Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “WEAR”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Interaction of sulfuric acid corrosion and mechanical wear of iron

Friction and wear experiment were conducted with elemental iron sliding on aluminum oxide in aerated sulfuric acid at concentrations ranging from very dilute (0.00007 N; i.e., 4 ppm) to very concentrated (96 percent acid). Load and reciprocating sliding speed were kept constant. With the most dilute acid concentration of 0.00007 to 0.0002 N, a complex corrosion product formed that was friable and often increased friction and wear. At slightly higher concentrations of 0.001 N, metal losses were essentially by wear alone. Because no buildup of corrosion products occurred, this acid concentration became the standard from which to separate metal loss from direct corrosion and mechanical wear losses. When the acid concentration was increased to 5 percent (1 N), the well-established high corrosion rate of iron in sulfuric acid strongly dominated the total wear loss. This strong corrosion increased to 30 percent acid and decreased somewhat to 50 percent acid in accordance with expectations. However, the low corrosion of iron expected at acid concentrations of 65 to 96 percent was not observed in the wear area. It was apparent that the normal passivating film was being worn away and a galvanic cell established that rapidly attacked the wear area. Under the conditions where direct corrosion losses were highest, the coefficient of friction was the lowest.

Rengstorff, G. W. P.↗

Ignition of a Combustible Atmosphere by Incandescent Carbon Wear Particles

A study was made to determine whether carbon wear particles from carbon elements in sliding contact with a metal surface were sufficiently hot to cause ignition of a combustible atmosphere. In some machinery, electric potential differences and currents may appear at the carbon-metal interface. For this reason the effect of these voltages and currents on the ability of carbon wear particles to cause ignition was evaluated. The test specimens used in the investigation were carbon vanes taken from a fuel pump and flat 21-inch-diameter 2 metal disks (440-C stainless steel) representing the pump housing. During each experiment a vane was loaded against a disk with a 0.5-pound force, and the disk was rotated to give a surface speed of 3140 feet per minute. The chamber of the apparatus that housed the vane and the disk was filled with a combustible mixture of air and propane. Various voltages and amperages were applied across the vane-disk interface. Experiments were conducted at temperatures of 75, 350, 400, and 450 F. Fires were produced by incandescent carbon wear particles obtained at conditions of electric potential as low as 106 volts and 0.3 ampere at 400 F. Ignitions were obtained only with carbon wear particles produced with an electric potential across the carbon-vane-disk interface. No ignitions were obtained with carbon wear particles produced in the absence of this potential; also, the potential difference produced no ignitions in the absence of carbon wear particles. A film supplement showing ignition by incandescent wear particles is available.

Buckley, Donald H.↗

Friction and Wear Properties of Selected Solid Lubricating Films: Magnetron-Sputtered and Plasma-Assisted, Chemical-Vapor-Deposited Diamondlike Carbon Films - Part 3

To evaluate commercially developed dry solid film lubricants for aerospace bearing applications, an investigation was conducted to examine the friction and wear behavior of magnetron-sputtered diamondlike carbon (MS DLC) and plasma-assisted, chemical-vapor-deposited diamondlike carbon (PACVD DLC) films in sliding contact with 6-mm-diameter American Iron and Steel Institute (AISI) 440C stainless steel balls. Unidirectional sliding friction experiments were conducted with a load of 5.9 N (600 g), a mean Hertzian contact pressure of 0.79 GPa (maximum Hertzian contact pressure of L-2 GPa), and a sliding velocity of 0.2 m/s. The experiments were conducted at room temperature in three environments: ultrahigh vacuum (vacuum pressure, 7x10(exp -7) Pa), humid air (relative humidity, approx.20 percent), and dry nitrogen (relative humidity, <1 percent). The resultant films were characterized by scanning electron microscopy, energy-dispersive x-ray spectroscopy, and surface profilometry. Marked differences in the friction and wear of the DLC films investigated herein resulted from the environmental conditions. The main criteria for judging the performance of the DLC films were coefficient of friction and wear rate, which had to be less than 0.3 and on the order of 10(exp -6) cu mm/N-m or less, respectively. MS DLC films and PACVD DLC films met the criteria in humid air and dry nitrogen but failed in ultrahigh vacuum, where the coefficients of friction were greater than the criterion, 0.3. In sliding contact with 440C stainless steel balls in all three environments the PACVD DLC films exhibited better tribological performance (i.e., lower friction and wear) than the MS DLC films. All sliding involved adhesive transfer of wear materials: transfer of DLC wear debris to the counterpart 440C stainless steel and transfer of 440C stainless steel wear debris to the counterpart DLC film.

