Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “LITHIUM 10”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Evaporated lithium surface coatings in NSTX.

Two lithium evaporators were used to evaporate more than 100 g of lithium on to the NSTX lower divertor region. Prior to each discharge, the evaporators were withdrawn behind shutters, where they also remained during the subsequent HeGDC applied for periods up to 9.5 min. After the HeGDC, the shutters were opened and the LITERs were reinserted to deposit lithium on the lower divertor target for 10 min, at rates of 10-70 mg/min, prior to the next discharge. The major improvements in plasma performance from these lithium depositions include: (1) plasma density reduction as a result of lithium deposition; (2) suppression of ELMs; (3) improvement of energy confinement in a low-triangularity shape; (4) improvement in plasma performance for standard, high-triangularity discharges; (5) reduction of the required HeGDC time between discharges; (6) increased pedestal electron and ion temperature; (7) reduced SOL plasma density; and (8) reduced edge neutral density.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Evaporated Lithium Surface Coatings in NSTX

Two lithium evaporators were used to evaporate more than 100 g of lithium on to the NSTX lower divertor region. Prior to each discharge, the evaporators were withdrawn behind shutters, where they also remained during the subsequent HeGDC applied for periods up to 9.5 min. After the HeGDC, the shutters were opened and the LITERs were reinserted to deposit lithium on the lower divertor target for 10 min, at rates of 10-70 mg/min, prior to the next discharge. The major improvements in plasma performance from these lithium depositions include: 1) plasma density reduction as a result of lithium deposition; 2) suppression of ELMs; 3) improvement of energy confinement in a low-triangularity shape; 4) improvement in plasma performance for standard, high-triangularity discharges; 5) reduction of the required HeGDC time between discharges; 6) increased pedestal electron and ion temperature; 7) reduced SOL plasma density; and 8) reduced edge neutral density.

10100 Impurities↗

Experimental studies of lithium-based surface chemistry for fusion plasma-facing materials applications

Lithium has enhanced the operational performance of fusion devices such as: TFTR, CDX-U, FTU, T-11 M, and NSTX. Lithium in the solid and liquid state has been studied extensively in laboratory experiments including its erosion and hydrogen-retaining properties. Reductions in physical sputtering up to 40–60% have been measured for deuterated solid and liquid lithium surfaces. Computational modeling indicates that up to a 1:1 deuterium volumetric retention in lithium is possible. This paper presents the results of systematic in situ laboratory experimental studies on the surface chemistry evolution of ATJ graphite under lithium deposition. Results are compared to post-mortem analysis of similar lithium surface coatings on graphite exposed to deuterium discharge plasmas in NSTX. Lithium coatings on plasma-facing components in NSTX have shown substantial reduction of hydrogenic recycling. Questions remain on the role lithium surface chemistry on a graphite substrate has on particle sputtering (physical and chemical) as well as hydrogen isotope recycling. This is particularly due to the lack of in situ measurements of plasma-surface interactions in tokamaks such as NSTX. Results suggest that the lithium bonding state on ATJ graphite is lithium peroxide and with sufficient exposure to ambient air conditions, lithium carbonate is generated. Further, correlation between both results is used to assess the role of lithium chemistry on the state of lithium bonding and implications on hydrogen pumping and lithium sputtering. In addition, reduction of factors between 10 and 30 reduction in physical sputtering from lithiated graphite compared to pure lithium or carbon is also measured.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Lithium in M67

Echelle spectra recorded at the Li I 6707-A line are reported for seven main-sequence members and one cool subgiant in M67. The spectral types of the seven dwarfs studied range from about F8 at the turnoff point to about G5. The principal result is that the average lithium abundance in the three hottest main-sequence stars is 0.45 x 10 to the -9th. Any enrichment of lithium in the gas of the Galactic disk in the last 5 Gyr therefore has not exceeded a factor of about two and probably is entirely negligible, when the corresponding results for NGC 752 and the Hyades are taken into account.

