Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Oxidation behavior”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Comparison of Short-Term Oxidation Behavior of Model and Commercial Chromia-Forming Ferritic Stainless Steels in Air with Water Vapor

A high-purity Fe-20Cr and commercial type 430 ferritic stainless steel were exposed at 700 and 800 C in dry air and air with 10% water vapor (wet air) and characterized by SEM, XRD, STEM, SIMS, and EPMA. The Fe-20Cr alloy formed a fast growing Fe-rich oxide scale at 700 C in wet air after 24 h exposure, but formed a thin chromia scale at 700 C in dry air and at 800 C in both dry air and wet air. In contrast, thin spinel + chromia base scales with a discontinuous silica subscale were formed on 430 stainless steel under all conditions studied. Extensive void formation was observed at the alloy-oxide interface for the Fe-20Cr in both dry and wet conditions, but not for the 430 stainless steel. The Fe-20Cr alloy was found to exhibit a greater relative extent of subsurface Cr depletion than the 430 stainless steel, despite the former's higher Cr content. Depletion of Cr in the Fe-20Cr after 24 h exposure was also greater at 700 C than 800 C. The relative differences in oxidation behavior are discussed in terms of the coarse alloy grain size of the high-purity Fe-20Cr material, and the effects of Mn, Si, and C on the oxide scale formed on the 430 stainless steel.

08 HYDROGEN↗

Hydrothermal corrosion and steam oxidation behavior comparison of UAM and conventional Zry-4

Here, hydrothermal corrosion and steam exposures on ultrasonic additively manufactured (UAM) Zircaloy-4 (Zry-4) specimens were conducted to compare to wrought Zry-4 performance in both simulated pressurized water reactor (PWR) operation (330°C, 15 MPa, <50 ppb oxygen, 500h) and representative accident conditions (100% H 2 O(g) at 700, 900, and 1100°C for up to 1h). UAM Zry-4 specimens showed 50% higher mass gain in PWR conditions and 50-80% more mass gain in steam oxidation due to internal oxidation between build layers in both cases. UAM Zry-4 in 900°C steam showed breakaway oxidation leading to sample deformation. Titanium used as an interlayer in the UAM process was detected in the substrate after the 1100°C exposure. Additional experiments to better link as-built defects to oxidation behavior are needed.

36 MATERIALS SCIENCE↗

Creep and oxidation behavior of modified CF8C-plus with W, Cu, Ni, and Cr

Here, the microstructures of modified CF8C-Plus (Fe-19Cr-12Ni-0.4W-3.8Mn-0.2Mo-0.6Nb-0.5Si-0.9C) with W and Cu (CF8CPWCu) and CF8CPWCu enhanced with 21Cr + 15Ni or 22Cr + 17.5Ni were characterized in the as-cast condition and after creep testing. When imaged at lower magnifications, the as-cast microstructure was similar among all three alloys as they all contained a Nb-rich interdendritic phase and Mn-based inclusions. Transmission electron microscopy (TEM) analysis showed the presence of nanoscale Cu-rich nanoprecipitates distributed uniformly throughout the matrix of CF8CPWCu, whereas in CF8CPWCu22/17, Cu precipitates were found primarily at the grain boundaries. The presence of these nanoscale Cu-rich particles, in addition to W-rich Cr 23 C 6 , nanoscale Nb carbides, and Z-phase (Nb 2 Cr 2 N 2 ), improved the creep strength of the CF8CPWCu steel. Modification of CF8CPWCu with Cr and Ni contents slightly decreased the creep strength but significantly improved the oxidation behavior at 1073 K (800 °C). In particular, the addition of 22Cr and 17.5Ni strongly enhanced the oxidation resistance of the stainless steel resulting in a 100 degrees or greater temperature improvement, and this composition provided the best balance between improving both mechanical properties and oxidation resistance.

