Engineering PapersSearch

SEARCH · Engineering Papers

Results for “Solid electrolytes”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Strategic Melamine Coating on Lithium Metal for Li 3 N-Rich Solid Electrolyte Interphase and Improved Battery Cycling Stability

The practical applications of lithium (Li) metal batteries (LMBs) are limited by challenges such as dendrite formation and unstable solid electrolyte interphase (SEI), especially at higher C-rates. Here, this study introduces melamine-coated Li metal anodes (LMAs), forming a Li 3 N-rich SEI layer that improves ionic conductivity and mechanical stability. The optimized melamine-coated LMA demonstrated uniform coverage resulting in denser Li deposition, nearly doubled cycle life (~148 cycles at 0.5 C, 1C = 4.1 mA cm -2 ), compared to Bare-Li. These findings emphasize that coating materials-induced beneficial SEI components could lead to improvement of LMB performance.

Batteries

Tuning Solid Electrolyte Interphase Formation before Plating Onset in Anode-Free Sodium Batteries

Sodium (Na) batteries are of growing interest due to the higher earth abundance of sodium than lithium, as well as their promising theoretical energy density when metallic Na anodes are used. However, Na plating and stripping are heavily influenced by the physicochemical properties of the solid electrolyte interphase (SEI), which is directly influenced by the solvent and salt used for the electrolyte. While most studies focus on the SEI that forms on the surface of Na metal after plating, we expand this analysis by identifying a nanoscale “pre-plating” SEI that forms on the current collector (CC) prior to the onset of Na plating. Here, we systematically investigate an array of Na salt and glyme solvents in the electrolyte and determine the associated impacts on pre-plating SEI formation on aluminum CCs. By combining analytical electrochemistry approaches with a multimodal suite of spectroscopy techniques (X-ray, infrared, and Raman), supported by density functional theory calculations, we reveal a direct correlation between the Na + coordination environment and pre-plating SEI composition. We find that longer-chain glymes produce larger proportions of organic alkoxide products in the interphase, consistent with increased Na + −glyme interactions, while the fraction of salt-derived inorganic products (e.g., NaF) correlates with Na + −anion coordination. These insights highlight the critical influence of electrolyte composition particularly solvent identity and Na + coordination on the initial SEI formation in anode-free Na batteries.

anode-free batteries

On the dynamics of the fluoroethylene carbonate generated solid electrolyte interphase on silicon anodes during calendar life aging

Here, the widespread use of silicon (Si)-rich anodes in lithium-ion batteries (LIBs) is impeded by an unstable solid electrolyte interphase (SEI) incurring insufficient cell life. Fluoroethylene carbonate (FEC) additive in the electrolyte significantly improves cycle life. However, the gains on calendar life remain unclear; the SEI structure still undergoes detrimental alterations at rest. Thus, elucidating the SEI dynamics during calendar aging is critical to mitigating time-dependent capacity degradation. ATR-FTIR, XPS, and ToF-SIMS are used herein to investigate the SEI structure before and after calendar aging. Si cycled without FEC exhibits no notable SEI chemistry changes Pre- and Post-aging, leaving poor passivation as the main failure pathway. Conversely, the FEC-SEI starts as short oligomeric species from FEC/EC electroreduction prior to aging; after calendar aging, polymerized carbonates become consistently more prominent. Unexpectedly, the deposition of self-polymerized FEC species results from time exposure to the delithiated Si specifically as opposed to the lithiated surface. This unexpected finding is supported by another recent Si calendar-aging research, which albeit not investigating FEC, finds global failure of the SEI upon delithiation resulting in ∼247 fold more reactive surface compared to the lithiated.

