Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SUPERALLOY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Custom-designed heat treatment simultaneously resolves multiple challenges facing 3D-printed single-crystal superalloys

Single-crystal Ni-based superalloys are currently the material of choice for turbine blade applications, especially with the emerging additive manufacturing (AM) that facilitates the manufacture/repair of these single crystals. This promising AM route, however, comes with a dilemma: in the fusion and heat affected zones after e-beam or laser induced melting, one needs a solutionizing annealing to relieve the residual stresses and homogenize the chemical/microstructure. The super-solvus solutionizing temperature is usually adopted from the protocol for the cast superalloys, which almost always causes recrystallization and stray grain growth, resulting in a polycrystalline microstructure and degrading the high-temperature mechanical performance. Here, in this paper, we demonstrate a custom-designed post-printing heat treatment to replace the conventional super-solvus one. The recovery and relatively low temperature diminish the driving force for recrystallization and the movement of stray grain boundaries, without suffocating the chemical/microstructural homogenization thanks to the narrow dendrite width and short element segregation distance. The optimal duration of the heat treatment is proposed to achieve atomic-diffusion mediated chemical homogenization while limiting γ'-particle coarsening in the interdendritic regions. Our strategy makes it practically feasible to resolve several bottleneck problems with one processing/treatment, removing a seemingly formidable obstacle to effective additive manufacturing of superalloy single crystal products.

36 MATERIALS SCIENCE↗

APS TBC performance on directionally-solidified superalloy substrates with HVOF NiCoCrAlYHfSi bond coatings

Directionally-solidified (DS) superalloy components with advanced thermal barrier coatings (TBC) to lower the metal operating temperature have the potential to replace more expensive single crystal superalloys for large land-based turbines. In order to assess relative TBC performance, furnace cyclic testing was used with superalloys 1483, X4 and Hf-rich DS 247 substrates and high velocity oxygen fuel (HVOF)-NiCoCrAlYHfSi bond coatings at 1100 °C with 1-h cycles in air with 10% H 2 O. With these coating and test conditions, there was no statistically-significant effect of substrate alloy on the average lifetime of the air plasma sprayed (APS) yttria-stabilized zirconia (YSZ) top coatings on small coupons. Using photo-stimulated luminescence piezospectroscopy maps at regular cycling intervals, the residual compressive stress in the α-Al 2 O 3 scale underneath the YSZ top coating and on a bare bond coating was similar for all three substrates and delaminations occurred at roughly the same rate and frequency. As a result, x-ray fluorescence (XRF) measurements collected from the bare bond coating surface revealed higher Ti interdiffusion occurring with the 1483 substrate, which contained the highest Ti content.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Fatigue Failures at Defective Grains in a Single Crystal Nickel-Base Superalloy

Single crystal nickel-base superalloys used as turbine engine blades can have much higher creep and fatigue resistance than many polycrystalline superalloys due to the absence of weak grain boundaries as well as the ability to orient the blades in the primary loading direction on to the low elastic modulus [001] orientation, which significantly lowers the stresses imposed on the blades. However, grain defects can occur in these crystals, impairing these advantages. In the present study, fatigue tests of a single crystal superalloy uncovered unexpected defective grains in the test specimens, which initiated premature fatigue failures. The characteristics of these defective grains and the associated failures were evaluated and related to the observed fatigue lives.

superalloy↗

Design of Novel Precipitate-Strengthened Al-Co-Cr-Fe-Nb-Ni High-Entropy Superalloys

Here, a series of non-equiatomic Al-Co-Cr-Fe-Nb-Ni high-entropy alloys, with varying levels of Co, Nb and Fe, were investigated in an effort to obtain microstructures similar to conventional Ni-based superalloys. Elevated levels of Co were observed to significantly decrease the solvus temperature of the γ' precipitates. Both Nb and Co in excessive concentrations promoted the formation of Laves and NiAl phases that formed either during solidification and remained undissolved during homogenization or upon high-temperature aging. Lowering the content of Nb, Co, or Fe prevented the formation of the eutectic type Laves. In addition, lowering the Co content resulted in a higher number density and volume fraction of the γ' precipitates, while increasing the Fe content led to the destabilization of the γ' precipitates. Various aging treatments were performed which led to different size distributions of the strengthening phase. Results from the microstructural characterization and hardness property assessments of these high-entropy alloys were compared to a commercial, high-strength Ni-based superalloy RR1000. Potentially, precipitation-strengthened high-entropy alloys could find applications replacing Ni-based superalloys as structural materials in power generation applications.

