Properties of RBSN and RBSN-SiC composites

Strengths, fracture toughnesses, hardnesses, and dimensional changes have been measured for RBSN and RBSN/SiC composites. Samples were made from mixtures of Si and either Si- or C-rich SiC powders. For pure, 75 pct dense RBSN dispersed with octanol, strengths up to 858 MPa have been achieved. Improved strengths result from a combination of microstructural perfection and increased fracture toughness. The mechanical properties of the composites were approximately equal to those of methanol processed RBSN but not quite equal to those of the octanol-processed RBSN. Results are discussed in terms of observed microstructural features.

Lightfoot, A.↗

Heat treatment study 2

The microstructural variations in nickel based superalloys that result from modifications in processing were examined. These superalloys include MAR-M246(HF) and PWA1480. Alternate heat treatments for equiaxed as-cast specimens were studied and a sample matrix of 42 variations in the heat treatments were processed, as well as different directional solidification parameters. Variation in temperature and times for both solution and aging were performed. Photomicrographs were made of the microstructure and volume fraction analysis of primary gamma-prime and aged gamma-prime precipitates were performed. The results of the heat treatment, cooling rate, and directional solidification experiments are discussed.

Workman, Gary L.↗

Nonequilibrium Phase Chemistry in High Temperature Structure Alloys

Titanium and nickel aluminides of nonequilibrium microstructures and in thin gauge thickness were identified, characterized and produced for potential high temperature applications. A high rate sputter deposition technique for rapid surveillance of the microstructures and nonequilibrium phase is demonstrated. Alloys with specific compositions were synthesized with extended solid solutions, stable dispersoids, and specific phase boundaries associated with different heat treatments. Phase stability and mechanical behavior of these nonequilibrium alloys were investigated and compared.

Wang, R.↗

The influence of advanced processing on PWA 1480

High thermal gradient casting of PWA 1480 was evaluated as an avenue for reducing the size of casting porosity. Hot isostatic pressing (HIP) was also employed for the elimination of casting pores. An alternate to the standard PWA 1480 coating plus diffusion bonding aging heat treatment cycle was also evaluated for potential improvements in the properties of interest to the Space Shuttle Main Engine (SSME) application. Microstructural changes associated with the high thermal gradient casting process were quantified by measurement of the size and density of the casting porosity, the amount of retained casting eutectic, and dendrite arm spacings. The results of the advanced processing have shown an improvement in material microstructure due to high thermal gradient casting. Improved homogeneity of PWA 1480 is advantageous in providing an improved solution heat treatment window and, potentially, easier HIP. High thermal gradient casting improves fatigue life by reducing casting pore size. The alternate heat treatment improves the balance of strength and ductility which appears to improve low cycle fatigue life, but with a reduction in short time stress rupture life. Based upon these tests, hot isostatic pressing appears to afford further improvements in cyclic life, though additional evaluation is suggested. Development of the alternate heat treatment is not recommended due to the reduced stress rupture capability and the need to develop a new properties data base. High thermal gradient casting and HIP are recommended for application to single crystal castings.

Fritzemeier, L. G.↗

Natural aging and reversion behavior of Al-Cu-Li-Ag-Mg alloy Weldalite (tm) 049

This study was initiated to understand the natural aging and reversion behavior of Weldalite (trademark) 049 in tempers without cold work. Of particular interest are: (1) the microstructural basis for the high strength in the T4 condition; (2) an explanation of the reversion phenomenon; and (3) the effect of re-aging at room temperature after a reversion treatment. Mechanical properties were measured and transmission electron microscopy (TEM) analysis performed at various stages of microstructural development during aging, reversion, and subsequent re-aging.

