Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Alloy”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,081 records · Page 60

Exploratory Investigation of Advanced-Temperature Nickel-Base Alloys

An investigation was conducted to provide an advanced-temperature nickel-base alloy with properties suitable for aircraft turbine blades as well as for possible space vehicle applications. An entire series of alloys that do not require vacuum melting techniques and that generally provide good stress-rupture and impact properties was evolved. The basic-alloy composition of 79 percent nickel, 8 percent molybdenum, 6 percent chromium, 6 percent aluminum, and 1 percent zirconium was modified by a series of element additions such as carbon, titanium, and boron, with the nickel content adjusted to account for the additives. Stress-rupture, impact, and swage tests were made with all the alloys. The strongest composition (basic alloy plus 1.5 percent titanium plus 0.125 percent carbon) displayed 384- and 574-hour stress-rupture lives at 1800 F and 15,000 psi in the as-cast and homogenized conditions, respectively. All the alloys investigated demonstrated good impact resistance. Several could not be broken in a low-capacity Izod impact tester and, on this basis, all compared favorably with several high-strength high-temperature alloys. Swaging cracks were encountered with all the alloys. In several cases, however, these cracks were slight and could be detected only by zyglo examination. Some of these compositions may become amenable to hot working on further development. On the basis of the properties indicated, it appears that several of the alloys evolved, particularly the 1.5 percent titanium plus 0.125 percent carbon basic-alloy modification, could be used for advanced- temperature turbine blades, as well as for possible space vehicle applications.

Freche, John C.↗

Characterization of Ternary NiTiPt High-Temperature Shape Memory Alloys

Pt additions substituted for Ni in NiTi alloys are known to increase the transformation temperature of the alloy but only at fairly high Pt levels. However, until now only ternary compositions with a very specific stoichiometry, Ni50-xPtxTi50, have been investigated and then only to very limited extent. In order to learn about this potential high-temperature shape memory alloy system, a series of over twenty alloys along and on either side of a line of constant stoichiometry between NiTi and TiPt were arc melted, homogenized, and characterized in terms of their microstructure, transformation temperatures, and hardness. The resulting microstructures were examined by scanning electron microscopy and the phase compositions quantified by energy dispersive spectroscopy."Stoichiometric" compositions along a line of constant stoichiometry between NiTi to TiPt were essentially single phase but by any deviations from a stoichiometry of (Ni,Pt)50Ti50 resulted in the presence of at least two different intermetallic phases, depending on the overall composition of the alloy. Essentially all alloys, whether single or two-phase, still under went a martensitic transformation. It was found that the transformation temperatures were depressed with initial Pt additions but at levels greater than 10 at.% the transformation temperature increased linearly with Pt content. Also, the transformation temperatures were relatively insensitive to alloy stoichiometry within the range of alloys examined. Finally, the dependence of hardness on Pt content for a series of Ni50-xPtxTi50 alloys showed solution softening at low Pt levels, while hardening was observed in ternary alloys containing more than about 10 at.% Pt. On either side of these "stoichiometric" compositions, hardness was also found to increase significantly.

Rios, Orlando↗

Elevated temperature aluminum alloys

Three aluminum-lithium alloys are provided for high performance aircraft structures and engines. All three alloys contain 3 wt % copper, 2 wt % lithium, 1 wt % magnesium, and 0.2 wt % zirconium. Alloy 1 has no further alloying elements. Alloy 2 has the addition of 1 wt % iron and 1 wt % nickel. Alloy 3 has the addition of 1.6 wt % chromium to the shared alloy composition of the three alloys. The balance of the three alloys, except for incidentql impurities, is aluminum. These alloys have low densities and improved strengths at temperatures up to 260.degree. C. for long periods of time.

