36 MATERIALS SCIENCE↗

Microstructure and temperature coefficient of resistance of thin cermet resistor films deposited from CrSi{sub 2}-Cr-SiC targets by S-gun magnetron

Technological solutions for producing nanoscale cermet resistor films with sheet resistances above 1000 {Omega}/{open_square} and low temperature coefficients of resistance (TCR) have been investigated. 2-40 nm thick cermet films were sputter deposited from CrSi{sub 2}-Cr-SiC targets by a dual cathode dc S-gun magnetron. In addition to studying film resistance versus temperature, the nanofilm structural features and composition were analyzed using scanning electron microscopy, atomic force microscopy, high-resolution transmission electron microscopy, energy-dispersive x-ray spectroscopy, and electron energy loss spectroscopy. This study has revealed that all cermet resistor films deposited at ambient and elevated temperatures were amorphous. The atomic ratio of Si to Cr in these films was about 2 to 1. The film TCR displayed a significant increase when the deposited film thickness was reduced below 2.5 nm. An optimized sputter process consisting of wafer degassing, cermet film deposition at elevated temperature with rf substrate bias, and a double annealing in vacuum, consisting of in situ annealing following the film sputtering and an additional annealing following the exposure of the wafers to air, has been found to be very effective for the film thermal stabilization and for fine tuning the film TCR. Cermet films with thicknesses in the range of 2.5-4 nm deposited using this technique had sheet resistances ranging from 1800 to 1200 {Omega}/{open_square} and TCR values from -50 ppm/ deg. C to near zero, respectively. A possible mechanism responsible for the high efficiency of annealing the cermet films in vacuum (after preliminary exposure to air), resulting in resistance stabilization and TCR reduction, is also discussed.

36 MATERIALS SCIENCE↗

High rate reactive magnetron sputter deposition of Al-doped ZnO with unipolar pulsing and impedance control system

Al-doped ZnO (AZO) films were deposited on quartz glass substrates, unheated and heated to 200 deg. C, using reactive sputtering with a special feedback system of discharge impedance combined with midfrequency pulsing. A planar Zn-Al alloy target was connected to the switching unit, which was operated in a unipolar pulse mode. The oxidation of the target surface was precisely controlled by a feedback system for the entire O{sub 2} flow ratio including ''the transition region''. The deposition rate was about 10-20 times higher than that for films deposited by conventional sputtering using an oxide target. A deposition rate of AZO films of 390 nm/min with a resistivity of 3.8x10{sup -4} {Omega} cm and a transmittance in the visible region of 85% was obtained when the films were deposited on glass substrates heated to 200 deg. C with a discharge power of 4 kW.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Initial growth stage evaluation of high quality ZnSe films deposited on glass substrate

Initial growth stage evaluation of high quality ZnSe films deposited on a glass substrate was investigated. The self-limiting monolayer epitaxial process was used to pregrowth the buffer layer for a zinc selenide (ZnSe) film deposited. After alternating depositions for several cycles, the growth mode was changed to the molecular beam deposition mode under growth conditions. Films deposited at substrate temperatures of 250-350 deg. C and Se/Zn beam equivalent pressure ratios of 0.77-1.87 were investigated. The crystal structure and the preferred orientation of as-grown ZnSe films were examined using x-ray diffraction patterns. The optical properties of the ZnSe films were revealed by photoluminescence spectra. The characteristics of the ZnSe films with and without a buffer layer were compared and discussed in detail. Finally, the results demonstrate how the quality of ZnSe film can be improved on glass substrates for application to various devices.

36 MATERIALS SCIENCE↗

Effect of process conditions on the microstructural formation of dc reactively sputter deposited AlN

Thin film aluminum nitride (AlN), because of its attractive properties, is a material with many applications. Its microstructure and hence properties are greatly influenced by the deposition process conditions. In this work, AlN was reactively deposited in a dc magnetron sputtering system at different proportions of nitrogen in the process gas mixture and at different process conditions. The microstructure and composition of the films were analyzed using x-ray diffraction data, energy dispersive spectroscopy, and scanning electron microscopy. Results show that for a process gas pressure of 0.67 Pa, a magnetron power of 100 W, and a substrate-target distance of 10 cm, a near stoichiometeric AlN can be prepared at nitrogen proportions as low as 20%. At these process conditions, (002) was the preferred crystal orientation. Dense fibrous structures were obtained, especially at low deposition rates with high proportions of nitrogen. Increase in magnetron power and decrease in distance result in a more porous structure. High kinetic energies (average) of the sputtered Al particles and high deposition rates tend to favor AlN(101) formation, while low kinetic energies of the Al particles and low deposition rates generally favor more of the AlN(100) formation.

