Characterizations of a hot-pressed polycrystalline spinel:Ce scintillator
Abstract Not Provided
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Abstract Not Provided
It is proposed that Apollo 14 type breccias lithify by sintering of particles of matrix glass under stress-free conditions. Meteorite impacts generate the heat necessary for sintering. Compacted angular particles of glass with the composition of an Apollo 14 rock were sintered experimentally. Loose clods of sub 37 micron grains form in several days at 700 C. Synthetic rocks, which texturally resemble the breccias, were produced at 795 C and above in 7.5 hours. Glass devitrified with increasing temperature. At 850 C, devitrification prevents much further densification of the synthetic breccias after 2 hours. Experiments compressing glass at 500 bars at 600 C produced dense vitreous masses which did not resemble lunar breccias. Confining pressure does not play a major role in lithifying the breccias. It is concluded that Apollo 14 type lunar breccias form at shallow depths at 800 C+ in a period of minutes to days.
Explore the source record for details and available documents.
Energy-absorbing Si3N4 surface layers on dense Si3N4 substrates were formed by in-place nitridation of fine-grained silicon powder. Ballistic impact tests performed on samples with 1-mm thick layers at room temperature and 1370 C showed up to an eightfold increase in the energy necessary to fracture the substrate. For maximum impact resistance, a small amount (about 20 vol %) of residual Si must be present in the reaction-sintered Si3N4 surface layer. Thermal cycling to 1370 C did not affect impact resistance, even though a considerable amount of SiO2 formed within the reaction-sintered Si3N4 layer during cycling. Erosion testing of samples in a Mach 0.8 burner rig at 1370 C resulted in minimal surface recession of the surface layer. Chemically vapor-deposited SiC-coated material similarly tested exhibited no surface recession.
Measurements of the electrical conductivity, Seebeck coefficient and Hall mobility from -300 K to -1300 K have been carried out on multiphase hotpressed samples of the nominal composition B6Si. In all samples the conductivity and the p-type Seebeck coefficient both increase smoothly with increasing temperature. By themselves, these facts suggest small-polaronic hopping between inequivalent sites. The measured Hall mobilities are always low, but vary in sign. A possible explanation is offered for this anomalous behavior.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
The subcritical growth of cracks from pre-existing flaws in ceramics can severely affect the structural reliability of a material. The ability to directly observe subcritical crack growth and rigorously analyze its influence on fracture behavior is important for an accurate assessment of material performance. A Mode I fracture specimen and loading method has been developed which permits the observation of stable, subcritical crack extension in monolithic and toughened ceramics. The test specimen and procedure has demonstrated its ability to generate and stably propagate sharp, through-thickness cracks in brittle high modulus materials. Crack growth for an aluminum oxide ceramic was observed to be continuously stable throughout testing. Conversely, the fracture behavior of a silicon nitride ceramic exhibited crack growth as a series of subcritical extensions which are interrupted by dynamic propagation. Dynamic initiation and arrest fracture resistance measurements for the silicon nitride averaged 67 and 48 J/sq m, respectively. The dynamic initiation event was observed to be sudden and explosive. Increments of subcritical crack growth contributed to a 40 percent increase in fracture resistance before dynamic initiation. Subcritical crack growth visibly marked the fracture surface with an increase in surface roughness. Increments of subcritical crack growth loosen ceramic material near the fracture surface and the fracture debris is easily removed by a replication technique. Fracture debris is viewed as evidence that both crack bridging and subsurface microcracking may be some of the mechanisms contributing to the increase in fracture resistance. A Statistical Fracture Mechanics model specifically developed to address subcritical crack growth and fracture reliability is used together with a damaged zone of material at the crack tip to model experimental results. A Monte Carlo simulation of the actual experiments was used to establish a set of modeling input parameters. It was demonstrated that a single critical parameter does not characterize the conditions required for dynamic initiation. Experimental measurements for critical crack lengths, and the energy release rates exhibit significant scatter. The resulting output of the model produces good agreement with both the average values and scatter of experimental measurements.
