Collision Welding of Dissimilar Materials by Vaporizing Foil Actuator: A Breakthrough Technology for Dissimilar Metal Joining

This work demonstrated and further developed Vaporizing Foil Actuator Welding (VFAW) as a viable technique for dissimilar-metal joining for automotive lightweighting applications. VFAW is a novel impact welding technology, which uses the pressure developed from electrically-assisted rapid vaporization of a thin aluminum foil (the consumable) to launch and ultimately collide two of more pieces of metal to create a solid-state bond between them. 18 dissimilar combinations of automotive alloys from the steel, aluminum and magnesium alloy classes were screened for weldability and characterized by metallography of weld cross sections, corrosion testing, and mechanical testing. Most combinations, especially a good number of Al/Fe pairs, were welded successfully. VFAW was even able to weld combinations of very high strength materials such as 5000 and 6000 series aluminum alloys to boron and dual phase steels, which is difficult to impossible by other joining techniques such as resistance spot welding, friction stir welding, or riveting. When mechanically tested, the samples routinely failed in a base metal rather than along the weld interface, showing that the weld was stronger than either of the base metals. As for corrosion performance, a polymer-based protective coating was used to successfully combat galvanic corrosion of 5 Al/Fe pairs through a month-long exposure to warm salt fog. In addition to the technical capabilities, VFAW also consumes little energy compared to conventional welding techniques and requires relatively light, flexible tooling. Given the technical and economic advantages, VFAW can be a very competitive joining technology for automotive lightweighting. The success of this project and related activities has resulted in substantial interest not only within the research community but also various levels of automotive supply chain, which are collaborating to bring this technology to commercial use.

36 MATERIALS SCIENCE↗

Low Activation Joining of SiC/SiC Composites for Fusion Applications

The use of SiC composites in fusion environments may require joining of plates using reactive joining or brazing. One promising reactive joining method is the use of solid-state displacement reactions between Si and TiC to produce Ti3SiC2 + SiC. We continue to explore the processing envelope for this type of joint for the TITAN collaboration to produce the best possible joints to undergo irradiation studies in HFIR. The TITAN collaboration has designed miniature torsion joints for preparation, testing, and irradiation in HFIR. As part of that project PNNL synthesized 40 miniature torsion joints and several were tested for shear strength prior to irradiation testing in HFIR. The resulting tests indicated that joint fixture alignment problems cause joint strengths to be lower than optimal but that several joints that were well aligned had high shear strengths and promising mechanical properties. High joint strengths cause non-planar shear fracture and complicate strength analysis for these miniature torsion joints.

36 MATERIALS SCIENCE↗

Low Activation Joining of SiC/SiC Composites for Fusion Applications: Miniature Torsion Specimen Shear Testing

The use of SiC composites in fusion environments likely requires joining of plates using reactive joining or brazing. One promising reactive joining method uses solid-state displacement reactions between Si and TiC to produce Ti3SiC2 + SiC. We continue to explore the processing envelope for this joint for the TITAN collaboration in order to produce optimal joints to undergo irradiation studies in HFIR. The TITAN collaboration has designed miniature torsion joints for preparation, testing, and irradiation in HFIR. PNNL synthesized 40 miniature torsion joints and several were tested for shear strength prior to irradiation testing in HFIR. The resulting tests indicated that (1) joint fixture alignment problems cause joint strengths to be lower than optimal, (2) that non-planar torsion test failures limit the effectiveness of the miniature specimen design, and (3) that several joints that were well aligned had high shear strengths and promising mechanical properties. In summary, we now show conclusively that high joint strengths cause non-planar shear fracture and complicate strength analysis for miniature torsion specimens.

36 MATERIALS SCIENCE↗

Low Activation Joining of SiC/SiC Composites for Fusion Applications

The use of SiC composites in fusion environments likely requires joining of plates using reactive joining or brazing. One promising reactive joining method uses solid-state displacement reactions between Si and TiC to produce Ti3SiC2 + SiC. We continue to explore the processing envelope for this joint for the Titan collaboration in order to produce optimal joints to undergo irradiation studies in HFIR. The TITAN collaboration has designed miniature torsion joints for preparation, testing, and irradiation in HFIR. PNNL synthesized 40 miniature torsion joints and several were tested for shear strength prior to irradiation testing in HFIR. The resulting tests indicated that 1) joint fixture alignment problems cause joint strengths to be lower than optimal, 2) that non-planar torsion test failures may limit the effectiveness of the miniature specimen design, and 3) that several joints that were well aligned had high shear strengths and promising mechanical properties. In summary, it appears that high joint strengths cause non-planar shear fracture and complicate strength analysis for miniature torsion specimens.