36 MATERIALS SCIENCE↗

Furnace Cyclic Oxidation Behavior of Multi-Component Low Conductivity Thermal Barrier Coatings

Ceramic thermal barrier coatings will play an increasingly important role in advanced gas turbine engines because of their ability to further increase engine operating temperatures and reduce cooling, thus helping achieve future engine low emission, high efficiency and improved reliability goals. Advanced multi-component zirconia-based thermal barrier coatings are being developed using an oxide defect clustering design approach to achieve the required coating low thermal conductivity and high temperature stability. Although the new composition coatings were not yet optimized for cyclic durability, an initial durability screening of the candidate coating materials was conducted using conventional furnace cyclic oxidation tests. In this paper, furnace cyclic oxidation behavior of plasma-sprayed zirconia-based defect cluster thermal barrier coatings was investigated at 1163 C using 45 min hot cycles. The ceramic coating failure mechanisms were studied using scanning electron microscopy (SEM) combined with X-ray diffraction (XRD) phase analysis after the furnace tests. The coating cyclic lifetime is also discussed in relation to coating processing, phase structures, dopant concentration, and other thermo-physical properties.

Zhu, Dong-Ming↗

High-Temperature Oxidation Behavior of Wrought and Additive Manufactured H282 in Direct-Fired Supercritical CO2 Power Cycle Environments

Materials selection is a key concern for corrosion resistance in high temperature and pressure direct-fired supercritical CO2 power cycles. The effect of elevated pressure on corrosion resistance can be critical, as impurities within the supercritical fluid such as H2O and O2 can result in additional corrosion behaviors. Utilizing additive manufacturing (AM) methods for construction of power cycle components requiring both compact and complex designs could be advantageous. AM H282 produced by laser powder bed fusion was exposed to direct-fired conditions (95CO2 – 4H2O – 1 O2) at 750 °C at both atmospheric pressure and supercritical conditions (20 MPa) for up to 4,000 hours. Oxidation behavior, sub-surface carbide formation, and chromia scale volatilization was dependent upon AM preparation techniques and surface modifications. These results are discussed in terms of the potential compatibility issues that may arise when using AM alloys in high temperature regions of direct-fired sCO2 power cycles, particularly for thin-walled components.

Carney, Casey↗

Oxidation Behavior of Welded Fe-Based and Ni-Based Alloys in Supercritical CO 2

Next-generation supercritical CO 2 (sCO 2 ) power cycles will require different classes of alloy throughout the operational temperatures to optimize tradeoff of creep strength, oxidation performance and cost. This will necessitate joining methods such as welding, which might pose compatibility concerns at the joined interfaces. In this study, similar and dissimilar metal welds were generated from a variety of candidate alloys for sCO 2 systems including ferritic/martensitic steels, austenitic steels, and Ni-based superalloys. Samples were extracted from different regions of the welds and exposed to sCO 2 at 550 °C and 20 MPa for 2500 h, then characterized to understand their behavior in this environment. Unsurprisingly, the local oxidation behavior was largely dictated by the Cr content in the underlying metal. High-Cr austenitic steels and Ni alloys formed slow-growing Cr-rich oxide scales with minimal carburization of the underlying metal, while low-Cr ferritic/martensitic steels formed fast-growing Fe-rich oxide scales with significant carburization. Most welds did not show any unusual oxidation behavior at the interfaces, considering the local Cr content. The one exception was the 347H similar metal weld, where a larger grain size and complex grain structure in the fusion zone led to a significantly higher rate of Fe-rich oxide nodule formation compared to the base metal. This suggests that microstructural changes at joined interfaces can play an important role on the oxidation-limited lifetimes in future sCO 2 systems. The composition changes across the interfaces enabled study of the effect of Fe on the growth rate of Cr-rich oxides and of the origins of the sub-surface recrystallization zone that forms beneath them.

36 MATERIALS SCIENCE↗

Long-term oxidation behavior of spinel-coated ferritic stainless steel for solid oxide fuel cell interconnect applications

Long-term tests (>8,000 hours) indicate that AISI 441 ferritic stainless steel coated with a Mn-Co spinel protection layer is a promising candidate material system for IT-SOFC interconnect applications. While uncoated AISI 441 showed a substantial increase in area-specific electrical resistance (ASR), spinel-coated AISI 441 exhibited much lower ASR values (11-13 mOhm-cm2). Formation of an insulating silica sublayer beneath the native chromia-based scale was not observed, and the spinel coatings reduced the oxide scale growth rate and blocked outward diffusion of Cr from the alloy substrate. The structure of the scale formed under the spinel coatings during the long term tests differed from that typically observed on ferritic stainless steels after short term oxidation tests. While short term tests typically indicate a dual layer scale structure consisting of a chromia layer covered by a layer of Mn-Cr spinel, the scale grown during the long term tests consisted of a chromia matrix with discrete regions of Mn-Cr spinel distributed throughout the matrix. The presence of Ti in the chromia scale matrix and/or the presence of regions of Mn-Cr spinel within the scale may have increased the scale electrical conductivity, which would explain the fact that the observed ASR in the tests was lower than would be expected if the scale consisted of pure chromia.