Miyoshi, Kazuhisa↗

Microstructure and wear characterization of aluminum matrix composites reinforced with industrial waste fly ash particulates synthesized by friction stir processing

Fly ash (FA) is a waste product of coal combustion in thermal power plants which is available in massive quantities all over the world causing land pollution. This paper reports the characterization of AA6061 aluminum matrix composites (AMCs) reinforced with FA particles synthesized using friction stir processing (FSP). The volume fraction of FA particles was varied from 0 to 18 in steps of 6. The prepared AMCs were characterized using optical microscopy (OM), scanning electron microscopy (SEM) and electron backscattered diagram (EBSD). The wear rate was estimated using a pin-on-disc wear apparatus. FA particles were observed to be distributed homogeneously in the AMC irrespective of the location within the stir zone. The EBSD micrographs revealed remarkable grain refinement in the AMC. The incorporation of FA particles enhanced the microhardness and wear resistance of the AMC. The strengthening mechanisms of the AMC were discussed and correlated to the observed microstructures. The wear mechanisms were identified by characterizing the wear debris and worn surfaces. - Highlights: •Industrial waste fly ash was used to produce aluminum matrix composites. •Friction stir processing was used to produce AA6061/Fly Ash composite. •Fly ash particles refined the grains of aluminum matrix. •Fly ash particles enhanced the hardness and wear resistance. •Successful utilization of fly ash to make aluminum composites reduces land pollution.

36 MATERIALS SCIENCE↗

Prevention of nanoscale wear in atomic force microscopy through the use of monolithic ultrananocrystaline diamond probes.

Nanoscale wear is a key limitation of conventional atomic force microscopy (AFM) probes that results in decreased resolution, accuracy, and reproducibility in probe-based imaging, writing, measurement, and nanomanufacturing applications. Diamond is potentially an ideal probe material due to its unrivaled hardness and stiffness, its low friction and wear, and its chemical inertness. However, the manufacture of monolithic diamond probes with consistently shaped small-radius tips has not been previously achieved. The first wafer-level fabrication of monolithic ultrananocrystalline diamond (UNCD) probes with <5-nm grain sizes and smooth tips with radii of 30-40 nm is reported, which are obtained through a combination of microfabrication and hot-filament chemical vapor deposition. Their nanoscale wear resistance under contact-mode scanning conditions is compared with that of conventional silicon nitride (SiN{sub x}) probes of similar geometry at two different relative humidity levels ({approx}15 and {approx}70%). While SiN{sub x} probes exhibit significant wear that further increases with humidity, UNCD probes show little measurable wear. The only significant degradation of the UNCD probes observed in one case is associated with removal of the initial seed layer of the UNCD film. The results show the potential of a new material for AFM probes and demonstrate a systematic approach to studying wear at the nanoscale.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Microscale wear behavior and crosslinking of PEG-like coatings for total hip replacements

The predominant cause of late-state failure of total hip replacements is wear-mediated osteolysis caused by wear particles that originate from the ultrahigh molecular weight polyethylene (UHMWPE) acetabular cup surface. One strategy for reducing wear particle formation from UHMWPE is to modify the surface with a hydrophilic coating to increase lubrication from synovial fluid. This study focuses on the wear behavior of hydrophilic coatings similar to poly(ethylene glycol) (PEG). The coatings were produced by plasma-polymerizing tetraglyme on UHMWPE in a chamber heated to 40C or 50C. Both temperatures yielded coatings with PEG-like chemistry and increased hydrophilicity relative to uncoated UHMWPE; however, the 40C coatings were significantly more resistant to damage induced by atomic force microscopy nanoscratching. The 40C coatings exhibited only one damage mode (delamination) and often showed no signs of damage after repeated scratching. In contrast, the 50C coatings exhibited three damage modes (roughening, thinning, and delamination), and always showed visible signs of damage after no more than two scratches. The greater wear resistance of the 40C coatings could not be explained by coating chemistry or hydrophilicity, but it corresponded to an approximately 26–32% greater degree of crosslinking relative to the 50C surfaces, suggesting that crosslinking should be a significant design consideration for hydrophilic coatings used for total hip replacements and other wear-dependent applications.

