Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “solid electrolyte interphase”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Impacts of Dissolved Ni 2+ on the Solid Electrolyte Interphase on a Graphite Anode

Transition metal (e.g. Ni) ions dissolved from layered-structured Ni-rich cathodes can migrate to the anode side and accelerate the failure of lithium-ion batteries. The investigations of the impact and distribution of Ni species on the solid electrolyte interphase (SEI) on the anode are crucial to understand the failure mechanism. Herein, we used time-of-flight secondary ion mass spectroscopy (TOF-SIMS) coupled with multivariate curve resolution (MCR) analysis to intuitively characterize the distribution of Ni species in the SEI. We find that the SEI on the graphite electrode using an EC-based electrolyte exhibits a multi-stratum structure. During accelerated aging of the LiNi 0.88 Co 0.08 Mn 0.04 O 2 /graphite full cell, the dissolution of Ni aggravates significantly upon cycling. A strong correlation between the dissolved-Ni and organic species in the SEI on graphite is illustrated. Here, the ion-exchange reaction between Ni 2+ and Li + ions in the SEI is demonstrated to be the main reason for the increase of SEI resistivity.

25 ENERGY STORAGE↗

A Facile Potential Hold Method for Fostering an Inorganic Solid-Electrolyte Interphase for Anode-Free Lithium-Metal Batteries

Anode-free lithium batteries are regarded as an ultimate form of high-energy-density lithium-ion batteries. Unfortunately, irreversible lithium loss during cycling plays a major role in degrading the overall cell performance in the anode-free configuration. To alleviate the deterioration, building a robust solid-electrolyte interface on an anode current collector is an indispensable requirement. Here, we present a facile in-situ electrochemical method of a potential hold during the first charge to guide more salt-derived (less solvent-derived) decomposition on the anode interface. Here we show the distinctive decomposition potential of lithium salts and ether/carbonate solvents, where the Li-solvation structures with salt contact-ion-pairs preferentially decompose to form LiF-rich and less organic components, leading to enhanced lithium Coulombic efficiency in Li||Cu cells as well as mitigating the capacity fade of Cu||LiFePO 4 and Cu||LiNi 0.8 Mn 0.1 Co 0.1 O 2 cells.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Delineating the Impact of Transition‐Metal Crossover on Solid‐Electrolyte Interphase Formation with Ion Mass Spectrometry

Abstract Lithium‐metal batteries (LMB) employing cobalt‐free layered‐oxide cathodes are a sustainable path forward to achieving high energy densities, but these cathodes exhibit substantial transition‐metal dissolution during high‐voltage cycling. While transition‐metal crossover is recognized to disrupt solid‐electrolyte interphase (SEI) formation on graphite anodes, experimental evidence is necessary to demonstrate this for lithium‐metal anodes. In this work, advanced high‐resolution 3D chemical analysis is conducted with time‐of‐flight secondary‐ion mass spectrometry (TOF‐SIMS) to establish spatial correlations between the transition metals and electrolyte decomposition products found on cycled lithium‐metal anodes. Insights into the localization of various chemistries linked to crucial processes that define LMB performance, such as lithium deposition, SEI growth, and transition‐metal deposition are deduced from a precise elemental and spatial analysis of the SEI. Heterogenous transition‐metal deposition is found to perpetuate both heterogeneous SEI growth and lithium deposition on lithium‐metal anodes. These correlations are confirmed across various lithium‐metal anodes that are cycled with different cobalt‐free cathodes and electrolytes. An advanced electrolyte that is stable to higher voltages is shown to minimize transition‐metal crossover and its effects on lithium‐metal anodes. Overall, these results highlight the importance of maintaining uniform SEI coverage on lithium‐metal anodes, which is disrupted by transition‐metal crossover during operation at high voltages.

