At least 109 records · Page 6

The nature of dark-etching rims in meteoritic taenite.

Taenite fields when etched develop a cloudy brown rim with approximate compositional limits of 25 and 40% Ni. In iron meteorites this cloudy zone is only a few microns wide, with a sharp, high-Ni edge about 1 micron from the kamacite interface and a diffuse edge several microns from the central plessite. It is always present in irons unless the meteorite has been cosmically or terrestrially reheated. X-ray and electron diffraction of grains scratched from exceptionally larger areas of cloudy taenite in the mesosiderite Estherville show that this etching zone contains a fine exsolution of kamacite. Detailed electron-probe investigations of taenite in Estherville show that there is a step in the M-shaped Ni profile at the sharp, high-Ni edge of the cloudy region, the Ni dropping suddenly from approximately 45 to 42%. It is proposed that exsolution in the cloudy region effectively froze in the Ni profile at that temperature. On subsequent cooling only the clear outer taenite continued to equilibrate with the kamacite matrix, producing the kink in the M profile. Cloudy taenite is therefore a variety of plessite differing from the usual varieties in that it forms at lower temperatures in areas much richer in Ni, and the morphology is not crystallographically oriented. Its absence can provide a sensitive indication of reheating.

Scott, E. R. D.↗

Surface roughness measured by optical signatures

To measure roughness of metal surfaces by nondestructive means direct laser beam at surface and record distribution pattern of intensity of reflected light to obtain optical signature for comparison with calibrated surface. Signature of machined surface with scratch compared to that of regularly-patterned machined surface may also detect imperfections.

Salvinski, R. J.↗

Inspection of transparent surfaces using photosensitive paper

Window surface is laid flat on top of photosensitive paper. Opposite side of glass is covered by black cloth. Window edges are then illuminated by light flash through fiber optics. Exposed paper is processed and inspected. Paper shows scratches, bubbles, dust particles, and fingerprints on glass surface.

Minton, F. R.↗

Low scatter lens design/development

The criteria for the optimum design of optical systems are discussed along with the selection of appropriate materials. The construction details of low scatter lens systems are tabulated. Scattering analysis; total energy diffracted; and computation of delta for a scratch, bubble, and microscopic irregularities are also discussed.

Gallipeau, R. B.↗

Surface topographical effects on the structural growth of thick sputtered metal and alloy coatings

Thick sputtered S-Monel, silver, and 304 stainless steel coatings were deposited on mica and metal substrates with various surface finishes to investigate the structural growth of the coating by scanning electron microscopy. The geometry and the surface structure of the nodules are characterized. Compositional changes within the coating were analyzed by X-ray dispersion microscopy. Defects in the surface finish (i.e., scratches, inclusions, etc.) act as preferential nucleation sites and form isolated and complex nodules and various surface overgrowths in the coating. The nodule boundaries are very vulnerable to chemical etching and these nodules do not disappear after full annealing. Further, they have undesirable effects on mechanical properties; cracks are initiated at the nodules when the coating is stressed by mechanical forces. These effects are illustrated by micrographs. Nodular growth within a coating can be minimized or eliminated by reducing the surface roughness.

Spalvins, T.↗

Growth defects in thick ion-plated coatings

Industrial ion plating conditions were selected to deposit metallic coatings such as copper, gold, and chromium 2 micrometer thick on metal and glass substrates. The surface finishes of 304 stainless steel, copper, and brass were utilized with mechanically and electrolytically polished surfaces. Nodular growth occurred in these coatings during ion plating as revealed by scanning electron microscopy. Surface irregularities such as scratches, steps, ledges, and so forth are responsible for outward growth, the typical cone type, whereas surface contaminants and loosely settled foreign particles are responsible for lateral growth; namely, the extreme localized surface outgrowths. These defect crystallographic features create porosity in the coatings when subjected to stresses and strains.