Gayle, Frank W.↗

Effect of a prior stretch on the aging response of an Al-Cu-Li-Ag-Mg-Zr alloy

Recently, a family of Al-Cu-Li alloys containing minor amounts of Ag, Mg, and Zr and having desirable combinations of strength and toughness were developed. The Weldalite (trademark) alloys exhibit a unique characteristic in that with or without a prior stretch, they obtain significant strength-ductility combinations upon natural and artificial aging. The ultra-high strength (approximately 690 MPa yield strength) in the peak-aged tempers (T6 and T8) were primarily attributed to the extremely fine T(sub 1) (Al2CuLi) or T(sub 1)-type precipitates that occur in these alloys during artificial aging, whereas the significant natural aging response observed is attributed to strengthening from delta prime (Al3Li) and GP zones. In recent work, the aging behavior of an Al-Cu-Li-Ag-Mg alloy without a prior stretch was followed microstructurally from the T4 to the T6 condition. Commercial extrusions, rolled plates, and sheets of Al-Cu-Li alloys are typically subjected to a stretching operation before artificial aging to straighten the extrusions and, more importantly, introduce dislocations to simulate precipitation of strengthening phases such as T(sub 1) by providing relatively low-energy nucleation sites. The goals of this study are to examine the microstructure that evolves during aging of an alloy that was stretch after solution treatment and to compare the observations with those for the unstretched alloy.

Kumar, K. S.↗

Sliding wear of self-mated Al2O3-SiC whisker reinforced composites at 23-1200 C

Microstructural changes occurring during sliding wear of self-mated Al2O3-SiC whisker reinforced composites were studied using optical, scanning electron microscopy, and transmission electron microscopy. Pin-on-disk specimens were slid in air at 2.7 m/sec sliding velocity under a 26.5 N load for 1 hr. Wear tests were conducted at 23, 600, 800, and 1200 C. Mild wear with a wear factor of 2.4 times 10(exp -7) to 1.5 times 10(exp -6) cu mm/Nm was experienced at all test temperatures. The composite shows evidence of wear by fatigue mechanisms at 800 C and below. Tribochemical reaction (SiC oxidation and reaction of SiO2 and Al2O3) leads to intergranular failure at 1200 C. Distinct microstructural differences existing at each test temperature are reported.

Farmer, Serene C.↗

Creep and fracture of dispersion-strengthened materials

The creep and fracture of dispersion strengthened materials is reviewed. A compilation of creep data on several alloys showed that the reported values of the stress exponent for creep varied between 3.5 and 100. The activation energy for creep exceeded that for lattice self diffusion in the matrix in the case of some materials and a threshold stress behavior was generally reported in these instances. The threshold stress is shown to be dependent on the interparticle spacing and it is significantly affected by the initial microstructure. The effect of particle size and the nature of the dispersoid on the threshold stress is not well understood at the present time. In general, most studies indicate that the microstructure after creep is similar to that before testing and very few dislocations are usually observed. It is shown that the stress acting on a dispersoid due to a rapidly moving dislocation can exceed the particle yield strength of the G sub p/1000, where G sub p is the shear modulus of the dispersoid. The case when the particle deforms is examined and it is suggested that the dislocation creep threshold stress of the alloy is equal to the yield strength of the dispersoid under these conditions. These results indicate that the possibility that the dispersoid creep threshold stress is determined by either the particle yield strength or the stress required to detach a dislocation from the dispersoid matrix interface. The conditions under which the threshold stress is influenced by one or the other mechanism are discussed and it is shown that the particle yield strength is important until the extent of dislocation core relaxation at the dispersoid matrix interface exceeds about 25 pct. depending on the nature of the particle matrix combination. Finally, the effect of grain boundaries and grain morphology on the creep and fracture behavior of dispersoid strengthened alloys is examined.

Raj, Sai V.↗

Measurements and mechanisms of localized aqueous corrosion in aluminum-lithium-copper alloys

Summary information is included for electrochemical aspects of stress corrosion cracking in alloy 2090 and an introduction to the work to be initiated on the new X2095 (Weldalite) alloy system. Stress corrosion cracking (SCC) was studied in both S-T and L-T orientations in alloy 2090. A constant load TTF test was performed in several environments with a potentiostatically applied potential. In the same environments the electrochemical behavior of phases found along subgrain boundaries was assessed. It was found that rapid failure due to SCC occurred when the following criteria was met: E(sub BR,T1) is less than E(sub applied) is less than E(sub Br, matrix phase). Although the L-T orientation is usually considered more resistant to SCC, failures in this orientation occurred when the stated criteria was met. This may be due to the relatively isotropic geometry of the subgrains which measure approximately 12 to 25 microns in diameters. Initial studies of alloy X2095 includes electrochemical characterization of three compositional variations each at three temperatures. The role of T(sub 1) dissolution in SCC behavior is addressed using techniques similar to those used in the research of 2090 described. SCC susceptibility is also studied using alternate immersion facilities at Reynolds Metals Corporation. Pitting is investigated in terms of stability, role of precipitate phases and constituent particles, and as initiation sites for SCC. In all research endeavors, attempts are made to link electrochemistry to microstructure. Previous work on 2090 provides a convenient basis for comparison since both alloys contain T(sub 1) precipitates but with different distributions. In 2090 T(sub 1) forms preferentially on subgrain boundaries whereas in X2095 the microstructure appears to be more homogeneous with finer T(sub 1) particles. Another point for comparison is the delta prime strengthening phase found in 2090 but absent in X2095.

