Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Interphases”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Quantifying Lithium Ion Exchange in Solid Electrolyte Interphase (SEI) on Graphite Anode Surfaces

Solid Electrolyte Interphase (SEI) has been identified as the most important and least understood component in lithium-ion batteries. Despite extensive studies in the past two decades, a few mysteries remain: what is the chemical form of and degree of mobility of Li + in the interphase? What fraction of Li + is permanently immobilized in the SEI, while the rest are still able to participate in the cell reactions via the ion-exchange process with Li + in the electrolyte? This study attempted to answer, in part, these questions by using 6 Li and 7 Li-isotopes to label SEIs and electrolytes, and then quantifying the distribution of permanently immobilized and ion-exchangeable Li + with solid-state NMR and ToF-SIMS. The results showed that the majority of Li + were exchanged after one SEI formation cycle, and a complete exchange after 25 cycles. Ion exchange by diffusion based on concentration gradient in the absence of applied potential also occurred simultaneously. This knowledge will provide a foundation for not only understanding but also designing better SEIs for future battery chemistries.

25 ENERGY STORAGE↗

Electronic and Structural Properties of the Polymer-Electrolyte Interphase in Electrochemically Doped Polymers

The advance of soft, polymer-based (photo)electrochemical energy transformation and storage applications requires a framework for polymer and electrolyte design that includes a deep understanding of the polymer–electrolyte interphase. Here, we report on the investigations of two napthalenediimide (NDI)–bithiophene (T2)-based semiconducting copolymers using computational modeling and in situ, ex situ, and operando techniques to reveal how changes in electrolyte and polymer chemistry modulate the electronic and structural properties of polymer electrodes during electrochemical (de)doping. These systems are shown to host an ensemble of polarons, in contrast with the single polaron-like character often reported, whose properties vary with the nature of the local environment. Importantly, these polarons serve as reporters of the nanoscale environments in which they reside. We demonstrate that controlling the polymer and electrolyte chemistry regulates the nature of the charge carriers generated upon electrochemical doping and/or exciton dissociation in a photoelectrochemical solar cell: For instance, divalent counterions enable polaron and bipolaron formation at lower reducing potentials, while supporting more bipolaron formation than monovalent counterions. A novel application of NEXAFS reveals insights into charge (de)localization, providing a pathway for future investigation of electron transport mechanisms. Finally, simulations of polymer swelling of an amorphous interphase show that charge formation has a large impact on polymer swelling and ion penetration. These studies deliver insights to enable the control of charge-carrier and ion transport, the rates of electron transfer and catalytic efficiency, device stability, and overall device performance.

14 SOLAR ENERGY↗

Control of Two Solid Electrolyte Interphases at the Negative Electrode of an Anode‐Free All Solid‐State Battery based on Argyrodite Electrolyte

Abstract Anode‐free all solid‐state batteries (AF‐ASSBs) employ “empty” current collector with three active interfaces that determine electrochemical stability; lithium metal – Solid electrolyte (SE) interphase (SEI‐1), lithium – current collector interface, and collector – SE interphase (SEI‐2). Argyrodite Li 6 PS 5 Cl (LPSCl) solid electrolyte (SE) displays SEI‐2 containing copper sulfides, formed even at open circuit. Bilayer of 140 nm magnesium/30 nm tungsten (Mg/W‐Cu) controls the three interfaces and allows for state‐of‐the‐art electrochemical performance in half‐cells and fullcells. AF‐ASSB with NMC811 cathode achieves 150 cycles with Coulombic efficiency (CE) above 99.8%. With high mass‐loading cathode (8.6 mAh cm −2 ), AF‐ASSB retains 86.5% capacity after 45 cycles at 0.2C. During electrodeposition of Li, gradient Li‐Mg solid solution is formed, which reverses upon electrodissolution. This promotes conformal wetting/dewetting by Li and stabilizes SEI‐1 by lowering thermodynamic driving force for SE reduction. Inert refractory W underlayer is required to prevent ongoing formation of SEI‐2 that also drives electrochemical degradation. Inert Mo and Nb layers likewise protect Cu from corroding, while Li‐alloying layers (Mg, Sn) are less effective due to ongoing volume changes and associated pulverization. Mechanistic explanation for observed Li segregation within alloying Li x Mg layer is provided through mesoscale modelling, considering opposing roles of diffusivity differences and interfacial stresses.

