Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ALLOY SYSTEMS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,099 records · Page 61

Internal friction sensitivity to precipitation in Al-12 wt% Mg alloy

Highlights: • Internal friction is sensible to semi coherent and non-coherent phases (β′ and β). • Internal friction is not enough sensible to coherent GP zones formation in Al-12 wt% Mg. • Appearance of two IF peaks is due to β′ and β phases formation and dissolution. - Abstract: In order to improve the understanding of the sensibility of the internal friction phenomena to different stages of precipitation in Al-Mg alloys, the ageing effect of a supersaturated solid solution on the Temperature Dependent Internal Friction (TDIF) spectra has been studied. The research showed that the dissolution of the β phase and the transfer of Mg atoms to a solid solution and the formation of β′ metastable phase have an effect on internal friction. Thus, it was proved that the precipitation or the dissolution of β phase plays an important role in the anelasticity of Al-Mg alloys. A detailed TDIF analysis revealed the sensibility of the internal friction technique to the formation of semi-coherent and non-coherent phases (β′ and β) but it is not sensitive enough to the formation of coherent phases (GP zones). Several observations on the nature and the shape of the precipitates are also discussed.

36 MATERIALS SCIENCE↗

Microstructure, mechanical properties and in vitro degradation behavior of novel Zn-Cu-Fe alloys

Highlights: • Zn-3Cu-xFe (x = 0, 0.5 and 1 wt%) alloys are proposed for the first time as candidate biodegradable materials. • The YS, UTS, and elongation of Zn-3Cu-0.5Fe alloy are 232 MPa, 284 MPa and 33%, respectively. • The in vitro degradation rate in SBF was successfully increased by about 52% by 1 wt% Fe addition for Zn-3Cu. - Abstract: Zn and Zn-based alloys as biodegradable material have drawn more and more attention in recent years due to their good mechanical properties, lower degradation rate than Mg and acceptable biocompatibility. However, too low degradation rate is a challenge for future application of Zn-based alloys. In this study, Zn-3Cu-xFe (x = 0, 0.5 and 1 wt%) alloys were proposed as candidate biodegradable materials. The microstructure, mechanical and in vitro biodegradable properties were investigated systematically. The Zn-3Cu alloy was composed of Zn matrix and CuZn{sub 5} phase, while the FeZn{sub 13} phase was newly formed with the addition of Fe. Due to the micro-galvanic effect produced by FeZn{sub 13} as a cathodic phase to the Zn matrix, in vitro degradation rate in simulated body fluid solution (SBF) was greatly increased by about 52.1%, from 45.3 ± 8.22 for Zn-3Cu alloy to 68.9 ± 7.34 μm/year for Zn-3Cu-1Fe alloy. Although the mechanical properties were decreased slightly due to the introduction of hard and brittle FeZn{sub 13} secondary phase to the Zn matrix, Zn-3Cu-0.5Fe alloy still exhibits good combined mechanical properties and the YS, UTS and elongation are 232 MPa, 284 MPa and 33%, respectively. Taken together, the mechanical properties and in vitro degradation behavior of the Zn-3Cu-xFe alloys are more suitable than Zn-3Cu alloy as candidate biodegradable materials.

36 MATERIALS SCIENCE↗

Influence of alloying element Zn on the microstructural, mechanical and corrosion properties of binary Mg-Zn alloys after severe plastic deformation