Meschter, Peter↗

Development and Characterization of Improved NiTiPd High-Temperature Shape-Memory Alloys by Solid-Solution Strengthening and Thermomechanical Processing

The need for compact, solid-state actuation systems for use in the aerospace, automotive, and other transportation industries is currently motivating research in high-temperature shape-memory alloys (HTSMA) with transformation temperatures greater than 100 C. One of the basic high-temperature alloys investigated to fill this need is Ni(19.5)Ti(50.5)Pd30. Initial testing has indicated that this alloy, while having acceptable work characteristics, suffers from significant permanent deformation (or ratcheting) during thermal cycling under load. In an effort to overcome this deficiency, various solid-solution alloying and thermomechanical processing schemes were investigated. Solid-solution strengthening was achieved by substituting 5at% gold or platinum for palladium in Ni(19.5)Ti(50.5)Pd30, the so-called baseline alloy, to strengthen the martensite and austenite phases against slip processes and improve thermomechanical behavior. Tensile properties, work behavior, and dimensional stability during repeated thermal cycling under load for the ternary and quaternary alloys were compared. The relative difference in yield strength between the martensite and austenite phases and the dimensional stability of the alloy were improved by the quaternary additions, while work output was only minimally impacted. The three alloys were also thermomechanically processed by cycling repeatedly through the transformation range under a constant stress. This so-called training process dramatically improved the dimensional stability in these samples and also recovered the slight decrease in work output caused by quaternary alloying. An added benefit of the solid-solution strengthening was maintenance of enhanced dimensional stability of the trained material to higher temperatures compared to the baseline alloy, providing a greater measure of over-temperature capability.

Bigelow, Glen↗

Effects of Annealing Process on the Formability of Friction Stir Welded Al-Li Alloy 2195 Plates

Large rocket cryogenic tank domes have typically been fabricated using Al-Cu based alloys like Al-Cu alloy 2219. The use of aluminum-lithium based alloys for rocket fuel tank domes can reduce weight because aluminum-lithium alloys have lower density and higher strength than Al-Cu alloy 2219. However, Al-Li alloys have rarely been used to fabricate rocket fuel tank domes because of the inherent low formability characteristic that make them susceptible to cracking during the forming operations. The ability to form metal by stretch forming or spin forming without excessive thinning or necking depends on the strain hardening exponent "n". The stain hardening exponent is a measure of how rapidly a metal becomes stronger and harder. A high strain hardening exponent is beneficial to a material's ability to uniformly distribute the imposed strain. Marshall Space Flight Center has developed a novel annealing process that can achieve a work hardening exponent on the order of 0.27 to 0.29, which is approximately 50% higher than what is typically obtained for Al-Li alloys using the conventional method. The strain hardening exponent of the Al-Li alloy plates or blanks heat treated using the conventional method is typically on the order of 0.17 to 0.19. The effects of this novel annealing process on the formability of friction stir welded Al-Li alloy blanks are being studied at Marshall Space Flight Center. The formability ratings will be generated using the strain hardening exponent, strain rate sensitivity and forming range. The effects of forming temperature on the formability will also be studied. The objective of this work is to study the deformation behavior of the friction stir welded Al-Li alloy 2195 blank and determine the formability enhancement by the new annealing process.

Chen, Po-Shou↗

The stress corrosion cracking behavior of alloys 690 and 152 WELD in a PWR environment.

Alloys 690 and 152 are the replacement materials of choice for Alloys 600 and 182, respectively. The latter two alloys are used as structural materials in pressurized water reactors (PWRs) and have been found to undergo stress corrosion cracking (SCC). The objective of this work is to determine the crack growth rates (CGRs) in a simulated PWR water environment for the replacement alloys. The study involved Alloy 690 cold-rolled by 26% and a laboratory-prepared Alloy 152 double-J weld in the as-welded condition. The experimental approach involved pre-cracking in a primary water environment and monitoring the cyclic CGRs to determine the optimum conditions for transitioning from the fatigue transgranular to intergranular SCC fracture mode. The cyclic CGRs of cold-rolled Alloy 690 showed significant environmental enhancement, while those for Alloy 152 were minimal. Both materials exhibited SCC of 10{sup -11} m/s under constant loading at moderate stress intensity factors. The paper also presents tensile property data for Alloy 690TT and Alloy 152 weld in the temperature range 25--870 C.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Dispersoid reinforced alloy powder and method of making

A method of making dispersion-strengthened alloy particles involves melting an alloy having a corrosion and/or oxidation resistance-imparting alloying element, a dispersoid-forming element, and a matrix metal wherein the dispersoid-forming element exhibits a greater tendency to react with an introduced reactive species than does the alloying element and wherein one or more atomizing parameters is/are modified to controllably reduce the amount of the reactive species, such as oxygen, introduced into the atomized particles so as to reduce anneal times and improve reaction (conversion) to the desired strengthening dispersoids in the matrix. The atomized alloy particles are solidified as solidified alloy particles or as a solidified deposit of alloy particles. Bodies are made from the dispersion strengthened alloy particles, deposit thereof, exhibit enhanced fatigue and creep resistance and reduced wear as well as enhanced corrosion and/or oxidation resistance at high temperatures by virtue of the presence of the corrosion and/or oxidation resistance imparting alloying element in solid solution in the particle alloy matrix.

