Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “rapid solidification”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Weld solidification cracking in 304 to 304L stainless steel

A series of annulus welds were made between 304 and 304L stainless steel coaxial tubes using both pulsed laser beam welding (LBW) and pulsed gas tungsten arc welding (GTAW). In this application, a change in process from pulsed LBW to pulsed gas tungsten arc welding was proposed to limit the possibility of weld solidification cracking since weldability diagrams developed for GTAW display a greater range of compositions that are not crack susceptible relative to those developed for pulsed LBW. Contrary to the predictions of the GTAW weldability diagram, cracking was found. This result was rationalized in terms of the more rapid solidification rate of the pulsed gas tungsten arc welds. In addition, for the pulsed LBW conditions, the material compositions were predicted to be, by themselves, 'weldable' according to the pulsed LBW weldability diagram. However, the composition range along the tie line connecting the two compositions passed through the crack susceptible range. Microstructurally, the primary solidification mode (PSM) of the material processed with higher power LBW was determined to be austenite (A), while solidification mode of the materials processed with lower power LBW apparently exhibited a dual PSM of both austenite (A) and ferrite-austenite (FA) within the same weld. The materials processed by pulsed GT A W showed mostly primary austenite solidification, with some regions of either primary austenite-second phase ferrite (AF) solidification or primary ferrite-second phase austenite (FA) solidification. This work demonstrates that variations in crack susceptibility may be realized when welding different heats of 'weldable' materials together, and that slight variations in processing can also contribute to crack susceptibility.

36 MATERIALS SCIENCE↗

Microstructural development in DED stainless steels: applying welding models to elucidate the impact of processing and alloy composition

Austenitic stainless steel microstructures produced by directed energy deposition (DED)are analogous to those developed during welding, particularly high energy density welding. To better understand microstructural development during DED, theories of microstructural evolution,which have been established to contextualize weld microstructures, are applied in this study to microstructural development in DED austenitic stainless steels. Phenomenological welding models that describe the development of oxide inclusions, compositional microsegregation, ferrite,matrix austenite grains, and dislocation substructures are utilized to clarify microstructural evolution during deposition of austenitic stainless steels. Two different alloys, 304L and 316L, arecompared to demonstrate the broad applicability of this framework for understanding microstmctural development during the DED process. Despite differences in grain morphology and solidification mode for these two alloys (which can be attributed to compositional differences),similar tensile properties are achieved. It is the fine-scale compositional segregation and dislocation structures that ultimately determine the strength of these materials. The evolution of microsegregation and dislocation structures is shown to be dependent on the rapid solidification and thermomechanical history of the DED processing method and not the composition of the starting material.

36 MATERIALS SCIENCE↗

Cascading microstructures in aluminum-steel interfaces created by impact welding

With the rising need to develop light weight structures joining dissimilar metals is inevitable. Thus a fundamental understanding of the microstructure evolution and bond formation mechanism is necessary. In this work we probe the welded interface in aluminum and steel joined using vaporizing foil actuator welding (VFAW) a novel impact welding process. The goal of such a detailed characterization campaign is to understand the bond formation mechanism. The study demonstrates that the interfacial microstructure has a pronounced hierarchical nature. At the macro scale, the interface is characterized by a wavy interface which is a result of extensive plastic deformation that accompanies the process. Detailed transmission electron microscopy shows evidence for the formation of a liquid film at the interface resulting in significant inter diffusion of Fe. The solidified structure at the interface consisted of crystalline α-Al and an amorphous metastable Al-Fe intermetallic compound similar to the observations in rapid solidification of Al-Fe alloys. The sub-nm scale characterization of the interface using atom probe tomography showed two distinct zones 1. A magnesium (5 at.%) and oxygen (15 at.%) rich (not detectable using energy dispersive spectroscopy) which was probably from the decomposition of the surface oxide film 2. The rapidly solidified reaction zone consisting of primary crystalline α-Al and an amorphous Al-Fe (15 at.%)-O (0.5 at.%)-Si (1.5 at.%).Based on these observations a mechanism for the bond formation is presented.