36 MATERIALS SCIENCE↗

Micro-Abrasion Wear Resistance of Borided 316L Stainless Steel and AISI 1018 Steel

The 316L stainless steel has high corrosion resistance but low tribological performance. In different industrial sectors (biomedical, chemical, petrochemical, and nuclear engineering), improvement upon wear resistance of 316L stainless steel components using accessible and inexpensive methods is critical. The AISI 1018 steel is widely used in industry, but its tribological performance is not the best among steels. Therefore, in this study the behavior of the borided 316L stainless steel and 1018 steel is evaluated under micro-abrasion wear. The boriding was carried out at 1223 K over 6 h of exposure time, resulting in a biphase layer composed of FeB/Fe{sub 2}B phases. In order to evaluate Fe{sub 2}B phase with no influence from FeB phase, AISI 1018 steel samples were borided at 1273 K for over 20 min and then diffusion annealed at 1273 K over 2 h to obtain a Fe{sub 2}B mono-phase layer. Micro-abrasion wear resistance was evaluated by a commercial micro-abrasion testing rig using a mix of F-1200 SiC particles with deionized water as abrasive slurry. The obtained wear rates for FeB and Fe{sub 2}B phases and for the 316L stainless steel were compared. Wear resistance of 316L stainless steel increases after boriding. The wear mechanisms for both phases and for the stainless steel were identified. Also, transient conditions for rolling and grooving abrasion were determined for the FeB and Fe{sub 2}B phases.

36 MATERIALS SCIENCE↗

Surface Modification by Friction Stir Processing of Low-Carbon Steel: Microstructure Investigation and Wear Performance

A low-carbon steel sheet with a thickness of 5 mm was subjected to friction stir processing (FSP) by one to four different passes. The microstructures of different regions were characterized using the optical microscopy and electron backscatter diffraction. The Vickers micro-harness was measured at the distance of 200 μm below the processed surfaces. The influence of pass numbers (PNs) on wear resistance was studied in terms of coefficients of friction (CoFs), weight losses and wear rates. SEM topographies of the worn surfaces were also studied to evaluate the wear mechanisms. Microstructure observations showed that Widmänstatten ferrite plates were formed in stir zones (SZs) and heat affected zones. As PN increased, these grains were widened due to the increment of the carbon diffusivity and lengthened because of the high heat input and microstructure anisotropy. Besides, increasing the PN causes increasing of the hardness and wear resistance, simultaneously. Specifically, the wear rate in the SZ was reduced from 2.8 × 10{sup −2} mm{sup 3} m{sup −1} in base metal to 0.3 × 10{sup −2} mm{sup 3} m{sup −1} in sample which was subjected to 4 FSP passes. However, variation in PN had no considerable effect on CoFs. Oxidative wear mechanism was observed on the worn surface of the steel and the FSPed samples while more debris was formed by increasing the PNs.

36 MATERIALS SCIENCE↗

Microstructure and Wear Resistance of FeCrBSi Plasma-Sprayed Coating Remelted by Gas Tungsten Arc Welding Process

Herein, an FeCrBSi coating was fabricated via plasma spray on AISI1045 steel, and subsequently, a gas tungsten arc welding (GTA) process was employed to remelt the coating. The microstructure, microhardness, fracture toughness and surface roughness of the coating before and after remelting were investigated, as well as the wear resistance was tested by a UMT-3-type sliding wear apparatus. The results showed that, upon remelting, most defects in the as-sprayed coating were effectively eliminated, the surface roughness decreased by 43%, and the coating–substrate interface bonding changed from mechanical to metallurgical. The phase composition of the as-sprayed coating was primarily α-Fe and a small amount of hard Fe{sub 3}B phase, while the remelted coating consisted of α-Fe and (Fe,Cr){sub 23}C{sub 6} and a small quantity of CrB. In addition, remelting the coating was found to induce a 287.6% increase in the fracture toughness, a 33.4% increase in the average microhardness, and a 47.5% decrease in the wear volume, while the failure mechanism changed from abrasive wear to fatigue wear upon remelting. Therefore, GTA remelting of plasma-sprayed coating was found to be a feasible method to obtain a coating with good wear resistance.

