The role of ultraviolet radiation during ultralow k films curing: Strengthening mechanisms and sacrificial porogen removal

This work proposes a fundamental understanding of structural transformation occurring during porogen extraction from as-deposited ultralow k (ULK) materials when exposed to ultraviolet (UV) radiation during thermal curing. Specific explanations are provided for as deposited films at high temperature (T>250 deg. C). This temperature range is sufficient to assess thin-film stability. Two distinguished regimes were identified in the curing process. During the first stage, the film shrinks strongly in similar proportion to SiCH{sub 3} break. Preferential impact of UV radiation on hydrocarbon porogen bonds leads also to a break of SiCH{sub 3} structures. In this work, 5 min of curing is enough to remove the porogen and create the max of porosity (33%). After the porogen removal step, the porous film shrinks under UV radiation leading to an increase of SiOSi bond concentration. A structural rearrangement of the bulk is initiated since the porogen is totally evacuated from the film. The increase of normalized infrared SiOSi peak during UV curing (related in literature to an improvement of mechanical properties) is mainly due to film densification (a few SiOSi bonds creation). The origin of shrinkage is explained by the breaking of SiCH{sub 3} which could turn into a SiH bond leading to a free volume reduction within the film. In this case, a correlation is found between shrinkage and elastic modulus. The resulting SiOSi structure densification drives, at first order, the improvement of the mechanical properties. UV radiation exposure shows no effect in silanol condensation and acts mainly on the porogen decomposition and bulk densification. Si-CH{sub 2}-Si structure formation, pointed out in the literature as a possible reaction way to enhance film crosslinking, is identified in the nuclear magnetic resonance (NMR) broadband spectrum of the ULK film. However, resulted NMR and infrared peaks intensities suggest its formation as a minor. This study gives a full understanding of UV curing impact on ULK films (k{<=}2.5) where structure densification is identified as a main process to enhance the film strength in addition to the crosslinking.

36 MATERIALS SCIENCE↗

High T{sub g} and fast curing epoxy-based anisotropic conductive paste for electronic packaging

Herein, our main objective is to prepare the fast curing epoxy system with high glass transition temperature (T{sub g}) by incorporating the multifunctional epoxy resin into the mixture of diglycidyl ether of bisphenol A (DGEBA) as a major epoxy component and aromatic diamine as a hardener. Furthermore, the curing behavior as well as thermal and thermomechanical properties were investigated by differential scanning calorimetry (DSC), dynamic mechanical analysis (DMA) and thermomechanical analysis (TMA). It was found that T{sub g} obtained from tan δ of DGEBA/aromatic diamine system increased from 100 °C to 205 °C with the presence of 30 percentage by weight of multifunctional epoxy resin. Additionally, the isothermal DSC results showed that the multifunctional epoxy resin can accelerate the curing reaction of DGEBA/aromatic diamine system. Namely, a high degree of curing (∼90%) was achieved after a few minutes of curing at low temperature of 130 °C, owing to a large number of epoxy ring of multifunctional epoxy resin towards the active hydrogen atoms of aromatic diamine.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

How Optical and Electrical Properties of ITO Coated Willow Glass Affect Photonic Curing Outcome for Upscaling Perovskite Solar Cell Manufacturing

Indium tin oxide (ITO) coated Willow® glass is an excellent substrate for roll-to-roll manufacturing of perovskite solar cells (PSCs) but can have large variability in its optical and electrical properties. Photonic curing uses intense light pulses instead of heat to process materials and can facilitate faster processing speeds in roll-to-roll manufacturing to upscale the production of PSCs. Since the entire film stack can absorb light and contributes to the photonic curing outcome, the substrate materials’ properties play an integral role. Furthermore, we present the effect of ITO transmittance on the photonic curing of nickel nitrate sol-gel precursors into nickel oxide and consequently the performance of PSCs fabricated with only photonic curing and no thermal annealing. Unexpectedly, ITO samples processed by photonic curing show improved optical and electrical properties.