Advanced engineered matrix composites (EMCs) require that the coefficient of thermal expansion (CTE) of the engineered matrix (EM) matches those of the fiber reinforcements as closely as possible in order to reduce thermal compatibility strains during heating and cooling of the composites. The present paper proposes a general concept for designing suitable matrices for long fiber reinforced composites using a rule of mixtures (ROM) approach to minimize the global differences in the thermal expansion mismatches between the fibers and the engineered matrix. Proof-of-concept studies were conducted to demonstrate the validity of the concept.
The present research effort was undertaken to develop a new generation of SiC fiber-reinforced engineered ceramic matrix composites (E-CMCs). In contrast to traditional CMCs with a brittle SiC matrix, an E-CMC is designed to consist of a matrix engineered to possess sufficient high temperature plasticity to minimize crack propagation, relatively high fracture toughness, and self-healing capabilities to prevent oxygen ingress to the BN-coated fibers through surface-connected cracks. The present paper discusses the bend strength, isothermal oxidation, microstructures and self-healing properties of several silicide-behaved engineered matrices. Based on the oxidation tests, where it was observed that some of the matrices exhibited either catastrophic oxidation ("pesting") or spalling of the oxide scale, two engineered matrices, CrSi2/SiC/Si3N4 and CrMoSi/SiC/Si3N4, were down-selected for further investigation. Four-point bend tests were conducted on these two engineered matrices between room temperature and 1698 degrees Kelvin. Although these matrices were brittle at low temperatures, it was observed that the bend strengths and bend ductility increased at high temperatures as the silicide particles became more ductile, which was qualitatively consistent with the theoretically expected behavior that crack blunting at these particles should increase the matrix strength. Additional studies were conducted to study the effects of different additives on the self-healing properties of the engineered matrices, which helped to identify the most effective additives.
Explore the source record for details and available documents.
A method for producing monolithic Zirconium Carbide (ZrC) is described. The method includes raising a pressure applied to a ZrC powder until a final pressure of greater than 40 MPa is reached; and raising a temperature of the ZrC powder until a final temperature of less than 2200.degree. C. is reached.
Experimental work on this project over the last four years has resulted in establishing processing and characterization techniques for producing both the Bi-based and Tl-based superconductors in their high temperature (2223) forms. In the bulk, dry pressed form, maximum critical temperatures (Tc) of 108.2 K and 117.8 K, respectively, were measured. Results have further shown that the Bi and Tl-based superconducting materials in bulk form are noticeably different from the Y-based 123 material in that superconductivity is considerably harder to achieve, maintain, and reproduce. This is due primarily to the difficulty in obtaining the higher Tc phase in pure form since it commonly co-exists with other undesirable, lower Tc phases. In particular, it has been found that long processing times for calcining and firing (20 - 200 hrs.) and close control of temperatures which are very near the melting point are required in order to obtain higher proportions of the desirable, high Tc (2223) phase. Thus far, the BSCCO bulk materials has been prepared in uniaxially pressed, hot pressed, and tapecast form. The uniaxially pressed material has been synthesized by the mixed oxide, coprecipitation, and melt quenching processes. The tapecast and hot pressed materials have been prepared via the mixed oxide process. In addition, thick films of BSCCO (2223 phase) have been prepared by screen printing on to yttria and magnesia stabilized zirconia with only moderate success; i.e., superconductivity was achieved in these thick films, but the highest Tc obtained in these films was 89.0 K. The Tc's of the bulk hot pressed, tapecast, and screen printed thick film materials were found to be 108.2, 102.4, and 89.0 K, respectively.
The metal matrix microencapsulated (M3) fuel concept for light water reactors (LWRs), consisting of coated fuel particles dispersed in a zirconium metal matrix, is introduced. Fabrication of M3 fuels by hot pressing, hot isostatic pressing, or extrusion methodologies has been demonstrated over the temperature range 800-1050 C. Various types of coated fuel particles with outermost layers of pyrocarbon, SiC, ZrC, and TiN have been incorporated into the zirconium metal matrix. Mechanical particle-particle and chemical particle-matrix interactions have been observed during the preliminary characterization of as-fabricated M3 specimens. Irradiation of three M3 rodlets with surrogate coated fuel particles was carried out at mean rod temperature of 400 C to 4.6 dpa in the zirconium metal matrix. Due to absence of texture in the metal matrix no irradiation growth strain (<0.09%) was detected during the post-irradiation examination.