Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “FLEXURAL STRENGTH”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Novel dense membrane for hydrogen separation for energy applications

The main objectives of this project are: (1) Characterization of the thermo mechanical properties of the novel dense HTM bulk sample; (2) Development of a correlation among the intrinsic factors (such as grain size and phase distribution), and the extrinsic factors (such as temperature and atmosphere) and the thermo-mechanical properties (such as strengths and stress) to predict the performance of a HTM system (HTM membrane and porous substrate) ; and (3) Evaluation of the stability of the novel HTM membrane and its property correlations after thermal cycling. Based on all results and analysis of the thermo mechanical properties for the HTM cermet bulk samples, several important conclusions were made. The mean σfs at room temperature is approximately 356 MPa for the HTM cermet. The mean σfs value decreases to 284 MPa as the temperature increases to 850?C. The Difference difference in atmosphere, such as air or N2, had an insignificant effect on the flexural strength values at 850?C for the HTM cermet. The HTM cermet samples at room temperature and at 500?C fractured without any significant plastic deformation. Whereas, at 850?C, the HTM cermet samples fractured, preceded by an extensive plastic deformation. It seems that the HTM cermet behaves more like an elastic material such as a nonmetal ceramic at the room temperature, and more like a ductile material at increased temperature (850?C). The exothermic peak during the TG/DTA tests centered at 600?C is most likely associated with both the enthalpy change of transformation from the amorphous phase into crystalline zirconia and the oxidation of Pd phase in HTM cermet in air. The endothermic peak centered at 800?C is associated with the dissociation of PdO to Pd for the HTM cermet sample in both inert N2 environment and air. There is a corresponding weight gain as oxidation occurs for palladium (Pd) phase to form palladium oxide (PdO) and there is a weight loss as the unstable PdO is dissociated back to Pd and oxygen. The normal stress and shear stresses from the Mohr?s circle indicate that the residual stress in the HTM cermet sample is mainly as compressive residual stress in the magnitude of -135 to -155 MP, and with very little shear stress (in the magnitude of 10 MPa). The magnitude of change in the normal stress and the shear stress is insignificant in the HTM after 120 thermal cycles. However, the principle normal stress changes from compressive to tensile residual stress and there is a significant increase in the shear stress after 500 thermal cycles. The calculated value based on the equation and the Mohr?s circle is found to be consistent with the experimental value for the as-received HTM cermet samples. At some rotation (φ) angle, the residual stress was found to be as tensile stress. Most ceramic material is weak in tension, and develops microscopic cracks. With treatment of 120 thermal cycles between 50?850?C, the HTM- sample exhibited thermally-induced cracks on the surface. Visually observable cracks appeared on the surface of HTM cermet with continuous thermal cycling, after 500 thermal cycles. The XRD powder diffraction analysis indicated an increased amount of crystalline PdO crystalline in HTM cermet after 120 and 500 thermal cycles as compare to the as-received samples. The Pd crystalline peaks were found to significantly decrease in peak intensity with thermal cycling. Higher peak intensity for PdO phase was observed with increased number of thermal cycles. A Monoclinic monoclinic zirconia phase was first identified in the as-received HTM as-received sample. However, with thermal cycling treatment of both 120 and 500 thermal cycles, the M-ZrO2 phase is transformed to the tetragonal YSZ, which is consistent with the thermal analysis results by TG/DTA. Correlations of the microstructural and thermo-mechanical properties of both selected reference material and ANL-3e HTM cermet bulk sample are affected mainly by porosity and microstructural features, such as grain size and pore size/distribution. The Young?s Modulus (E-value), especially, is positively proportional to the flexural strength for materials with similar crystallographic structure. For different crystallographic materials, physical properties such as E and density are independent of mechanical properties, such as flexural strength.. Microstructural properties, particularly, grain size and crystallographic structure, and thermodynamic properties are the main factors affecting the mechanical properties at both room and high temperatures. The oxidation and the plasticity of Pd phase mainly affect the mechanical properties of HTM cermet at high temperature or with thermal cycling treatment. Changes in the residual stress and microstructure affect the mechanical properties of HTM when subjected to high temperature or thermal cycling treatment.