14 SOLAR ENERGY↗

Photonic Curing of Nickel Oxide Transport Layer and Perovskite Active Layer for Flexible Perovskite Solar Cells: A Path Towards High-Throughput Manufacturing

High-throughput roll-to-roll (R2R) manufacturing of perovskite solar cells (PSCs) is currently limited by thermal processes that take tens of minutes each, translating to impractically long annealing tools at high web speeds. In addition, PSCs are usually made with metal oxide transport layer materials that require high temperatures for thermal annealing. Here, we demonstrate the fabrication of PSCs using photonic curing, instead of thermal annealing, to convert NiO x directly from sol-gel precursors for hole transport layers and to crystallize methylammonium lead iodide (MAPbI 3 ) active layers on flexible Willow ® Glass substrates. Photonic curing uses short, intense pulses of light to process materials at a high speed, hence it is compatible with R2R manufacturing. We achieved power conversion efficiencies (PCEs) of 11.7% in forward-scan and 10.9% in reverse-scan for PSCs made with photonic cured NiO x and MAPbI 3 films. Furthermore, both NiO x and MAPbI 3 films could be processed with a single photonic curing pulse, with a web speed of 5.7 m/min, and still produce PCEs comparable to thermally annealed control samples. Based on the single-pulse photonic curing condition for each film, we project a web speed of 26 m/min, laying a pathway to high-throughput production of perovskite solar modules.

14 SOLAR ENERGY↗

Porosity Detection and Localization During Composite Cure Inside an Autoclave Using Ultrasonic Inspection

Composite materials offer unique benefits in aerospace applications such as increased strength-to-weight ratio and improved fatigue properties. They are increasingly being used in major commercial aircraft programs. However, current processing methods can lead to defects in composite parts, which must be detected using post-manufacturing inspection methods. Porosity (i.e., pores, voids) is a critical defect from the cure process that is detrimental to performance of the composite part. It is therefore necessary to understand and eliminate the formation of porosity defects. At NASA Langley Research Center, an in-situ cure monitoring system was developed to detect porosity defects as they form in real-time inside an autoclave. A capability to directly detect and localize porosity within a composite during cure did not exist before. This study is focused on an elevated-temperature ultrasonic inspection system to detect porosity defects in composites during autoclave cure. The ultrasonic inspection system operated inside an autoclave within an enclosure cooled by intermittent liquid nitrogen (LN_2) injections. A high-temperature, 2.25 MHz, transducer transmitted ultrasonic waves through the tool plate and into the composite part and measured the amplitude and time of flight of the reflected waves with a 1 mm × 1 mm step size/areal resolution. Porosity was observed via the ultrasonic reflections, which experienced increased attenuation in regions of high porosity. Distinct regions of increased porosity were present due to uneven pressure across the panel, which was driven by an intentional misfit between the flat caul plate and the tapered composite panel with ply drops. The results were validated by post-cure ultrasonic inspection and micrographs. The in-situ inspection system was able to successfully provide porosity detection and localization in the tapered ply-drop panel. The successful results indicate the promise of this system for future implementation in the manufacturing of composite structures for aerospace applications.

Composites↗

Latent Cure Epoxy Resins for Reliable Joints in Secondary-Bonded Composite Structures

In high-performance polymer matrix composite assemblies, adhesive bonding is generally superior to mechanical fastening in structural performance and manufacturing efficiency. However, adhesive bonds are susceptible to minute levels of contamination accumulated during assembly that can lead to unpredictable, weak bonds. Current methods of measuring bond strength are all destructive mechanical tests. To overcome these challenges, redundant load paths (e.g., mechanical fasteners) are often implemented in secondary-bonded, primary-structures, which can greatly reduce structural performance. This study investigated reformulated aerospace epoxy matrix resins with stoichiometric offset to inhibit cure of the matrix resin prior to assembly. Inhibited resins can reflow and mix across the joint interface, which eliminates the material discontinuity and forms a homogenous joint with reliable fracture properties. The goal of this study was to develop and demonstrate secondary composite assemblies that are mechanically and microscopically indistinguishable from a co-cured composite joint. This article describes the development of latent epoxy resins, the fabrication of test articles, and the mechanical properties measured from experimental joints compared with conventional, co-cured laminates. Methods of in-line quality control using and infrared spectroscopy and post-assembly forensics are also described. The final mode-II fracture toughness measured from precracked AERoBOND specimens was similar to that measured from co-cured laminates indicating that later cure epoxy materials could be a suitable replacement for secondary bonding.