Wang, Yixian [Materials Science and Engineering Pr↗

Solvation Rule for Solid‐Electrolyte Interphase Enabler in Lithium‐Metal Batteries

Abstract Despite the exceptionally high energy density of lithium metal anodes, the practical application of lithium‐metal batteries (LMBs) is still impeded by the instability of the interphase between the lithium metal and the electrolyte. To formulate a functional electrolyte system that can stabilize the lithium‐metal anode, the solvation behavior of the solvent molecules must be understood because the electrochemical properties of a solvent can be heavily influenced by its solvation status. We unambiguously demonstrated the solvation rule for the solid‐electrolyte interphase (SEI) enabler in an electrolyte system. In this study, fluoroethylene carbonate was used as the SEI enabler due to its ability to form a robust SEI on the lithium metal surface, allowing relatively stable LMB cycling. The results revealed that the solvation number of fluoroethylene carbonate must be ≥1 to ensure the formation of a stable SEI in which the sacrificial reduction of the SEI enabler subsequently leads to the stable cycling of LMBs.

Su, Chi‐Cheung↗

Stabilizing the Solid‐Electrolyte Interphase with Polyacrylamide for High‐Voltage Aqueous Lithium‐Ion Batteries

Abstract The introduction of “water‐in‐salt” electrolyte (WiSE) concept opens a new horizon to aqueous electrochemistry that is benefited from the formation of a solid‐electrolyte interphase (SEI). However, such SEI still faces multiple challenges, including dissolution, mechanical damaging, and incessant reforming, which result in poor cycling stability. Here, we report a polymeric additive, polyacrylamide (PAM) that effectively stabilizes the interphase in WiSE. With the addition of 5 molar % PAM to 21 mol kg −1 LiTFSI electrolyte, a LiMn 2 O 4 ∥L‐TiO 2 full cell exhibits enhanced cycling stability with 86 % capacity retention after 100 cycles at 1 C. The formation mechanism and evolution of PAM‐assisted SEI was investigated using operando small angle neutron scattering and density functional theory (DFT) calculations, which reveal that PAM minimizes the presence of free water molecules at the anode/electrolyte interface, accelerates the TFSI − anion decomposition, and densifies the SEI.

Hou, Xu↗

Multiple Functional Bonds Integrated Interphases for Long Cycle Sodium-Ion Batteries

Sodium-ion batteries (SIBs) have garnered significant interest as one of the most promising energy suppliers for power grid energy storage. However, the poor electrode/electrolyte interfacial stability leads to continual electrolyte decomposition and transition metal dissolution, resulting in rapid performance degradation of SIBs. In this work, we propose a strategy integrating multiple functional bonds to regulate electrode/electrolyte interphase by triple-coupling of succinonitrile (SN), sodium hexafluorophosphate (NaPF 6 ) and fluorinated ethylene carbonate (FEC). Theoretical calculation and experiment results show that the solvation structure of Na + and ClO 4 – is effectively reconfigured by the solvated FEC, SN and PF 6 – in PC-based carbonate electrolyte. The newly developed electrolyte demonstrates increased Na + -FEC coordination, weakened interaction of Na + -PC and participation of SN and PF 6 – anions in solvation, resulting in the formation of a conformal interfacial layer comprising of sodium oxynitrides (NaN x O y ), sodium fluoride (NaF) and phosphorus oxide compounds (NaP x O y ). Consequently, a 3 Ah pouch full cell of hard carbon//NaNi 1/3 Fe 1/3 Mn 1/3 O 2 exhibits an excellent capacity retention of 90.4 % after 1000 cycles. Detailed postmortem analysis of interface chemistry is further illustrated by multiple characterization methods. Finally, this study provides a new avenue for developing electrolyte formulations with multiple functional bonds integrated interphases to significantly improve the long-term cycling stability of SIBs.