Displacement Reaction↗

Low Activation Joining of SiC/SiC Composites for Fusion Applications: Modeling Miniature Torsion Tests with Elastic and Elastic-Plastic Models

The international fusion community designed miniature torsion specimens for joint testing and irradiation in test reactors with limited irradiation volumes since SiC and SiC-composites used in fission or fusion environments require joining methods for assembling systems. Torsion specimens fail out-of-plane when joints are strong and when elastic moduli are comparable to SiC, which causes difficulties in determining shear strengths for many joints or for comparing unirradiated and irradiated joints. A finite element damage model was developed to treat elastic joints such as SiC/Ti3SiC2+SiC and elastic-plastic joints such as SiC/epoxy and steel/epoxy. The model uses constitutive shear data and is validated using epoxy joint data. The elastic model indicates fracture is likely to occur within the joined pieces to cause out-of-plane failures for miniature torsion specimens when a certain modulus and strength ratio between the joint material and the joined material exists. Lower modulus epoxy joints always fail in plane and provide good model validation.

Damage Mechanics↗

Joining of High Strength Low Ductility AA7055 by Friction Self-piercing Rivet

High strength aluminum (Al) alloy is one of higher specific strength materials for decarbonization in transportation industries. Because of low ductility at room temperature, conventional mechanical fastening such as self-piercing riveting produces cracks at the joint. In this work, we applied friction self-piercing riveting to join Al alloy (AA) 7055. No cracks were observed in the joints because of the improved local ductility of Al alloy by the generated frictional heat during joining step. Numerical modeling of joining process was applied to guide rivet geometry design and rivet material strength. Mechanical integrity of the AA7055 joints was assessed by lap shear tensile and cross-tension testing. Metallurgical characterizations revealed solid-state bonding formed not only between the rivet and surround Al materials, but also upper and lower Al sheets at the joint interface. Both solid-state bonding and mechanical interlocking between the flared rivet and bottom AA7055 sheet were the major joint mechanisms.

Lim, Yong Chae↗

High speed butt joining of 1” thick 2139-T8

Thick plate (=1”) butt joining of Al alloys is challenging due to high tool forces, uneven material flow, and heat distribution in the through-thickness direction. Tool design and welding parameters used for executing thick plate butt joining have remained mostly static over the past decade. Reported welding speeds that produce viable joint strength (mostly on 6xxx alloys) typically range below 100 mm/min (4inches /min). Researchers at Pacific Northwest National Laboratory (PNNL) in association with Ground Vehicle Systems Center (US Army GVSC) have been working to demonstrate greater joining efficiency at higher welding speeds in a 1” thick AA2139-T8 plate. Using innovative tool features and effective force and temperature control a joint efficiency of 80% was demonstrated at a welding speed of 7 inches /min (178mm/min).

Das, Hrishikesh↗

Joining of Thermoset Carbon Fiber Reinforced Polymer and AZ31 Magnesium Alloy Sheet Via Friction Stir Interlocking

A new technique called friction stir interlocking (FSI) was applied for lap-joining of AZ31 magnesium sheet and thermoset carbon fiber reinforced polymer (TS-CFRP) sheet. Instead of directly joining AZ31 and TS-CFRP, a series of magnesium interlocks were used to friction stir weld with AZ31 sheet to enable joining with TS-CFRP. Microstructural characterization of joint cross sections showed that a tool rotation rate of 800 rpm produced incomplete mixing of magnesium interlocks and the top AZ31 sheet, while 1200 rpm achieved sufficient material mixing to avoid unwelded regions. Mechanical property characterization showed that AZ31/TS-CFRP dissimilar joints failed through the magnesium interlock shanks during lap shear tensile testing, with a maximum normalized joint strength reaching ~100 MPa.