08 HYDROGEN↗

Research on graphite reinforced glass matrix composites

A composite that can be used at temperatures up to 875 K with mechanical properties equal or superior to graphite fiber reinforced epoxy composites is presented. The composite system consist of graphite fiber, uniaxially or biaxially, reinforced borosilicate glass. The mechanical and thermal properties of such a graphite fiber reinforced glass composite are described, and the system is shown to offer promise as a high performance structural material. Specific properties that were measured were: a modified borosilicate glass uniaxially reinforced by Hercules HMS graphite fiber has a three-point flexural strength of 1030 MPa, a four-point flexural strength of 964 MPa, an elastic modulus of 199 GPa and a failure strain of 0.0052. The preparation and properties of similar composites with Hercules HTS, Celanese DG-102, Thornel 300 and Thornel Pitch graphite fibers are also described.

Bacon, J. F.↗

Polyimide Composites from 'Salt-Like' Solution Precursors

Four NASA Langley-developed polyimide matrix resins, LaRC(TM)-IA, LaRC(TM)-IAX, LaRC(TM)-8515 and LaRC(TM)-PETI-5, were produced via a 'saltlike' process developed by Unitika Ltd. The salt-like solutions (65% solids in NMP) were prepregged onto Hexcel IM7 carbon fiber using the NASA LaRC multipurpose tape machine. Process parameters were determined and composite panels fabricated. The temperature dependent volatile depletion rates, the thermal crystallization behavior and the resin rheology were characterized. Composite molding cycles were developed which consistently yielded well consolidated, void-free laminated parts. Composite mechanical properties such as the short beam shear strength; the longitudinal and transverse flexural strength and flexural modulus; the longitudinal compression strength and modulus; and the open hole compression strength and compression after impact strength were measured at room temperature and elevated temperatures. The processing characteristics and the composite mechanical properties of the four intermediate modulus carbon fiber/polyimide matrix composites were compared to existing data on the same polyimide resin systems and IM7 carbon fiber manufactured via poly(amide acid) solutions (30-35% solids in NMP). This work studies the effects of varying the synthetic route on the processing and mechanical properties of the polyimide composites.

Cano, Roberto J.↗

Nano-modification to improve the ductility of cementitious composites

Effect of nano-sized mineral additions on ductility of engineered cementitious composites (ECC) containing high volumes of fly ash was investigated at different hydration degrees. Various properties of ECC mixtures with different mineral additions were compared in terms of microstructural properties of matrix, fiber-matrix interface, and fiber surface to assess improvements in ductility. Microstructural characterization was made by measuring pore size distributions through mercury intrusion porosimetry (MIP). Hydration characteristics were assessed using thermogravimetric analysis/differential thermal analysis (TGA/DTA), and fiber-matrix interface and fiber surface characteristics were assessed using scanning electron microscopy (SEM) through a period of 90 days. Moreover, compressive and flexural strength developments were monitored for the same period. Test results confirmed that mineral additions could significantly improve both flexural strength and ductility of ECC, especially at early ages. Cheaper Nano-CaCO{sub 3} was more effective compared to nano-silica. However, the crystal structure of CaCO{sub 3} played a very important role in the range of expected improvements.

36 MATERIALS SCIENCE↗

Enhancement of thermal shock resistance of reaction sintered mullite–zirconia composites in the presence of lanthanum oxide

Mullite–zirconia composites containing 20 wt.% zirconia were prepared by reaction sintering of zircon flour, sillimanite beach sand and calcined alumina. 0 to 8 mol% of La{sub 2}O{sub 3} with respect to zirconia was used as sintering aid. The effect of additive on the various physical, microstructures, mechanical and thermo-mechanical properties was studied. Quantitative phase analysis shows the change in tetragonal zirconia content with incorporation of lanthanum oxide. La{sub 2}O{sub 3} addition has significantly improved the thermal shock resistance of the samples. Samples without additive retained only 20% of initial flexural strength after 5 cycles, whereas samples containing 5 mol% La{sub 2}O{sub 3} retained almost 78% of its initial flexural strength even after 15 thermal shock cycles. - Highlights: • Mullite–zirconia composites were prepared by reaction sintering route utilizing zircon and sillimanite beach sand. • Lanthanum oxide was used as sintering aid. • The presence of lanthanum oxide decreased the densification temperature. • Lanthanum oxide significantly improved the thermal shock resistance of the composites.