36 MATERIALS SCIENCE↗

Laser‐Powder Melt Pool Solidification Dynamics and Microstructural Engineering of Ti‐5553 Microlattices

The fine geometric and topological control afforded by additive manufacturing technologies has enabled the manufacture of architected materials across length scales, and enabling tunable mechanical performance as a function of local and global design. Progress has been made to tune the mechanical response of architected materials through geometry, but understanding how the geometry and processing conditions will inform the microstructure remains a challenge due to the rapid solidification in laser powder bed fusion. This study uses in situ X-ray imaging and electron backscatter diffraction microscopy to demonstrate that the melt pool size, microstructure morphology, and elastic strain distribution is influenced by a combination of lattice geometry and laser processing conditions. These results indicate that within larger melt pools the local thermal gradients are sufficient to enable a columnar-to-equiaxed transition across the melt pool. Furthermore, the solidification mechanisms producing these microstructures are examined across the first 5 ms of melting and solidification, described via in situ high-speed X-ray imaging and mirrored via multiphysics simulation.

additive manufacturing↗

Microstructure and Hard Magnetic Properties of Sm 1-x Zr x (Fe,Co) 11.3-y Ti 0.7 By Ingots and Thick Melt-Spun Ribbons

Permanent magnets made from Sm(Fe,Co) 12 -based compounds are being actively pursued through nanostructuring and powder metallurgy. This study was aimed at the development of hard magnetic properties in bulk as-cast alloys and in melt-spun alloys for very low wheel speeds. Slower solidification rates and alloying with Zr promote the tetragonal ThMn 12 -type crystal structure, whereas higher solidification rates and alloying with B replace the ThMn 12 structure type with the TbCu 7 structure type. When introduced simultaneously, Zr and B dramatically reduce the alloy solidification rates required for both the refinement of the 1:12 crystallites and their replacement with the 1:7 phase. In bulk arc-melted alloys, this allowed for a microstructure of separated 1:12 crystallites 1–3 μm in size, although, because of the ferromagnetic nature of a minority phase, the coercivity of these fine-grained alloys reached only 0.73 kOe. A moderately accelerated solidification further refined the 1:12 crystallites and increased the coercivity; a Sm 0.7 Zr 0.4 (Fe,Co) 10.8 Ti 0.7 B 0.5 alloy exhibited a coercivity of 1.5 kOe and a maximum energy product of 3.4 MGOe when it was melt-spun into a 0.26-mm-thick ribbon. A more rapid solidification suppressed the 1:12 phase and after annealing at 800–850 °C, the alloys modified with Zr and B developed reasonably high coercivity and maximum energy product even when melt-spun at a wheel speed of 6 m/s. For the above-mentioned alloy, these values were 4.1 kOe and 7.8 MGOe, respectively. Further, a similarly processed very-Sm-lean Sm 0.5 Zr 0.6 (Fe,Co) 10.6 Ti 0.7 B 0.7 alloy exhibited a remanence of 8.8 kG and an energy product of 7.4 MGOe.

36 MATERIALS SCIENCE↗

In Situ X-ray Radiography and Computational Modeling to Predict Grain Morphology in $\beta$-Titanium during Simulated Additive Manufacturing

The continued development of metal additive manufacturing (AM) has expanded the engineering metallic alloys for which these processes may be applied, including beta-titanium alloys with desirable strength-to-density ratios. To understand the response of beta-titanium alloys to AM processing, solidification and microstructure evolution needs to be investigated. In particular, thermal gradients (Gs) and solidification velocities (Vs) experienced during AM are needed to link processing to microstructure development, including the columnar-to-equiaxed transition (CET). In this work, in situ synchrotron X-ray radiography of the beta-titanium alloy Ti-10V-2Fe-3Al (wt.%) (Ti-1023) during simulated laser-powder bed fusion (L-PBF) was performed at the Advanced Photon Source at Argonne National Laboratory, allowing for direct determination of Vs. Two different computational modeling tools, SYSWELD and FLOW-3D, were utilized to investigate the solidification conditions of spot and raster melt scenarios. The predicted Vs obtained from both pieces of computational software exhibited good agreement with those obtained from in situ synchrotron X-ray radiography measurements. The model that accounted for fluid flow also showed the ability to predict trends unobservable in the in situ synchrotron X-ray radiography, but are known to occur during rapid solidification. A CET model for Ti-1023 was also developed using the Kurz–Giovanola–Trivedi model, which allowed modeled Gs and Vs to be compared in the context of predicted grain morphologies. Both pieces of software were in agreement for morphology predictions of spot-melts, but drastically differed for raster predictions. The discrepancy is attributable to the difference in accounting for fluid flow, resulting in magnitude-different values of Gs for similar Vs.