Batteries

Three-Man Solid Electrolyte Carbon Dioxide Electrolysis Breadboard

The development of the Three-Man (2.2 lb CO2/man-day) Solid Electrolyte CO2 Electrolysis Breadboard consisted of a Phase 1 and 2 effort. The Phase 1 effort constituted fabrication of three electrolysis cell types and performing parametric testing, off-design testing, and cell life testing. The Phase 2 consisted of the preliminary design, incorporation of palladium (Pd) tubes for hydrogen separation from the electrolyzer cathode feed gases, design support testing, final design, fabrication, and performance testing of the breadboard system. The results of performance tests demonstrated that CO2 electrolysis in an oxygen reclamation system for long duration space-based habitats is feasible. Closure of the oxygen system loop, therefore, can be achieved by CO2 electrolysis. In a two step process the metabolic CO2 and H2O vapor are electrolyzed into O2, H2, and CO. The CO can subsequently be disproportionated into carbon and CO2 in a carbon deposition reactor and the CO2 in turn be recycled and electrolyzed for total O2 recovery. The development effort demonstrated electrolyzer system can be designed and built to operate safely and reliably and the incorporation of Pd tubes for hydrogen diffusion can be integrated safely with predictable performance.

Isenberg, Arnold O.

Heterogeneous Solid Electrolyte Interphase Interactions Dictate Interface Instability in Sodium Metal Electrodes

Sodium (Na) metal batteries have attracted recent attention due to their low cost and high abundance of Na. However, the advancement of Na metal batteries is impeded due to key challenges such as dendrite growth, solid electrolyte interphase (SEI) fracture, and low Coulombic efficiency. This study examines the coupled electro‐chemo‐mechanical interactions governing the electrodeposition stability and morphological evolution at the Na/electrolyte interface. The SEI heterogeneities influence transport and reaction kinetics leading to the formation of current and stress hotspots during Na plating. Further, it is demonstrated that the heterogeneity‐induced Na metal evolution and its influence on the stress distribution critically affect the mechanical overpotential, contributing to a faster SEI failure. The analysis reveals three distinct failure mechanisms—mechanical, transport, and kinetic—that govern the onset of instabilities at the interface. Finally, a comprehensive comparative study of SEI failure in Na and lithium (Li) metal anodes illustrates that the electrochemical and mechanical characteristics of the SEI are crucial in tailoring the anode morphology and interface stability. This work delineates mechanistic stability regimes cognizant of the SEI attributes and underlying failure modes and offers important guidelines for the design of artificial SEI layers for stable Na metal electrodes.

25 ENERGY STORAGE

The Solid Electrolyte Interphase Dispersion Can Predict Cycle and Calendar Lifetimes in Silicon Anodes for Lithium-Ion Batteries

The solid electrolyte interphase (SEI) plays a critical role in lithium-ion battery (LIB) anodes. It is responsible for passivating the reactive surface of lithiated anodes against degradation of the electrolyte which enables long cycle and calendar lifetimes for LIBs. This role is especially important in high energy density anodes like silicon, that undergo massive volumetric changes during electrochemical cycling. The mechanism by which the SEI performs this role, however, is not clear which makes designing an SEI to passivate silicon anodes impossible. Through decades of research, dozens of chemical species have been identified within the SEI ranging from inorganic solids to polymeric coatings all of which simultaneously exist in a 'mosaic' composition at the anode surface. This mosaic creates a highly dispersive environment in which electrostatic screening of the anode surface from the electrolyte is not always complete. Here, we present an electrochemical technique to directly test the dispersion at the anode surface. We use this technique to screen more than 20 different electrolytes against silicon anodes and find correlations between both the cycle life and calendar life. The insights from this study offer a new framework to think about the SEI and a rapid screening method to test novel electrode/electrolyte combinations.

battery

Revealing the roles of the solid–electrolyte interphase in designing stable, fast-charging, low-temperature Li-ion batteries