Highlights: • Mg-Zn alloys are processed by equal channel angular pressing with back-pressure. • The α-Mg matrix consists of highly deformed and partially recrystallized areas. • Zn concentration varies in the α-Mg matrix by up to 2 at.%. • The alloys exhibit mechanical anisotropy and a significant increase in strength. • Equal channel angular pressing increases corrosion rate of Mg-Zn alloys. - Abstract: This work presents an analysis of the microstructural, mechanical and corrosion properties of two binary Mg-Zn alloys. Mg-6 wt%Zn and Mg-12 wt%Zn cast alloys were subjected to annealing followed by quenching and processed via equal channel angular pressing with applied back-pressure (ECAP-BP). After ECAP-BP, both alloys were thoroughly examined and showed partially recrystallized and highly deformed areas. High-angle annular dark-field imaging revealed a difference in Zn content across the α-Mg matrix of the Mg-12 wt%Zn after ECAP-BP due to the growth of MgZn{sub 2} nanoparticles. Electron energy-loss spectroscopy (EELS) was carried out to qualify an average Zn content in these areas, and a variation in Zn content up to 2 at.% was found. Compression tests revealed mechanical anisotropy and a significant increase in the strength of both alloys after ECAP-BP. The yield strength, σ{sub 02}, was in the range from 269 to 385 MPa depending on the composition and compression axis. The initial state alloys showed yield strengths, σ{sub 02}, of only 75–150 MPa but improved ductility. The corrosion rates of the Mg-Zn alloys in the initial state, evaluated using a hydrogen evolution method in NaCl solution, were higher for Mg-12 wt%Zn. The corrosion rates of both alloys after ECAP-BP were higher than those of the initial state. Light microscopy observations did not reveal any preference for corrosion propagation, including transcrystalline, intercrystalline or interphase corrosion, in any of the materials.

36 MATERIALS SCIENCE↗

Microstructures and deformation mechanisms of Cr26Mn20Fe20Co20Ni14 alloys

Highlights: • The single-phase FCC alloy as the annealing temperature exceeding 1015 °C • The dual-phase structure as the annealing temperature lower than 1000 °C • The σ phases grow primarily at grain boundaries. • The single-phase alloy deforms via dislocations and twins. • In-situ tensile experiment reveals twinning at the crack tip. - Abstract: We investigated microstructures and tension properties of Cr{sub 26}Mn{sub 20}Fe{sub 20}Co{sub 20}Ni{sub 14} alloys that were produced by arc-melting and subsequent thermal-mechanical processing—hot-rolling → cold-rolling → annealing at different temperatures ranging from 500 °C to 1100 °C for 1 h → air cooling. Microstructure characterization shows the single-phase solid solution with face centered cubic structure as the annealing temperature exceeding 1015 °C while the dual-phase structure (Cr-rich σ phase and FCC solid solution) as the annealing temperature lower than 1000 °C. The σ phases grow primarily at grain boundaries and act as precipitation strengthening units to enhance strain hardening rate. The single-phase solid solution deforms plastically via dislocations and twins. Twin boundaries associated with deformation twinning impede dislocation motion, enhancing the strain hardening capacity. In-situ tensile experiment in transmission electron microscope further reveals that twinning occurs at the crack tip and facilitates the deflection of crack propagation towards twinning shear direction. This work implies that a strength-ductility combination can be realized by coupling precipitation strengthening and twinning-induced plasticity in multiple principle elements alloys.

36 MATERIALS SCIENCE↗

Effects of cold predeformation on dissolution of second-phase Al2Cu particles during solution treatment of 2219 Al-Cu alloy forgings

Highlights: • Cold predeformation (CPD) was performed on 2219 Al-Cu alloy forgings. • CPD promoted the dissolution of coarse Al{sub 2}Cu particles during solution treatment. • CPD increased the driving force to precipitate θ′ phases during aging treatment. • Increasing CPD improved the tensile properties of the forgings. - Abstract: Cold predeformation (CPD, before solution treatment) at different pre-compressing deformations of 0, 5, and 10% was performed on 2219 Al-Cu alloy forgings, and its effect on the dissolution of second-phase Al{sub 2}Cu particles during solution treatment was investigated. The results indicated that a higher number of coarse Al{sub 2}Cu particles dissolved in the Al matrix during solution treatment in samples processed with CPD. Upon increasing CPD from 0 to 10%, the area fraction of the coarse particles decreased from 2.57 to 0.57%, while their mean size decreased from 12.5 to 8.7 μm. The corresponding driving force for precipitation during the subsequent aging treatment process increased, the main precipitates in the material transitioned from the θ″ phase to the θ′ phase, and the area fraction of the precipitates increased from 6.1 to 18.1%. As a result, a significant increase in ultimate tensile strength (by 61.2 MPa), yield strength (by 63.2 MPa), and tensile elongation (by 2.2%) was obtained.