Wang, Tianhao↗

Joining AA7099 to Ni-Cr-Mo Steel Using Single Pass Friction Stir Dovetailing and AA6061 Butter Layer

A novel single pass friction stir dovetailing (FSD) was developed to join thick plate AA7099 to Ni-Cr-Mo steel in a lap configuration through the use of an AA6061 butter layer. The butter layer approach can be shown to significantly reduce interfacial failures by inhibiting the formation of brittle Fe–Al intermetallic compounds (IMCs) which are typically formed during conventional friction stir welding (FSW) of AA7099 directly to steel. This study evaluates the strength and microstructural evolution of the aluminum/steel joint interface between single pass FSD of AA7099/AA6061(butter)/steel fabricated using three different FSD tool configurations. The butter layer was achieved by placement of a free-floating strip of AA6061 within the dovetail groove that was pre-machined in the steel substrate. Friction stir welding was then used to simultaneously join the thick plate AA7099, the AA6061 strip and the AA7099 in a single weld pass. To optimize the joining process, three different pin geometries (full thread, half smooth/half thread, no thread) were evaluated; it was demonstrated that the half smooth/half thread tool produced the strongest weld joint due to the absence of a Zn rich layer at the Al/steel interface. The efficacy of this unique processing technique was tested using lap shear tensile testing as well as high resolution transmission electron microscopy (TEM). A discussion of the new FSD technique, joint configurations, and process parameters are provided along with joint microstructural analyses and mechanical performance.

Olszta, Matthew J.↗

Pol I DNA polymerases stimulate DNA end-joining by Escherichia coli DNA ligase

Highlights: • Pol I DNA polymerases stimulate E. coli DNA ligase activity. • End-joining activity is enhanced by up to 600%, nick closure is slightly enhanced. • T4 ligase is not similarly effected. Klenow and Klentaq are the large fragment domains of the Pol I DNA polymerases from Escherichia coli and Thermus aquaticus, respectively. Herein, we show that both polymerases can significantly stimulate complementary intermolecular end-joining ligations by E.coli DNA ligase when the polymerases are present at concentrations lower than that of the DNA substrates. In contrast, high polymerase concentrations relative to the DNA substrates inhibit the intermolecular ligation activity of DNA ligase. Neither polymerase was able to stimulate the DNA ligase from T4 bacteriophage. Additionally, nick-closure by E. coli DNA ligase (but not T4 ligase) is slightly stimulated by both polymerases, but only at about 10% of the magnitude seen for end-joining enhancement. The data represent one of the first observations of direct polymerase-ligase interactions in prokaryotes, and suggest that the polymerases stabilize the associated DNA ends during intermolecular ligation, and that such a complex can be taken advantage of by some, but not all, DNA ligases.

60 APPLIED LIFE SCIENCES↗

In vivo gene correction with targeted sequence substitution through microhomology-mediated end joining

Highlights: • A novel microhomology mediated end joining (MMEJ) gene correction method was tested. • MMEJ resulted in precise targeted sequence substitution (TSS) in vitro and in vivo. • MMEJ-TSS showed superior efficiency than homology-directed repair (HDR) in vitro. • MMEJ-TSS resulted in the survival of mice model of hereditary tyrosinemia in vivo. • MMEJ-TSS could overcome the limitations of HDR for gene therapy. Genome editing technology using programmable nucleases has rapidly evolved in recent years. The primary mechanism to achieve precise integration of a transgene is mainly based on homology-directed repair (HDR). However, an HDR-based genome-editing approach is less efficient than non-homologous end-joining (NHEJ). Recently, a microhomology-mediated end-joining (MMEJ)-based transgene integration approach was developed, showing feasibility both in vitro and in vivo. We expanded this method to achieve targeted sequence substitution (TSS) of mutated sequences with normal sequences using double-guide RNAs (gRNAs), and a donor template flanking the microhomologies and target sequence of the gRNAs in vitro and in vivo. Our method could realize more efficient sequence substitution than the HDR-based method in vitro using a reporter cell line, and led to the survival of a hereditary tyrosinemia mouse model in vivo. The proposed MMEJ-based TSS approach could provide a novel therapeutic strategy, in addition to HDR, to achieve gene correction from a mutated sequence to a normal sequence.