36 MATERIALS SCIENCE↗

Mechanical, Dynamic Mechanical and Thermal Properties of Banana Fiber/Recycled High Density Polyethylene Biocomposites Filled with Flyash Cenospheres

This study presents the preparation of Natural fiber-reinforced biocomposites based on Recycled High Density Polyethylene (RHDPE)/Banana Fiber (BF)/Fly ash Cenospheres (FACS) and aims to increase the economic value of these waste materials. Maleic anhydride grafted HDPE (MA-g-HDPE) was used as a compatibilizer to increase the dispersion of fibers into the polymer matrix as well as to increase the compatibility between the matrix and fillers. Variation in mechanical, thermal and dynamic mechanical properties with the addition of FACS in RHDPE/BF composites was investigated. It was observed that 7.5 wt% FACS, 30 wt% BF and 3 wt% MA-g-HDPE within RHDPE matrix resulted in an increase in tensile strength to 17%, tensile modulus to 188%, flexural strength to 38%, flexural modulus to 159% and hardness to 37% as compared with the RHDPE matrix. Significant enhancement in the thermal stability of the RHDPE/BF biocomposites was also observed in presence of FACS under thermogravimetric analysis. The morphology of the prepared biocomposites has been examined by using scanning electron microscopy. Dynamic mechanical analysis tests revealed an increase in storage and loss modulus of the biocomposite system. The use of such recycled material, agricultural and industrial wastes increased the properties of the final product suggesting their use to be a good alternative in the production of polymeric composites.

36 MATERIALS SCIENCE↗

Semi-2-interpenetrating polymer networks of high temperature systems

A semi-interpenetrating (semi-IPN) polymer system of the semi-2-IPN type is described in which a polymer of acetylene-terminated imidesulfone (ATPISO2) is cross linked in the presence of polyimidesulfone (PISO2). Six different formulations obtained by mixing of either ATPISO2-1n or ATPISO2-3n with PISO2 in three different proportions were characterized in terms of glass transition temperature, thermooxidative stability, inherent viscosity, and dynamic mechanical properties. Adhesive (lap shear) strength was tested at elevated temperatures on aged samples of adhesive scrim cloth prepared from each resin. Woven graphite (Celion 1000)/polyimide composites were tested for flexural strength, flexural modulus, and shear strength. The network polymers have properties intermediate between those of the component polymers alone, have greatly improved processability over either polyimide, and are able to form good adhesive bonds and composites, making the semi-2-IPN systems superior materials for aerospace structures.

Hanky, A. O.↗

Characteristics of Si3N4-SiO2-Ce2O3 compositions sintered in high-pressure nitrogen

Full-density Si3N4-SiO2-Ce2O3 compositions were prepared by sintering with 2.5 MPa nitrogen pressure at temperatures of 1900 and 2090 C. Room-temperature flexural strengths near 700 MPa for sintered material compared favorably with the strength of hot-pressed material. At 1370 C, where flexural strengths as high as 363 MPa were obtained, it was observed that the coarsest structure was the strongest and the finest structure was the weakest. One of the compositions tested, Si3N4-8.7 wt pct SiO2-8.3 wt pct-Ce2O3, was found to have excellent 200-h oxidation resistance at 700, 1000, and 1370 C, without incidence of 700 to 1000 C phase instability and cracking.