Chemistry↗

Engineering Solid Electrolyte Interphase Composition by Assessing Decomposition Pathways of Fluorinated Organic Solvents in Lithium Metal Batteries

Studies have shown fluorinated electrolyte solvents can form desirable solid electrolyte interphase (SEI) in lithium metal batteries. In this study, we develop a detailed mechanistic understanding of two high performing electrolytes, Fluoroethylene Carbonate (FEC) and Difluoroethylene Carbonate (DFEC) to demonstrate minimal structural variations can lead to different decomposition products, and thereby the nature of the SEI. Using density functional theory (DFT) calculations, we find different initial bond-breaking mechanisms between FEC and DFEC. We develop free energy diagrams for the decomposition pathways including both electrochemical and chemical steps. Using the computational Li electrode, we identify the largest limiting potential of 1.77 V for FEC decomposition, associated with the formation of lithium fluoride, lithium oxide and FEC oligomers, and 1.53 V for DFEC, which correspond to the formation of polymerized vinylene carbonate and lithium fluoride. We suggest the formation of oligomers in the case of FEC instead of long polymers may lead to better SEI compactness. We also demonstrate the SEI components of FEC and DFEC are not stable on typical cathode voltage (3.87 V). This study presents a unified electrocatalytic perspective on SEI formation and decomposition.

25 ENERGY STORAGE↗

Toward quantifying capacity losses due to solid electrolyte interphase evolution in silicon thin film batteries

To understand the origins of failure and limited cycle life in lithium-ion batteries (LIBs), it is imperative to quantitatively link capacity-fading mechanisms to electrochemical and chemical processes. This is extremely challenging in real systems where capacity is lost during each cycle to both active material loss and solid electrolyte interphase (SEI) evolution, two indistinguishable contributions in traditional electrochemical measurements. Here, we have used a model system in combination with (1) precision measurements of the overall Coulombic efficiency via electrochemical experiments and (2) x-ray reflectivity measurements of the active material losses. The model system consisted of a 515 Å thick amorphous silicon (a-Si) thin film on silicon carbide in half-cell geometry using a carbonate electrolyte with LiPF6 salt. This approach allowed us to quantify the capacity lost during each cycle due to SEI evolution. Combined with electrochemical analysis, we identify SEI growth as the major contribution to capacity fading. Specifically, the continued SEI growth results in increasing overpotentials due to increased SEI resistance, and this leads to lower extent of lithiation when the cutoff voltage is reached during lithiation. Our results suggest that SEI grows more with increased time spent at low voltages where electrolyte decomposition is favored. Finally, we extracted a proportionality constant for SEI growth following a parabolic growth law. Our methodology allows for the quantitative determination of lithium-ion loss mechanisms in LIBs by separately tracking lithium ions within the active materials and the SEI and offers a powerful method of quantitatively understanding LIB loss mechanisms.

25 ENERGY STORAGE↗

Automatic Generation of Chemical Mechanisms for Electrochemical Systems: Solid Electrolyte Interphase Formation in Lithium Batteries

Electrolytes in many lithium ion batteries decompose at the low potentials near the anode. The decomposition products form a layer termed the solid electrolyte interphase (SEI). The composition and growth of the SEI layer significantly affect both the capacity fade and safety of lithium ion batteries. However, SEI formation and growth kinetics are not well understood. In this work, we present an extension of the Reaction Mechanism Generator (RMG) software to automatically generate mechanisms for SEI formation. We extend RMG’s solvation correction framework to account for kinetic solvent effects and demonstrate the accuracy of our technique. We calculate thermochemical parameters for 252 species and rate coefficients for 69 reactions, most with associated solvation corrections. This and additional quantum chemistry data are used to extend RMG’s thermodynamic group additivity and solute parameter estimation schemes to handle lithiated species and add 14 new reaction families to RMG. RMG is additionally extended to simulate electrocatalytic systems. Lastly, we demonstrate RMG on the decomposition of acetonitrile and ethylene carbonate near a battery anode. Furthermore, while this framework does not yet resolve individual ions, as appropriate thermochemistry estimators are not available, and thus, cannot yet resolve more complex electrochemical pathways, RMG is able to generate reasonable pathways for SEI formation that match literature pathways and products. In particular, RMG identifies a new important reaction pathway that is not present in literature.