36 MATERIALS SCIENCE↗

Evolution of Σ3n CSL boundaries in Ni-Cr-Mo alloy during aging treatment

Highlights: • Σ3{sup n} boundary distribution characteristics are changed during aging treatment at 600 °C. • The increase in fractions of Σ9 and Σ27 boundaries depends on interaction between Σ3{sup n} boundaries. • The consumption of Σ3{sub c} boundaries is modeled with migration of random HABs. • Generation mechanism of Σ3{sub ic} boundaries differs from traditional models. - Abstract: The evolution of Σ3{sup n} (n = 1,2,3) boundaries in a Ni-Cr-Mo alloy during an aging treatment at 600 °C was investigated based on electron backscatter diffraction (EBSD) measurements. Incoherent Σ3 (Σ3{sub ic}) and coherent Σ3 (Σ3{sub c}) boundaries were identified using the single-section trace analysis method. The results show that the Σ3{sup n} boundary distribution characteristics are changed and that a Pt{sub 2}Mo-type Ni{sub 2}(Cr,Mo) superlattice phase precipitates during the aging treatment. Through the analysis and comparison of the average grain diameters measured under the different conditions, the migration behaviors of both the Σ3{sub ic} boundaries and random high-angle boundaries (HABs) are found. The migration of the Σ3{sub ic} boundaries provides the probability of interaction between Σ3{sup n} boundaries. This interaction is responsible for some different types of triple junctions, the increase in Σ9 and Σ27 boundary fractions and interrupted connectivity of the network of random HABs. However, the Σ3{sub c} boundaries' consumption caused by the migration of random HABs and the difficulty of forming new Σ3{sub c} boundaries lead to the decreased fraction of Σ3{sub c} boundaries. The further discussion about the increase in the fraction of Σ3{sub ic} boundaries indicates that the generation mechanism of the Σ3{sub ic} boundaries during the aging treatment differs from the models applied to recrystallization and subsequent grain growth processes.

36 MATERIALS SCIENCE↗

Microstructural characterization and mechanical properties of a novel TiC-based cermet bonded with Ni3(Al,Ti) and NiAl duplexalloy

A novel TiC/Ni{sub 3}(Al,Ti)-NiAl composite has been designed and synthesized by in-situ reactive hot-pressing a mixture of Ti{sub 3}AlC{sub 2} and Ni powders. After hot-press sintering at 1500 °C and 30 MPa, almost fully dense composite was obtained and the in-situ formed TiC grains were well-bonded with Ni{sub 3}(Al,Ti) and NiAl alloys. Due to the nanolaminated structure in Ti{sub 3}AlC{sub 2} materials that weakly bonded Al layers are more prone to be out-diffused from Ti{sub 3}AlC{sub 2} lattice than that of Ti atoms. The deintercalated AlTi atoms would react with Ni to give rise to the formation of Ni{sub 3}(Al,Ti) and NiAl alloys, and meanwhile a crystal lattice structure transformation happened from hexagonal Ti{sub 3}AlC{sub 2} to cubic lattice TiC. The formation of phases, grains morphologies, sintering behavior and mechanical properties were associated with sintering temperature. The as prepared TiC/Ni{sub 3}(Al,Ti)-NiAl composite under 1500 °C exhibited superior mechanical properties comparing with the counterparts fabricated under 1350 °C and 1400 °C because of the enhanced microstructures and eliminations of pores. Hardness, flexural strength and fracture toughness of the TiC/Ni{sub 3}(Al,Ti)-NiAl composite at room temperature were determined as 9.9 ± 0.35 GPa, 665 ± 26 MPa and 10.23 ± 0.4 MPa·m{sup 1/2}, respectively. Interestingly, the flexural strength and fracture toughness increases with temperature rising from 600 to 800 °C, the maximum of flexural strength and fracture toughness could reach 775 ± 25 MPa and 11.6 ± 0.4 MPa·m{sup 1/2} at 800 °C.

