Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Oxide Particles”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Structure and Early Soot Oxidation Properties of Laminar Diffusion Flames

Soot is an important unsolved problem of combustion science because it is present in most hydrocarbon-fueled flames and current understanding of the reactive and physical properties of soot in flame environments is limited. This lack of understanding affects progress toward developing reliable predictions of flame radiation properties, reliable predictions of flame pollutant emission properties and reliable methods of computational combustion, among others. Motivated by these observations, the present investigation extended past studies of soot formation in this laboratory, to consider soot oxidation in laminar diffusion flames using similar methods. Early work showed that O2 was responsible for soot oxidation in high temperature O2-rich environments. Subsequent work in high temperature flame environments having small O2 concentrations, however, showed that soot oxidation rates substantially exceeded estimates based on the classical O2 oxidation rates of Nagle and Strickland-Constable and suggests that radicals such as O and OH might be strong contributors to soot oxidation for such conditions. Neoh et al. subsequently made observations in premixed flames, supported by later work, that showed that OH was responsible for soot oxidation at these conditions with a very reasonable collision efficiency of 0.13. Subsequent studies in diffusion flames, however, were not in agreement with the premixed flame studies: they agreed that OH played a dominant role in soot oxidation in flames, but found collision efficiencies that varied with flame conditions and were not in good agreement with each other or with Neoh et al. One explanation for these discrepancies is that optical scattering and extinction properties were used to infer soot structure properties for the studies that have not been very successful for representing the optical properties of soot. Whatever the source of the problem, however, these differences among observations of soot oxidation in premixed and diffusion flames clearly must be resolved. Motivated by these findings, the present study undertook measurements of soot and flame properties within the soot oxidation region of some typical laminar diffusion flames and exploited the new measurements to identify soot oxidation mechanisms for these conditions. Present considerations were limited to the early stages of soot oxidation (carbon consumption less than 70%) where reactions at the surface of primary soot particles dominate the process, rather than the later stages when particle porosity and internal particle oxidation become important as discussed by Neoh et al.

El-Leathy, A. M.↗

Formation of Oxides in the Interior of Friction Stir Welds

In friction stir welding (FSWing) the actual solid state joining takes place between the faying surfaces which form the weld seam. Thus the seam trace is often investigated for clues when the strength of the weld is reduced. Aluminum and its alloys are known to form a native, protective oxide on the surface. If these native surface oxides are not sufficiently broken up during the FSW process, they are reported to remain in the FSW interior and weaken the bond strength. This type of weld defect has been referred to as a lazy "S", lazy "Z", joint line defect, kissing bond, or residual oxide defect. Usually these defects are mitigated by modification of the process parameters, such as increased tool rotation rate, which causes a finer breakup of the native oxide particles. This study proposes that there may be an alternative mechanism for formation of oxides found within the weld nugget. As the oxidation rate increases at elevated temperatures above 400ºC, it may be possible for enhanced oxidation to occur on the interior surfaces during the FSW process from entrained air entering the seam gap. Normally, FSWs of aluminum alloys are made without a purge gas and it is unknown how process parameters and initial fit up could affect a potential air path into the interior during the processing. In addition, variations in FSW parameters, such as the tool rotation, are known to have a strong influence on the FSW temperature which may affect the oxidation rate if internal surfaces are exposed to entrained air. A series of FSWs were made in 3 different thickness panels of AA2219 (0.95, 1.27 and 1.56 cm) at 2 different weld pitches. As the thickness of the panels increased, there was an increased tendency for a gap to form in advance of the weld tool. If sufficient air is able to enter the workpiece gap prior to consolidation, the weld temperature can increase the oxidation rate on the interior surfaces. These oxidation rates would also be accelerated in areas of localized liquation. Metallographs from the weld panels showed indications of liquation at the grain boundaries. In FSWs of thicker panels, these regions of liquation were found to be heavily oxidized. The quality of the FSWs was evaluated from tensile testing at room temperature. As the panel thickness increased, a slight decrease in tensile strength was observed which was attributed to the presence of oxides. No oxide formation was observed in the thinner workpieces, although there were indications of localized liquation at the grain boundaries. Results from this study will assist in a better understand of the mechanisms of oxide formation in FSW interiors and provide methodology for minimizing their occurrence.