36 MATERIALS SCIENCE↗

The Application of Differential Scanning Calorimetry to Investigate Precipitation Behavior in Nickel-Base Superalloys Under Continuous Cooling and Heating Conditions

In this study, a suite of experimental tools and fast-acting, numerical-simulation techniques was used to quantify the precipitation behavior of three nickel-base superalloys: IN-100, LSHR, and 718. Experimental methods comprised differential scanning calorimetry (DSC) to establish the specific heat as a function of temperature and selected direct-resistance heating trials (using a Gleeble ® machine) to obtain samples for microstructural analysis. For the DSC experiments, each alloy was cooled at a prescribed constant rate (between 5 and 20 K/min) after an initial soak/equilibration in the high-temperature, single-phase (supersolvus) temperature regime. On-heating DSC trials beginning at ambient temperature were also performed on alloy 718 in three different starting conditions: super- δ -solvus solution treated and water quenched (denoted as ST), solution treated and aged (STA), and solution treated and overaged (STOA). DSC results, revealing the thermal signatures associated with the kinetics of precipitation of γ ' (IN-100, LSHR) or γ ' and γ " (718), were interpreted using a previously-developed fast-acting routine that treats concurrent nucleation, growth, coarsening, and dissolution. For these simulations, special attention was paid to various thermo-kinetic input parameters including equilibrium solvus-approach curves, bulk free energies of transformation, matrix-precipitate interface energies, and effective diffusivities. For the γ - γ ' superalloys (IN-100 and LSHR), estimates of precipitate volume fraction as a function of temperature from the specific-heat data revealed semi-quantitative agreement with simulation predictions. For the γ - γ '- γ " superalloy (718), simulation predictions of precipitate volume fractions were converted to specific heat as a function of temperature and showed semi-quantitative agreement with the direct measurements.

36 MATERIALS SCIENCE↗

Minor Elements and Solidification Cracking During Laser Powder-Bed Fusion of a High $\gamma ^{\prime }$ CoNi-Base Superalloy

Here, the cracking behavior of a high γ' volume fraction CoNi-base superalloy fabricated via laser powder bed fusion (LPBF) is studied in relation to the content of carbon and boron. Severe cracking occurred with the increase in boron content from 0.08 to 0.16 at. pct (0.015 to 0.029 wt pct), while compositions with 0.1 to 0.36 at. pct C (0.02 to 0.076 wt pct) and 0.08 at. pct B exhibited minimal cracking. Assessment of cracks in the high-boron composition shows a variation in crack density with printing parameters, and alignment of the cracks with the build direction. Scanning electron microscopy (SEM) of the crack surfaces shows evidence of a solidification cracking mode. Differential thermal analysis (DTA) reveals a decreased incipient melting temperature for the high-boron composition, and atom probe tomography (APT) is used to measure the enrichment at grain boundaries, revealing distinct boron segregation. Scheil-Gulliver solidification simulations for the different C and B levels are consistent with the incipient melting behavior observed with DTA. Evaluation of the solidification cracking susceptibility from the simulations allow for comparison of the CoNi alloy behavior to Ni-base superalloys studied for LPBF fabrication and displays how such metrics may aid in the design of new precipitation-strengthened superalloys for additive manufacturing (AM).