Spalvins, T.↗

Morphological growth of sputtered MoS2 films

Sputtered MoS2 films from 300 A to 20,000 A thick were deposited on metal and glass surfaces. The substrate effects such as surface temperature, finish, pretreatment and chemistry as they affect the film formation characteristics were investigated by optical, electron transmission, electron diffraction, and scanning electron microscopy. Substrate temperature and surface chemistry were found to be the prime variables as to the formation of a crystalline or amorphous film. The friction characteristics are strictly influenced by the type of film formed. Surface chemistry and surface pretreatment account for compound formation and corresponding grain growth, which directly affect the adhesion characteristics, resulting in poor adherence. The type of surface finish (topography) as related to scratches, impurities, inhomogeneities, etc., are favorable nucleation sites for the growth of isolated and complex nodules within the film, and various complex surface overgrowths on the film. These nodular growth features have progressively more undesirable effects on the film behavior as the film thickness increases.

Spalvins, T.↗

Nodular growth in thick-sputtered metallic coatings

Thick-sputtered S-Monel, silver, and 304 stainless steel coatings were deposited on mica and metal substrates with various surface finishes to investigate the nodular growth in the coating by scanning electron microscopy. The geometry and the surface structure of the nodules are characterized. Compositional changes within the coating were analyzed by energy dispersive X-ray analysis. Defects in the surface finish (i.e., scratches, inclusions, etc.), act as preferential nucleation sites and form isolated and complex nodules and various surface overgrowths in the coating. The nodule boundaries are very vulnerable to chemical etching and these nodules do not disappear after full annealing. Further, they have undesirable effects on mechanical properties; cracks are initiated at the nodules when the coating is stressed by mechanical forces. These effects are illustrated by micrographs. Nodular growth within a coating can be minimized or eliminated by increasing the surface smoothness.

Spalvins, T.↗

Dynamics of solid lubrication as observed by optical microscopy

A bench metallograph was converted into a micro contact imager by the addition of a tribometer employing a steel ball in sliding contact with a glass disk. The sliding contact was viewed in real time by means of projection microscope optics. The dynamics of abrasive particles and of solid lubricant particles within the contact were observed in detail. The contact was characterized by a constantly changing pattern of elastic strain with the passage of surface discontinuities and solid particles. Abrasive particles fragmented upon entering the contact, embedded in one surface and scratched the other; in contrast, the solid lubricant particles flowed plastically into thin films. The rheological behavior of the lubricating solids gave every appearance of a paste-like consistency within the Hertzian contact.

Sliney, H. E.↗

Morphological growth of sputtered MoS2 films

Sputtered MoS2 films from 300 A to 20,000 A thick were deposited on metal and glass surfaces. The substrate effects such as surface temperature, finish, pretreatment, and chemistry as they affect the film formation characteristics were investigated by optical, electron transmission, electron diffraction, and scanning electron microscopy. Substrate temperature and surface chemistry were found to be the prime variables as to the formation of a crystalline or amorphous film. The friction characteristics are strictly influenced by the type of film formed. Surface chemistry and surface pretreatment account for compound formation and corresponding grain growth, which directly affect the adhesion characteristics, resulting in poor adherence. Scratches, impurities, inhomogeneities, etc., are favorable nucleation sites for the growth of isolated and complex nodules within the film.

Spalvins, T.↗

Dynamics of solid lubrication as observed by optical microscopy

A bench metallograph was converted into a 'micro contact imager' by the addition of a tribometer employing a steel ball in sliding contact with a glass disk. The sliding contact was viewed in real time by means of projection microscope optics. The dynamics of abrasive particles and of solid lubricant particles within the contact were observed in detail. The contact was characterized by a constantly changing pattern of elastic strain with the passage of surface discontinuities and solid particles. Abrasive particles fragmented upon entering the contact, embedded in one surface and scratched the other; in contrast, the solid lubricant particles flowed plastically into thin films. The rheological behavior of the lubricating solids gave every appearance of a paste-like consistency within the Hertzian contact.