25 ENERGY STORAGE↗

Enhanced Radiation Damage Tolerance of Amorphous Interphase and Grain Boundary Complexions in Cu-Ta

Amorphous interfacial complexions are particularly resistant to radiation damage and have been primarily studied in alloys with good glass-forming ability, yet recent reports suggest that these features can form even in immiscible alloys such as Cu-Ta under irradiation. In this work, the mechanisms of damage production and annihilation due to primary knock-on atom collisions are investigated for amorphous interphase and grain boundaries in a Cu-Ta alloy using atomistic simulations. Amorphous complexions, in particular amorphous interphase complexions that separate Cu and Ta grains, result in less residual defect damage than their ordered counterparts. Stemming from the nanophase chemical separation in this alloy, the amorphous complexions exhibit a highly heterogeneous distribution of atomic excess volume, as compared to a good glass former like Cu-Zr. Complexion thickness, a tunable structural descriptor, plays a vital role in damage resistance. Thicker interfacial films are more damage-tolerant because they alter the defect production rate due to differences in intrinsic displacement threshold energies during the collision cascade. Overall, the findings of this work highlight the importance of interfacial engineering in enhancing the properties of materials operating in radiation-prone environments and the promise of amorphous complexions as particularly radiation damage-tolerant microstructural features.

36 MATERIALS SCIENCE↗

Ionic conductive polymers as artificial solid electrolyte interphase films in Li metal batteries – A review

Lithium (Li) metal has been considered as the ultimate anode material for next-generation rechargeable batteries due to its ultra-high theoretical specific capacity (3860 mAh g -1 ) and the lowest reduction voltage (-3.04 V vs the standard hydrogen electrode). However, the dendritic Li formation, uncontrolled interfacial reactions, and huge volume variations lead to unstable solid electrolyte interphase (SEI) layer, low Coulombic efficiency and hence short cycling lifetime. Designing artificial solid electrolyte interphase (artificial SEI) films on the Li metal electrode exhibits great potential to solve the aforementioned problems and enable Li–metal batteries with prolonged lifetime. Polymer materials with good ionic conductivity, superior processability and high flexibility are considered as ideal artificial SEI film materials. In this review, according to the ionic conductive groups, recent advances in polymeric artificial SEI films are summarized to afford a deep understanding of Li ion plating/stripping behavior and present design principles of high-performance artificial SEI films in achieving stable Li metal electrodes. Perspectives regarding to the future research directions of polymeric artificial SEI films for Li–metal electrode are also discussed. The insights and design principles of polymeric artificial SEI films gained in the current review will be definitely useful in achieving the Li–metal batteries with improved energy density, high safety and long cycling lifetime toward next-generation energy storage devices.

25 ENERGY STORAGE↗

Uniform lithiophilic layers in 3D current collectors enable ultrastable solid electrolyte interphase for high-performance lithium metal batteries

Uniform lithium plating/stripping during charging/discharging in 3D lithiophilic current collectors (3DLCC) is essential to suppress growth of lithium dendrites and to mitigate infinite volume variations of lithium metal for long-lived lithium metal batteries. Additionally, this study reveals the decisive role played by uniformity of the lithiophilic layer of the 3DLCC in achieving uniform lithium plating/stripping. Herein, a series of metal oxide-based 3DLCCs are successfully fabricated with a simple and an ultrafast solution combustion method, from which formation of a uniform and stable lithium dendrite-free solid electrolyte interphase via a uniform lithiophilic layer is demonstrated. Taking Co 3 O 4 as the lithiophilic material deposited on a nickel foam as the 3DLCC (Co@NF) for a proof of concept, the loading amount of Co 3 O 4 , closely correlated with the uniformity of the Co 3 O 4 layer, is modulated to optimize its lithium ion hosting performances. With a uniform Co 3 O 4 layer grown in the 3DLCC, an ultralow nucleation overpotential of 33.4 mV is achieved in half-cell tests at 1 mA cm -2 and 1 mAh cm -2 , and a high Coulombic efficiency of 97.1% is maintained after 210 cycles under a severe cycling condition of 2 mA cm -2 and 1 mAh cm -2 . A small polarization voltage of 13 mV together with an ultralong cycle life of 2400 h at 0.5 mA cm -2 and 1 mAh cm -2 in symmetric Li cells is achieved. Moreover, the composite Li anode delivers sensational rate capability and cyclability in full-cells. This work not only provides new and valuable insights into the interphasial chemistry of solid electrolyte interphase layers, but also sheds light on the development of ultrastable lithium metal batteries.