36 MATERIALS SCIENCE↗

Influence of Melt Superheating Treatment on Solidification Characteristics and Rupture Life of a Third-Generation Ni-Based Single-Crystal Superalloy

The influence of melt superheating treatment on the melt properties, solidification characteristics, and rupture life of a third-generation Ni-based single-crystal superalloy was investigated to reveal the critical temperature range of melt structure evolution and its effect on rupture life. The results showed that the viscosity of superalloy decreased but the surface tension increased with increasing superheating temperature. Two characteristic temperature points where the melt viscosity and undercooling degree suddenly change were determined to be 1600 °C and 1700 °C, respectively. Similarly, the stability of the solidification interface firstly improved and then weakened with increasing superheating temperature. The dendrite arms were well refined and the segregation was reduced at 1700 °C. In addition, the rupture life obtained at 1100 °C and 137 MPa increased by approximately 30 pct, approaching the rupture life of the corresponding superalloy containing 2 pct Ru, with increasing superheating temperature from 1500 °C to 1700 °C. When the melt was further heated to 1800 °C, the rupture life decreased. The evolutions of solidification characteristics and rupture life with increasing melt superheating temperature were attributed to changes in the melt structure.

36 MATERIALS SCIENCE↗

Micromechanism of High-Temperature Tensile Deformation Behavior of a Directionally Solidified Nickel Base Superalloy

High-temperature tensile deformation behavior of directionally solidified nickel base superalloy CM 247 DS is studied by conducting tensile tests in temperature range RT-955 °C employing a constant strain rate of 10{sup −3} s{sup −1} and carrying out extensive electron microscopic examinations to understand the concomitant substructural evolution. The alloy exhibits yield strength anomaly (YSA) behavior like many other superalloys, and the yield strength maxima occur at 750 °C. However, unlike in most of the superalloys, ductility continuously increases with temperature. The deformation behavior of the alloy changes significantly with temperature. Transmission electron microscopic examination confirmed that at lower temperature (≤ 750 °C), γ′ shearing is the dominant deformation mechanism; whereas at temperatures above 750 °C, thermally activated dislocation looping around γ′ precipitate is dominant. Substructures evolved during deformation at 750 °C consists mainly of superlattice stacking faults (SSFs) inside γ′ precipitates, whereas at 850 °C uniform dislocation tangles are observed in γ matrix. Superlattice stacking faults result from shearing of γ′ precipitate by a/3〈112〉 dislocations, which arise from the decomposition of a/2〈110〉 matrix dislocations. YSA in this alloy is attributed to dislocation interactions inside γ′; however, the enhanced ductility even at 750 °C is due to formation of SSFs.

36 MATERIALS SCIENCE↗

Creep Deformation and Damage Mechanisms in an Advanced High-Temperature Additively Manufactured Nickel-Base Superalloy

Abstract This research investigates the processing–structure–properties–performance relationship in a novel nickel-base superalloy, ABD ® -900AM, designed for extreme environments. Specifically tailored for additive manufacturing (AM), ABD ® -900AM maintains mechanical integrity at high temperatures and is comparable to other nickel-based superalloys with a 30–40% gamma-prime volume fraction. A comprehensive study was conducted using laser-beam powder bed fusion and electron-beam powder bed fusion methods. Factors such as heat treatment, porosity, build orientation, and hot isostatic pressing were evaluated to understand their effects on microstructure and mechanical performance. Microstructural characterization revealed significant differences in grain size and orientation across build processes and heat treatments. High-temperature mechanical testing indicated that grain size, heat treatment, and orientation significantly influence creep behavior. A super-solvus heat treatment led to recrystallization and grain growth, significantly improving creep properties compared to a near-solvus heat treatment. Various creep mechanisms were identified across different conditions, and creep rupture models were developed for each build process. Post-test microstructural analysis showed grain boundary damage, with differences in creep cavitation morphology under varying stress conditions. It was shown that MC carbides grow at the expense of gamma-prime near grain boundaries, leading to precipitate-free zones in specimens tested at higher temperatures. This study fills a significant gap in fundamental research by offering a deeper insight into the high-temperature mechanical behavior of additively manufactured nickel-base superalloys. It also explores critical research questions regarding the role of carbides and the significance of heat treatment. The insights gained enhance confidence in the industry adoption of ABD ® -900AM and similar alloys for high-temperature applications, bridging the knowledge gap and supporting the development of reliable AM processes for extreme environments.