Sanders, W. A.↗

Specimen geometry effects on graphite/PMR-15 composites during thermo-oxidative aging

Studies were conducted to establish the effects of specimen geometry on the thermo-oxidative stability and the mechanical properties retention of unidirectional Celion 12000 graphite fiber reinforced PMR-15 polyimide composites. Weight loss, flexural strength and interlaminar shear strength are measured at isothermal aging times as long as 1639 hr at a temperature of 316 C for three different specimen geometries. It is found that the three different types of specimen surfaces exhibit different values of weight loss/unit area. The mechanical properties retention is also found to be dependent on geometry for these composites. The interlaminar shear strength decreases significantly over the complete range of aging times. The flexural strength retention starts showing geometric dependency after about 1000 hr of aging at 316C. Weight loss fluxes, associated with the three different types of exposed surfaces, are calculated and used to develop an empirical mathematical model for predicting the weight loss behavior of unidirectional composites of arbitrary geometries. Data are presented comparing experimentally determined weight loss with weight loss values predicted using the empirical model.

Bowles, K. J.↗

Specimen geometry effects on graphite/PMR-15 composites during thermo-oxidative aging

Studies were conducted to establish the effects of specimen geometry on the thermo-oxidative stability and the mechanical properties retention of unidirectional Celion 12000 graphite fiber reinforced PMR-15 polyimide composites. Weight loss, flexural strength and interlaminar shear strength are measured at isothermal aging times as long as 1639 hr at a temperature of 316 C for three different specimen geometries. It is found that the three different types of specimen surfaces exhibit different values of weight loss/unit area. The mechanical properties retention is also found to be dependent on geometry for these composites. The interlaminar shear strength decreases significantly over the complete range of aging times. The flexural strength retention starts showing geometric dependency after about 1000 hr of aging at 316 C. Weight loss fluxes, associated with the three different types of exposed surfaces, are calculated and used to develop an empirical mathematical model for predicting the weight loss behavior of unidirectional composites of arbitrary geometries. Data are presented comparing experimentally determined weight loss with weight loss values predicted using the empirical model.

Bowles, K. J.↗

Physicochemical properties of digital light processing 3D-Printed alumina and mullite ceramics

Alumina ceramics fabricated using conventional techniques such as uniaxial pressing or injection molding are popular due to their low density, excellent insulation, and mechanical properties. However, these methods often limit the fabrication of complex geometries with high dimensional accuracy due to tooling constraints and limited design freedom. To overcome these limitations, this study employed Digital Light Processing (DLP) additive manufacturing (AM), which enables the production of precise structures. In addition, the optimization of sintering parameters to enhance the densification and performance of alumina and mullite ceramics was investigated, with a specific focus on how varying sintering temperatures and hold times affect part shrinkage, geometric accuracy, and material integrity. Flexural strength of both alumina and mullite specimens was clearly influenced by the way the layers was stacked. When layers were arranged across the direction of the applied load (Z = 4; XZ), the strength was higher than when they were stacked along the same direction as the load (Z = 3; XY). Weibull analysis based on these results showed high modulus values across all samples, indicating good reliability in the flexural strength measurements. This reliability, combined with the clear influence of sintering parameters, highlights how processing conditions effect the material properties and mechanical performance of parts produced through DLP additive manufacturing. In conclusion, these findings open new avenues for ceramic AM across various applications, enhancing the potential for innovation in fields such as aerospace, biomedical engineering, and energy.

36 MATERIALS SCIENCE↗

Mechanical strength of [HA/Bioplastic/Sericin] composite part printed by bioprinter

The aim of this research was to determine the effect of hydroxyapatite (HA) content in printed biocomposite to its mechanical strength. The biocomposite paste was prepared by composing HA, bioplastic and sericin with various ratios of [HA/Bioplastic]: 40/60, 50/50, 60,40 and 70/30. Sericin of 0.3% weight was added to the biocomposite. Mechanical test was conducted to observe tensile (ASTM D 638 type 4) and flexural strength (ASTM D 790). Both type of specimens were fabricated using 3D Printer. Printing process parameter (infill speed, print speed and layer height) were set up as 60 mm/s, 10 mm/s, 0.35 mm, respectively. Results showed that biocomposite with [HA/Biplastic]. weight ratio of 60/40(w/w) has an optimum tensile (3.89 ± 1.26 MPa) and flexural strength (2.51 ± 0.45 MPa). Scanning electron microscope observation indicated that microstructure of specimen was influenced by the percentage of the hydroxyapatite. There was no agglomeration of HA particle within the composite.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Processing and Properties of a Phenolic Composite System