36 MATERIALS SCIENCE↗

Improving Corrosion Resistance and Corrosive Wear Resistance of Aluminum Alloy Drill Pipe by Surface Nanocrystallization and Micro-arc Oxidation

To improve the corrosion and wear resistance performance of aluminum alloy drill pipes in geological and petroleum drilling applications, a strengthening coating was prepared on the surface of the 2618 aluminum alloy by combining treatment with ultrasonic cold forging technology (UCFT) and micro-arc oxidation (MAO). The effects of the strengthening coating on the corrosion and wear resistance of the aluminum alloy were evaluated by electrochemical and tribological tests. The results demonstrated that the corrosion and wear resistance of the aluminum alloy were improved by the UCFT and MAO technologies, especially the salt corrosion resistance. The corrosion morphology of the strengthening coating primarily included pitting, micro-cracks and NaCl attachment. In addition, the UCFT + MAO composite coating exhibited the best wear performance. The wear rate of the UCFT + MAO composite coating was lower than that of the aluminum alloy by 94%. The results provided support for this excellent surface treatment technology for the corrosion and wear resistance of aluminum alloy drill pipes, and they also present a feasible evaluation method for drill pipes.

36 MATERIALS SCIENCE↗

Friction and Wear Behavior of TiAl Matrix Composites Incorporated with Silver and Molybdenum Disulfide

TiAl matrix composites incorporated with silver (Ag) and molybdenum disulfide (MoS{sub 2}) are investigated to identify the improved friction and wear behavior over a wide temperature range. The results show that the excellent friction-reducing and anti-wear properties are obtained by the incorporation of Ag and MoS{sub 2}, and the composite with 8 wt.% Ag and 4 wt.% MoS{sub 2} exhibits the lowest friction coefficients and wear rates under all testing temperatures. Such phenomenon is attributed to the adaptive-lubricating action of Ag and MoS{sub 2} as the temperature changes. Specifically, Ag and MoS{sub 2} are responsible for the improvements in friction and wear performance within 300 °C; MoS{sub 2}, MoO{sub 3} and Ag{sub 2}MoO{sub 4} are be beneficial to the decrease in friction coefficient and wear rate at 500 °C; Ag{sub 2}MoO{sub 4} plays a supporting role in obtaining favorable frictional capability and good wear resistance at 700 °C.

36 MATERIALS SCIENCE↗

Sliding Wear of Spark Plasma Sintered CrFeCoNiCu High-Entropy Alloy Coatings: Effect of Aluminum Addition

High-entropy alloys (HEAs) are considered as attractive coating materials due to their high hardness, good wear and corrosion resistance. Al{sub x}CrFeCoNiCu (x = 0, 1, 2, 3) high-entropy alloy coatings were fabricated on carbon steel substrate using spark plasma sintering. The microstructure evolved from FCC to FCC–BCC mixed structure. Al{sub 3}CrFeCoNiCu coating possesses an average hardness of approximately 682 HV{sub 0.2}, which is the highest hardness in all of the HEA coatings. The dry sliding wear behavior of the HEA coatings was investigated using a ball-on-disk sliding tribo-meter with a silicon nitride ball. In all of the HEA coatings, Al{sub 3}CrFeCoNiCu presents the lowest wear rate 8.81 × 10{sup −5} mm{sup 3} m{sup −1} and Al{sub 2}CrFeCoNiCu has the lowest coefficient of friction 0.195 during 1000 m sliding distance at 0.1 m s{sup −1} sliding velocity under 20 N normal load. Comparing with AISI 52100 steel, spark plasma sintered Al{sub 2}CrFeCoNiCu and Al{sub 3}CrFeCoNiCu HEA coatings exhibit outstanding sliding wear resistance and extremely low friction coefficient. The wear resistance of Al{sub 3}CrFeCoNiCu HEA coating is approximately four times better than the bearing steel, showing a promising application as a wear-resistant material.