Bridges, Alex (ORCID:000000030338759X)↗

Lattice parameter misfit evolution during creep of a cobalt-based superalloy single crystal with cuboidal and rafted gamma-prime microstructures

A [h00] oriented Co-based superalloy single crystal was crept under tension at 940 °C=100 MPa, resulting in a P-type raft morphology with extensive particle coalescence along the [h00] loading direction. However, particle coalescence was also observed in two perpendicular directions on the (h00) plane, normal to the loading axis. Tensile creep experiments were performed with in-situ neutron diffraction at 800 °C=500 MPa on this initially rafted $\gamma$ microstructure, and for comparison at (i) 900 °C=260 MPa, and at (ii) 750 °C=875 MPa, both with initially cuboidal $\gamma$ microstructures. The alloy was shown to exhibit a positive lattice parameter misfit, and during the first hour of creep at 900 °C=260 MPa, the lattice parameter evolution indicated changes in phase composition associated with $\gamma$ dissolution as the alloy achieved phase equilibrium at 900 °C. For all three in-situ creep measurements, there was a significant divergence of the $\gamma$ and g lattice parameters as creep proceeded. The lattice parameter misfit values between the precipitates and the matrix approached their unconstrained values during creep, and were notably large compared to those of Ni-based superalloys. This is indicative of a loss of coherency at the precipitate/matrix interfaces. Such a loss of coherency at the precipitate/matrix interfaces will likely degrade certain mechanical properties such as fatigue resistance, as has been shown for the Ni-based superalloys.

36 MATERIALS SCIENCE↗

A transport-based framework for solidification cracking in Ni-based superalloys processed by laser powder bed fusion

Solidification cracking remains a persistent barrier to laser powder bed fusion (LPBF) processing of solid-solution-strengthened (SSS) Ni-based superalloys and is commonly attributed to carbide formation, liquation-type failure, or elemental segregation. In this work, the cracking behavior of three SSS Ni-based superalloys—Inconel 625 (625), Inconel 617 (617), and Haynes 230 (230)—is examined under comparable LPBF conditions to evaluate the origins of their cracking susceptibility. Carbides were present in both 625 and 230, yet cracking behavior differed significantly. MC-type carbides in 625 remain discrete and preserve liquid connectivity, whereas Cr-rich M23C6 carbides in 230 form at cellular triple junctions that bottleneck the interdendritic liquid network, influencing cracking through liquid connectivity rather than as an independent cause. Alloy 617 exhibited anomalous segregation without resolvable secondary phases yet cracked mildly, indicating that extensive carbide formation is not a prerequisite for cracking. To rationalize these observations, a transport-limited framework is proposed in which cracking occurs when terminal-liquid feeding cannot accommodate solidification-induced strain; among the mechanisms evaluated, this framework is most consistent with the physical constraints imposed by LPBF solidification. Transport-based crack-susceptibility indexes incorporating permeability, viscosity, and solidification kinetics distinguish the alloy hierarchy; permeability ratios Krat increased from approximately 7 (625) to 11.5 (617) and 14.5 (230), with corresponding increases in the μ-weighted mushy zone risk index (CSIMZRM). These results are consistent with transport-limited liquid feeding as a rate-limiting contributor to solidification cracking in LPBF-processed SSS Ni-based superalloys, providing a physically grounded basis for alloy and process design.