Wall, Douglas↗

A study of fracture mechanisms in ATD roller bearing

The purpose was to investigate how microstructures, especially anisotropy, affects internal stresses and the overall mechanical response of bearings. Samples with the stress axis along the aligned carbide direction possessed high modulus values compared to those with their axis perpendicular to the carbide stringers. The difference in the modulus was found to be more than a factor of two. A series of experiments was conducted on rolled samples to further investigate this effect; the two sets of results were consistent with each other. The degree of anisotropy of the microstructure in terms of the carbide and matrix orientations was determined using x-ray diffraction. The stress state determination was conducted using neutron diffraction. It was found that there was little variation in the distribution of the internal stresses amongst different samples, indicating that small changes in the processing and geometrical conditions did not result in significant variations in the internal stress. A nominal tensile hoop stress of 39 ksi was obtained for the inner raceway. Furthermore, during the course of the investigation, it was apparent that there was a need to determine the stress state induced by the shrink fitting process. Therefore, a series of experiments was conducted using strain gages to identify the stress distribution in a shrink fitting process in three different types of geometries. Correlations were obtained to estimate the highest stress values in the outer and inner groove geometry. A finite element program based on the ANSYS system was developed to compute the stress distribution in the inner raceway geometry. This analysis indicates that the highest tensile stress in the system occurs at the ID of the ring with a stress value of over 5 times that of the applied radial stress. Results from all these facets were correlated with one another. It appears that the material does not fail as a result of any one single factor, but results from a combination of the various factors investigated.

Zee, Ralph H.↗

Physical and chemical analysis of a Ni/H2 cell

A cycled aerospace nickel hydrogen (Ni/H2) cell was subjected to destructive physical analysis to determine the reason for a capacity loss after 5,967 cycles at 60 percent depth of discharge. The positive plates in the cell were analyzed in terms of chemical composition, active material utilization, charge efficiency, and thickness increase. The microstructure of a cross section of the positive plate was determined by backscattered electron image analysis. The results suggest that the capacity loss in the cell is caused by low charge acceptance and low active material utilization at the positive plate. The oxidized nickel species content of the positive plate increased due to corrosion of the nickel sintered skeleton. This appears to circumvent the orderly reaction of the active material. Microstructural analysis has indicated that a new phase of active material is formed with cycling.

H Vaidyanathan↗

The effect of hydrogen on the deformation and fracture behavior of a single crystal nickel-base superalloy

The room temperature and 300 C tensile behavior of a single crystal superalloy, PWA 1480, has been studied as a function of internal hydrogen concentration and microstructure. Hydrogen is trapped at the porosity and eutectic gamma/gamma in the microstructure, and the effect of these trapping sites on the tensile behavior will be discussed. There is no effect of hydrogen on strength, however, the strain to failure decreases steadily with increasing hydrogen content up to 200 ppm. Cleavage of the eutectic gamma/gamma occurs without hydrogen, but the presence of internal hydrogen causes cracking in the eutectic gamma/gamma at a much earlier stage of deformation leading to a small total strain. In contrast to many superalloys with a high volume fraction of gamma precipitates, there was no evidence of shearing of the gamma, and it was found that at all strains the dislocations are trapped in the gamma matrix. The effect of hydrogen on this behavior and its relation to fracture is described.