36 MATERIALS SCIENCE↗

Formation Mechanism of Nanoscale Al{sub 3}Fe Phase in Al-Fe Alloy During Semisolid Forming Process

The formation mechanism of nanoscale Al{sub 3}Fe phase in Al-1Fe (wt pct) alloy during rheo-extrusion was investigated, and the mechanical property of the prepared alloy was also measured. The results show that the average length of Al{sub 3}Fe phase in Al-1Fe alloy prepared by rheo-extrusion is 300 nm, which is much more refined than the needlelike Al{sub 3}Fe phase in as-cast Al-1Fe alloy (50 μm). In rheo-extrusion, Al{sub 3}Fe phase formed by eutectic reaction is bonelike, but it could be continuously refined by the shear deformation in the wheel groove, in equal channel angular flow, and in expansion extrusion mold. The total equivalent strain of the shear deformation is higher than 4.82. The tensile strength and elongation of Al-1Fe alloy prepared by rheo-extrusion are 135 MPa and 30 pct, respectively. The tensile strength of Al-1Fe alloy prepared by rheo-extrusion is 58.8 pct higher than that of as-cast Al-1Fe alloy, and the elongation is 19 pct higher than that of as-cast Al-1Fe alloy. Compared with as-cast Al-1Fe alloy, the improvements of tensile strength and elongation caused by shear deformation in rheo-extrusion are higher than the reported improvements induced by rare earth modification.

36 MATERIALS SCIENCE↗

The Effect of Hydroxyapatite Coatings on the Passivation Behavior of Oxidized and Unoxidized Superelastic Nitinol Alloys

Nitinol alloys have been used in various biological applications due to their superior properties. In this study, a bipolar pulsed current electrodeposition technique was applied to produce a hydroxyapatite (HA) film on the Nitinol alloy. Also, the protection performance of the coating was evaluated on both abraded and thermochemically modified alloy. According to obtained data, reducing the electrocrystallization rate by the pulse deposition technique can promote HA formation on both abraded and modified substrates. Based on scanning electron microscopy and high-resolution transmission electron microscopy data, the HA coatings revealed a flake-like morphology and each flake was composed of nano-crystalline grains. Atomic force microscopy images revealed that flakes on the abraded substrate were smaller in size than that of the modified alloy. Comparing the corrosion resistance of the bare substrates revealed that the modified alloy has a higher corrosion resistance than the abraded alloy and the modified surface is well passivized during anodic polarization in Ringer’s solution. However, this condition is reversed after the deposition of HA film. It seems that because of the lower crystallization sites on the abraded alloy, the produced HA film is denser and more protective against the corrosive mediums as compared to the coating on the modified alloy. Although the HA coating can improve the bioactivity of both substrates, the resulted film on the oxidized alloy is porous and deteriorates the implant permanence in the vicinity of body fluids.

36 MATERIALS SCIENCE↗

Effects of Nb on Superelasticity and Low Modulus Properties of Metastable β-Type Ti-Nb-Ta-Zr Biomedical Alloys

In this work, a series of Ti-xNb-2Ta-3Zr (x = 25, 30, 35, 40 wt.%) alloys are designed, and the transformation of β-phase to α″ martensitic, β-phase stability, microstructure, mechanical properties and corrosion performance of these alloys are investigated. The phase analysis shows as the Nb content increases, the α″ phase in these alloys decreases, while the intensity of the two main peaks β(110) and β(211) of Ti-40Nb-2Ta-3Zr alloy is reduced. These results can be attributed to the variation of β-phase stability caused by Nb element of alloy and cold rolling process. The mechanical properties test shows that the elastic modulus (52 GPa) of the Ti-35Nb-2Ta-3Zr alloy is the lowest and the elongation (18.8%) is the maximum. In addition, the alloy is susceptible to β-phase elastic deformation and stress-induced martensitic transformation resulting in the highest recovery strain of the alloy (66.87%). The polarization curves show that the Ti-35Nb-2Ta-3Zr alloy has the highest corrosion potential (− 0.34 V) and the lowest corrosion current density (0.21 μA cm{sup −2}) exhibiting the best corrosion resistance.