Hobbs, L. M.↗

A Lithium Superionic Sulfide Cathode for Lithium-Sulfur Batteries

This work presents a facile synthesis approach for core-shell structured Li2S nanoparticles, which have Li2S as the core and Li3PS4 as the shell. This material functions as lithium superionic sulfide (LSS) cathode for long-lasting, energy-efficient lithium-sulfur (Li-S) batteries. The LSS has an ionic conductivity of 10-7 S cm-1 at 25 oC, which is 6 orders of magnitude higher than that of bulk Li2S (~10-13 S cm-1). The high lithium-ion conductivity of LSS imparts an excellent cycling performance to all-solid Li-S batteries, which also promises safe cycling of high-energy batteries with metallic lithium anodes.

batteries↗

Evaporated lithium surface coatings in NSTX

Two lithium evaporators were used to evaporate more than 100 g of lithium on to the NSTX lower divertor region. Prior to each discharge, the evaporators were withdrawn behind shutters, where they also remained during the subsequent HeGDC applied for periods up to 9.5 min. After the HeGDC, the shutters were opened and the LITERs were reinserted to deposit lithium on the lower divertor target for 10 min, at rates of 10–70 mg/min, prior to the next discharge. Overall, the major improvements in plasma performance from these lithium depositions include: (1) plasma density reduction as a result of lithium deposition; (2) suppression of ELMs; (3) improvement of energy confinement in a low-triangularity shape; (4) improvement in plasma performance for standard, high-triangularity discharges; (5) reduction of the required HeGDC time between discharges; (6) increased pedestal electron and ion temperature; (7) reduced SOL plasma density; and (8) reduced edge neutral density.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Sol–gel synthesis and lithium ion conduction properties of garnet-type Li{sub 6}BaLa{sub 2}Ta{sub 2}O{sub 12}

Graphical abstract: Li{sub 6}BaLa{sub 2}Ta{sub 2}O{sub 12}, prepared by sol–gel synthesis method, shows a total Li-ion conductivity of 1.69 × 10{sup −5} S/cm at 298 K and an activation energy is 0.40 eV. Highlights: ► Garnet-type fast ion conductor LLBTO was synthesized by modified sol–gel Pechini method. ► The synthesis temperature is significantly lower (200 K) than conventional solid state synthesis methods. ► The ionic conductivity of sol–gel synthesized LLBTO is 1.69 × 10{sup −5} S/cm. -- Abstract: High lithium ion conductive garnet-type barium lanthanum lithium tantalate, Li{sub 6}BaLa{sub 2}Ta{sub 2}O{sub 12} (LLBTO), was prepared by a modified sol–gel Pechini method from the appropriate mixtures of lithium carbonate, lanthanum oxide, barium carbonate and tantalum ethoxide. The thermal decomposition of the precursor powder was investigated by TG/DTA analysis. The LLBTO precursor powders were annealed at various temperatures between 923 and 1123 K for 6 h in air. The transformation process from precursor powder to crystalline garnet-like phase was analyzed by X-ray powder diffraction (XRPD). The morphology of the powders annealed at various temperatures was investigated by scanning electron microscopy (SEM). The resultant pelletized Li{sub 6}BaLa{sub 2}Ta{sub 2}O{sub 12}, prepared by sol–gel synthesis method, shows a total Li-ion conductivity of 1.69 × 10{sup −5} S/cm at 298 K and an activation energy is 0.40 eV. The ionic conductivities reported in this study are slightly higher than those reported for LLBTO sample synthesized by conventional solid state synthesis route.