25 ENERGY STORAGE↗

Depth-Dependent Understanding of Cathode Electrolyte Interphase (CEI) on the Layered Li-Ion Cathodes Operated at Extreme High Temperature

The high-temperature operation of Li-ion batteries is highly dependent on the stability of the cathode electrolyte interphase (CEI) formed during lithiation-delithiation reactions. However, knowledge on the nature of the CEI is limited and its stability under extreme temperatures is not well understood. Therefore, herein, we investigate a proof-of-concept study on stabilizing CEI on model LiNi 0.33 Mn 0.33 Co 0.33 O 2 (NMC333) at extreme operation condition of 100 oC using thermally stable pyrrolidinium based ionic liquid electrolyte. The electrochemical lithiation-delithiation reactions at 100 oC and the CEI evolution upon different cycling conditions are investigated. Further, the depth-dependent CEI chemistry was investigated using energy tunable synchrotron-based hard X-ray photoelectron spectroscopy (HAXPES). Overall, the results reveal that the high temperature operation accelerated the CEI formation compared to room temperature, and the surface of the interphase layer is rich in boron-based inorganic moieties than the deeper surface. Further, bulk sensitive X-ray absorption spectroscopy (XAS) was used to investigate the transition metal redox contributors during high temperature electrochemical reactions, similar to room temperature, the Ni2+/4+redox couple is the only charge compensating redox couple during high temperature operation. Finally, the physical nature of the conformal CEI on the cathode particles was visualized with high-resolution transmission electron microscopy, which confirms that the significant degradation of cathode particles without conformal CEI is due to the transformation of layer to spinel formation at extreme temperature. In this study, understanding this high temperature interfacial chemistry of NMC cathodes through advanced spectroscopy and microscopy will shed light on transforming ambient temperature Li-ion chemistry to high temperature applications.

25 ENERGY STORAGE↗

Resolving Nanoscopic and Mesoscopic Heterogeneity of Fluorinated Species in Battery Solid-Electrolyte Interphases by Cryogenic Electron Microscopy

The stability of lithium batteries is tied to the physicochemical properties of the solid-electrolyte interphase (SEI). Owing to the difficulty in characterizing this sensitive interphase, the nanoscale distribution of SEI components is poorly understood. Here, we use cryogenic scanning transmission electron microscopy (cryo-STEM) to map the spatial distribution of SEI components across the metallic Li anode. We reveal that LiF, an SEI component widely believed to play an important role in battery passivation, is absent within the compact SEI film (~15 nm); instead, LiF particles (100–400 nm) precipitate across the electrode surface. We term this larger length scale as the indirect SEI regime. On the basis of these observations, we conclude that LiF cannot be a dominant contribution to anode passivation nor does it influence Li+ transport across the compact SEI film. We refine the traditional SEI structure derived from ensemble-averaged characterizations and nuance the role of SEI components on battery performance.