60 APPLIED LIFE SCIENCES↗

Characterization of intermetallics in aluminum to zinc coated interstitial free steel joining by pulsed MIG brazing for automotive application

In order to meet the demand for lighter and more fuel efficient vehicles, a significant attempt is currently being focused toward the substitution of aluminum for steel in the car body structure. It generates vital challenge with respect to the methods of joining to be used for fabrication. However, the conventional fusion joining has its own difficulty owing to formation of the brittle intermetallic phases. In this present study AA6061-T6 of 2 mm and HIF-GA steel sheet of 1 mm thick are metal inert gas (MIG) brazed with 0.8 mm Al–5Si filler wire under three different heat inputs. The effect of the heat inputs on bead geometry, microstructure and joint properties of MIG brazed Al-steel joints were exclusively studied and characterized by X-ray diffraction, field emission scanning electron microscopy (FESEM), electron probe micro analyzer (EPMA) and high resolution transmission electron microscopy (HRTEM) assisted X-ray spectroscopy (EDS) and selective area diffraction pattern. Finally microstructures were correlated with the performance of the joint. Diffusion induced intermetallic thickness measured by FESEM image and concentration profile agreed well with the numerically calculated one. HRTEM assisted EDS study was used to identify the large size FeAl{sub 3} and small size Fe{sub 2}Al{sub 5} type intermetallic compounds at the interface. The growth of these two phases in A2 (heat input: 182 J mm{sup −1}) is attributed to the slower cooling rate with higher diffusion time (~ 61 s) along the interface in comparison to the same for A1 (heat input: 155 J mm{sup −1}) with faster cooling rate and shorter diffusion time (~ 24 s). The joint efficiency as high as 65% of steel base metal is achieved for A2 which is the optimized parameter in the present study. - Highlights: • AA 6061 and HIF-GA could be successfully joined by MIG brazing. • Intermetallics are exclusively studied and characterized by XRD, FESEM and EPMA. • Intermetallic formation by diffusion is worth considering or not. • HRTEM-EDS, SAD pattern identifies the morphologies and size of intermetallics. • A compromise concerning formation of IMC is necessary.

36 MATERIALS SCIENCE↗

A governing parameter for the melting phenomenon at nanocontacts by Joule heating and its application to joining together two thin metallic wires

For cutting and joining extremely thin metallic wires, the issue of Joule heating in the wires is considered. The middle of a section of a thin Pt wire with a diameter of about 800 nm was melted locally by a direct current supply, and the wire was cut at a predetermined point by applying a force to shear the molten part of the wire. Furthermore, a constant current was applied to a system in which the free ends of two Pt wires were contacted, and the wires were joined together. A parameter, which governs the melting phenomenon at the point of contact of very thin wires, is proposed. It was verified that the conditions required for joining thin wires were able to be determined by the parameter that depends on the applied current, the length and cross sectional area of the wires, and a function of the geometrical quantities for calibrating the thermal conditions.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Nanostructure evolution in joining of Al and Fe nanoparticles with femtosecond laser irradiation

The joining of Al-Fe nanoparticles (NPs) by femtosecond (fs) laser irradiation is reported in this paper. Fe and Al NPs were deposited on a carbon film in vacuum via fs laser ablation. Particles were then exposed to multiple fs laser pulses at fluences between 0.5 and 1.3 mJ/cm{sup 2}. Transmission Electron Microscopy (TEM) and Electron Diffraction X-ray observations indicate that Al and Fe NPs bond to each other under these conditions. For comparison, bonding of Al to Al and Fe to Fe NPs was also investigated. The nanostructure, as observed using TEM, showed that individual Al NPs were monocrystalline while individual Fe NPs were polycrystalline prior to joining and that these structures are retained after the formation of Al-Al and Fe-Fe NPs. Al-Fe NPs produced by fs laser joining exhibited a mixed amorphous and crystalline phase at the interface. Bonding is suggested to originate from intermixing within a region of high field intensity between particles.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Self-healing of cracks in Ag joining layer for die-attachment in power devices

Sintered silver (Ag) joining has attracted significant interest in power devices modules for its ability to form stable joints with a porous interconnection layer. A function for the self-healing of cracks in sintered porous Ag interlayers at high temperatures is discovered and reported here. A crack which was prepared on a Ag joining layer was closed after heating at 200 °C in air. The tensile strength of pre-cracked Ag joining layer specimens recovers to the value of non-cracked specimens after heating treatment. Transmission electron microscopy (TEM) was used to probe the self-healing mechanism. TEM images and electron diffraction patterns show that a large quantity of Ag nanoparticles formed at the gap with the size less than 10 nm, which bridges the crack in the self-healing process. This discovery provides additional motivation for the application of Ag as an interconnection material for power devices at high temperature.