36 MATERIALS SCIENCE↗

Elaborating the phases and mechanical properties of multiphase alloy: Experimental two-dimensional mapping combined with theoretical calculations

Highlights: • Mechanical modulus and hardness distribution mapping is obtained for the first time by NanoBlitz 3D. • Phases mapping and exact element ratio are characterized for the nano multielement carbides by EPMA. • Carbides types are confirmed by acid etching and XRD refinement. • Young's modulus of multiple carbides is verified by DFT calculations and Voigt-Reuss-Hill model. - Abstract: The relationship between types of phases, microstructure and mechanical properties is always a critical challenge for the research and application of multiphase alloys. We report for the first time that NanoBlitz 3D method implemented in iNano is used to investigate the distribution of micro mechanical modulus and hardness for the entire complex multiphase alloy Fe-6.0W-5.0Mo-4.0Cr-2.0V-0.83C by constructing the two-dimensional mapping. In order to build the correlation between the microstructure and properties, the carbides in this tempering state steel are confirmed to be Fe{sub 3}(W, Mo){sub 3}C, Cr{sub 15.58}Fe{sub 7.42}C{sub 6} and V{sub 8}C{sub 7} by acid etching and XRD refinement. The phases mapping is obtained by electron probe micro-analysis. Exact element ratio is characterized for the nano-scale multielement carbides precipitates. The Young's modulus and hardness of the precipitated carbides are up to 330 GPa and 22 GPa, respectively. The distribution range of Young's modulus and hardness is during 150 to 250 GPa and 2.5 to 7.0 GPa for the matrix phases, respectively. The experimental Young's modulus and hardness results are verified by first-principles calculations combined with Voigt-Reuss-Hill approximation. In fact, this work provides a successful demonstration to three-dimensionally characterize the micro mechanical properties for all the ceramics and alloys.

36 MATERIALS SCIENCE↗

The compressive deformation mechanisms of a coarse-grained AgInCd alloy

Highlights: • The compressive deformation mechanisms of a coarse-grained AgInCd alloy are investigated. • The deformation mechanisms are full dislocation slip and multiplication when strain is small. • Dominant deformation mechanisms convert into deformation twinning when strain reaches 50%. • Dislocation densities and twin thicknesses reduce in twinned grains with strain increasing. - Abstract: The compressive deformation mechanisms of a coarse-grained AgInCd alloy have been investigated in the present study. When compressive strain is not higher than 30%, the deformation mechanisms transform from full dislocation slip and multiplication into the two coefficient mechanisms of full dislocation slip and partial dislocation emission with increasing compressive strain. When compressive strain reaches 50%, the dominant deformation mechanisms convert into deformation twinning. With further increasing strain, the dislocation densities decrease and the twin thicknesses reduce in the nano-twinned grains. Twin boundary possesses a weaker strengthening effect comparing with grain boundary for the AgInCd alloys.

36 MATERIALS SCIENCE↗

Dynamic microstructural evolution of an Al–Zn–Mg–Cu alloy (7075) during continuous heating and the influence on the viscoelastic response

Highlights: • A TEM/HRTEM, FIB-SEM and APT analysis of an Al–Zn–Mg–(Cu) alloy is performed. • Microstructural evolution is analyzed during constant heating rate heat-treatment. • Composition, size, number density and vol. fraction of present phases are reported. • Vol. fraction and kinetic data from rate equations in the literature are validated. • Viscoelastic behavior of the alloy is associated to microstructural transformations. - Abstract: The microstructural evolution of an Al–Zn–Mg–Cu alloy under continuous heating over the temperature range of 298 to 648 K (25 to 375 °C) is characterized by focused ion beam-scanning electron microscopy, transmission electron microscopy, and atom probe tomography. The chemical composition, dimensions, number density, and volume fraction of precipitates are measured comprehensively. Quantitative measurements of Guinier-Preston zones volume fraction and η′/η phase volume fraction are correlated to the viscoelastic response of the Al–Zn–Mg–Cu alloy with temperature in the studied range. This provides valuable evidence indicating that observed variations in the viscoelastic behavior of the Al–Zn–Mg–Cu alloy may be associated with phase transformations involving Guinier-Preston zones and phases η′ and η.