Designing the solid–electrolyte interphase (SEI) is critical for stable, fast-charging, low-temperature Li-ion batteries. Fostering a “fluorinated interphase,” SEI enriched with LiF, has become a popular design strategy. Although LiF possesses low Li-ion conductivity, many studies have reported favorable battery performance with fluorinated SEIs. Such a contradiction suggests that optimizing SEI must extend beyond chemical composition design to consider spatial distributions of different chemical species. In this work, we demonstrate that the impact of a fluorinated SEI on battery performance should be evaluated on a case-by-case basis. Sufficiently passivating the anode surface without impeding Li-ion transport is key. We reveal that a fluorinated SEI containing excessive and dense LiF severely impedes Li-ion transport. In contrast, a fluorinated SEI with well-dispersed LiF (i.e., small LiF aggregates well mixed with other SEI components) is advantageous, presumably due to the enhanced Li-ion transport across heterointerfaces between LiF and other SEI components. An electrolyte, 1 M LiPF 6 in 2-methyl tetrahydrofuran (2MeTHF), yields a fluorinated SEI with dispersed LiF. This electrolyte allows anodes of graphite, μSi/graphite composite, and pure Si to all deliver a stable Coulombic efficiency of 99.9% and excellent rate capability at low temperatures. Pouch cells containing layered cathodes also demonstrate impressive cycling stability over 1,000 cycles and exceptional rate capability down to −20 °C. Through experiments and theoretical modeling, we have identified a balanced SEI-based approach that achieves stable, fast-charging, low-temperature Li-ion batteries.

25 ENERGY STORAGE

Chemical stability enhancement of lithium conducting solid electrolyte plates using sputtered LiPON thin film

Sputter deposition of LiPON films directly onto high Li+ conductivity solid electrolyte plates has been investigated as a means to minimize the reactivity of the plates to metallic Li. The LiPON films were shown to effectively passivate the plates in contact with metallic Li, in contrast to unpassivated plates that reacted immediately in contact with Li metal.

LiPON lithium metals electrolyte plates

Composite Solid Electrolyte for Li Battery Applications

The electrochemical, bulk and interfacial properties of the polyethylene oxide (PEO) based composite solid electrolyte (CSE) comprising LiI, PEO, and Al2O3 have been evaluated for Li battery applications. The bulk interfacial and transport properties of the CSEs seem to strongly depend on the alumina particle size. For the CSE films with 0.05 micron alumina while the bulk conductivity is around 10(exp -4) (mho/cm) at 103 C, the Li ion transport number seems to be close to unity at the same temperature. Compared to the PEO electrolyte this polymer composite electrolyte seems to exhibit robust mechanical and interfacial properties. We have studied three different films with three different alumina sizes in the range 0.01-0.3 micron. Effects of Al2O3 particle size on the electrochemical performance of polymer composite electrolyte is discussed. With TiS2 as cathode a 10 mAh small capacity cell was charged and discharged at C/40 and C/20 rates respectively.

Nagasubramanian, G.

Solid-state prealkylation of electrode architectures to tune solid electrolyte interphase composition

Efficient electrochemical cycling of certain Si anodes is limited by irreversible Li consumption to form and continually reform the solid electrolyte interface (SEI) due to Si expansion/contraction and fracture. Prelithiation can compensate for these losses; however, the starting open circuit potential (VOC) becomes highly reducing and, therefore, the electrolyte reduction chemistry that influences the SEI composition can change. Herein, we compare SEI formation for electrodes prelithiated using Solid State Prealkylation of Electrode Architectures (SPEAR) versus traditional electrochemically lithiated architectures (ECLAR), focusing on SEI compositional changes as a function of stoichiometry (0.28 ≤ x ≤ 1.38 in LixSi). Increasing SPEAR prelithiation decreased the initial VOC of Si anodes vs. Li/Li+ from ∼3 V (Li0.28Si) to < 0.5 V for Li1.38Si, enabling simultaneous competitive reduction of EC, EMC, and LiPF6 at low potentials. Ex situ7Li and 29Si cross-polarization NMR and XPS reveal that SPEAR drives thicker SEI formation with substantially increased P/F contributions and a predominantly inorganic insoluble SEI (71.4% inorganic for Li1.38Si), consistent with accelerated LiPF6-derived POx/LiPFx/LiF formation relative to ECLAR analogs which exhibit carbonate-rich organic SEI compositions. Symmetric-cell EIS further indicates SPEAR-specific impedance features consistent with pore reduction (filling) during LixSi formation. In full cells, SPEAR prelithiation increases the initial coulombic efficiency (ICE) and accelerates SEI formation and stabilization with Li1.38Si reaching 99.4% coulombic efficiency (CE) by cycle 2.