36 MATERIALS SCIENCE↗

Design of heterogeneous structured Al alloys with wide processing window for laser-powder bed fusion additive manufacturing

Required microstructural attributes of an alloy vary with structural applications. The microstructural fine-tuning capability of laser-powder bed fusion (L-PBF) additive manufacturing (AM) enables application specific manufacture of the components. Such manufacture with L-PBF AM requires alloys that exhibit wide processing window and are amenable to multiple deformation mechanisms. However, high hot cracking susceptibility of Al alloys poses a barrier to such printability-performance synergy. In this work we show that an integration of, a) grain refinement through heterogeneous nucleation, and b) eutectic solidification, leads to crack-free parts at wide range of process parameters, microstructural heterogeneity, and hierarchy in the Al-Ni-Ti-Zr alloy. Such an integration targets hot cracking at multiple stages of solidification in L-PBF as opposed to the contemporary alloy design strategies that target hot-cracking at only specific stages of solidification. The Al-Ni-Ti-Zr alloy exhibits excellent printability and a high as-built tensile performance. Due to the wide processing window and amenability to multiple deformation mechanisms, the alloy microstructure and subsequently the performance, can be fine-tuned. Here, such strategy opens the gateway for application-specific manufacture of Al alloys with L-PBF AM and establishes a fundamental shift in current methodologies for design of these alloys for L-PBF AM.

36 MATERIALS SCIENCE↗

PdAgAu alloy with high resistance to corrosion by H 2 S

PdAgAu alloy films were prepared on porous stainless steel supports by sequential electroless deposition. Two specific compositions, Pd 83 Ag 2 Au 15 and Pd 74 Ag 14 Au 12 , were studied for their sulfur tolerance. The alloys and a reference Pd foil were exposed to 1000 H 2 S /H 2 at 623 K for periods of 3 and 30 hours. The microstructure, morphology and bulk composition of both nonexposed and H 2 S-exposed samples were characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM) and energy-dispersive X-ray spectroscopy (EDS). XRD and SEM analysis revealed time-dependent growth of a bulk Pd{sub 4}S phase on the Pd foil during H 2 S exposure. In contrast, the PdAgAu ternary alloys displayed the same FCC structure before and after H 2 S exposure. In agreement with the XRD and SEM results, sulfur was not detected in the bulk of either ternary alloy samples by EDS, even after 30 hours of H 2 S exposure. X-ray photoelectron spectroscopy (XPS) depth profiles were acquired for both PdAgAu alloys after 3 and 30 hours of exposure to characterize sulfur contamination near their surfaces. Very low S 2p and S 2s XPS signals were observed at the top-surfaces of the PdAgAu alloys, and those signals disappeared before the etch depth reached ~ 10 nm, even for samples exposed to H 2 S for 30 hours. The depth profile analyses also revealed silver and gold segregation to the surface of the alloys; preferential location of Au on the alloys surface may be related to their resistance to bulk sulfide formation. In preliminary tests, a PdAgAu alloy membrane displayed higher initial H{sub 2} permeability than a similarly prepared pure Pd sample and, consistent with resistance to bulk sulfide formation, lower permeability loss in H 2 S than pure Pd.

36 MATERIALS SCIENCE↗

Structural stability of mechanically alloyed amorphous (FeCoNi) 70 Ti 10 B 20 under high-temperature and high-pressure

Nanostructured (FeCoNi) 70 Ti 10 B 20 (at%) alloy was synthesized by mechanical alloying from elemental powder mixture of Fe, Co, Ni, Ti and B using ball milling. The effect of ball milling time on the evolution of structure and morphology was investigated by X-ray diffraction, scanning and transmission electron microscopy and differential thermal analysis. It was observed that the formation of solid solution of (FeCoNi) 70 Ti 10 B 20 started from the very onset of the milling process. Crystallite size and lattice strains seemed to be leveled off after 20 h of milling with no further major changes. The milling process for longer periods introduced severe plastic deformations causing formation of amorphous phase of (FeCoNi) 70 Ti 10 B 20 . The amorphous alloy composition was confirmed by energy dispersive X-ray spectroscopy analysis that showed an excellent homogeneity of the alloying elements. The phase stability of the mechanically alloyed amorphous sample was further verified by employing high-temperature and high-pressure studies. The alloy samples heat-treated at 700 °C revealed crystallization of the amorphous phase. However, synchrotron-based high-pressure ambient temperature X-ray diffraction studies confirmed that the amorphous phase of the alloy remained stable up to the pressure of 30 GPa. Here, the 50 h milled sample after being annealed at 350 °C showed improvement in the soft magnetic properties of the alloy, which was due to the probable elimination of the residual stress in the amorphous phase of the alloy powders.