Phenolic resin systems generate water as a reaction by-product via condensation reactions during curing at elevated temperatures. In the fabrication of fiber reinforced phenolic resin matrix composites, volatile management is crucial in producing void-free quality laminates. A commercial vacuum-bag moldable phenolic prepreg system was selected for this study. The traditional single-vacuum-bag (SVB) process was unable to manage the volatiles effectively, resulting in inferior voidy laminates. However, a double vacuum bag (DVB) process was shown to afford superior volatile management and consistently yielded void-free quality parts. The DVB process cure cycle (temperature /pressure profiles) for the selected composite system was designed, with the vacuum pressure application point carefully selected, to avoid excessive resin squeeze-outs and achieve the net shape and target resin content in the final consolidated laminate parts. Laminate consolidation quality was characterized by optical photomicrography for the cross sections and measurements of mechanical properties. A 40% increase in short beam shear strength, 30% greater flexural strength, 10% higher tensile and 18% higher compression strengths were obtained in composite laminates fabricated by the DVB process.

Hou, Tan-Hung↗

Modelling the interlayer bond strength of 3D printed concrete with surface moisture

Highlights: • An analytical model for interlayer adhesion of 3DPC is proposed based on the amount of surface moisture on the interlayer. • For this mix, the model accurately (RMSE=2.5%) predicts the reduction in interlayer adhesion from 30% to 50%. • Internal curing with superabsorbent polymers increases the interlayer adhesion by 10% and flexural strength by 19%. • SAPs also improve the initial thixotropy by 49% and buildability by 25% compared to the reference. Providing additional water to the hydrating cementitious particles is essential to achieve the optimal mechanical performance of the low w/b concrete mixes preferred for 3D printing. This study incorporates superabsorbent polymers (SAP) and additional water in 3D printed concrete (3DPC) to promote the hydration process through delayed internal water release. The study shows that a retentive SAP modifies the rheological development by absorbing the pore fluid for a short period after printing. The absorption-induced stiffening increases the thixotropy and buildability by 49% and 25%, respectively. A retentive SAP increases the flexural strength and interlayer adhesion by 19% and 10%, respectively. This is due to the internal water release that promotes hydration. Evaporation of the interlayer moisture during the pass time has the opposite effect— evaporation reduces the interlayer adhesion. Based on this assumption, an analytical model is proposed. The model accounts for the pass time, bleeding, and the environmental evaporation rate to estimate the surface moisture and predict the lack of interlayer adhesion. In this study, the model accurately (RMSE = 2.5%) predicted an interlayer adhesion reduction from 30% to 50%. The interlayer adhesion results of other studies could also be predicted.

36 MATERIALS SCIENCE↗

Bio-composites fabricated by sandwiching sisal fibers with polypropylene (PP)

Sisal fibers reinforced polypropylene (PP) composites were successfully fabricated using sandwiching sisal fibers with PP sheets. The ratio of fiber and polymer matrix was 50:50 (wt. %). Untreated short and long sisal fibers, and alkali treated short sisal fibers in 6% NaOH at 100°C for 1 and 3 h were used as reinforcement or fillers. A small amount (3 wt. %) of maleic anhydride grafted polypropylene (MAPP) was added as a coupling agent. Scanning electron microscopy (SEM) and Fourier transform infrared (FTIR) spectroscopy were used to characterize the surface morphology and chemical composition of the fibers, respectively. Flexural test of sisal/PP composites was done according to ASTM D 790-02. The results showed that flexural strength of untreated long fiber reinforced composite is much higher than that of the untreated and alkali treated short fibers reinforced composites with and without the addition of MAPP. Alkalization related to fiber surface modification, fiber length/fiber orientation and a composite fabrication technique are important factors in contributing to the fiber distribution within the matrix, the bonding between the fiber and the matrix and the enhancement of flexural strength of the bio-composite.