Chemical reactions↗

Modeling the influence of the solid electrolyte interphase on the sand’s time and dendrite formation on lithium metal electrodes

Lithium metal is a sought after battery material for its high energy density due to the low electrochemical potential and density. However, lithium metal is also highly reactive, which results in a strong propensity for dendrite formation. The Sand’s time has previously been used to predict the time of dendrite initiation on metals that do not form a solid-electrolyte interphase (SEI), but it has been shown that the Sand’s time is not accurate for lithium electrodes when using transport parameters associated with the electrolyte. Thus, we built a numerical model to simulate lithium ion transport through a growing SEI to predict the Sand’s time. The numerical model is shown to be more accurate than previous analytical solutions, especially for low current densities. We then analyze the sensitivity of the Sand’s time to different SEI properties and the chemical potential gradients present in the SEI, driving lithium transport. The results showed that high lithium concentration has a greater impact at high current density, while fast diffusivity is more important at low current density. Lastly, we modeled the influence of surface roughness on the plating evolution and chemical potential gradients when an SEI is present in comparison to the electrolyte. As a result, we demonstrate that the SEI plays a critical role in lithium electrode stability, and that improved characterization techniques are needed to better understand transport through the SEI and increase lithium metal utilization in energy storage devices.

Chemistry↗

Stabilizing the Solid‐Electrolyte Interphase with Polyacrylamide for High‐Voltage Aqueous Lithium‐Ion Batteries

Abstract The introduction of “water‐in‐salt” electrolyte (WiSE) concept opens a new horizon to aqueous electrochemistry that is benefited from the formation of a solid‐electrolyte interphase (SEI). However, such SEI still faces multiple challenges, including dissolution, mechanical damaging, and incessant reforming, which result in poor cycling stability. Here, we report a polymeric additive, polyacrylamide (PAM) that effectively stabilizes the interphase in WiSE. With the addition of 5 molar % PAM to 21 mol kg −1 LiTFSI electrolyte, a LiMn 2 O 4 ∥L‐TiO 2 full cell exhibits enhanced cycling stability with 86 % capacity retention after 100 cycles at 1 C. The formation mechanism and evolution of PAM‐assisted SEI was investigated using operando small angle neutron scattering and density functional theory (DFT) calculations, which reveal that PAM minimizes the presence of free water molecules at the anode/electrolyte interface, accelerates the TFSI − anion decomposition, and densifies the SEI.

Hou, Xu↗

Stable Solid Electrolyte Interphase Layer Formed by Electrochemical Pretreatment of Gel Polymer Coating on Li Metal Anode for Lithium–Oxygen Batteries

Lithium (Li)-oxygen (O2) batteries (LOBs) exhibit the highest theoretical specific energy density among candidates of the next-generation energy storage systems, but the instability of Li metal anode (LMA), air electrode, and electrolyte largely limit the practical energy density of these batteries. Herein, we report an effective method to protect LMA against side reactions between LMA and crossover contaminants such as highly reactive oxygen moieties. A solid electrolyte interphase (SEI) layer rich in inorganic components was formed on a LMA coated with polyethylene oxide thin-film through an in-situ electrochemical pre-charging step under oxygen atmosphere. This uniformly distributed stiff SEI layer interacted with flexible polymer matrix and formed a submicron-sized gel-like polymer layer. This polymer supported SEI layer leads to much longer cycle life (130 vs. 65 cycles) as compared to those of pristine cell under the same testing conditions (1.0 mAh cm-2 at 0.2 mA cm-2 in the voltage range of 2 to 5 V without any catalysts). It is also very effective during low voltage (2 to 4.5 V) cycling with a redox mediator (0.1 and 0.15M (2,2,6,6-tetramethylpiperidin-1-yl) oxidanyl). Therefore, this approach can be used to stabilize LMA/electrolytes interphase and improve the cycle life of rechargeable LOBs.