36 MATERIALS SCIENCE↗

Gas atomized precursor alloy powder for oxide dispersion strengthened ferritic stainless steel

Gas atomization reaction synthesis (GARS) was employed as a simplified method for producing precursor powders for oxide dispersion strengthened (ODS) ferritic stainless steels (e.g., Fe-Cr-Y-(Ti,Hf)-O), departing from the conventional mechanical alloying (MA) process. During GARS processing a reactive atomization gas (i.e., Ar-O 2 ) was used to oxidize the powder surfaces during primary break-up and rapid solidification of the molten alloy. This resulted in envelopment of the powders by an ultra-thin (t < 150 nm) metastable Cr-enriched oxide layer that was used as a vehicle for solid-state transport of O into the consolidated microstructure. In an attempt to better understand the kinetics of this GARS reaction, theoretical cooling curves for the atomized droplets were calculated and used to establish an oxidation model for this process. Subsequent elevated temperature heat treatments, which were derived from Rhines pack measurements using an internal oxidation model, were used to promote thermodynamically driven O exchange reactions between trapped films of the initial Cr-enriched surface oxide and internal Y-enriched intermetallic precipitates. This novel microstructural evolution process resulted in the successful formation of nano-metric Y-enriched dispersoids, as confirmed using high energy X-ray diffraction and transmission electron microscopy (TEM), equivalent to conventional ODS alloys from MA powders. The thermal stability of these Y-enriched dispersoids was evaluated using high temperature (1200°C) annealing treatments ranging from 2.5 to 1,000 hrs of exposure. In a further departure from current ODS practice, replacing Ti with additions of Hf appeared to improve the Y-enriched dispersoid thermal stability by means of crystal structure modification. Additionally, the spatial distribution of the dispersoids was found to depend strongly on the original rapidly solidified microstructure. To exploit this, ODS microstructures were engineered from different powder particle size ranges, illustrating microstructural control as a function of particle solidification rate. The consolidation of ultra-fine powders (dia. ≤ 5μm) resulted in a significant reduction in dispersoid size and spacing, consistent with initial scanning electron microscopy studies on as-atomized cross-sectioned particles that suggested that these powders solidified above the threshold velocity to effectively solute trap Y within the α-(Fe,Cr) matrix. Interestingly, when the solidification velocity as a function of particle size was extracted from the aforementioned theoretical particle cooling curves, it could be offered as supporting evidence for these microstructure observations. Thermal-mechanical treatments also were used to create and evaluate the stability of a dislocation substructure within these alloys, using microhardness and TEM analysis of the alloy sub-grain and grain structure. Moreover, elevated temperature tensile tests up to 800°C were used to assess the initial mechanical strength of the ODS microstructure.