36 MATERIALS SCIENCE↗

Enhanced strength and electrical conductivity of ultrafine-grained Al-Mg-Si alloy processed by hydrostatic extrusion

Highlights: • Al-Mg-Si alloy was subjected to hydrostatic extrusion combined with aging treatment. • UFG Al-Mg-Si alloy with UTS of 332 MPa and conductivity of 58% IACS was obtained. • Precipitation process depended on applied strains and crystallographic texture. • Strengthening effect was achieved by UFG structure and needle-like β″ precipitates. • Precipitation of β″ and spherical β′/β particles at GB provided high conductivity. - Abstract: The effect of hydrostatic extrusion combined with an artificial aging on microstructure, mechanical and electrical properties of 6101 Al-Mg-Si alloy was investigated. It has been shown that such thermo-mechanical treatment is an effective method for producing of long wires with an ultrafine-grained microstructure (grain size of 300–400 nm) and enhanced ultimate tensile strength (> 330 MPa) and electrical conductivity (up to 58% IACS). The mechanical behavior of 6101 Al-Mg-Si alloy depended strongly on applied strains by hydrostatic extrusion and crystallographic texture. Higher accumulative strain accelerated the precipitation kinetics but decreased the age hardening response. The double fiber <100> and <111> texture was observed for hydrostatically extruded samples. The <001> grains with homogenously distributed needle-like β″ precipitates provided precipitation strengthening of material while <111> grains resulted in more efficient grain boundary strengthening. Quantitative microstructure characterization allowed adjusting physical model to estimate the electrical conductivity and compare it with experimental data. The high conductivity was provided mainly by decomposition of solid solution due to precipitation of needle-like β″ precipitates in the grain interior and spherical β′ or β particles located at grain boundaries.

36 MATERIALS SCIENCE↗

The partial substitution of Y with Gd on microstructures and mechanical properties of as-cast and as-extruded Mg-10Zn-6Y-0.5Zr alloy

Highlights: • The as-extruded Mg-10Zn-6Y-0.5Zr and Mg-10Zn-3Y-3Gd-0.5Zr alloys show bimodal microstructure and DRXed microstructure. • In addition to W phase, Icosahedral quasicrystal phase layer is observed at the surface of some W phase particles in as-extruded Mg-10Zn-3Y-3Gd-0.5Zr (wt. %) alloy. • The as-extruded Mg-10Zn-6Y-0.5Zr (wt. %) alloy exhibits TYS of 341 MPa, UTS of 368 MPa and elongation to failure of 6.8%. While the as-extruded Mg-10Zn-3Y-3Gd-0.5Zr (wt. %) alloy shows lower TYS of 247 MPa, UTS of 330 MPa and higher elongation to failure of 19.8%. - Abstract: Mg-10Zn-6Y-0.5Zr (wt%) alloy and Mg-10Zn-3Y-3Gd-0.5Zr (wt%) alloy with medium RE content have been fabricated by conventional casting and indirect extrusion. The as-extruded Mg-10Zn-6Y-0.5Zr (wt%) alloy shows a bimodal microstructure containing dynamic recrystallized (DRXed) grains with average grain size of 2 μm and deformed regions. In addition to the fragmented W phase particle bands distributing along the extrusion direction, large amount of nano W phase and small amount of nano β{sub 2}′ phase are precipitated in the matrix. While the as-extruded Mg-10Zn-3Y-3Gd-0.5Zr (wt%) alloy exhibits completely dynamic recrystallized microstructure with average grain size of 3 μm. The broken W phase particles are distributed homogeneously in the matrix. Icosahedral quasicrystal phase layer is observed at the surface of some W phase particles in the as-extruded Mg-10Zn-3Y-3Gd-0.5Zr alloy. The as-extruded Mg-10Zn-6Y-0.5Zr (wt%) alloy exhibits yield strength of 341 MPa, ultimate tensile strength of 368 MPa and elongation to failure of 6.8%. While the as-extruded Mg-10Zn-3Y-3Gd-0.5Zr (wt%) alloy shows lower yield strength of 247 MPa, ultimate tensile strength of 330 MPa and higher elongation to failure of 19.8%. The higher strength in the as-extruded Mg-10Zn-6Y-0.5Zr (wt%) alloy is mainly attributed to higher area fraction of unDRXed regions with strong texture and the precipitation of nano W and β{sub 2}′ phase. The fully recrystallized microstructure with weak texture and the formation of icosahedral quasicrystal phases with good coherent bond with α-Mg contribute to the good ductility of the as-extruded Mg-10Zn-3Y-3Gd-0.5Zr alloy.