lithium-oxygen batteries, lithium metal anodes, ar↗

A solid electrolyte interphase to protect the sulfurized polyacrylonitrile (SPAN) composite for Li–S batteries: computational approach addressing the electrolyte/SPAN interfacial reactivity

This study addresses the reactivity of multiple solvents and lithium bis(fluorosulfonyl)imide (LiFSI) at the interface with sulfurized polyacrylonitrile (SPAN) in multiple stages of lithiation via ab initio molecular dynamics simulations. Here, both ether 1,3-dioxolane (DOL) and dimethyl carbonate (DMC) proved stable on the lithiated SPAN surface regardless of the lithium content, meaning that neither of these species likely contributes to growing a solid electrolyte interphase (SEI) coating to protect the SPAN composite. Conversely, cyclic carbonates, ethylene carbonate (EC) and fluoroethylene carbonate (FEC) are shown to be very active. The EC reduction occurs only on a highly lithiated surface with a 3.0 Li/S molar ratio, the equivalent of the SPAN composite in an over-discharge regime with voltages close to 0.0 V vs. Li/Li + . The FEC reduction starts with a 2.0 Li/S molar ratio and above, suggesting that FEC could act as a useful additive in electrolyte formulations with EC. Both EC and FEC follow multiple reduction mechanisms to produce complex reduction products and LiF in the FEC case. We provide a mechanistic description for each detected decomposition path. The LiFSI salt also proves reactive against the lithiated SPAN surface. The FSI – defluorination is the dominant reduction path. However, the SO 2 NSO 2 F – and SO 2 NSO 2 2– species proved stable against S–N cleavage. This behavior makes the LiFSI salt a potential candidate for SPAN-based Li–S batteries because it produces LiF without releasing SO 2 .

25 ENERGY STORAGE↗

Effect of Water Concentration in LiPF 6 -Based Electrolytes on the Formation, Evolution, and Properties of the Solid Electrolyte Interphase on Si Anodes

A trace amount of water in an electrolyte is one of the factors detrimental to the electrochemical performance of silicon (Si)-based lithium-ion batteries that adversely affect the formation and evolution of the solid electrolyte interphase (SEI) on Si-based anodes and change its properties. Thus far, a lack of fundamental and mechanistic understanding of SEI formation, evolution, and properties in the presence of water has inhibited efforts to stabilize the SEI for improved electrochemical performance. As such, we investigated the SEI formed in a Gen2 electrolyte (1.2 M LiPF6 in ethylene carbonate/ethyl methyl carbonate, 3:7 wt %, water content: <10 ppm) with and without additional water (50 ppm) at varying potentials (1.0, 0.5, 0.2, and 0.01 V vs Li/Li + ). The impact of additional water on the morphological, (electro)chemical, and structural properties of SEI was studied using microscopic (atomic force microscopy and scanning spreading resistance microscopy) and spectroscopic (X-ray photoelectron spectroscopy, attenuated total reflection Fourier-transform infrared spectroscopy, and time-of-flight secondary ion mass spectrometry) techniques. The SEI exhibits both potential- and water concentration-dependent trends in its morphology and chemical composition. The presence of additional water in the electrolyte causes parasitic reactions, which onset at ~1.0 V, resulting in a reduction of electrolyte components and result in the formation of an insulating, fluorophosphate-rich SEI. In addition, hydrolysis of LiPF 6 creates hydrofluoric acid, which reacts with the surface oxide layer on the Si electrode, leading to a pitted and inhomogeneous SEI structure.