36 MATERIALS SCIENCE↗

Direct simulation Monte Carlo study of effects of thermal nonuniformities in electron-beam physical vapor deposition

In a typical electron-beam physical vapor deposition system, there is limited control over how the high-power electron beam heats the metal surface. This leads to thermal nonuniformities at the melt. Three-dimensional direct simulation Monte Carlo simulations were performed with the aim of quantifying the effect of such spatial variations of source temperature in thin film depositions using an electron-beam physical vapor deposition system. The source temperature distribution from a typical deposition process was used in the direct simulation Monte Carlo simulations performed for various mass flow rates. The use of an area-averaged temperature is insufficient for all mass flow rates due to the highly nonlinear relationship between temperature and saturation number density, and hence, the mass flux. The mass flow rate equivalent temperature was determined, and the simulations performed with this temperature were compared with those corresponding to the actual nonuniform temperature distribution. For low mass flow rates, the growth rates depend very weakly on the spatial variation of temperature as long as an equivalent temperature corresponding to the same mass flow rate was used. However, as the mass flow rate increases, the error associated with this approximation increases. For deposition processes with source Knudsen numbers less than 0.05, it is not possible to account for the spatial nonuniformities in temperature using the total mass flow rate without significant errors. For a given mass flow rate, the errors associated with using an equivalent temperature decrease with increasing collector plane distance since the flow is allowed to expand further, thereby decreasing the effects of slit temperature nonuniformities.

36 MATERIALS SCIENCE↗

Metal oxide morphology in argon-assisted glancing angle deposition

Glancing angle deposition (GLAD) is a thin film deposition technique capable of fabricating columnar architectures such as posts, helices, and chevrons with control over nanoscale film features. Argon bombardment during deposition modifies the GLAD process, producing films with new morphologies which have shown promise for sensing and photonic devices. The authors report modification of column tilt angle, film density, and specific surface area for 12 different metal oxide and fluoride film materials deposited using Ar-assisted GLAD. For the vapor flux/ion beam geometry and materials studied here, with increasing argon flux, the column tilt increases, film density increases, and specific surface area decreases. With a better understanding of the nature of property modification and the mechanisms responsible, the Ar-assisted deposition process can be more effectively targeted towards specific applications, including birefringent thin films or photonic crystal square spirals.

36 MATERIALS SCIENCE↗

In situ study of erosion and deposition of amorphous hydrogenated carbon films by exposure to a hydrogen atom beam

This paper reports on the first dual-beam experiment employing a hydrogen atom beam for sample exposure and an ion beam for analysis, enabling in situ and real-time studies of hydrogen atom interaction with materials. The erosion of an amorphous hydrogenated carbon (a-C:H) layer by deuterium atoms at 580 K sample temperature was studied and the uptake of deuterium during the erosion process was measured in real time. The deuterium areal density increased at the beginning to 7.3 Multiplication-Sign 10{sup 15} D cm{sup -2}, but then stabilized at a constant value of 5.5 Multiplication-Sign 10{sup 15} D cm{sup -2}. Formation of a polymer-like deposit on an a-C:H layer held at room temperature and subjected to the deuterium atom beam was observed and also studied in situ. For both erosion and deposition studies an a-{sup 13}C:H layer on top of an Si substrate was used as a sample, making the experiments isotopically fully specified and thereby differentiating the deposited from the original layer and the interacting D atoms from H atoms present in the layer and in the residual vacuum. From the deposition study it was shown that carbon in the deposited layer originates from carbon-carrying species in the background vacuum that interact with hydrogen atoms. The areal density of the carbon at the surface was determined from the energy shift of the Si edge in the Rutherford backscattering spectrum. The cross section for {sup 7}Li on D at 4.3 MeV Li ion energy and at a recoil angle of 30 Degree-Sign was also determined to be (236 {+-} 16) Multiplication-Sign 10{sup -27} cm{sup 2}/sr. This is a factor of 3 {+-} 0.2 times higher than the Rutherford elastic cross section.

