Structure and high-temperature thermoelectric properties of SrAl{sub 2}Si{sub 2}
Single crystals of SrAl{sub 2}Si{sub 2} were synthesized by reaction of the elements in an aluminum flux at 1000 deg. C. SrAl{sub 2}Si{sub 2} is isostructural to CaAl{sub 2}Si{sub 2} and crystallizes in the hexagonal space group P-3m1 (90 K, a=4.1834 (2), c=7.4104 (2) A, Z=1, R1=0.0156, wR2=0.0308). Thermal analysis shows that the compound melts at {approx}1020 deg. C. Low-temperature resistivity on single crystals along the c-axis shows metallic behavior with room temperature resistivity value of {approx}7.5 m{omega} cm. High-temperature Seebeck, resistivity, and thermal conductivity measurements were made on hot-pressed pellets. The Seebeck coefficient shows negative values in entire temperature range decreasing from {approx}-78 {mu}V K{sup -1} at room temperature to -34 {mu}V K{sup -1} at 1173 K. Seebeck coefficients are negative indicating n-type behavior; however, the temperature dependence is consistent with contribution from minority p-type carriers as well. The lattice contribution to the thermal conductivity is higher than for clathrate structures containing Al and Si, approximately 50 mW cm{sup -1} K, and contributes to the overall low zT for this compound. - Abstract: Single crystals of SrAl{sub 2}Si{sub 2} have been prepared via an Al flux reaction and are of the CaAl{sub 2}Si{sub 2} structure type. The melting point is approximately 1020deg. C. Low temperature resistivity curve is similar to that observed for single crystals of CaAl{sub 2}Si{sub 2} High temperature Seebeck coefficient is negative, indicating n-type carriers. Display Omitted.