Musgrove, Amanda [ORNL] (ORCID:0009000220910389)

Revealing Solvent-Assisted Li+ Transport in the Solid Electrolyte Interphase operando

The performance of energy-dense lithium metal batteries is critically influenced by the properties of the solid electrolyte interphase (SEI). Yet, progress in understanding this layer has been limited by the lack of accurate operando characterization because the SEI evolves dynamically during cycling. Here, we apply dynamic electrochemical impedance spectroscopy (dEIS) to resolve the real-time evolution of the SEI on lithium metal in ether-based electrolytes with varying degrees of fluorination. We find that faster stabilization of the compact SEI resistance correlates with improved passivation and higher Coulombic efficiency. Unexpectedly, compact SEI resistance correlates directly with Li+ solvation energy, revealing that weaker Li+ solvation increases not only bulk but also interphase resistance. These findings challenge the conventional view of the SEI as a purely solid-phase conductor and instead support a solvent-assisted Li+ transport mechanism within the compact SEI. This framework emphasizes the need to balance SEI ionic conductivity with the Li+ solvation environment to maximize lithium metal battery performance.

Sacci, Robert [ORNL] (ORCID:0000000200735221)

Harnessing Chemical Short‐Range Disorder to Improve Lithium Retention in Epitaxial LLTO Solid‐Electrolyte Thin Films

Lithium lanthanum titanate Li 3x La 2/3-x TiO 3 (LLTO) is a promising perovskite-based solid-state electrolyte for next-generation lithium-ion batteries, but controlling crystallinity and Li stoichiometry in thin-film form is challenging because high growth temperatures are required to achieve good crystallinity while Li remains strongly volatile. Here, we systematically investigate the effect of substrate temperature on epitaxial LLTO thin films grown by pulsed laser deposition. We identify a narrow growth window (750–800°C) in which LLTO films grow as c-axis oriented with atomically flat surfaces. Lower growth temperatures (<750°C) stabilize laterally extended, chemically disordered stripe domains that coexist with ordered LLTO regions, whereas higher temperatures (≥825°C) suppress these defects but promote island morphologies and Al/Ti interdiffusion. While spectroscopy measurements show that Ti remains in the 4+ oxidation state and Li is globally deficient for all films, our depth-resolved time-of-flight secondary ion mass spectrometry studies reveal that the 700°C film retains the highest Li content across its thickness. These results clarify how growth temperature controls crystallinity, chemical short-range disorder, and Li retention, and highlight moderate growth temperatures (∼700°C) as a route to mitigate Li loss in epitaxial solid-electrolyte films.

chemical short-range disorder

Design and Synthesis of Cubic K 3−2 x Ba x SbSe 4 Solid Electrolytes for K–O 2 Batteries

Developing K-ion conducting solid-state electrolytes (SSEs) plays a critical role in the safe implementation of potassium batteries. In this work, a chalcogenide-based potassium ion SSE is reported, K 3 SbSe 4 , which adopts a trigonal structure at room temperature. Single-crystal structural analysis reveals a trigonal-to-cubic phase transition at the low temperature of 50 °C, which is the lowest among similar compounds and thus provides easy access to the cubic phase. The substitution of barium for potassium in K 3 SbSe 4 leads to the creation of potassium vacancies, expansion of lattice parameters, and a transformation from a trigonal phase to a cubic phase. As a result, the maximum conductivity of K 3−2x Ba x SbSe 4 reaches around 0.1 mS cm −1 at 40 °C for K 2.2 Ba 0.4 SbSe 4 , which is over two orders of magnitude higher than that of undoped K 3 SbSe 4 . This novel SSE is successfully employed in a K–O 2 battery operating at room temperature where a polymer-laminated K 2.2 Ba 0.4 SbSe 4 pellet serves as a separator between the oxygen cathode and the potassium metal anode. Effective protection of the K metal anode against corrosion caused by O 2 is demonstrated.