36 MATERIALS SCIENCE↗

Enabling Extreme Fast-Charging: Challenges at the Cathode and Mitigation Strategies

We report charging lithium-ion batteries (LiBs) in 10 to 15 min via extreme fast-charging (XFC) is important for the widespread adoption of electric vehicles (EVs). Lately, the battery research community has focused on identifying XFC bottlenecks and determining novel design solutions. Like other LiB components, cathodes can present XFC bottlenecks, especially when considering long-term battery life. Therefore, it is necessary to develop a comprehensive understanding of how XFC conditions degrade LiB cathodes. The present article reviews relevant cathode-focused studies and summarizes the current understanding regarding cathode performance and aging issues under XFC conditions. Dominant aging modes and mechanisms are identified at different length-scales with electrochemical correlations for LiNi x Mn y Co z O 2 (NMC)-based cathodes. A range of electrochemical techniques and models provide key insights into cathode performance and life issues. A suite of multimodal and multiscale microscopy and X-ray techniques is surveyed to quantify chemical, structural, and crystallographic NMC-cathode degradation. Cathode cycle-life is scaled to equivalent EV miles to illustrate how cathode degradation translates to real-world scenarios and quantifies cathode-related bottlenecks that hinder XFC adoption. Finally, the article discusses several cathode cycle-life aging mitigation strategies with example case studies and identifies remaining challenges.

25 ENERGY STORAGE↗

Novel Zwitterionic Polyurethane-in-Salt Electrolytes with High Ion Conductivity, Elasticity, and Adhesion for High-Performance Solid-State Lithium Metal Batteries

This study presents a novel polymer-in-salt (PIS) zwitterionic polyurethane-based solid polymer electrolyte (zPU-SPE) that offers high ionic conductivity, strong interaction with electrodes, and excellent mechanical and electrochemical stabilities, making it promising for high-performance all solid-state lithium batteries (ASSLBs). The zPU-SPE exhibits remarkable lithium-ion (Li+) conductivity (3.7 × 10⁻⁴ S cm−1 at 25 °C), enabled by exceptionally high salt loading of up to 90 wt.% (12.6 molar ratio of Li salt to polymer unit) without phase separation. It addresses the limitations of conventional SPEs by combining high ionic conductivity with a Li+ transference number of 0.44, achieved through the incorporation of zwitterionic groups that enhance ion dissociation and transport. The high surface energy (338.4 J m−2) and elasticity ensure excellent adhesion to Li anodes, reducing interfacial resistance and ensuring uniform Li+ flux. When tested in Li||zPU||LiFePO₄ and Li||zPU||S/C cells, the zPU-SPE demonstrated remarkable cycling stability, retaining 76% capacity after 2000 cycles with the LiFePO4 cathode, and achieving 84% capacity retention after 300 cycles with the S/C cathode. Molecular simulations and a range of experimental characterizations confirm the superior structural organization of the zPU matrix, contributing to its outstanding electrochemical performance. The findings strongly suggest that zPU-SPE is a promising candidate for next-generation ASSLBs.

Wang, Kun↗

Effect of Ionic Liquid Components on the Coil Dimensions of PEO

Here, small-angle neutron scattering is used to measure the infinite dilution radius of gyration ($R_{g,0}$) for a range of molecular weights (10–250 kg/mol) of perdeuterated poly(ethylene oxide) (d-PEO) in various imidazolium-based ILs at 80 °C. The Flory exponents ($\nu$) evaluated in the ILs studied (1-butyl-3-methylimidazolium bis(trifluoromethylsulfonyl)imide ([BMIM][TFSI]), 1-butyl-3-methylimidazolium hexafluorophosphate ([BMIM][PF 6 ]), and 1-hexyl-3-methylimidazolium tetrafluoroborate ([HMIM][BF 4 ])) lie between 0.58 and 0.60, indicating good solvent behavior. The coil dimensions of d-PEO increase on increasing the alkyl chain length of the cation and on decreasing the anion basicity. A more pronounced effect on coil dimensions is observed upon altering the anion, compared to the dependence on cation alkyl chain length. The temperature dependence of $R_{g,0}$ is found to be moderate in 1-ethyl-3-methylimidazolium tetrafluoroborate ([EMIM][BF 4 ]), where the coil size decreases upon increasing the temperature from 80 to 135 °C. Addition of up to 10 wt % of a salt, lithium bis(trifluoromethylsulfonyl)imide, to mixtures of d-PEO and [BMIM][TFSI] has no significant effect on $R_{g,0}$. These results are discussed in terms of the relative interactions among PEO, the cation, and the anion.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Magnon gap tuning in lithium-doped MnTe