Schneider, Judy↗

A Phase-Field Study on Internal to External Oxidation Transition in High-Temperature Structural Alloys

Structural alloys applied at high temperatures rely on an external dense layer of oxide scale for protection. As some reactive alloy components are selectively oxidized internally, understanding how these dispersed metal oxide particles reach the surface to form a protective scale—the so-called internal to external oxidation transition—is crucial for designing these alloys. While the literature is replete with experimental studies on oxidation of alloys, there is a lack of computational studies in this realm due to the complex nature of coupled reaction and diffusion processes in multicomponent multi-phase alloy systems. In this work, we apply a recently developed phase-field model to simulate the oxidation processes under different compositions and nucleation scenarios to gain insights into how a continuous oxide scale can be established. The results show that while alloy composition is critical for internal to external oxidation transition, the oxide nuclei size, shape and distribution also have significant impact on the transition kinetics.

36 MATERIALS SCIENCE↗

Metal oxide-polymer composites

A method of making metal oxide clusters in a single stage by reacting a metal oxide with a substoichiometric amount of an acid in the presence of an oxide particle growth terminator and solubilizer. A method of making a ceramer is also disclosed in which the metal oxide clusters are reacted with a functionalized polymer. The resultant metal oxide clusters and ceramers are also disclosed.

Wellinghoff, Stephen T.↗

Metal oxide-polymer composites

A method of making metal oxide clusters in a single stage by reacting a metal oxide with a substoichiometric amount of an acid in the presence of an oxide particle growth terminator and solubilizer. A method of making a ceramer is also disclosed in which the metal oxide clusters are reacted with a functionalized polymer. The resultant metal oxide clusters and ceramers are also disclosed.

Wellinghoff, Stephen T.↗

Highly porous and mechanically strong ceramic oxide aerogels

Structurally stable and mechanically strong ceramic oxide aerogels are provided. The aerogels are cross-linked via organic polymer chains that are attached to and extend from surface-bound functional groups provided or present over the internal surfaces of a mesoporous ceramic oxide particle network via appropriate chemical reactions. The functional groups can be hydroxyl groups, which are native to ceramic oxides, or they can be non-hydroxyl functional groups that can be decorated over the internal surfaces of the ceramic oxide network. Methods of preparing such mechanically strong ceramic oxide aerogels also are provided.

Leventis, Nicholas↗

Highly porous and mechanically strong ceramic oxide aerogels

Structurally stable and mechanically strong ceramic oxide aerogels are provided. The aerogels are cross-linked via organic polymer chains that are attached to and extend from surface-bound functional groups provided or present over the internal surfaces of a mesoporous ceramic oxide particle network via appropriate chemical reactions. The functional groups can be hydroxyl groups, which are native to ceramic oxides, or they can be non-hydroxyl functional groups that can be decorated over the internal surfaces of the ceramic oxide network. Methods of preparing such mechanically strong ceramic oxide aerogels also are provided.

Leventis, Nicholas↗

Oxidation of Silicon Particles Suspended in Mullite Matrix With Dual-Mode Vacancy Diffusion of Oxygen

Mullite bond coats filled with silicon particles have recently been proposed for the next generation of environmental barrier coatings (EBCs). The sacrificial oxidation of the silicon particles eliminates some of the environmental durability issues associated with traditional EBC designs. To investigate this novel design approach, a mathematical formulation and resulting numerical method have been developed for simulating the oxidation of silicon particles embedded in a mullite matrix. The focus is on the oxidation of the silicon in a dry oxygen environment where the oxidant is presumably oxygen. Oxygen transport from the exterior environment through the mullite is assumed to occur via two lattice defect diffusion mechanisms. As a result, the rate of oxygen transport is dictated by the self-diffusivity of the lattice defects. The numerical method is implemented using the COMSOL Multiphysics® program (COMSOL, Inc.). The method is applied to simulate the oxidation of silicon particles in a mullite pellet in recent oxidation experiments. Numerical results compare favorably with the oxidation behavior observed in the oxidation experiments. The numerical method is also used to investigate the effects of various features of the mullite-silicon particle system on the oxidation behavior.

