Compositional tuning of atomic layer deposited MgZnO for thin film transistors
Thin film transistors (TFTs) have been fabricated using magnesium zinc oxide (MgZnO) layers deposited by atomic layer deposition at 200 °C. The composition of the MgZnO is systematically modified by varying the ratio of MgO and ZnO deposition cycles. A blue-shift of the near band-edge photoluminescence after post-deposition annealing at 300 °C indicates significant activation of the Mg dopant. A 7:1 ratio of ZnO:MgO deposition cycles was used to fabricate a device with a TFT channel width of 2000 μm and a channel length of 60 μm. This transistor yielded an effective saturation mobility of 4 cm{sup 2}/V s and a threshold voltage of 7.1 V, respectively. The on/off ratio was 1.6×10{sup 6} and the maximum interface state density at the ZnO/SiO{sub 2} interface is ∼6.5×10{sup 12} cm{sup −2}.