36 MATERIALS SCIENCE↗

Bonding Energy of Silicon and Sapphire Wafers at Elevated Temperatures of Joining

The hydrophilicity of surfaces and the bonding energy of silicon and sapphire wafers at the temperature of joining 50°C are studied. It is established that heating of the Si and Al{sub 2}O{sub 3} wafers to 50°C is accompanied by an increase in the degree of hydrophilicity of the wafer surfaces. The effect is attributed to improvement in the surface purity due to the desorption of impurity atoms into vacuum and to an increase in the density of dangling bonds. It is found that the bonding energy of silicon and sapphire wafers joined at a temperature of 50°C and upon further heating in the range 100–250°C is higher compared to the bonding energy of wafers joined at room temperature. The activation energy of the growth of the bonding energy is determined. It is found that this activation energy is 0.57 eV.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Mitigating Corrosion in Mg Sheet in Conjunction with a Sheet-Joining Method that Satisfies Structural Requirements within Sub-assemblies

This work was undertaken as a LightMAT project funded by the DOE-Vehicles Technology Office. The goal of this work was to develop corrosion protection strategies that simultaneously mitigate corrosion and achieve Class-A surface finish for Mg components in automotive applications. While automotive metals such as steel and aluminum are protected against corrosion through a variety of coating schemes/packages, the efficacy of these existing coating schemes for Mg and Mg- joints is not clear and needs to be determined. Therefore, five commercially available coating schemes and two joining techniques (riveting and Arplas resistance spot welding) were evaluated. The corresponding individual Mg sheet coupons or Mg/Mg joint test coupons were provided by Magna that were then corrosion tested at PNNL using ASTM B117 procedure. The microstructures and mechanical properties of the coupons were analyzed to determine the effectiveness of the joining and corrosion mitigation strategies. Of the coating schemes evaluated, Henkel Bonderite MgC 2.0 pre-treatment + E-coat showed the best corrosion protection and surface finish for individual Mg coupons and Arplas resistance spot welded coupons. However, the strength of Mg/Mg welded joint was reduced after corrosion testing due to some corrosion at the weld nugget. Mg/Mg rivet joints in conjunction with Chemetall oxisilan pre-treatment + polyurethane coating showed good corrosion resistance and some discoloration on the surface finish. Coating schemes comprising pre-treatment with Alodine 5200 + E-coat or Bonderite 1455 + polyurethane coating, in conjunction with Al rivet joints, showed significant corrosion and extensive discoloration of the surface. We anticipate that the results from this work will provide useful guidance to the automotive industry in selecting the appropriate combinations of corrosion protection coatings and joining techniques to fabricate light-weight Mg-based automotive components.

36 MATERIALS SCIENCE↗

High Velocity Joining of Multi-material Stacks Containing 3rd Generation Advanced High-Strength Stainless Steel and Aluminum Extrusion and Casting (Abstract)

Advanced lightweight materials, including multi-phase steels, aluminum extrusions and aluminum castings, have increasingly replaced mild steel to meet original equipment manufacturer (OEM) demand for increased fuel economy and crash-safety requirements. Third Generation (Gen 3) AHSS provides a superior combination of strength and ductility for crash energy management components in the vehicle body-in-white (BIW). Aluminum extrusions are widely used for bumper, door rocker panel, cradle and battery frame applications. Aluminum castings are increasingly being used in electric vehicles to provide part consolidation, weight saving and increased driving range. Rocker panels are, for example, an important component of the battery electric vehicle (BEV) body structure. The rocker panel serves several purposes, including structural support, crash resistance, protection for the vehicle's underbody and battery tray, and contributing to the overall aesthetics. In order to reduce weight, rocker panels are usually constructed using outer panels consisting of 3rd generation advanced high strength steels (AHSS) and an inner multicell aluminum extrusion structure for energy absorption which protects the batteries in a crash event. It is well known, however, that these material combinations provide significant challenges for joining and are susceptible to liquid metal embrittlement and loss of strength. The overall goal is to find a solution that addresses these challenges in order to produce multi-material vehicle components with reduced weight and minimal galvanic and recyclability issues. The approach being proposed here is to utilize a novel high velocity (HiVe) riveting and clinching technique recently demonstrated by Pacific Northwest National Laboratory (PNNL) to join (2T/3T) sheets of aluminum alloys and steel. This process will not only address the aforementioned challenges but also help significantly reduce the joining cycle time. This work will also demonstrate use of HiVe assemblies to be retrofitted to existing body-shop robots thus having minimal impact to existing body shop operations.

36 MATERIALS SCIENCE↗