Hyer, Holden [ORNL] (ORCID:0000000343915561)↗

Microstructural response to heat affected zone cracking of prewelding heat-treated Inconel 939 superalloy

The microstructural response to cracking in the heat-affected zone (HAZ) of a nickel-based IN 939 superalloy after prewelding heat treatments (PWHT) was investigated. The PWHT specimens showed two different microstructures: 1) spherical ordered {gamma} Prime precipitates (357-442 nm), with blocky MC and discreet M{sub 23}C{sub 6} carbides dispersed within the coarse dendrites and in the interdendritic regions; and 2) ordered {gamma} Prime precipitates in 'ogdoadically' diced cube shapes and coarse MC carbides within the dendrites and in the interdendritic regions. After being tungsten inert gas welded (TIG) applying low heat input, welding speed and using a more ductile filler alloy, specimens with microstructures consisting of spherical {gamma} Prime precipitate particles and dispersed discreet MC carbides along the grain boundaries, displayed a considerably improved weldability due to a strong reduction of the intergranular HAZ cracking associated with the liquation microfissuring phenomena. - Highlights: Black-Right-Pointing-Pointer Homogeneous microstructures of {gamma} Prime spheroids and discreet MC carbides of Ni base superalloys through preweld heat treatments. Black-Right-Pointing-Pointer {gamma} Prime spheroids and discreet MC carbides reduce the intergranular HAZ liquation and microfissuring of Nickel base superalloys. Black-Right-Pointing-Pointer Microstructure {gamma} Prime spheroids and discreet blocky type MC carbides, capable to relax the stress generated during weld cooling. Black-Right-Pointing-Pointer Low welding heat input welding speeds and ductile filler alloys reduce the HAZ cracking susceptibility.

36 MATERIALS SCIENCE↗

Thermal evolution behavior of carbides and {gamma} Prime precipitates in FGH96 superalloy powder

The characteristics of rapidly solidified FGH96 superalloy powder and the thermal evolution behavior of carbides and {gamma} Prime precipitates within powder particles were investigated. It was observed that the reduction of powder size and the increase of cooling rate had transformed the solidification morphologies of atomized powder from dendrite in major to cellular structure. The secondary dendritic spacing was measured to be 1.02-2.55 {mu}m and the corresponding cooling rates were estimated to be in the range of 1.4 Multiplication-Sign 10{sup 4}-4.7 Multiplication-Sign 10{sup 5} K{center_dot}s{sup -1}. An increase in the annealing temperature had rendered the phase transformation of carbides evolving from non-equilibrium MC Prime carbides to intermediate transition stage of M{sub 23}C{sub 6} carbides, and finally to thermodynamically stable MC carbides. The superfine {gamma} Prime precipitates were formed at the dendritic boundaries of rapidly solidified superalloy powder. The coalescence, growth, and homogenization of {gamma}' precipitates occurred with increasing annealing temperature. With decreasing cooling rate from 650 Degree-Sign C{center_dot}K{sup -1} to 5 Degree-Sign C{center_dot}K{sup -1}, the morphological development of {gamma} Prime precipitates had been shown to proceed from spheroidal to cuboidal and finally to solid state dendrites. Meanwhile, a shift had been observed from dendritic morphology to recrystallized structure between 900 Degree-Sign C and 1050 Degree-Sign C. Moreover, accelerated evolution of carbides and {gamma}' precipitates had been facilitated by the formation of new grain boundaries which provide fast diffusion path for atomic elements. - Highlights: Black-Right-Pointing-Pointer Microstructural characteristic of FGH96 superalloy powder was investigated. Black-Right-Pointing-Pointer The relation between microstructure, particle size, and cooling rate was studied. Black-Right-Pointing-Pointer Thermal evolution behavior of {gamma} Prime and carbides in loose FGH96 powder was studied.

