Investigation of single crystal ferrite thin films

Materials suitable for use in magnetic bubble domain memories were developed for aerospace applications. Practical techniques for the preparation of such materials in forms required for fabrication of computer memory devices were considered. The materials studied were epitaxial films of various compositions of the gallium-substituted yttrium gadolinium iron garnet system. The major emphasis was to determine their bubble properties and the conditions necessary for growing uncracked, high quality films.

Mee, J. E.↗

Modified ferritic iron alloys with improved high-temperature mechanical properties and oxidation resistance

An alloy modification program was conducted in which the compositions of two existing Fe-Cr-Al alloys (Armco 18SR and GE-1541) were changed to achieve either improved high-temperature strength or improved fabricability. Only modifications of Armco 18SR were successful in achieving increased strength without loss of fabricability or oxidation resistance. The best modified alloy, designated NASA-18T, had twice the rupture strength of Armco 18SR at 800 and 1000 C. The NASA-18T alloy also had better oxidation resistance than Armco 18SR and comparable fabricability. The nominal composition of NASA-18T is Fe-18Cr-2Al-1Si-1.25Ta. All attempted modifications of the GE-1541 alloy were unsuccessful in terms of achieving better fabricability without sacrificing high-temperature strength and oxidation resistance.

Oldrieve, R. E.↗

Structure and elevated temperature properties of carbon-free ferritic alloys strengthened by a Laves phase

A Laves phase, Fe2Ta, was utilized to obtain good elevated temperature properties in a carbon-free iron alloy containing 1 at. pct Ta and 7 at. pct Cr. Room temperature embrittlement resulting from the precipitation of the Laves phase at grain boundaries was overcome by spheroidizing the precipitate. This was accomplished by thermally cycling the alloys through the alpha to gamma transformation. The short-time yield strength of the alloys decreased very slowly with increase in test temperature up to 600 C, but above this temperature, the strength decreased rapidly. Results of constant load creep and stress rupture tests conducted at several temperatures and stresses indicated that the rupture and creep strengths of spheroidized 1 Ta-7 Cr alloy were higher than those of several commercial steels containing chromium and/or molybdenum carbides but lower than those of steels containing substantial amounts of tungsten and vanadium. When molybdenum was added to the base Fe-Ta-Cr alloy, the rupture and creep strengths were considerably increased.

Bhandarkar, M. D.↗

The suppression of low-temperature intergranular brittleness in ferritic Fe-Mn alloys

A method for obtaining cryogenic toughness in an Fe-12Mn-0.2Ti alloy by a controlled cooling technique is presented. The intergranular fracture surface of the quenched alloy, using an AES, revealed no significant difference from that obtained by the bulk transgranular fracture surface, indicating the absence of large-scale grain boundary segregation during the austenitizing treatment. Attention is given to the step cooling method, using a furnace at temperatures of 100 to 120 C, followed by fast cooling to ambient temperature, which in turn produces a high-impact toughness without intergranular brittleness. It is concluded that the sources of brittle intergranular fracture in the alloy are both chemical, operating in martensitic structure, and nonchemical, active during quenching from the austenitizing treatment.

Hwang, S. K.↗

Producing gapped-ferrite transformer cores

Improved manufacturing techniques make reproducible gaps and minimize cracking. Molded, unfired transformer cores are cut with thin saw and then fired. Hardened semicircular core sections are bonded together, placed in aluminum core box, and fluidized-coated. After winding is run over box, core is potted. Economical method significantly reduces number of rejects.

Mclyman, W. T.↗

Computer-aided design of stripline ferrite junction circulators

A general design procedure is presented for stripline Y-junction circulators employing solid dielectric between ground planes. The resonator design and impedance matching are derived in a form suitable for computer evaluation. The procedure is applicable to cases where either the circulator bandwidth or the ground plane spacing is specified. An experimental S-band switching circulator design illustrates the technique.

Uzdy, Z.↗

Designing high frequency ac inductors using ferrite and Molypermalloy Powder Cores (MPP)

The major considerations in the design of high frequency ac inductors are reviewed. Two methods for designing the inductor: the area product method and the core geometry method, are presented. The two major effects of the inductor air gap, fringing flux power loss and increase of inductance, are discussed. Equations for the inductor design and a step-by-step design procedure are given. The use of a lumped air gap or a distributed air gap are discussed and a comparison of the losses resulting from these gaps, together with experimental results are presented.

Mclyman, W. T.↗

Modeling the long-term evolution of the primary damage in ferritic alloys using coarse-grained methods

Atomic displacement cascades in solids are complex phenomena, the outcome of which can be statistically characterised by properties such as their spatial extent, morphology and the spatial correlation of defects. Some properties scale in a simple way with parameters such as the cascade energy, others have limited variability with energy, for example point defect cluster size distributions. Taking advantage of the latter invariance, we use Object Kinetic Monte Carlo simulations to demonstrate that most properties of displacement cascade play no significant role in the evolution of point defect cluster size distributions after long enough time. It is suggested that reliable long-term predictions are possible, when using only the self-interstitial and vacancy cluster size distributions from low energy displacement cascades as building blocks to represent the complete spectrum of cascade energies obtained under neutron irradiation conditions. This is shown on the basis of recursive properties of displacement cascades evidenced for the first time and taking only approximately into account the average volumes in which vacancies and self-interstitial atoms are confined. The model has been successfully used to simulate the evolution of point defect clusters in iron for displacement rates in the range of 10-6 dpa/s and doses of the order of 0.1 dpa. The applicability beyond this range and to more complex materials is discussed.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