Data in this DOI includes: 1) Powder Diffraction at HFIR POWDER (HB-2A) of pure MnTe and 5%-lithium doped MnTe at various temperatures ranging from T = 4 - 360 K for pure MnTe and T = 4 - 290 K for 5% lithium doped MnTe. 2) Inelastic neutron scattering at ARCS of pure MnTe and 5% lithium doped MnTe at T = 10 K measured with incident energy Ei = 30 meV and 150 meV, and corresponding background files (i.e. empty can measurements)

diffraction↗

HPC4Mfg with Sepion

We employed ab-initio simulations and quantum chemical calculations to develop a computational framework for simulating the microscopic structure and mechanical properties of novel polymer membranes used in lithium sulfur batteries. To meet industry targets, next generation batteries with high specific energy (Wh/kg) are essential. Efforts to commercialize light-weight, energy-dense lithium-sulfur secondary batteries (2510 Wh/kg) have been stalled by ongoing problems with the battery’s separator membrane, which should prevent cross-over of active material from cathode to anode that, if unchecked, limits cycle-life. However, Sepion Technologies’ polymer membranes yield long-lasting lithium-sulfur cells. Advancing to 10 Ah battery prototypes, Sepion faces challenges in membrane manufacturing related to polymer processing and the molecular basis for membrane performance and durability. High performance computing offers critical new insight into these phenomena, which in turn will accelerate product entry into the market.

25 ENERGY STORAGE↗

New Aptes Cross-linked Polymers from Poly(ethylene oxide)s and Cyanuric Chloride for Lithium Batteries

A new series of polymer electrolytes for use as membranes for lithium batteries are described. Electrolytes were made by polymerization between cyanuric chloride and diamino-terminated poly(ethylene oxide)s, followed by cross-linking via a sol-gel process. Thermal analysis and lithium conductivity of freestanding polymer films were studied. The effects of several variables on conductivity were investigated, such as length of backbone PEO chain, length of branching PEO chain, extent of branching, extent of cross-linking, salt content, and salt counterion. Polymer films with the highest percentage of PEO were found to be the most conductive, with a maximum lithium conductivity of 3.9 x 10(exp -5) S/cm at 25 C. Addition of plasticizer to the dry polymers increased conductivity by an order of magnitude.

Tigelaar, Dean M.↗

Extreme Fast Charge Challenges for Lithium-Ion Battery: Variability and Positive Electrode Issues

Enabling a 10 min fast charge for electric vehicles is a possible route to reduce range anxiety and increase the utility of electric vehicles. While lithium plating during fast charging is a known challenge, the full suite of limitations which occur in full cells during a 10 min fast charge are unknown. In the present work the central constraints of extreme fast charging are explored through extensive experiments and analysis in single layer graphite/NMC532 pouch cells. Methods of developing fast-charging protocols considering the impedance and transport limitations are presented and the relative benefits of altering the charging rate, profile, relaxation, etc., are investigated. Analysis during and at the end of cycling identified both known and unexpected aging pathways. The most distinct outcomes from the work are a significant increase in cell-to-cell variability as the number of fast charge cycles increase [up to 11% (1σ)] and the identification of distinct aging of the NMC532 positive electrode including cracking of the secondary particles and a trend toward under-lithiation of the positive electrode. Here, while significant aging of the positive electrode was observed, only a few conditions had discernible Li plating and no distinct reversible Li signature was seen during periodic reference performance tests.