36 MATERIALS SCIENCE↗

Microstructural, mechanical and weldability assessments of the dissimilar welds between γ′- and γ″-strengthened nickel-base superalloys

Dissimilar welding of γ′- and γ″-strengthened nickel-base superalloys has been investigated to identify the relationship between the microstructure of the welds and the resultant mechanical and weldability characteristics. γ′-Strengthened nickel-base Alloy 500 and γ″-strengthened nickel-base Alloy 718 were used for dissimilar welding. Gas tungsten arc welding operations were utilized for performing the autogenous dissimilar welding. Alloy 500 and Alloy 718 base metals showed various types of phases, carbides, intermetallics and eutectics in their microstructure. The results for Alloy 500 weld metal showed severe segregation of titanium to the interdendritic regions. The Alloy 718 weld metal compositional analysis confirmed the substantial role of Nb in the formation of low-melting eutectic-type morphologies which can reduce the weldability. The microstructure of dissimilar weld metal with dilution level of 65% wt.% displayed semi-developed dendritic structure. The less segregation and less formation of low-melting eutectic structures caused to less susceptibility of the dissimilar weld metal to the solidification cracking. This result was confirmed by analytic modeling achievements. Dissolution of γ″-Ni{sub 3}Nb precipitations took place in the Alloy 718 heat-affected zone leading to sharp decline of the microhardness in this region. Remelted and resolidified regions were observed in the partially-melted zone of Alloy 500 and Alloy 718. Nevertheless, no solidification and liquation cracking happened in the dissimilar welds. Finally, this was concluded that dissimilar welding of γ′- and γ″-strengthened nickel-base superalloys can successfully be performed. - Highlights: • Dissimilar welding of γ′- and γ″-strengthened nickel-base superalloys is studied. • Microstructural, mechanical and weldability aspects of the welds are assessed. • Microstructure of welds, bases and heat-affected zones is characterized in detail. • The type, morphology and distribution of the phases are thoroughly investigated. • Dissimilar welding is successfully performed without occurrence of any hot cracks.

36 MATERIALS SCIENCE↗

A comparative study of quantitative microsegregation analyses performed during the solidification of the Ni-base superalloy CMSX-10

Quantitative microsegregation analyses were systematically carried out during the solidification of the Ni-base superalloy CMSX-10 to clarify the methodological effect on the quantification of microsegregation and to fully understand the solidification microstructure. Three experimental techniques, namely, mushy zone quenching (MZQ), planar directional solidification followed by quenching (PDSQ), and random sampling (RS), were implemented for the analysis of microsegregation tendency and the magnitude of solute elements by electron probe microanalysis. The microprobe data and the calculation results of the diffusion field ahead of the solid/liquid (S/L) interface of PDSQ samples revealed that the liquid composition at the S/L interface is significantly influenced by quenching. By applying the PDSQ technique, it was also found that the partition coefficients of all solute elements do not change appreciably during the solidification of primary γ. All three techniques could reasonably predict the segregation behavior of most solute elements. Nevertheless, the RS approach has a tendency to overestimate the magnitude of segregation for most solute elements when compared to the MZQ and PDSQ techniques. Moreover, the segregation direction of Cr and Mo predicted by the RS approach was found to be opposite from the results obtained by the MZQ and PDSQ techniques. This conflicting segregation behavior of Cr and Mo was discussed intensively. It was shown that the formation of Cr-rich areas near the γ/γ′ eutectic in various Ni-base superalloys, including the CMSX-10 alloy, could be successfully explained by the results of microprobe analysis performed on a sample quenched during the planar directional solidification of γ/γ′ eutectic. - Highlights: • Methodological effect on the quantification of microsegregation was clarified. • The liquid composition at the S/L interface was influenced by quenching. • The segregation direction of Cr varied depending on the experimental techniques. • Cr and Mo segregation in Ni-base superalloys was fully understood.

36 MATERIALS SCIENCE↗

Potential and limitations of microanalysis SEM techniques to characterize borides in brazed Ni-based superalloys