25 ENERGY STORAGE

Vitreous solid electrolyte sheets of Li ion conducting sulfur-based glass and associated structures, cells and methods

A lithium ion-conductive solid electrolyte including a freestanding inorganic vitreous sheet of sulfide-based lithium ion conducting glass is capable of high performance in a lithium metal battery by providing a high degree of lithium ion conductivity while being highly resistant to the initiation and/or propagation of lithium dendrites. Such an electrolyte is also itself manufacturable, and readily adaptable for battery cell and cell component manufacture, in a cost-effective, scalable manner.

Visco, Steven J.

LaCl 3 -based sodium halide solid electrolytes with high ionic conductivity for all-solid-state batteries

To enable high performance of all solid-state batteries, a catholyte should demonstrate high ionic conductivity, good compressibility and oxidative stability. Here, a LaCl 3 -based Na + superionic conductor (Na 1–x Zr x La 1–x Cl 4 ) with high ionic conductivity of 2.9 × 10 –4 S cm –1 (30 °C), good compressibility and high oxidative potential (3.80 V vs. Na 2 Sn) is prepared via solid state reaction combining mechanochemical method. X-ray diffraction reveals a hexagonal structure (P6 3 /m) of Na 1–x Zr x La 1–x Cl 4 , with Na + ions forming a one-dimensional diffusion channel along the c-axis. First-principle calculations combining with X-ray absorption fine structure characterization etc. reveal that the ionic conductivity of Na 1–x Zr x La 1–x Cl 4 is mainly determined by the size of Na + -channels and the Na + /La 3+ mixing in the one-dimensional diffusion channels. When applied as a catholyte, the NaCrO 2 ||Na 0.7 Zr 0.3 La 0.7 Cl 4 ||Na 3 PS 4 ||Na 2 Sn all-solid-state batteries demonstrate an initial capacity of 114 mA h g –1 and 88% retention after 70 cycles at 0.3 C. In addition, a high capacity of 94 mA h g –1 can be maintained at 1 C current density.

36 MATERIALS SCIENCE

Identification of Solid-Electrolyte Interphase Species by Joint Characterization of Li-Ion Battery Chemistry by Mass Spectrometry and Electrochemical Reaction Networks

The formation and stability of the solid-electrolyte interphase (SEI) play central roles in determining the long-term performance and safety of modern electrochemical energy storage systems. Despite decades of research, the SEI’s heterogeneous, dynamic, and multiphase nature has defied comprehensive molecular-level characterization, creating a critical knowledge gap that limits rational battery design. In this work, we introduce a computational−experimental framework that integrates high-throughput quantum chemistry calculations, data-driven electrochemical reaction networks (eCRNs), stochastic algorithms, and laser desorption/ionization Fourier transform ion cyclotron resonance mass spectrometry (LDI-FTICR-MS) to unravel SEI formation in carbonatebased electrolytes without imposing predefined mechanisms. We constructed the most comprehensive eCRN to date, spanning over 10,000 species and 209 million reactions. Through stochastic network analysis, we successfully recovered 27 species that were previously reported in the literature and predicted 28 novel SEI species nearly doubling our scientific knowledge in this area. Each new species was rigorously confirmed through advanced mass spectral analysis of its distinct molecular and isotopic signatures. We kinetically refined the formation pathways for a select set of both previously reported and novel SEI products, revealing kinetically feasible elementary reaction mechanisms with activation barriers below 1 eV. This computational−experimental approach deepens our molecular-level understanding of SEI chemistry by resolving which species form and through which decomposition mechanisms they emerge. Such knowledge provides the foundation necessary to connect electrolyte composition to the resulting SEI components, a critical step toward a more informed electrolyte development in next-generation lithium-based batteries.

25 ENERGY STORAGE