silicon oxidation↗

Refining Methods to Determine the Isotopic Composition of Uranium Particles by Laser Ablation MC-ICP-MS

We report on efforts to mitigate the generation of isotopic anomalies during the ablation of micrometer-sized uranium oxide particles and analysis by MC-ICP-MS. The results of testing on particles of U200 indicate that laser fluence and frequency can affect isotopic data produced by laser ablation, but no settings were tested that could eradicate the signal spiking effect and generation of anomalous isotopic data for 234U/238U and 236U/238U. These anomalies are more frequent in samples with higher 235U enrichments, which is expected given their higher abundances of 234U and 236U. Of the standards tested here, only U005-A was anomaly-free. Efforts to compare the laser traces for particles with normal and anomalous isotopic compositions showed subtle differences in the behavior of the 234U/238U and 236U/238U ratios. However, it would be challenging to identify anomalous data points from a population of unknowns using this distinction, i.e., this is unlikely to be diagnostic. Thus, using current analytical hardware, we cannot eradicate the signal spiking phenomenon and cannot unambiguously identify isotopic anomalies from laser ablation traces. Ultimately, laser ablation ICP-MS would either require dramatic improvement to the ablation process and generation of more homogenous aerosols and/or improvements to detector electronics to identify and correct for the spiking phenomenon. Even if the reliability of the technique could be improved, a broader question to address is whether current data quality is of a high enough standard for laser ablation MC-ICP-MS to be used as a complementary technique to LG-SIMS for Safeguards.

organic↗

Location of nanophase Fe-oxides in palagonitic soils: Implication for Martian pigments

Palagonitic materials from Mauna Kea, Hawaii, were identified as Mars analogs based on their spectral and magnetic properties. These materials probably resulted from hydrothermal alteration during eruption of the volcano and/or from weathering under ambient conditions. The reflectance spectra of the Mars surface obtained by Earth-based telescopes and the reflectance spectra of analogs obtained in the laboratory show features due to electronic transitions of Fe(III) in oxide particles that range in size from nanometer (nanophase) to micrometer sized or larger. The presence of Fe(III) suggests oxidizing conditions during the alteration process in Mars that may have occurred in the past or during a slow ongoing process. Two naturally altered basaltic samples from Hawaii (HWMK12 and HWMK13) and a laboratory-altered (PH-13-DCGT2) basaltic glass similar in elemental composition to the above two samples was examined. All three samples exhibited spectral characteristics similar to martian bright-region spectra. Chemical and mineralogical changes occurring at the surface of these basalts were studied in order to understand the basis for their Mars-like properties. The spectral properties of the three samples were examined after the removal of Fe oxides by chemical extractants.

Golden, D. C.↗

Temperature-dependent formation of gradient structures with anomalous hardening in an Al–Si alloy

The temperature effect on forming gradient structure in an Al-Si alloy during surface severe deformation is studied in this report. The intermediate temperature (473 K) produces the steepest gradient structure by an anomalous hardening on the top layer compared to lower (300 K) and higher temperature (673 K) counterparts. Our analysis shows profuse aluminum oxide particles in the top layer of the gradient structure under 473 K and thus lead to anomalous hardening by oxide-dispersion strengthening. Here, the counterintuitive enhancement of strengthening at the intermediate temperature is explained by the dynamic interplay between thermal-driven, mechanical-aided oxidation and the wear-induced loss of surface materials as a function of temperature, which yields a critical processing temperature to achieve the steepest gradient structure.