25 ENERGY STORAGE↗

Stable Solid Electrolyte Interphase Layer Formed by Electrochemical Pretreatment of Gel Polymer Coating on Li Metal Anode for Lithium–Oxygen Batteries

Lithium (Li)-oxygen (O2) batteries (LOBs) exhibit the highest theoretical specific energy density among candidates of the next-generation energy storage systems, but the instability of Li metal anode (LMA), air electrode, and electrolyte largely limit the practical energy density of these batteries. Herein, we report an effective method to protect LMA against side reactions between LMA and crossover contaminants such as highly reactive oxygen moieties. A solid electrolyte interphase (SEI) layer rich in inorganic components was formed on a LMA coated with polyethylene oxide thin-film through an in-situ electrochemical pre-charging step under oxygen atmosphere. This uniformly distributed stiff SEI layer interacted with flexible polymer matrix and formed a submicron-sized gel-like polymer layer. This polymer supported SEI layer leads to much longer cycle life (130 vs. 65 cycles) as compared to those of pristine cell under the same testing conditions (1.0 mAh cm-2 at 0.2 mA cm-2 in the voltage range of 2 to 5 V without any catalysts). It is also very effective during low voltage (2 to 4.5 V) cycling with a redox mediator (0.1 and 0.15M (2,2,6,6-tetramethylpiperidin-1-yl) oxidanyl). Therefore, this approach can be used to stabilize LMA/electrolytes interphase and improve the cycle life of rechargeable LOBs.

lithium-oxygen batteries, lithium metal anodes, ar↗

Fluorinated Interphase Enables Reversible Zn 2+ Storage in Aqueous ZnSO 4 Electrolytes

Aqueous zinc-ion batteries (AZIBs) using ZnSO 4 aqueous electrolytes complement Li-ion batteries and offer high safety, low cost, and scalability. However, an inferior cycle life, attributed to the generation of basic layered double hydroxides (LDHs) on the cathode during cycling, hampers the development of AZIBs. Although Zn(CF 3 SO 3 ) 2 (Zn(OTf) 2 ) electrolytes demonstrate exceptional performance, their higher cost in comparison to ZnSO 4 offsets their electrochemical stability benefits. Toward this end, we propose a fluorinated interphase strategy to achieve a stable battery with ZnSO 4 electrolytes by in situ pre-constructing the cathode-electrolyte interphase (CEI) of ZnOTf-LDH on the cathode surface. Unlike ZnSO 4 - LDH, which obstructs the diffusion channel of zinc ions, ZnOTf-LDH facilitates the desolvation of zinc ions, thereby enhancing the cycling stability (over 50 cycles at a low current density of 200 mA g -1 ). Further, this work offers valuable insights into the degradation mechanism of AZIBs and provides an effective approach for developing stable and low-cost AZIBs.

25 ENERGY STORAGE↗

Revealing Solvent-Assisted Li+ Transport in the Solid Electrolyte Interphase operando

The performance of energy-dense lithium metal batteries is critically influenced by the properties of the solid electrolyte interphase (SEI). Yet, progress in understanding this layer has been limited by the lack of accurate operando characterization because the SEI evolves dynamically during cycling. Here, we apply dynamic electrochemical impedance spectroscopy (dEIS) to resolve the real-time evolution of the SEI on lithium metal in ether-based electrolytes with varying degrees of fluorination. We find that faster stabilization of the compact SEI resistance correlates with improved passivation and higher Coulombic efficiency. Unexpectedly, compact SEI resistance correlates directly with Li+ solvation energy, revealing that weaker Li+ solvation increases not only bulk but also interphase resistance. These findings challenge the conventional view of the SEI as a purely solid-phase conductor and instead support a solvent-assisted Li+ transport mechanism within the compact SEI. This framework emphasizes the need to balance SEI ionic conductivity with the Li+ solvation environment to maximize lithium metal battery performance.

Sacci, Robert [ORNL] (ORCID:0000000200735221)↗

Impact of dual-layer solid-electrolyte interphase inhomogeneities on early-stage defect formation in Si electrodes