36 MATERIALS SCIENCE↗

Effects of Solidification Cooling Rates on Microstructures and Physical Properties of Fe-6.5%Si Alloys

Compared to the widely used Fe-3.2wt%Si steel, Fe-6.5wt%Si has superior electric and magnetic properties, including higher electrical resistivity, lower iron loss, higher permeability, and near zero magnetostriction. However, Fe-6.5wt%Si sheet is difficult to produce using traditional manufacturing processes as the high silicon content favors the formation of ordered phases that embrittle the material. Fortunately, these ordered phases can be suppressed if the alloy is cooled fast enough from a high temperature kinetically trapping the disordered solid solution or amorphous state. Planar flow casting is known for its rapid solidification rate. In order to consider it as a viable method to manufacture ductile Fe-6.5wt%Si sheets, the effect of cooling rate on physical properties of Fe-6.5wt%Si alloy are systematically investigated. In this work, various cooling rates are achieved by changing melt-spin wheel speeds, which significantly affect the solidification temperature profile and have profound effects on ordering, microstructures, textures, hardness, and magnetic properties. High cooling rates result in refined grains, reduced ordering, enhanced <100> out of the plane texture, decreased hardness, and increased coercivity. This study demonstrates a critical cooling rate at ~1.7 × 10 5 K/s, corresponding to a tangential wheel speed of 5-7 m/s, below which the hardness significantly increases in agreement with the sudden increase of the ordered phases that causes the material embrittlement.

36 MATERIALS SCIENCE↗

Nanoscale interfacial melting enables bonding during high velocity microparticle impacts

Melting during high-velocity particle impact has been understood to be typically detrimental to bonding by lowering the strength at the interface and promoting rebound before solidification can occur. Here we establish a possible remedy to this challenge: by dramatically restricting the volume of molten material, its resolidification is accelerated, effectively forming a nanoscale, braze-type joint during impact. In-situ single particle impact imaging is combined with post-mortem structural and chemical analyses to reveal a regime where adhesion is governed not by extensive plastic deformation, but by the kinetics of melt layer resolidification. Furthermore, these findings redefine the role of melting in impact-based processes, establishing transient melting and rapid solidification as a viable strategy for engineering successful adhesion events.

Additive manufacturing↗

Laser Intensity Profile Effects on the Solidification Microstructure of Ti-6Al-4V and Ti-5553

Traditional machining of Ti-6Al-4V and Ti-5Al-5Mo-5V-3Cr (Ti-5553) is challenging due to high chemical reactivity, adiabatic shear band formation, and material cost. Titanium is attractive because of its high tensile strength, low density, corrosion resistance, and ability to withstand extreme temperatures. Selective Laser Melting (SLM) is capable of manufacturing geometrically complicated parts at a lower expense. Exceptional tolerances can be obtained with properly tuned processing parameters. Alterations on scan parameters permit microstructure and melt pool control. Single track laser melting experiments were performed on Ti-6Al-4V and Ti- 5553 using elliptical intensity profiles. Results show that maintaining constant energy density but increasing power results in a melt pool failing to penetrate the substrate for Ti-5553. Increasing laser energy density increases melt pool width and can increase powder bed denudation. Comparing Ti64 and Ti-5553 microstructures contributes to a better understanding of rapid solidification in titanium.

36 MATERIALS SCIENCE↗

Localized orientation gradients in additively manufactured stainless steel 316H structures

The high solidification rates during additive manufacturing cause highly localized thermal and strain gradients. The effect of these gradients on the evolution of local orientation misorientations within a grain is not well understood. In this study, stainless steel 316H parts were fabricated via laser powder bed fusion using three different energy densities: 43, 71, and 135 J/mm 3 . Electron backscatter diffraction showed that the maximum misorientations of the grains can be up to 25° along the build direction. Misorientation gradients (RM g ) within grains are process-dependent and can change from 0.036°/μm to 0.015°/μm with increased volumetric energy densities. In conclusion, the characterized misorientation gradients are an indication of the level of dislocations and, to an extent, the plastic deformation resulting from the rapid solidification during laser powder bed fusion.