36 MATERIALS SCIENCE↗

Solid-State Welding of the Nanostructured Ferritic Alloy 14YWT Using a Capacitive Discharge Resistance Welding Technique

Joining nanostructured ferritic alloys (NFAs) has proved challenging, as the nano-oxides that provide superior strength, creep resistance, and radiation tolerance at high temperatures tend to agglomerate, redistribute, and coarsen during conventional fusion welding. In this study, capacitive discharge resistance welding (CDRW)—a solid-state variant of resistance welding—was used to join end caps and thin-walled cladding tubes of the NFA 14YWT. The resulting solid-state joints were found to be hermetically sealed and were characterized across the weld region using electron microscopy (macroscopic, microscopic, and nanometer scales) and nanoindentation. Microstructural evolution near the weld line was limited to narrow (~50–200 μm) thermo-mechanically affected zones (TMAZs) and to a reduction in pre-existing component textures. Dispersoid populations (i.e., nano-oxides and larger oxide particles) appeared unchanged by all but the highest energy and power CDRW condition, with this extreme producing only minor nano-oxide coarsening (~2 nm → ~5 nm Ø). Despite a minimal microstructural change, the TMAZs were found to be ~10% softer than the surrounding base material. These findings are considered in terms of past solid-state welding (SSW) efforts—cladding applications and NFA-like materials in particular—and in terms of strengthening mechanisms in NFAs and the potential impacts of localized temperature–strain conditions during SSW.

36 MATERIALS SCIENCE↗

Nanotechnology Investigated for Future Gelled and Metallized Gelled Fuels

The objective of this research is to create combustion data for gelled and metallized gelled fuels using unique nanometer-sized gellant particles and/or nanometer-sized aluminum particles. Researchers at the NASA Glenn Research Center are formulating the fuels for both gas turbine and pulsed detonation engines. We intend to demonstrate metallized gelled fuel ignition characteristics for pulse detonation engines with JP/aluminum fuel and for gas turbine engines with gelled JP, propane, and methane fuel. The fuels to be created are revolutionary as they will deliver the highest theoretically maximum performance of gelled and metallized gelled fuels. Past combustion work has used micrometer-sized particles, which have limited the combustion performance of gelled and metallized gelled fuels. The new fuel used nanometer-sized aluminum oxide particles, which reduce the losses due to mismatch in the gas and solid phases in the exhaust. Gelled fuels provide higher density, added safety, reduced fuel slosh, reduced leakage, and increased exhaust velocity. Altogether, these benefits reduce the overall size and mass of the vehicle, increasing its flexibility.

Palaszewski, Bryan A.↗

Development of Composite Photocatalyst Materials that are Highly Selective for Solar Hydrogen Production and their Evaluation in Z-Scheme Reactor Designs

The key technology gap preventing a vertically stacked dual-bed particle suspension reactor from achieving the DOE MYRD&D ultimate cost target for H 2 production remains the lack of materials in particle form factor that exhibit ≥10% solar-to-H 2 energy conversion (STH) efficiency as a suspension. Therefore, our project goals centered around strategies to increase the STH efficiency by enhancing photophysical properties of perovskite oxide particles including increased visible-light absorption, increased selectivity for electrocatalysis of the H 2 evolution reaction (HER) and the O 2 evolution reaction (OER) through development of ultrathin oxide coatings, correlating composition and structure to function, and improving understanding of multiscale transport and kinetic processes.

08 HYDROGEN↗

Charging Reactions Promoted by Geometrically Necessary Dislocations in Battery Materials Revealed by In Situ Single-Particle Synchrotron Measurements

Crystallographic defects exist in many redox active energy materials, e.g., battery and catalyst materials, which significantly alter their chemical properties for energy storage and conversion. However, there is lack of quantitative understanding of the interrelationship between crystallographic defects and redox reactions. Herein, crystallographic defects, such as geometrically necessary dislocations, are reported to influence the redox reactions in battery particles through single-particle, multimodal, and in situ synchrotron measurements. Through Laue X-ray microdiffraction, many crystallographic defects are spatially identified and statistically quantified from a large quantity of diffraction patterns in many layered oxide particles, including geometrically necessary dislocations, tilt boundaries, and mixed defects. The in situ and ex situ measurements, combining microdiffraction and X-ray spectroscopy imaging, reveal that LiCoO 2 particles with a higher concentration of geometrically necessary dislocations provide deeper charging reactions, indicating that dislocations may facilitate redox reactions in layered oxides during initial charging. The present study illustrates that a precise control of crystallographic defects and their distribution can potentially promote and homogenize redox reactions in battery materials.

25 ENERGY STORAGE↗