36 MATERIALS SCIENCE↗

Quantification of Inactive Lithium and Solid–Electrolyte Interphase Species on Graphite Electrodes after Fast Charging

Rapid charging of Li-ion batteries is limited by lithium plating on graphite anodes, whereby Li+ ions are reduced to Li metal on the graphite particle surface instead of inserting between graphitic layers, which directly contributes to cell capacity loss because of the low reversibility of the Li plating/stripping process. Furthermore, precisely identifying the onset and amount of Li plating is therefore vital in order to remedy these issues. We demonstrate a titration technique with a detection limit of 20 nmol (5 × 10 –4 mAh) of Li that can be used to quantify inactive Li that remains on the graphite electrode after fast charging. The titration is extended to quantify the total amount of solid carbonate species and lithium acetylide (Li 2 C 2 ) within the solid–electrolyte interphase (SEI), and electrochemical modeling is used to determine the Li plating exchange current density (10 A/m 2 ) and stripping efficiency (65%) of plated Li metal on graphite. These techniques provide a highly accurate measure of the onset of Li plating and quantitative insight into graphite SEI evolution during fast charging.

25 ENERGY STORAGE↗

3D Artificial Solid-Electrolyte Interphase for Lithium Metal Anodes Enabled by Insulator–Metal–Insulator Layered Heterostructures

Despite considerable efforts to prevent lithium (Li) dendrite growth, stable cycling of Li metal anodes with various structures remains extremely difficult due to the direct contact of the liquid electrolyte with Li. Rational design of solid-electrolyte interphase (SEI) for 3D electrodes is a promising but still challenging strategy for preventing Li dendrite growth and avoiding lithium–electrolyte side reactions in Li-metal batteries. Here, a 3D architecture is constructed with g-C 3 N 4 /graphene/g-C 3 N 4 insulator–metal–insulator sandwiched nanosheets to guide uniform Li plating/stripping in the van der Waals gap between the graphene and the g-C 3 N 4 , and the function of which can be regarded as a 3D artificial SEI. Li deposition on the surface of g-C 3 N 4 is suppressed due to its insulating nature. However, its uniform lithiophilic sites and nanopore channels enable homogeneous lithium plating between the graphene and the g-C 3 N 4 , prohibiting the direct contact of the electrolyte with the Li metal. The use of the g-C 3 N 4 -layer-modified 3D anode enables long-term Li deposition with a high Coulombic efficiency and stable cycling of full cells under high cathode loading, limited Li excess, and lean electrolyte conditions. The concept of a 3D artificial SEI will shed light on developing safe and stable Li-metal anodes.

25 ENERGY STORAGE↗

The Chemistry, Formation and Passivation of Solid-Electrolyte Interphase (SEI) from FSI- Breakdown at Li-metal Potential

LiFSI-based liquid electrolytes are promising for realizing high Coulombic efficiency (CE) and long cycle life of next-generation high-energy Li metal battery. Nevertheless, the fundamentals of both the chemistry and formation of solid-electrolyte interphase (SEI) in these electrolytes have remained elusive. Herein, we extensively combine electrochemistry and X-ray photoelectron spectroscopy (XPS) to illustrate the reaction pathways of electrolyte decomposition, especially FSI- breakdown, as well as the dissolution trend of various inorganic SEI components. The SEI-forming reactions at Cu/electrolyte interface manifest a potential (E) dependence, driven by direct electron-transfer (ET) and Li underpotential-deposition (Li UPD) at high and low E regions, respectively. By closely correlating the XPS data obtained with and without solvent washing, we demonstrate that not all the products derived from SEI reactions are incorporated into forming a passivating surface layer, with a notable portion dissolving into liquid electrolyte instead. Importantly, high-CE electrolyte dictated by the chemical identity of solvent, is found to exhibit minimized interfacial reactivity of SEI formation enabling more effective interphasial passivation, via preferential integration of passivating ingredients such as LiF. Overall, this work formulates a systematic understating of bridging the SEI chemistry, formation and passivation while identifying key characteristics of high-performance electrolyte for guiding future design.