25 ENERGY STORAGE↗

Generation of meter-scale hydrogen plasmas and efficient, pump-depletion-limited wakefield excitation using 10 GeV electron bunches

High repetition rates and efficient energy transfer to the accelerating beam are important for a future linear collider based on the beam-driven plasma wakefield acceleration scheme (PWFA-LC). This paper reports the first results from the Plasma Wakefield Acceleration Collaboration (E300) that are beginning to address both of these issues using the recently commissioned FACET-II facility at SLAC national accelerator laboratory. Here we have generated meter-scale hydrogen plasmas using time-structured 10 GeV electron bunches from FACET-II, which hold the promise of dramatically increasing the repetition rate of PWFA by rapidly replenishing the gas between each shot compared to the hitherto used lithium plasmas that operate at 1–10 Hz. Furthermore, we have excited wakes in such plasmas that are suitable for high gradient particle acceleration with high drive-bunch to wake energy transfer efficiency- a first step in achieving a high overall energy transfer efficiency. We have done this by using time-structured electron drive bunches that typically have one or more ultra-high current (> 30 kA) femtosecond spike(s) superimposed on a longer (~0.4 ps) lower current (< 10 kA) bunch structure. The first spike effectively field-ionizes the gas and produces a meter-scale (30–160 cm) plasma, whereas the subsequent beam charge creates a wake. The length and amplitude of the wake depends on the longitudinal current profile of the bunch and plasma density. We find that the onset of pump depletion, when some of the drive beam electrons are nearly fully depleted of their energy, occurs for hydrogen pressure ≥ 1.5Torr. We also show that some electrons in the rear of the bunch can gain several GeV energies from the wake. These results are reproduced by particle-in-cell simulations using the QPAD code. At a pressure of ~2Torr, simulation results and experimental data show that the beam transfers about 60% of its energy to the wake.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Evaluation of cermet materials suitable for lithium lubricated thrust bearings for high temperature operation

Cerment materials (HfC - 10 wt% W; HfC - 10 wt% TaC - 10 wt%W; HfC - 2 wt% CbC - 8 wt% Mo;Hfn - 10 wt% W; Hfn - 10 wt% TaN - 10 wt% W; and ZrC - 17 wt% W) were evaluated for possible use as lithium-lubricated bearings in the control system of a nuclear reactor. Tests of compatibility with lithium were made in T-111 (Ta-8W-2Hf) capsules at temperatures up to 1090 C. The tendencies of HfC-TaC-W, HfC-CbC-Mo, and HfN-W to bond to themselves and to the refractory alloys T-111 and TZM when enclosed in lithium-filled capsules under a pressure of 2000 psi at 980 and 1200 C for 1933 hours were evaluated. Thermal expansion characteristics were determined for the same three materials from room temperature to 1200 C. On the basis of these tests, HfC-10 TaC-10W and HfN-10W were selected as the best and second best candidates, respectively, of the materials tested for the bearing application.

Sinclair, J. H.↗

Role of ligands in the stability of B n X n and CB n-1 X n (n = 5–10; X = H, F, CN) and their potential as building blocks of electrolytes in lithium ion batteries

Stabilizing small multiply charged negative ions in the gas phase has been of considerable interest in recent years. B12H122- is one of the most well-known dianions which is stable against auto-detachment of its second electron in the gas phase by 0.9 eV, whereas BnHn2- with n < 12 is unstable. Using density functional theory, we have examined systematically the role of ligands in stabilizing smaller mono- and di-anions of BnXn and CBn-1Xn (n = 5–10; X = H, F, CN). We show that the stability of the negative ions of these complexes increases with the electron affinity of the ligand and Bn(CN)n2- can even be stable against electron emission for n ≥ 5. We also show that CBn-1(CN)n2- is stable against electron emission for n ≥ 8, even though these moieties contain one electron more than needed to satisfy the Wade–Mingos rule. We have examined the potential of these stable negative ions as building blocks of electrolytes in Li-ion batteries. By calculating the binding energies between the CBn-1Xn1-,2- and Li+, we find that some of these clusters may even outperform CB11H12- as electrolytes in metal-ion batteries.

Zhong, MingMin↗