316H↗

Refining Microstructures in Additively Manufactured Al/Cu Gradients Through TiB 2 Inclusions

Here, the additive manufacture of compositionally graded Al/Cu parts by laser engineered net shaping (LENS) is demonstrated. The use of a blue light build laser enabled deposition on a Cu substrate. The thermal gradient and rapid solidification inherent to selective laser melting enabled mass transport of Cu up to 4 mm from a Cu substrate through a pure Al deposition, providing a means of producing gradients with finer step sizes than the printed layer thicknesses. Divorcing gradient continuity from layer or particle size makes LENS a potentially enabling technology for the manufacture of graded density impactors for ramp compression experiments. Printing graded structures with pure Al, however, was prevented by the growth of Al 2 Cu 3 dendrites and acicular grains amid a matrix of Al 2 Cu. A combination of adding TiB 2 grain refining powder and actively varying print layer composition suppressed the dendritic growth mode and produced an equiaxed microstructure in a compositionally graded part. Material phase was characterized for crystal structure and nanoindentation hardness to enable a discussion of phase evolution in the rapidly solidifying melt pool of a LENS print.

36 MATERIALS SCIENCE↗

Microstructure Development of 308L Stainless Steel During Additive Manufacturing

$In$ $situ$ high-energy X-ray diffraction measurements were completed during deposition of 308L stainless steel wire onto a 304L stainless steel substrate. Attempts were made to extract microstructural features such as phase fraction and internal stress, as well as temperature evolution immediately following the deposition. The limited data that could be collected during deposition and rapid solidification are critically examined. High-energy X-rays coupled with relatively slow detectors were utilized to enable determination of orientation-dependent lattice parameters accurately enough to comment on phase strain evolution between austenite and ferrite. Here, information about the hydrostatic and deviatoric stress states of the constituent phases was determined on time scales that are relevant to their development. However, the time resolution of the technique was insufficient to monitor phase evolution during the solid–solid phase transformation and, more so, during solidification. Moreover, the accurate and absolute determination of inherently statistical parameters, such as phase fraction, depends critically on the ability to sample a statistically significant numbers of grains in the microstructure.

36 MATERIALS SCIENCE↗

High-Temperature Properties and Microstructural Stability of the AISI H13 Hot-Work Tool Steel Processed by Selective Laser Melting

The microstructural stabilities, softening resistance, and high-temperature tensile properties of the H13 hot-work tool steel by selective laser melting (SLM) were systematically studied. A series of tempering procedures were performed on the as-SLMed specimens. Afterwards, the mechanism of softening resistance behavior was discussed based on the XRD, SEM, EBSD observations, hardness measurements, and high-temperature tensile tests. It was found that the as-SLMed H13 consisted of α-iron and γ-iron. The carbide-stabilizing elements aggregated as the cell-like substructures for the rapid solidification of the SLM process. After the softening resistance treatment, the retained austenite transformed to ferrite and carbide mixtures. The cell-like substructures dissolved slowly into the matrix when the temperature was below 550 °C. These factors increased the hardness and retarded the softening of the material. When the temperature was 600 °C, the microstructural constituents transformed to soft ferrite and globular carbides, which lead to a considerable decrease of the hardness. Due to the grain refinement, solid solution strengthening, and residual stress, the as-SLMed H13 exhibited better mechanical properties than that of the wrought counterparts.

36 MATERIALS SCIENCE↗

Tribological Performance of Ni{sub 3}Al Matrix Self-Lubricating Composites Containing Multilayer Graphene Prepared by Additive Manufacturing

In order to improve tribological performance of Ni{sub 3}Al-based alloy, Ni{sub 3}Al matrix composites containing 1.5 wt.% multilayer graphene (MLG) are prepared through additive manufacturing (AM) and spark plasma sintering (SPS), which are denoted as NMAM and NMSPS, respectively. Tribological behaviors of NMAM and NMSPS against Si{sub 3}N{sub 4} balls are researched under constant speed (0.2 m/s) and varied loads (from 4 to 16 N) for evaluating the tribological properties of NMAM and NMSPS. The results present that NMAM exhibits the excellent tribological properties [low friction coefficients (0.26-0.40) and considerable wear resistance (2.8-4.6 × 10{sup −5} mm{sup 3} N{sup −1} m{sup −1})] as compared to NMSPS, which attributes to the uniform enrichment of MLG with properties of high tensile strength and being easily sheared off on the worn surfaces. Owing to the use of spherical prealloyed powder containing multilayer graphene and the characteristics of layer by layer depositing in the AM process, NMAM has a more compact and uniform substrate, which persistently provides a source of the formation of continuous and stable frictional layer. Due to the characteristics of AM rapid solidification, NMAM has the small grain size and well-compacted microstructure, which can effectively reduce the probability of spalling wear and lead to the increase in wear resistance of materials. The research can offer the reference for self-lubricating materials prepared by AM technology.