Sliney, H. E.↗

Boron trifluoride coatings for plastics

Tough, durable coatings of boron triflouride can be deposited on plastic optical components to protect them from destructive effects of abrasion, scratching, and environment. Coating material can be applied simultaneously with organic polymers, using plasma glow-discharge methods, or it can be used as base material for other coatings to increase adhesion.

Kubacki, R. M.↗

Window flaw detection by backscatter lighting

Portable fiber-optic probe detects tiny flaws in transparent materials. Probe transmits light through surface to illuminate interior of material by backscattering off its edges. Light-sensitive contact paper records scratch pattern. Technique can be used for rapid visual checks. Flexible fiber optics are safely used in explosive or flammable areas; they present no hazard of breakage or contamination in controlled environments.

Crockett, L. K.↗

Precision cleaver for "soft" crystals

"Soft" crystals are cleaved as thin 0.005 inch with special cleaver. Thin slices of soft crystalline materials are used in X-ray spectrometers. Slices are usually cut by hand with wire or blade. Wire tends to scratch surface and to produce slices of nonuniform thickness. Device will rapidly cut soft crystals in smooth, thin, uniform slices.

Benedicto, J. S. J.↗

SDMS: A scientific data management system

SDMS is a data base management system developed specifically to support scientific programming applications. It consists of a data definition program to define the forms of data bases, and FORTRAN-compatible subroutine calls to create and access data within them. Each SDMS data base contains one or more data sets. A data set has the form of a relation. Each column of a data set is defined to be either a key or data element. Key elements must be scalar. Data elements may also be vectors or matrices. The data elements in each row of the relation form an element set. SDMS permits direct storage and retrieval of an element set by specifying the corresponding key element values. To support the scientific environment, SDMS allows the dynamic creation of data bases via subroutine calls. It also allows intermediate or scratch data to be stored in temporary data bases which vanish at job end.

Massena, W. A.↗

Repairing sealing surfaces on aluminum castings

Approach using stylus nickel plating instead of copper and cadmium plating has simplified repair procedure. Damaged sealing surfaces are stylus nickelplated in one step. Superficial scratches and porous areas are removed more easily from repaired surface by simply lapping sealing areas to required finish. Although method is aimed for aerospace components, it may be easily incorporated into conventional aluminumcasting technology. One-step repair can be considered for cast-aluminum automobile and aircraft engines to reduce time and costs.

Hanna, T. L.↗

Fatigue behavior of two alloys for Space Shuttle applications

Two superalloys used extensively in the Space Shuttle main engine are Incoloy 903 and Inconel 718. The fatigue behavior of the two alloys under varying conditions is considered. Three heats of Incoloy 903 and two of Inconel 718 were used in the study. Material was tested in several conditions, including mill polish, longitudinal mill polish, transverse mill polish, chemically milled, chemically milled plus shotpeened on one side and on both sides, gas tungsten arc welded, and electron beam welded. Both round and flat tensile specimens were tested in universal test machines. It was found that surface condition influences test results. Transverse scratches resulting from polishing and rougher surfaces lower the stress at runout in relation to that obtained on longitudinally polished and/or smooth-surfaced specimens.

Adsit, N. R.↗

Segmentation, dynamic storage, and variable loading on CDC equipment

Techniques for varying the segmented load structure of a program and for varying the dynamic storage allocation, depending upon whether a batch type or interactive type run is desired, are explained and demonstrated. All changes are based on a single data input to the program. The techniques involve: code within the program to suppress scratch pad input/output (I/O) for a batch run or translate the in-core data storage area from blank common to the end-of-code+1 address of a particular segment for an interactive run; automatic editing of the segload directives prior to loading, based upon data input to the program, to vary the structure of the load for interactive and batch runs; and automatic editing of the load map to determine the initial addresses for in core data storage for an interactive run.

Tiffany, S. H.↗