Effect of Molecular Weight and Layer Thickness on Dielectric Breakdown Strength of Neat and Homopolymer Swollen Lamellar Block Copolymer Films
Designing next-generation lightweight pulsed power devices hinges on understanding the factors influencing the energy storage performance of dielectric materials. Polymer dielectric films have a quadratic dependence of energy storage on the voltage breakdown strength and strategies to enhance the breakdown strength are expected to yield a path toward high energy storage densities. Highly stratified lamellar block copolymer (L-BCP) films of model polystyrene-b-polymethylmethacrylate (PS-b-PMMA) exhibited as much as ~50% enhancement in breakdown voltage (E BD ), (225 % increase in stored energy density, U~ E BD 2 ), compared to unordered as-cast L-BCP films. Such an energy density using amorphous polymer is on par with industry-standard semi-crystalline biaxially oriented polypropylene (BOPP), and as such a notable development in the field. This work develops a deeper understanding of the molecular mechanisms of E BD enhancement in L-BCP films, due to combination of interface formation and spatial isolation of the chain ends into segregated zones. We further confirm the role of chain ends in the breakdown process blending a low M n L-BCP with matched M n homopolymers to attain same layer spacing as neat L-BCP of higher M n . E BD shows a significant decrease at low homopolymer fractions due to increased net chain end density within swollen ordered L-BCP domains in wet-brush regime, followed by increased E BD due to layer thickness increase via segregated “interphase layer” formation by excess homopolymers. Notably, E BD of homopolymer swollen L-BCPs is always lower than neat L-BCP of the same domain spacing, due to overall adverse chain ends contribution from homopolymers. These findings provide important selection rules for L-BCPs for designing next-generation flexible electronics with high energy density solid-state BCP film capacitors.