Stevenson, Jeffry W.↗

Theoretical Study of the Oxidation Behavior of Precipitation Hardening Steel

The oxidation of precipitation hardening (PH) steels is a rather unexplored area. In the present work an attempt is made is made to estimate the kinetics of a PH steel. For this purpose specimens of the material under examination were isothermally heated at 850, 900 and 950 deg. C for 15 hr. Kinetics was based on TGA results. During heating a thick scale is formed on the substrate surface, which is composed by different oxides. The layer close to the substrate is compact and as a result it impedes corrosion. The mathematical analysis of the collected data shows that the change of the mass of the substrate per unit area versus time is described by a parabolic law.

36 MATERIALS SCIENCE↗

Effect of the theta-alpha-Al2O3 transformation on the oxidation behavior of beta-NiAl+Zr

Isothermal oxidation of NiAl+Zr has been performed over the temperature range of 800-1200 C and studied by TGA, XRD, and SEM. A discontinuous decrease in growth rate of two orders of magnitude was observed at 1000 C due to the formation of alpha-Al2O3 from theta-Al2O3. This transformation also resulted in a dramatic change in the surface morphology of the scales, as a whisker topography was changed into a weblike network of oxide ridges and radial transformation cracks. It is believed that the ridges are evidence for a short-circuit outward aluminum diffusion growth mechanism that has been documented in a number of O-18 tracer studies.

Rybicki, George C.↗

Oxidation Behavior of Zirconium Diboride Nanoparticles

The products of oxidation of ZrB{sub 2} powders with average particle sizes of ~100 and ~30 nm by atmospheric oxygen under isothermal conditions and during heating have been characterized by thermal analysis, X-ray diffraction, scanning electron microscopy, IR frustrated total internal reflection spectroscopy, energy dispersive X-ray analysis, and elemental analysis. The oxidation onset has been observed at 594 and 396°C, respectively. Oxidation at temperatures of ≥800°C leads to the formation of boron oxide and monoclinic ZrO{sub 2}, independent of the particle size of ZrB{sub 2}. The reaction rate constants for the oxidation of ZrB{sub 2} nanoparticles ~100 and ~30 nm in size have been determined to be 0.03, 0.15, and 0.31 h{sup –1} at 600, 650, and 700°C and 0.11, 0.35, and 0.81 h{sup –1} at 500, 600, and 700°C, respectively. The apparent activation energies for the oxidation of the ZrB{sub 2} nanoparticles ~100 and ~30 nm in size are 161 ± 4 and 62 ± 3 kJ/mol, respectively, as evaluated from the temperature dependence of the rate constants at the above temperatures.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Effect of Surface Treatment on High-Temperature Oxidation Behavior of IN 713C

The effects of surface preparations on oxidation kinetics and oxide scale morphology for the commercially available Ni-based superalloy IN 713C have been investigated. The ground and polished samples were exposed in air at 800-1100 °C. The ground specimens were found to demonstrate lower oxidation kinetics compared to those after polishing. The grinding also affected the oxide scale morphology, resulting in a protective alumina scale, while the polished samples developed Ni-/Cr-rich mixed oxides on the surface. Better oxidation resistance of the ground surfaces is related to a higher concentration of defects in the near-surface region introduced by cold working. These defects facilitate the outward transport of the scale-forming element Al and thus are beneficial for protective oxidation. The oxidation mechanism at lower temperatures was introduced. The model based on the generalized Darken method and multiphase approximation was proposed.