36 MATERIALS SCIENCE↗

Effect of Oxygen Content on Wear and Cutting Performance of AlCrON Coatings

In this work, AlCrON coatings with various oxygen contents were deposited by multi-arc-ion plating technology. The effects of oxygen content on the microstructure, mechanical properties, wear and cutting performance of AlCrON coatings were investigated. The result showed that the O contents in the AlCrON coatings increased from 0 to 8.8 wt.% by changing the O{sub 2}/N{sub 2} flow ratios during the deposition process. The AlCrON coatings mainly included fcc-CrN and fcc-AlN phases, and the Al{sub 2}O{sub 3} and Cr{sub 2}O{sub 3} were also confirmed by the XPS results. Addition of oxygen improved the adhesion strength of AlCrON coatings. The AlCrON coating with 4.0 wt.% oxygen content showed the low surface roughness, low friction coefficient and the minimum wear rate. Cutting results also showed that addition of oxygen improved the service life of AlCrON coatings under various cutting conditions. The service life of AlCrON coatings increased firstly and then decreased with increasing oxygen contents, and the AlCrON coating with 4.0 wt.% oxygen content had the maximum cutting length under various cutting conditions, which might be due to the decrease of surface roughness, increase of adhesion strength and hardness. The wear mechanism involved in cutting process included abrasive wear, adhesive wear and oxidation wear.

36 MATERIALS SCIENCE↗

Effects of Co{sub 3}O{sub 4} Addition on Friction and Dry Sliding Wear Characteristics of 8 mol% Yttria-Stabilized Cubic Zirconia

The aim of the present study was to investigate the influence of Co{sub 3}O{sub 4} additive on the microstructure, wear, and tribological properties of 8 mol% yttria-stabilized cubic zirconia (8YSZ) using a pin-on-disk tribometer, surface profilometer, hardness tester, and a scanning electron microscopy system. Specimens were produced by doping 1-15 wt.% Co{sub 3}O{sub 4} in 8YSZ using a colloidal process, sintering at 1500 °C for 1 h, and subsequent annealing at 1500 °C for 10 and 50 h. Microstructural analysis showed that Co{sub 3}O{sub 4} dissolved partially in 8YSZ, with the undissolved Co{sub 3}O{sub 4} precipitating as a secondary phase at the grain boundaries. Further, the addition of Co{sub 3}O{sub 4} enhanced the grain size. Wear tests were carried out using an Al{sub 2}O{sub 3} ball as the counterface against ceramic disk under dry sliding friction conditions at room temperature (24 °C). The wear volume of 8YSZ decreased from 0.30 to 0.11 mm{sup 3} as a result of the addition of 15 wt.% Co{sub 3}O{sub 4}. Additionally, friction coefficient of the 8YSZ significantly reduced from 0.55 to 0.17 at the beginning stage of the sliding after the addition of 15 wt.% Co{sub 3}O{sub 4}. This was because Co{sub 3}O{sub 4} creates a thin lubricating layer on the friction surface. In addition, the undoped and Co{sub 3}O{sub 4}-doped 8YSZ specimens exhibited abrasive wear under the dry sliding friction conditions, owing to the formation and propagation of microcracks, which resulted in the removal of material from the surface. The specific wear rate of 8YSZ decreased with increasing the Co{sub 3}O{sub 4} content. Thus, the addition of Co{sub 3}O{sub 4} to 8YSZ improves its wear resistance and surface topography.

36 MATERIALS SCIENCE↗

Microstructures and Impact Wear Behavior of Al-Alloyed High-Mn Austenitic Cast Steel After Aging Treatment

The microstructural evolution and impact wear behavior of Al-alloyed ultra-high-Mn austenitic cast steel were investigated after different heat treatments, including quenching (Q) and quenching + aging (Q + A). Another ultra-high-Mn austenitic cast steel without Al was compared under the same experimental condition. After Q + A, Al addition contributed to the precipitation of κ-carbides which improves the yield strength and wear resistance of the austenite matrix. However, the mechanical properties and wear resistance of the Al-free steel were strongly deteriorated due to the precipitation of plate-like M{sub 3}C-type carbides, as well as the worn surface of the Al-free steel had the feature of micro-scratches. After Q + A (2 h), the Al-alloyed steel obtained optimal wear resistance and the main wear feature was strain fatigue. But, excessive aging time (4 h) would lead to a large fragile peeling from the worn surface and the wear resistance was decreased. Also, the worn subsurface microstructures with different heat treatments were observed by transmission electron microscopy (TEM). These results show that the deformation microstructures of the Al-free steel contained stacking faults, dislocation tangle and deformation twins. The deformation character of Al-alloyed steel is dominated by planar glide, and with increase in the aging time, planar dislocation substructures gradually evolved, relating to dislocation pileups, Taylor lattices and micro-bands.