36 MATERIALS SCIENCE↗

Effects of strain amplitude and temperature on the damping capacity of an Fe-19Mn alloy with different microstructures

The influences of strain amplitude (10{sup -5}-10{sup -4}) and temperature (25 deg. C-500 deg. C) on the internal friction of a cold-drawn and solution treated Fe-19Mn alloy were investigated. The internal friction was measured using reversal torsion pendulum and multifunction internal friction equipment. The microstructure was observed using scanning electron microscopy. The phase transformation temperatures were determined using differential scanning calorimetry. The results indicated that the internal friction of the solution treated alloy was related to strain amplitude, which could be explained using the movement of Shockley partial dislocations (bowing out and breaking away). But the internal friction of the cold-drawn alloy was independent of strain amplitude because of high density dislocations formed by cold forming. Moreover, when the temperature was changed between 25 deg. C and 500 deg. C, the internal friction of the cold-drawn alloy increased slowly from 25 deg. C to 375 deg. C, and then increased quickly from 375 deg. C to 500 deg. C. However, for the solution treated alloy, there was an internal friction peak at about 210 deg. C in the heating process (from 25 deg. C to 500 deg. C), and there was another internal friction peak at about 150 deg. C in the cooling process. These peaks could be explained using the heat-assisted movement of dislocations. - Research Highlights: {yields}Internal friction of solution treated Fe-19Mn alloy is related to strain amplitude. {yields}Internal friction of cold-drawn Fe-19Mn alloy is independent of strain amplitude. {yields}IF of cold-drawn alloy increases from RT to 500 deg. C. {yields}There is an IF peak of solution treated alloy in heating and cooling process separately. {yields}The results can be explained using the movement of dislocations.

36 MATERIALS SCIENCE↗

Effects of Ce additions on the age hardening response of Mg–Zn alloys

The effects of Ce additions on the precipitation hardening behaviour of Mg–Zn are examined for a series of alloys, with Ce additions at both alloying and microalloying levels. The alloys are artificially aged, and studied using hardness measurement and X-ray diffraction, as well as optical and transmission electron microscopy. It is found that the age-hardening effect is driven by the formation of fine precipitates, the number density of which is related to the Zn content of the alloy. Conversely, the Ce content is found to slightly reduce hardening. When the alloy content of Ce is high, large secondary phase particles containing both Ce and Zn are present, and remain stable during solutionizing. These particles effectively reduce the amount of Zn available as solute for precipitation, and thereby reduce hardening. Combining hardness results with thermodynamic analysis of alloy solute levels also suggests that Ce can have a negative effect on hardening when present as solutes at the onset of ageing. This effect is confirmed by designing a pre-ageing heat treatment to preferentially remove Ce solutes, which is found to restore the hardening capability of an Mg–Zn–Ce alloy to the level of the Ce-free alloy. - Highlights: • The effects of Ce additions on precipitation in Mg–Zn alloys are examined. • Additions of Ce to Mg–Zn slightly reduce the age-hardening response. • Ce-rich secondary phase particles deplete the matrix of Zn solute. • Hardening is also decreased when Ce is present in solution. • Pre-ageing to preferentially precipitate out Ce restores hardening capabilities.