Bao, Zhenan [SLAC National Accelerator Laboratory ↗

Knowledge-driven design of solid-electrolyte interphases on lithium metal via multiscale modelling

Abstract Due to its high energy density, lithium metal is a promising electrode for future energy storage. However, its practical capacity, cyclability and safety heavily depend on controlling its reactivity in contact with liquid electrolytes, which leads to the formation of a solid electrolyte interphase (SEI). In particular, there is a lack of fundamental mechanistic understanding of how the electrolyte composition impacts the SEI formation and its governing processes. Here, we present an in-depth model-based analysis of the initial SEI formation on lithium metal in a carbonate-based electrolyte. Thereby we reach for significantly larger length and time scales than comparable molecular dynamic studies. Our multiscale kinetic Monte Carlo/continuum model shows a layered, mostly inorganic SEI consisting of LiF on top of Li 2 CO 3 and Li after 1 µs. Its formation is traced back to a complex interplay of various electrolyte and salt decomposition processes. We further reveal that low local Li + concentrations result in a more mosaic-like, partly organic SEI and that a faster passivation of the lithium metal surface can be achieved by increasing the salt concentration. Based on this we suggest design strategies for SEI on lithium metal and make an important step towards knowledge-driven SEI engineering.

25 ENERGY STORAGE↗

Preventing Electrolyte Decomposition on a Ca Metal Electrode Interface Using an Artificial Solid‐Electrolyte Interphase

Abstract Calcium ion batteries are gaining attention as alternatives to lithium‐ion technology because they offer comparable properties at reduced cost and improved safety. However, progress has been limited because of the inability to efficiently and reversibly plate and strip Ca metal anodes in organic electrolytes. Moreover, the inorganic components of the solid‐electrolyte interphase (SEI) that form via decomposition of the electrolyte often do not allow for the diffusion of Ca ions. In this work, an approach combining density functional theory and ab initio molecular dynamics (AIMD) simulations is utilized to show that the use of a preformed artificial SEI layer of amorphous can potentially prevent electrolyte decomposition. First, Ca is shown to be able to intercalate into an amorphous layer (up to Ca 1.5 Al 2 O 3 ) and diffuse through on a reasonable time scale. Through calculation of the density of states, the system is found to remain insulating up to the equilibrium stoichiometry. Finally, AIMD simulations with a realistic organic electrolyte environment are used to show that this calcinated layer completely prevents the decomposition of solvent molecules. This approach can provide a route to efficient rechargeable Ca ion batteries, paving the way for cheap large‐scale energy storage.

Young, Joshua↗

Salt-rich solid electrolyte interphase for safer high-energy-density Li metal batteries with limited Li excess

We propose a carbonate-based electrolyte optimized with dual cations and ionic liquid for high-efficiency Li metal batteries with a high-voltage cathode. An average coulombic efficiency of Li deposition of 99.6% is achieved due to the salt-rich solid electrolyte interphase and Na guided uniform Li plating. The Li||NCM811 cells can be cycled with limited Li (N/P = 1) over 90 cycles. An additional advantage is that it improves the thermal stability of the NCM811 cathode.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Anion modification for stable solid electrolyte interphase in anode-free lithium metal batteries

The durability of anode-free Li metal batteries is largely limited by the undesired Li plating/stripping irreversibility on the current collector due to the infinite volume change, uncontrollable Li dendrite growth, and continuous parasitic reactions between Li metal and the electrolyte. To address these challenges, the formation of a stable and robust solid electrolyte interphase (SEI) with high ionic conductivity and strong mechanical strength is critical. Here, we developed an advanced electrolyte by introducing LiNO 3 into the localized high concentration electrolyte (LHCE) with lithium bis(fluorosulfonyl)imide (LiFSI) salt, 1,2-dimethoxyethane (DME) solvent, and 1,1,2,2-tetrafluoroethyl-2,2,3,3-tetrafluoropropylether (TFTE) diluent to in situ construct a LiF and Li x N y O z co-enriched passivation layer on the Cu current collector. The synergetic effect of high mechanical strength of LiF and high ionic conductivity of Li x N y O z endows the Li metal anode with a high Coulombic efficiency (CE) of 99.35%. In conclusion, in anode-free Li metal pouch cell using LiFePO 4 (LFP) as a cathode holds an exceptionally improved capacity retention under the charging/discharging rate of 1/3 C, demonstrating great promise for developing dendrite-free and safe Li metal batteries.

25 ENERGY STORAGE↗