Brazed Ni-based superalloys containing complex phases of different Boron contents remain difficult to characterize at the micrometer scale. Indeed Boron is a light element difficult to measure precisely. The state-of-the-art microanalysis systems have been tested on a single crystal MC2 based metal brazed with BNi-2 alloy to identify boride precipitates. Effort has been made to evaluate the accuracy in Boron quantitation. Energy-dispersive and wavelength-dispersive X-ray spectroscopy attached to a Scanning Electron Microscope have first been used to determine the elemental composition of Boron-free phases, and then applied to various types of borides. Results have been compared to the ones obtained using a dedicated electron probe microanalysis, considered here as the reference technique. The most accurate method to quantify Boron using EDS is definitely by composition difference. A precision of 5 at.% could be achieved with optimized data acquisition and post-processing schemes. Attempts that aimed at directly quantifying Boron with various standards using EDS or coupled EDS/WDS gave less accurate results. Ultimately, Electron Backscatter Diffraction combined with localized EDS analysis has proved invaluable in conclusively identifying micrometer sized boride precipitates; thus further improving the characterization of brazed Ni-based superalloys. - Highlights: • We attempt to accurately identify Boron-rich phases in Ni-based superalloys. • EDS, WDS, EBSD systems are tested for accurate identification of these borides. • Results are compared with those obtained by electron probe microanalysis. • Boron was measured with EDS by composition difference with a precision of 5 at. %. • Additional EBSD in phase identification mode conclusively identifies the borides.

36 MATERIALS SCIENCE↗

Microstructural characterization of a new mechanically alloyed Ni-base ODS superalloy powder

The microstructure of a new Ni-base oxide dispersion strengthened superalloy powder was studied for high temperature gas turbine applications after the mechanical alloying process. In this study, an atomized powder with a composition similar to the CMSX-10 superalloy was mechanically alloyed with yttria and Hf powders. The mechanically alloyed powder included only the supersaturated solid solution γ phase without γ′ and yttria provided by severe plastic deformation, while after the 3-step aging, the γ′ phase was precipitated due to the partitioning of Al and Ta to the γ′ and Co, Cr, Re, W, and Mo to the γ phase. Mechanical alloying modified the morphology of γ′ to the new coherent γ–γ′ nanoscale lamellar structure to minimize the elastic strain energy of the precipitation, which yielded a low lattice misfit of 0.16% at high temperature. The γ′ lamellae aligned preferentially along the elastically soft [100] direction. Also, the precipitated oxide particles were refined in the γ phase by adding Hf from large incoherent YAlO{sub 3} to fine semi-coherent Y{sub 2}Hf{sub 2}O{sub 7} oxide particles with the average size of 7 nm and low interparticle spacing of 76 nm. - Highlights: • A new Ni-base ODS superalloy powder was produced by mechanical alloying. • The nanoscale γ–γ′ lamellar structure was precipitated after the aging treatment. • Fine semi-coherent Y{sub 2}Hf{sub 2}O{sub 7} oxide particles were precipitated by addition of Hf.

36 MATERIALS SCIENCE↗

The effect of aging treatment on the fracture toughness and impact strength of injection molded Ni-625 superalloy parts

In this study, the effect of aging heat treatment on fracture toughness and impact strength of Ni-625 superalloy fabricated by using powder injection molding (PIM) method was examined. After a feedstock was prepared by mixing the prealloyed Ni-625 superalloy powder, which was fabricated by gas atomisation, with a polymeric binder system and then it was granulated, it was shaped through the use of injection. The molded specimens were sintered at 1300 °C for 3 h after a two-stage debinding process. Once the sintered specimens were treated in the solution at 1150 °C for 2 h, they were quenched. Aging treatment was performed by keeping specimens at 745 °C for 22 h. Fracture toughness and impact tests were performed on sintered and aged specimens. Microstructure examinations were performed by using optical microscope, scanning electron microscope, and transmission electron microscope. The results revealed that aging heat treatment led to the formation of some carbides and intermetallic phases in the microstructure. While the hardness of the aged specimens increased due to these phases, their fracture toughness and impact strength values decreased. - Highlights: • Ni-625 superalloy components were produced by means of powder injection molding. • The produced components were subjected to aging treatment. • Aging process provided approximately 50% increase in the hardness of components. • Intermetallic precipitates, carbides and TCP phases occurred within the aged parts. • Fracture toughness and impact strength values decreased due to the hard phases.

36 MATERIALS SCIENCE↗