36 MATERIALS SCIENCE↗

Wear Resistance and Tribological Features of Ultra-Fine-Grained Al-Mg Alloys Processed by Constrained Groove Pressing-Cross Route

In the present study, the wear behavior of ultra-fine grained (UFG) Al-Mg alloys produced by a severe plastic deformation (SPD) method was assessed and compared against the annealed coarse-grained alloy. To this end, weight loss, wear resistance, friction coefficient, and morphology of the worn surfaces was investigated. Constrained groove pressing-cross route (CGP-CR) process, an SPD technique, was implemented at ambient temperature up to two passes to impose an equivalent plastic strain of about 4.64. Formation of a UFG structure with an average sub-grain size of ~ 350 nm with an enhanced tensile strength of up to ~ 225 MPa and indentation hardness of up to ~ 95 HV were achieved upon two passes of CGP-CR process. The pin-on-disk dry wear sliding testing was conducted up to a distance of 1000 m under normal loads of 5, 7, and 9 N at a constant sliding speed of 0.5 m/s. The trends measured for the evaluation of wear properties/mechanisms are discussed based on the microstructural features and mechanical property of UFGed alloys. The results showed that by employing the CGP-CR process and through the formation of UFG structure, the wear resistance was considerably increased. This was even beyond two times (~ 100%) larger depending on the normal loading with the lowest coefficient of friction around 0.6. Observation and study of the morphology of the worn surfaces under field emission-scanning electron microscopy (FE-SEM) revealed a change in the wear mechanism from sticking followed by formation of plastic deformation bands and delamination in the coarse-grained annealed alloy into a combined abrasive-adhesive behavior in the UFG material.

36 MATERIALS SCIENCE↗

Fabrication, microstructure, and wear performance of WC-Fe composite/metal coating fabricated by resistance seam welding

Highlights: • WC-Fe/metal coating consisted of WC-Fe layer and metal interlayer was fabricated by resistance seam welding. • The microstructure, hardness and wear performance of coatings with different WC particles size were analyzed. • The wear mechanism of coatings showed huge difference following various sliding distance. - Abstract: WC-Fe composite/metal coatings consisting of a WC-Fe composite layer and a metal interlayer were successfully fabricated on an Al 6061 substrate by resistance seam welding. The microstructures and phase compositions of the WC-Fe composite/metal coatings with different WC particle sizes (nano, fine, and coarse) were investigated. The WC-Fe composite layer consisted of WC particles and a Fe-C-Si super hard alloy (SHA) component, whereas the metal interlayer was composed of SHA, FeAl{sub 3}, Fe{sub 2}Al{sub 5}, and Al 6061. The surface microhardness of the WC-Fe composite/metal coating increased with increasing WC particle size. The wear performance of the coatings tested with different sliding distances is discussed in detail. Coating-C (coarse) showed the best wear resistance. The wear rates of both coating-N (nano) and coating-C decreased as the sliding distance increased, while coating-F (fine) demonstrated the opposite behavior. The wear mechanisms of the coatings were drastically different owing to the significantly different WC particle behavior at various sliding distances.

36 MATERIALS SCIENCE↗

Effect of laser surface texturing (LST) on tribochemical films dynamics and friction and wear performance

Surface texturing or topographical design is one of the primary techniques to control friction and wear performance of surfaces in tribological contact. Laser surface texturing (LST), whereby a laser beam is used to produce regular arrays of dimples on a surface, has been demonstrated to reduce friction in conformal lubricated contacts. Friction and wear behavior under boundary lubrication is also known to be dependent on the formation and durability of the tribochemical film formed from lubricant additives. In this paper, the effects of LST on the formation and durability of tribochemical films and its consequent impacts on friction and wear behavior in various lubrication regimes were evaluated. Friction and wear tests that cycled through different lubrication regimes were conducted with both polished and LST treated surfaces using a synthetic lubricant with and without model additives of ZDDP and MoDTC mixture. In the base oil without additives, LST produced noticeable reduction in friction in all lubrication regimes. However, with low-friction model additives, friction was higher in tests with LST due to significant differences in the tribochemical film formation in the polished and LST surfaces, as well as the sliding counterface. Continuous tribo-films were formed on ball conterface rubbed against polished surfaces while the films were streaky and discontinuous in ball rubbed against LST surfaces. LST produced more wear on the ball counterface in both base and additized oils. Lastly, no measurable wear was observed in both the polished and LST flat specimens.

36 MATERIALS SCIENCE↗