36 MATERIALS SCIENCE↗

First-principles study of the structural and dynamic properties of the liquid and amorphous Li–Si alloys

We have performed density functional theory calculations and ab initio molecular dynamics to investigate the structures and dynamic properties of the liquid and amorphous Li{sub x}Si alloys over a range of composition from x = 1.0 − 4.8. Our results show that Si atoms can form a variety of covalently bonded polyanions with diverse local bonding structures in the liquid alloys. Like in c-LiSi, Si atoms can form a continuous bond network in liquid Li{sub 1.0}Si at 1050 K, while it gradually disintegrates into many smaller Si polyanions as the Li content increases in the alloys. The average sizes of Si polyanions in these liquid alloys were found to be relatively larger than those in their crystalline counterparts, which can even persist in the highly lithiated Li{sub 4.81}Si alloy at 1500 K. Our results also show that amorphous Li{sub x}Si alloys have similar local bonding structures but a largely increased short-range order as compared to their liquid counterparts. The differences between the average coordination number of each atomic pair in amorphous solids and that in the liquids are less than 1.1. Furthermore, our calculations reveal that Li and Si atoms can exhibit very distinct dynamic behaviors in the liquids and their diffusivities appear to be largely dependent on the chemical composition of the alloys. The diffusivity of Li was found to increase with the Li content in the alloys primarily because of the reduced interactions between Li and Si atoms, while the Si diffusivity also increases due to the gradual disintegration of the strongly interconnected Si bond network. The diffusivity of Li in amorphous Li{sub x}Si was predicted to lie in the range between 10{sup −7} and 10{sup −9} cm{sup 2}/s at 300 K, which is more than 20-fold larger than that of Si over the composition range considered. Our calculations further show that the diffusivities of both Li and Si can increase by two orders of magnitude as x increases from 1.0 to 3.57 in amorphous Li{sub x}Si, indicating a more profound dependence on the alloy composition than those in the liquid state.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A Novel Low-Activation VCrFeTa x W x (x = 0.1, 0.2, 0.3, 0.4, and 1) High-Entropy Alloys with Excellent Heat-Softening Resistance

The microstructure, Vickers hardness, and compressive properties of novel low-activation VCrFeTa x W x (x = 0.1, 0.2, 0.3, 0.4, and 1) high-entropy alloys (HEAs) were studied. The alloys were fabricated by vacuum-arc melting and the characteristics of these alloys were explored. The microstructures of all the alloys exhibited a typical morphology of dendritic and eutectic structures. The VCrFeTa 0.1 W 0.1 and VCrFeTa 0.2 W 0.2 alloys are essentially single phase, consisting of a disordered body-centered-cubic (BCC) phase, whereas the VCrFeTa 0.2 W 0.2 alloy contains fine, nanoscale precipitates distributed in the BCC matrix. The lattice parameters and compositions of the identified phases were investigated. The alloys have Vickers hardness values ranging from 546 HV0.2 to 1135 HV0.2 with the x ranging from 0.1 to 1, respectively. The VCrFeTa 0.1 W 0.1 and VCrFeTa 0.2 W 0.2 alloys exhibit compressive yield strengths of 1341 MPa and 1742 MPa, with compressive plastic strains of 42.2% and 35.7%, respectively. VCrFeTa 0.1 W 0.1 and VCrFeTa 0.2 W 0.2 alloys have excellent hardness after annealing for 25 h at 600–1000 °C, and presented compressive yield strength exceeding 1000 MPa with excellent heat-softening resistance at 600–800 °C. By applying the HEA criteria, Ta and W additions into the VCrFeTaW are proposed as a family of candidate materials for fusion reactors and high-temperature structural applications.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Characterization of Elevated Temperature Properties of Heat Exchanger and Steam Generator Alloys

The Next Generation Nuclear Plant project is considering Alloy 800H and Alloy 617 for steam generator and intermediate heat exchangers. It is envisioned that a steam generator would operate with reactor outlet temperatures from 750 to 800°C, while an intermediate heat exchanger for primary to secondary helium would operate up to an outlet temperature of 950°C. Although both alloys are of interest due in part to their technical maturity, a number of specific properties require further characterization for design of nuclear components. Strain rate sensitivity of both alloys has been characterized and is found to be significant above 600°C. Both alloys also exhibit dynamic strain aging, characterized by serrated flow, over a wide range of temperatures and strain rates. In general dynamic strain aging is observed to begin at higher temperatures and serrated flow persists to higher temperatures in Alloy 617 compared to Alloy 800H. Dynamic strain aging is a concern for these materials since it is observed to result in reduced ductility for many solid solution alloys. The role of dynamic strain aging in the creep-fatigue behavior of Alloy 617 at temperatures of 800°C and above has also been examined in detail. Serrated flow is found to persist in cyclic stress-strain curves up to nearly the cycle to failure in some temperature and strain regimes. Results of those experiments and implications for creep-fatigue testing protocols will be described.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