Walston, W. S.↗

Influence of convection on rod spacing of eutectics

This paper describes a three-dimensional numerical model to study the influence of convection on the rod-like microstructure of an eutectic system. This model is based on a central finite difference approach. By applying it, the average concentration near the solid/liquid interface of a growing rod-like eutectic was determined for eutectic compositions C(e) of 0.03, 0.05, and 0.10. Following Jackson and Hunt (1966), the average interfacial composition was converted to a change of undercooling at the interface and, finally, to spacing between the rods. The change in rod spacing with increasing intensity of convection was calculated assuming the eutectic grows at minimum interfacial undercooling. It was confirmed that an increase in convection should coarsen the microstructure (i.e., the rod spacing increases with increasing intensity of stirring).

Caram, R.↗

Continuous fiber-reinforced titanium aluminide composites

An account is given of the fabrication techniques, microstructural characteristics, and mechanical behavior of a lightweight, high service temperature SiC-reinforced alpha-2 Ti-14Al-21Nb intermetallic-matrix composite. Fabrication techniques under investigation to improve the low-temperature ductility and environmental resistance of this material system, while reducing manufacturing costs to competitive levels, encompass powder-cloth processing, foil-fiber-foil processing, and thermal-spray processing. Attention is given to composite microstructure problems associated with fiber distribution and fiber-matrix interfaces, as well as with mismatches of thermal-expansion coefficient; major improvements are noted to be required in tensile properties, thermal cycling effects, mechanical damage, creep, and environmental effects.

Mackay, R. A.↗

The role of the gamma/gamma-prime eutectic and porosity on the tensile behavior of a single-crystal nickel-base superalloy

The microstructure of a single-crystal nickel-base superalloy, PWA 1480, has been varied by heat treatment and hot isostatic pressing in order to study the role of the gamma/gamma-prime eutectic and porosity on subsequent tensile behavior. The level of porosity was found not to affect any of the tensile properties, while the gamma/gamma-prime eutectic strongly influenced ductility. Eliminating the gamma/gamma-prime eutectic increased ductility which was attributed to the cleavage fracture of this constituent. It is proposed that such cleavage of the gamma/gamma-prime eutectic is initiated by the stress created from impinging slip bands, promoting shear localization, and final fracture along 111 slip planes. The precise nature of this fracture process is discussed, with emphasis on the role of the gamma/gamma-prime microstructure. The deformation structure of PWA 1480 was also studied, and while different in some respects from many other single-crystal superalloys, its fracture process appears to be similar.

Walston, W. S.↗

Cleavage crystallography of liquid metal embrittled aluminum alloys

The crystallography of liquid metal-induced transgranular cleavage in six aluminum alloys having a variety of microstructures has been determined via Laue X-ray back reflection. The cleavage crystallography was independent of alloy microstructure, and the cleavage plane was 100-plane oriented in all cases. It was further determined that the cleavage crystallography was not influenced by alloy texture. Examination of the fracture surface indicated that there was not a unique direction of crack propagation. In addition, the existence of 100-plane cleavage on alloy 2024 fracture surfaces was inferred by comparison of secondary cleavage crack intersection geometry on the 2024 surfaces with the geometry of secondary cleavage crack intersections on the test alloys.

Reynolds, A. P.↗

Directional solidification in immiscible systems - The influence of gravity

The possibility of producing aligned fibrous composite microstructures with a high volume fraction of the immiscible phase, L2, through the directional solidification of hypermonotectic alloys is examined. Early work suggests that low gravity conditions are necessary to prevent sedimentation of the more dense L2 phase. However, if convective flows result, they disrupt the formation of the desired fibrous microstructure and produce a disperse structure. The need for long-duration low-g experiments is emphasized.

Andrews, J. B.↗

Processing and properties of SiC whisker- and particulate-reinforced reaction bonded Si3N4

The microstructure and mechanical properties of reaction bonded Si3N4 (RBSN) reinforced with SiC whiskers of particles were investigated using RBSN composites made from colloidally pressed octanol dispersions of high-purity Si powders mixed with either SiC whiskers or alpha-SiC particles. Results of investigations, revealing high conversions of Si to Si3N4, specific surface areas, and constant relative densities and strengths, showed that the uniform microstructure and small flaw size of the matrix were maintained in the composites and that no degradation of the reinforcements was taking place. Neither the monolithic nor the composite materials exhibited R-curve behavior. A modest increase in fracture toughness was observed only in the RBSN containing 33 vol pct SiC(p).

Lightfoot, A.↗