36 MATERIALS SCIENCE↗

Biaxial texture development in aluminum nitride layers during off-axis sputter deposition

Polycrystalline aluminum nitride (AlN) layers were deposited by pulsed-dc reactive magnetron sputtering from a variable deposition angle {alpha} = 0 Degree-Sign -84 Degree-Sign in 5 mTorr pure N{sub 2} at room temperature. X-ray diffraction pole figure analyses show that layers deposited from a normal angle ({alpha} = 0 Degree-Sign ) exhibit fiber texture, with a random in-plane grain orientation and the c-axis tilted by 42 Degree-Sign {+-} 2 Degree-Sign off the substrate normal, yielding wurtzite AlN grains with the {l_brace}1012{r_brace} plane approximately parallel ({+-}2 Degree-Sign ) to the substrate surface. However, as {alpha} is increased to 45 Degree-Sign , two preferred in-plane grain orientations emerge, with populations I and II having the c-axis tilted toward and away from the deposition flux, by 53 Degree-Sign {+-} 2 Degree-Sign and 47 Degree-Sign {+-} 1 Degree-Sign off the substrate normal, respectively. Increasing {alpha} further to 65 Degree-Sign and 84 Degree-Sign , results in the development of a single population II with a 43 Degree-Sign {+-} 1 Degree-Sign tilt. This developing biaxial texture is attributed to a competitive growth mode under conditions where the adatom mobility is sufficient to cause intergrain mass transport, but insufficient for the thermodynamically favored low energy {l_brace}0001{r_brace} planes to align parallel to the layer surface. Consequently, AlN nuclei are initially randomly oriented and form a kinetically determined crystal habit exposing {l_brace}0001{r_brace} and {l_brace}1120{r_brace} facets. The expected direction of its highest growth rate is 49 Degree-Sign {+-} 5 Degree-Sign tilted relative to the c-axis, in good agreement with the 42 Degree-Sign -53 Degree-Sign measured tilt. The in-plane preferred orientation for {alpha} > 0 Degree-Sign is well explained by the orientation dependence in the cross section of the asymmetric pyramidal nuclei to capture directional deposition flux. The observed tilt is ideal for shear mode electromechanical coupling, which is maximized at 48 Degree-Sign .

36 MATERIALS SCIENCE↗

Low temperature deposition of Ga{sub 2}O{sub 3} thin films using trimethylgallium and oxygen plasma

Gallium oxide (Ga{sub 2}O{sub 3}) thin films were deposited by plasma-enhanced atomic layer deposition (ALD) using trimethylgallium as the gallium precursor and oxygen plasma as the oxidant. A wide ALD temperature window was observed from 100 to 400 Degree-Sign C, where deposition rate was constant at {approx}0.53 A/cycle. X-ray photoelectron spectroscopy survey scans indicated the presence of gallium, oxygen, and carbon elements with concentrations of {approx}36, {approx}51.8, and {approx}12.2 at. %, respectively. As-deposited films were amorphous; upon annealing at 900 Degree-Sign C under N{sub 2} atmosphere for 30 min, polycrystalline {beta}-Ga{sub 2}O{sub 3} phase with a monoclinic crystal structure was obtained. Refractive index and root mean square roughness of the annealed Ga{sub 2}O{sub 3} film were higher than those of the as-deposited due to crystallization.

36 MATERIALS SCIENCE↗

Comparison between ZnO films grown by plasma-assisted atomic layer deposition using H{sub 2}O plasma and O{sub 2} plasma as oxidant

Zinc oxide (ZnO) thin films have attracted significant attention for application in thin film transistors (TFTs) due to their specific characteristics, such as high mobility and transparency. In this paper, the authors fabricated TFTs with ZnO thin films as channel layers deposited by plasma-assisted atomic layer deposition (PAALD) at 100 Degree-Sign C using two different plasma sources, water (H{sub 2}O-plasma) and oxygen gas (O{sub 2}-plasma), as oxidants, and investigated the effects of the plasma sources on TFT performances. The TFT with ZnO channel layer deposited with H{sub 2}O-plasma indicated higher performances such as a field effect mobility ({mu}) of 1.1 cm{sup 2}/Vs. Analysis of the ZnO films revealed that the residual carbon in the film deposited with H{sub 2}O-plasma was lower than that of O{sub 2}-plasma. In addition, the c-axis preferred orientation was obtained in the case of the ZnO film deposited with H{sub 2}O-plasma. These results suggest that it is possible to fabricate high-performance ZnO TFTs at low temperatures by PAALD with H{sub 2}O-plasma.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Nanoscale compositional analysis of NiTi shape memory alloy films deposited by DC magnetron sputtering