36 MATERIALS SCIENCE↗

Pulse current auxiliary forging of sintered TiAl alloys based on the investigation of dynamic recrystallization and phase transformation

Highlights: • DRX kinetics model of sintered near γ TiAl alloy was established. • DRX process was accompanied by twinning when compressed at 1125 °C/0.1 s{sup − 1}. • Hot deformation has a promotion to the phase transformation of γ → α. - Abstract: Pulse current auxiliary forging is a new and efficient way to fabricate high performance TiAl based alloys. Dynamic recrystallization (DRX) and phase transformation have a pronounced effect on the subsequent deformability of TiAl based alloys. Hence, the dynamic recrystallization kinetics were determined at the temperature range of 1125–1275 °C and strain rate range of 0.1–0.001 s{sup − 1}. In addition, the DRX mechanism and phase transformation of TiAl based alloys were investigated to model the microstructure evolution in order to provide guidance for the pulse current auxiliary forging process. When the specimens were compressed at 1125 °C/0.1 s{sup − 1}, twinning played an important role in the DRX process. With increasing deformation temperature, the microstructure transformed from near gamma into duplex microstructure. In addition, according to the kinetics of dynamic recrystallization and phase transformation, fully DRXed TiAl based alloys were fabricated through pulse current auxiliary forging. The as-forged TiAl-based alloys show good superplastic performance with an elongation over 410%.

36 MATERIALS SCIENCE↗

Effect of microstructure on exfoliation corrosion resistance in an Al-Zn-Mg alloy

Highlights: • A quantitative method was proposed to characterize EXCO resistance. • The EXCO product lead to strain in ND and elongation in RD on nearby grains. • Recrystallized grains are more susceptible to EXCO than fibrous grains. • High fraction of high-angle grain boundaries reduces EXCO resistance. • High coverage ratio of η phases on high-angle grain boundaries reduces EXCO resistance. - Abstract: In this work, the effect of microstructure on exfoliation corrosion (EXCO) resistance in an Al-Zn-Mg alloy were investigated using standard EXCO test, together with detailed microstructural examinations mainly by scanning electron microscopy (SEM) and high-angle annular detector dark-field scanning transmission electron microscopy (HAADF-STEM). An EXCO product model was built based on morphologies of EXCO product on longitudinal section and cross section for further measurement and analysis. A quantitative characterization of EXCO resistance by measuring average thickness of EXCO product was conducted, showing average results of 6.94 μm, 10.21 μm and 18.14 μm, which are corresponding to EXCO ratings of P, EA and EB under ASTM G34 standard, respectively. It was concluded that recrystallization, high fraction of high-angle grain boundaries (HAGBs) and high coverage ratio of η phases on HAGBs reduced EXCO resistance.

36 MATERIALS SCIENCE↗

Determination of the volume fraction of precipitates in a nitrided Fe-0.354 wt% C-2.93 wt% Cr model alloy by anomalous small angle X-ray scattering

Highlights: • Anomalous small-angle X-ray scattering (ASAXS) is used to study nitriding of Fe-Cr-C steels. • ASAXS gives access to chemical information of nanoscaled nitrides. • The volume fraction of nitrides is determined along the diffusion layer. - Abstract: Anomalous small angle scattering (ASAXS) is a powerful non-destructive technique that can provide characteristic features of nanoscale precipitates such as the volume fraction, and chemical composition. In this paper, the technique is used for the first time to explore nanoscale MN nitrides (M = Cr,Fe) after nitriding of a model iron alloy (Fe-0.354 wt% C-2.93 wt% Cr).

36 MATERIALS SCIENCE↗

TEM investigations on lath martensite substructure in quenched Fe-0.2C alloys

Highlights: • Twin can be lath martensite substructure in low-carbon steels. • Detwinning behavior occurs in an auto-tempering process during quenching. • Detwinning may result in the formation of twinned laths. • Detwinning may result in the laths with dislocation-like contrast as substructure. - Abstract: Lath martensite in low-carbon steels is the main microstructural feature in the quenched state, and dislocations have been generally recognized as the substructure of lath martensite. However, the effects of quenching conditions on the quenched substructure have not yet been fully understood. In the present work, a Fe-0.2C (wt%) alloy was selected for detailed investigations on the microstructural evolution at various austenitizing temperatures. Microstructural characterization was carried out by using a conventional transmission electron microscope (TEM). The substructure of lath martensite was found to vary with austenitizing temperature. In the 1200 °C-water-quenched (WQ) samples, twinned laths (two specific variants having a {112}<111>-type twin relationship) and a twinned region (laths with the twin structure as their substructure) can be observed. Almost all lath martensite with a high density of fine twins as its substructure can be obtained in the 1300 °C-WQ samples. The twins gradually disappear or detwinning-occurs during TEM observations carried out with in situ heating. A further increase in temperature results in the formation of twinned laths and then lath with dislocation-like contrasts or lines appears as the substructure. These results suggested that a completely twin structure can be the initial substructure of lath martensite, and lath with dislocation-like contrasts or lines as its substructure is most likely the auto-tempering result of twinning.