36 MATERIALS SCIENCE↗

Oxidation Behavior of Austenitic Steels in Supercritical Water Containing Dissolved Oxygen

Oxidation tests of austenitic steel Super304H and HR3C were conducted at 550-600 °C in supercritical water under 25 MPa with the dissolved oxygen content. The oxidation rate of Super304H rapidly increased with increasing temperature, while the weight change of HR3C at 600 °C is slightly larger than that at 550 °C. A double-layer oxide scale developed on Super304H and HR3C steel, which was made up of an Fe-rich outer layer and a Cr-rich inner layer. The criterion contents of Cr were calculated for Super304H and HR3C. The effect of temperature and the Cr content on oxidation rate and oxide composition were discussed.

36 MATERIALS SCIENCE↗

Oxidation Behavior of Irradiated and Unirradiated NBG-25 Graphite

This presentation discusses The xxidation behavior of irradiated and unirradiated NBG-25 Graphite results of thermogravimetric analysis of same-source specimens from the AGC-1 experiement. Minimal annealing effects, Substantial increase in OR with Irradiation using Conventional Rate Analysis, Apparent Dose Dependency, Examination of Onset (Alternate Analysis) Shows Competing Irradiation Effects, and Similar Test Matrix (without annealing) now under way with NBG-18 Graphite is reviewed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effect of H2O and CO2 on The Oxidation Behavior and Durability at High Temperature of ODS-FeCrAl

Cyclic oxidation testing was conducted on alloy MA956 and two different batches of alloy PM2000 at 1100 and 1200 C in different atmospheres rich in O2, H2O and CO2. Compared to 1h cycles in dry O2, exposure in air+10 vol.% H2O resulted in an increase of the oxidation rate and a decrease of the time to breakaway for all alloys at 1200 C, and a faster consumption of Al in the MA956 alloy. One hour cyclic testing in 49.25%CO2+50%H2O+0.75% O2 had a smaller effect on the oxidation rate but led to increased formation of voids in alloy MA956, which had an impact on the alloy creep resistance. At 1100 C, exposure in 50%CO2+50%H2O resulted in significant oxide spallation compared with oxidation in air, but this was not the case when 0.75% O2 was added to the CO2/H2O mixture as a buffer. The control of impurity levels drastically improved the oxidation resistance of PM2000.

CO2↗

Influence of cyclic thermal treatments on the oxidation behavior of Ti-6Al-2Sn-4Zr-2Mo alloy

Highlights: • The oxidation kinetics of commercially titanium alloys has been extensively investigated following isothermal treatments. • Components in aerospace applications are subjected to temperature gradients which can modify the oxidation kinetics of Ti-6242. • The main goal of the present research is to study the formation of the oxide scale and the alpha case layer under cyclic thermal treatments • Results are with those achieved by isothermal treatments. - Abstract: Ti-6Al-2Sn-4Zr-2Mo is one of the most common titanium alloys for aerospace industry. This alloy experiences oxidation phenomenon at elevated temperatures. In the present study, cyclic thermal treatments were performed in air at 500, 593 and 700 °C, up to 500 cycles, in order to determine the oxidation kinetics and to analyze the oxide scale and alpha-case formation. Moreover, results were compared to those achieved under isothermal conditions to elucidate differences between both thermal conditions. In this sense, metallographic techniques and X-ray diffraction, together with a detailed advanced characterization of the microstructure by Field Emission Scanning Electron Microscopy and Focus Ions Beam, were used to analyze surface oxidation evolution. Results pointed out that cyclic treatments induced a strong increase of the weight gain compared to isothermal treatments. The analysis of the oxide scale revealed the formation of not only rutile, as isothermal treatments, but also anatase. Thickness of the oxide scale was higher for cyclic conditions, while alpha case did not exceed values reached by isothermal treatments and even became lower at 500 °C.

36 MATERIALS SCIENCE↗

Subparabolic Oxidation Behavior of Silicon Carbide at 1300 C

The phenomenon of subparabolic oxide growth rate, more the rule than the exception in the oxidation of silica formers, is examined in light of data sets acquired in SiC oxidation experiments at 1300 C. Negative deviation from parabolic kinetics is shown to correlate with oxide crystallinity. The data sets were analyzed to ascertain the predominant and contributing growth laws, and tested with models that describe the overall kinetics as combinations of the familiar growth laws.

Ogbuji, Linjus U. J. T.↗