While intensive efforts have been devoted to studying the nature of the solid-electrolyte interphase (SEI), little attention has been paid to understanding its role in the mechanical failures of electrodes. Here we unveil the impact of SEI inhomogeneities on early-stage defect formation in Si electrodes. Buried under the SEI, these early-stage defects are inaccessible by most surface-probing techniques. With operando full field diffraction X-ray microscopy, we observe the formation of these defects in real time and connect their origin to a heterogeneous degree of lithiation. This heterogeneous lithiation is further correlated to inhomogeneities in topography and lithium-ion mobility in both the inner- and outer-SEI, thanks to a combination of operando atomic force microscopy, electrochemical strain microscopy and sputter-etched X-ray photoelectron spectroscopy. Our multi-modal study bridges observations across the multi-level interfaces (Si/LixSi/inner-SEI/outer-SEI), thus offering novel insights into the impact of SEI homogeneities on the structural stability of Si-based lithium-ion batteries. Severe structural deformation during (de)lithiation is the main factor limiting the stability of Si anodes in Li-ion batteries. Here, a multi-modal approach is used to visualize these deformations in their early-stage and link them to inhomogeneities in the dual-layer solid-electrolyte interphase.

25 ENERGY STORAGE↗

Additive engineering for robust interphases to stabilize high-Ni layered structures at ultra-high voltage of 4.8 V

Nickel-rich layered cathode materials promise high energy density for next-generation batteries when coupled with lithium metal anodes. However, the practical capacities accessible are far less than the theoretical values due to their structural instability during cycling, especially when charged at high voltages. Here we demonstrate that stable cycling with an ultra-high cut-off voltage of 4.8 V can be realized by using an appropriate amount of lithium difluorophosphate in a common commercial electrolyte. The Li||LiNi 0.76 Mn 0.14 Co 0.10 O 2 cell retains 97% of the initial capacity (235 mAh g -1 ) after 200 cycles. The cycling stability is ascribed to the robust interphase on the cathode. It is formed by lithium difluorophosphate decomposition, which is facilitated by the catalytic effect of transition metals. The decomposition products (Li 3 PO 4 and LiF) form a protective interphase. This suppresses transition metal dissolution and cathode surface reconstruction. It also facilitates uniform Li distribution within the cathode, effectively mitigating the strain and crack formation.

25 ENERGY STORAGE↗

Linking void and interphase evolution to electrochemistry in solid-state batteries using operando X-ray tomography

Despite progress in solid-state battery engineering, our understanding of the chemo-mechanical phenomena that govern electrochemical behavior and stability at solid-solid interfaces remains limited compared to solid-liquid interfaces. Here, we use operando synchrotron X-ray computed microtomography to investigate the evolution of lithium/solid-state electrolyte interfaces during battery cycling, revealing how the complex interplay among void formation, interphase growth, and volumetric changes determines cell behavior. Void formation during lithium stripping is directly visualized in symmetric cells, and the loss of contact that drives current constriction at the interface between lithium and the solid-state electrolyte (Li10SnP2S12) is quantified and found to be the primary cause of cell failure. The interphase is found to be redox-active upon charge, and global volume changes occur due to partial molar volume mismatches at either electrode. Finally, these results provide new insight into how chemo-mechanical phenomena can impact cell performance, which is necessary to understand for the development of solid-state batteries.

42 ENGINEERING↗

Measuring the buried interphase between solid electrolytes and lithium metal using neutrons

Interfaces are the key to next-generation high-energy batteries including solid-state Li metal batteries. In solid-state batteries, the buried nature of solid–solid electrolyte–electrode interfaces makes studying them difficult. Neutrons have significant potential to non-destructively probe these buried solid–solid interfaces. This work presents a comparative study using both neutron depth profiling (NDP) and neutron reflectometry (NR) to study a model lithium metal–lithium phosphorus oxynitride (LiPON) solid electrolyte system. In the NDP data, no distinct interphase is observed at the interface. NR shows a difference between electrodeposited, and vapor deposited LiPON–Li interfaces but finds both are gradient interphases that are less than 30 nm thick. Additional simulations of the LiPON–Li 2 O–Li system demonstrate that NDP has an excellent resolution in the 50 nm–1 μm regime while NR has an ideal resolution from 0.1–200 nm with different sample requirements. Together NDP and NR can provide a complementary understanding of interfaces between Li metal and solid electrolytes across relevant length scales.

Westover, Andrew S. [Oak Ridge National Laboratory↗