36 MATERIALS SCIENCE↗

Selective laser melting of Co-29Cr-6Mo alloy with laser power 180–360 W: Cellular growth, intercellular spacing and the related thermal condition

Highlights: • Increasing laser power increases the track size but not the track shape significantly. • Solidification mode and texture are similar over the range of laser power used. • Intercellular spacing is not affected by laser power but decreases slightly with growth angle. • Thermal gradient and cooling rate have been estimated to be ~ 2 × 10{sup 7} K/m and ~ 2 × 10{sup 6} K/s, respectively. - Abstract: A feature of solidification during selective laser melting (SLM) is cellular growth. Thus, how growth direction and cell size may be affected and possibly be controlled by SLM parameters are important to be understood. Furthermore, intercellular spacing (λ{sub 1}) is suggestive of the thermal condition during solidification which needs to be known for advancing the understanding of SLM. In this work, grain solidification orientation and λ{sub 1} of a Co-Cr-Mo alloy produced by SLM over a range of laser power (P = 180–360 W) with other parameters kept unchanged have been evaluated. It has been found that the overall preferred growth of cellular solidification is not significantly affected by P. This is because, over the range of P values used, the shape of track did not change sufficiently to result in a significant variation of growth direction during epitaxial growth. It has also been found that P does not affect λ{sub 1}. This suggests, since growth rate (R) relates to scan speed (v) which is unchanged, P does not significantly affect the temperature gradient of the solidification front (G). From the measured λ{sub 1} and estimated R, G and thus cooling rate ( T-dot ) can be estimated following the commonly used primary arm spacing model. The estimated G and T-dot which could not be directly measured will be compared with those predicted by simulation and the estimated T-dot will also be compared with those determined by using an emperical relationship from literature.

36 MATERIALS SCIENCE↗

A novel interface strengthening layer: Nanoscale AuCu super-structure formed during Au80Sn20/Cu rapid solidification soldering process

Highlights: • The nanoscale AuCu super-structure formed in Au80Sn20/Cu soldering joint. • The phase-transformation diffusion mechanism of Au80Sn20/Cu soldering process was studied. • The orientation relationship of Au80Sn20/Cu intermetallic compounds was investigated. • The interfacial strengthening mechanism of nanoscale AuCu layer was discussed. - Abstract: Phase composition and orientation of intermetallic compounds layers determine the functional and mechanical properties of solder joints. In this paper, interfacial reaction and strengthening mechanism of Au80Sn20/Cu joint by rapid solidification reflow soldering were studied. The Au80Sn20/Cu solder joint by rapid solidification reflow soldering exhibit a superior shear property, and the shear strength reaches up to 90 MPa. It is found that a new nanoscale AuCu super-structure formed in the interfacial intermetallic compounds layer, which is coherent with the [001] Cu substrate. The orientation relationship of Cu matrix/interfacial intermetallic compounds is determined to be [001]{sub Cu}∥[001]{sub AuCu}∥[ 2-bar 4 2-bar 3]{sub (AuCu){sub 5Sn}} and (200){sub Cu}∥(200){sub AuCu}∥(10 1-bar 0){sub (AuCu){sub 5Sn}}. Nanoscale AuCu super-structure influences the interface slip direction and provides interface misfit dislocation, hinder the dislocation movement, lead to the interface strengthening effect. Our finding on nanoscale AuCu super-structure formed during Au80Sn20/Cu soldering process not only sheds light on future research direction but also provides practical guidance to the engineers in solder industry.

77 NANOSCIENCE AND NANOTECHNOLOGY↗