36 MATERIALS SCIENCE↗

Processing Parameter Effects on Residual Stress and Mechanical Properties of Selective Laser Melted Ti6Al4V

Selective laser melting (SLM) process is characterized by large temperature gradients resulting in high levels of residual stress within the additively manufactured metallic structure. SLM-processed Ti6Al4V yields a martensitic microstructure due to the rapid solidification and results in a ductility generally lower than a hot working equivalent. Post-process heat treatments can be applied to SLM components to remove in-built residual stress and improve ductility. Residual stress buildup and the mechanical properties of SLM parts can be controlled by varying the SLM process parameters. This investigation studies the effect of layer thickness on residual stress and mechanical properties of SLM Ti6Al4V parts. This is the first-of-its kind study on the effect of varying power and exposure in conjunction with keeping the energy density constant on residual stress and mechanical properties of SLM Ti6Al4V components. It was found that decreasing power and increasing exposure for the same energy density lowered the residual stress and improved the % elongation of SLM Ti6Al4V parts. Increasing layer thickness resulted in lowering the residual stress at the detriment of mechanical properties. The study is based on detailed experimental analysis along with finite element simulation of the process using ABAQUS to understand the underlying physics of the process.

36 MATERIALS SCIENCE↗

Microstructure and Work Hardening Behavior of Micro-plasma Arc Welded AISI 316L Sheet Joint

The aim of this research is to investigate the microstructural changes and work hardening behavior of AISI 316L 0.5-mm-thick sheet due to micro-plasma arc welding. AISI 316L similar sheets were welded in single-pass square butt joint configuration. The microstructure in the fusion zone typically contains a variety of complex δ-ferrite-austenitic structure, which significantly increased hardness value compared to the base material because of rapid solidification of the weld pool. Systematic tensile test was performed to investigate strain rate sensitivity of the welded joint under quasi-static loading conditions. The multistage work hardening behavior was determined by Kocks–Mecking (K–M) model and differential Crussard–Jaoul analysis. In both the cases, stage III work hardening behavior and stage IV work hardening behavior were observed. The stress–strain curves of welded specimen at different strain rates were analyzed in terms of Hollomon, Ludwik and Swift equations to determine work hardening exponent values. The welded joints were ruptured in the transition zone of heat affected and fusion zones. The fractographic observation exhibited variation in dimple and void density over strain rate from 0.0001 to 0.0015 s{sup −1}.

36 MATERIALS SCIENCE↗

The Application of Canned Deformation to a Hard-Deformed Spray-Deposited Al-Zn-Mg-Cu Alloy

A wide variety of industrial applications require Al-Zn-Mg-Cu alloys with high strength and ductility. However, Zn-rich Al-Zn-Mg-Cu alloys prepared by rapid solidification methods usually show excellent strength but poor formability, which restricts their wide application in complex forming. In this study, we developed a new deformation method for the spray-deposited Zn-rich Al-Zn-Mg-Cu alloy to avoid crack formation and achieve isotropic properties. The microstructure evolution and crystallographic textures were analyzed and compared with the results of a normal deformation process. Crack-free forgings with the ultimate tensile strength (UTS), yield strength (YS) and elongation of 727 ± 5 MPa, 690 ± 3 MPa, 5.0 ± 0.7% along the radial direction and 735 ± 2 MPa, 693 ± 3 MPa, 6.3 ± 0.2% along the tangential direction were finally obtained. The improvement in the mechanical properties can be attributed to the larger amount of subgrains and substructures generated in the canned deformed alloy. The results of this study show excellent advantages and potential application prospects of the canned deformation to hard-deformed Al-Zn-Mg-Cu alloys.

36 MATERIALS SCIENCE↗