36 MATERIALS SCIENCE↗

Corrosion resistance characterization of porous alumina membrane supports

Tubular porous alumina ceramic membrane supports were fabricated by an extrusion-drying-sintering process and then characterized in detail in terms of corrosion resistance in both H{sub 2}SO{sub 4} and NaOH aqueous solutions. Variations in the properties of the alumina supports such as mass loss percent, mechanical strength, open porosity and pore size distribution were studied before and after corrosion under different conditions. In addition, the microstructures were analyzed using scanning electron microscopy, energy dispersive spectroscopy and X-ray diffraction before and after corrosion. The fabricated porous alumina supports offer possibilities for some potential applications as micro-filtration or ultra-filtration membrane supports, as well as in the pre-treatment of strongly acidic industrial waste-liquids. - Research highlights: {yields} Porous alumina membrane supports fabricated by extrusion-drying-sintering process. {yields} Corrosion resistance in 20 wt.% H{sub 2}SO{sub 4} and 1, 5, 10 wt.% NaOH aqueous solutions. {yields} Rapid mass loss and loss of flexural strength occurred in hot NaOH solution. {yields} Resistant to strong acid corrosion with low mass loss, low flexural strength loss. {yields} Porous alumina supports have potential for treatment of strong acid waste liquids.

36 MATERIALS SCIENCE↗

Strengthening of C/SiC Composites by Electrophoretic Deposition of CNTs on a SiC Coating

The current study reports the enhancement of mechanical properties of carbon fiber-reinforced silicon carbide ceramic matrix composites (C/SiC CMCs) by the application of a carbon nanotube/silicon carbide (CNT/SiC) coating. CNTs were deposited on the surfaces of C/SiC composites using electrophoretic deposition (EPD), after which infiltration by SiC was achieved through a chemical vapor infiltration process. An EPD duration of 5 min was associated with a 40% increase in the ultimate flexural strength relative to that of composites with a pure SiC coating. The observed enhancement was rationalized by the microstructural observations of SiC infiltration into the porous CNT morphology and the subsequent formation of CNT/SiC layers on the surfaces of the composites and by the inherent toughness of the SiC whiskers. The flexural strength decreased with EPD durations greater than 5 min due to the formation of thick CNT meshes, which decreased the open porosity and thereby obstructed further SiC infiltration. This is a viable methodology for the improvement of mechanical properties of CMCs by the introduction of a ceramic coating containing CNT.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Preparation, microstructure and properties of AlN/CBC composites

Highlights: • AlN/CBC composites can be prepared by gelcasting and pressureless sintering method. • Suitable sintering additive content and increasing sintering temperature help to improve properties of composite. • Relative density, C content and microstructure et al. have effect on properties of composite. - Abstract: Gelcasting method with nontoxic biopolymer as gel former can be used to prepare ceramics with complex shape. AlN ceramic bonded carbon (AlN/CBC) composites with light weight were fabricated by gelcasting and pressureless sintering method using nontoxic agarose as gel former with Y{sub 2}O{sub 3} + CaF{sub 2} as sintering additive. The effect of sintering additive content and sintering temperature on the microstructure, flexural strength and thermal conductivity of composites was investigated. The results reveal that, as the temperature decreases, the raw powders solidify into three-dimensional net structures through abundant hydrogen bonds in the agarose. High sintering temperature facilitates densification and improves mechanical and thermal properties of the composites. Increasing sintering additive content can also tune the density and raise flexural strength. The AlN/CBC composite containing 7 wt% sintering additive content, which was sintered at 2000 °C, exhibits the highest thermal conductivity. Relative density, C content and microstructure uniformity have effects on properties of AlN/CBC composite.

36 MATERIALS SCIENCE↗