The formation of surface oxide layer as well as compositional changes along the thickness for NiTi shape memory alloy thin films deposited by direct current magnetron sputtering at substrate temperature of 300 °C in the as-deposited condition as well as in the postannealed (at 600 °C) condition have been thoroughly studied by using secondary ion mass spectroscopy, x-ray photoelectron spectroscopy, and scanning transmission electron microscopy-energy dispersive x-ray spectroscopy techniques. Formation of titanium oxide (predominantly titanium dioxide) layer was observed in both as-deposited and postannealed NiTi films, although the oxide layer was much thinner (8 nm) in as-deposited condition. The depletion of Ti and enrichment of Ni below the oxide layer in postannealed films also resulted in the formation of a graded microstructure consisting of titanium oxide, Ni{sub 3}Ti, and B2 NiTi. A uniform composition of B2 NiTi was obtained in the postannealed film only below a depth of 200–250 nm from the surface. Postannealed film also exhibited formation of a ternary silicide (Ni{sub x}Ti{sub y}Si) at the film–substrate interface, whereas no silicide was seen in the as-deposited film. The formation of silicide also caused a depletion of Ni in the film in a region ∼250–300 nm just above the film substrate interface.

36 MATERIALS SCIENCE↗

Vibration atomic layer deposition for conformal nanoparticle coating

A vibration atomic layer deposition reactor was developed for fabricating a conformal thin-film coating on nanosize particles. In this study, atomic layer deposition of 10–15-nm-thick Al{sub 2}O{sub 3} films was conducted on a high-surface-area acetylene black powder with particle diameters of 200–250 nm. Intense vibration during the deposition resulted in the effective separation of particles, overcoming the interparticle agglomeration force and enabling effective diffusion of the precursor into the powder chunk; this phenomenon led to the formation of a conformal film coating on the nanopowder particles. It was also confirmed that the atomic layer deposition Al{sub 2}O{sub 3} films initially grew on the high-surface-area acetylene black powder particles as discrete islands, presumably because chemisorption of the precursor and water occurred only on a few sites on the high-surface-area acetylene black powder surface. Relatively sluggish growth of the films during the initial atomic layer deposition cycles was identified from composition analysis.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Integration of molecular-layer-deposited aluminum alkoxide interlayers into inorganic nanolaminate barriers for encapsulation of organic electronics with improved stress resistance

Diffusion barrier stacks for the encapsulation of organic electronics made from inorganic nanolaminates of Al{sub 2}O{sub 3} and TiO{sub 2} with aluminum alkoxide interlayers have been deposited by atomic layer deposition (ALD) and molecular layer deposition (MLD). As a part of the MLD process development, the deposition of aluminum alkoxide with low a density of about 1.7 g/cm{sup 3} was verified. The ALD/MLD diffusion barrier stack is meant to be deposited either on a polymer film, creating a flexible barrier substrate, or on top of a device on glass, creating a thin-film encapsulation. In order to measure the water vapor transmission rate (WVTR) through the barrier, the device is replaced by a calcium layer acting as a water sensor in an electrical calcium test. For the barrier stack applied as thin-film encapsulation on glass substrates, high resolution scanning electron microscopy investigations indicate that the inorganic nanolaminates without MLD interlayers are brittle as they crack easily upon the stress induced by the corroding calcium below. The introduction of up to three MLD interlayers of 12 nm each into the 48 nm barrier film laminate successfully mitigates stress issues and prevents the barrier from cracking. Using the three MLD interlayer configurations on glass, WVTRs of as low as 10{sup −5} g/m{sup 2}/d are measured at 38 °C and 32% relative humidity. On polymer barrier substrates, the calcium is evaporated onto the barrier stack and encapsulated with a cavity glass. In this configuration, the corroding calcium has space for expansion and gas release without affecting the underlying barrier film. In consequence, a WVTR of about 3 × 10{sup −3} g/m{sup 2}/d is measured for all samples independently of the number of MLD interlayers. In conclusion, a stabilization and preservation of the ALD barrier film against mechanical stress is achieved by the introduction of MLD interlayers into the inorganic nanolaminate.

36 MATERIALS SCIENCE↗