Polymer-matrix composites (PMCs)↗

Impact of carbamate formation on the surface tension of epoxy‐amine curing systems

Abstract Epoxy‐amine reactive systems, including their surface tension, have been studied due to their use and importance in composites and adhesives in laboratory and industrial applications. Understanding how the system's surface tension changes during curing could help target applications for tailored composites. Using the Wilhelmy plate method, surface tensions for epoxy‐curing agent systems were investigated under different environments. While the epoxy exhibited an expected negative temperature coefficient of −0.096 mN/m/°C, the curing agent exhibited a positive temperature coefficient of 0.073 mN/m/°C, which is due to the curing agent reacting with atmospheric CO 2 to form carbamate through a zwitterion pathway and functional groups accumulating at the surface of the reacting systems. Carbamate formation results in a surface tension below that of the individual constituents in the epoxy‐amine curing agent system. Fourier transform infrared (FTIR) spectroscopy was used to verify in situ formation of carbamate, and by reducing the system's temperature, it was demonstrated that the system surface tension profiles displayed micellar surfactant‐like characteristics. FTIR was used to explore the difference in composition between the surface and the bulk, in particular carbamate formation at the surface, resulting in a lowering of the surface tension of reacting systems.

Shenk, Timothy M.↗

Chemical structure and curing dynamics of bisphenol S, PEEK™-like, and resveratrol phthalonitrile thermoset resins

This effort provides a multifaceted analysis of the structural changes and material dynamics of thermally driven softening and curing of three distinct phthalonitrile (PN) resins that cross-link into thermally stable and oxidation-resistant thermosets. Although this material system has yielded a large subset of fire-retardant composites that require facile processing and low-temperature curing, to date, insufficient information had been available on the fundamental processes that drive their softening and curing stages. Our approach conducted a complementary analysis the chemistry, monomer mobility, and rheology of three PN polymers in order to correlate the curing processes with corresponding structural and behavioral transformations of thermosets. Here, we focused on PNs with a bisphenol S backbone, a bisphenol A (PEEK™-like) backbone, and a resveratrol backbone. We relied on quasi-elastic neutron scattering (QENS) in order to analyze the in situ dynamics and self-diffusion properties of PN monomers, and to track changes in their mobilities during cross-linking and staging. Our analysis facilitates proper control over the staging and final curing of these resins and enables more efficient processing of these thermosets.

36 MATERIALS SCIENCE↗

Understanding curing dynamics of arylacetylene and phthalonitrile thermoset blends

Tetrakis(phenylethynyl)benzene (TPEB), a high char yield arylacetylene resin, was blended with a resorcinol-based PEEK™-like oligomeric phthalonitrile resin (Res). Here, we observed the influence of each polymer precursor on the structural changes and material dynamics of different mixtures of these resins during thermal curing to produce thermosets with high char retention. We provide insight to help understand fundamental processes that control and tune this complex thermally driven curing mechanism, which, to date, has not been well understood. We show that an equivalent blend of Res and TPEB mitigates the exothermic curing process and exhibits a low viscosity, which may facilitate processing of these thermosetting blends for composite manufacturing. To obtain a more comprehensive overview of the different dynamics of these polymers during curing, we correlated thermodynamic changes with rheology, materials characterization, and molecular dynamics derived from neutron scattering. Our efforts shed more light on the thermally driven chemical changes, physical transformation, and gelation dynamics that drive or accompany softening and curing of these two distinct crosslinking resin groups.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Effect of curing conditions on the dimensional and thermal stability of calcium phosphate cement for elevated temperature applications

Calcium phosphate cements (CPCs) are attractive materials for elevated temperature applications, like moulds to process thermoplastics up to 300 °C. The CPC resulting from the reaction of wollastonite with phosphoric acid cured at room temperature however contains hydrated phases like brushite, and is thus not stable when exposed to temperatures above 200 °C. A non-contact method based on digital image correlation demonstrated that isothermal curing at 60 °C reduces the thermal shrinkage up to 300 °C by 25%. This curing method results in the direct formation of the more stable monetite in a shorter curing time. The correlated results of TGA, pH of the filtration water, and DSC analysis on partially cured material indicate this. XRD diffractograms and SEM images in combination with EDX show the evolution of the transformation of wollastonite into monetite, and the structure and morphology of the formed material.

36 MATERIALS SCIENCE↗

X-ray computed tomography of microstructure evolution during matrix impregnation and curing in unidirectional fiber beds

Microstructural evolution during axial impregnation and subsequent curing of a preceramic polymer in unidirectional ceramic fiber beds is studied using X-ray computed tomography. The principal goal is to identify connections between void locations, void sizes, local fiber bed porosity, fiber movement, and impregnation conditions. The degree of saturation after impregnation is found to increase with instantaneous capillary number. But, because of the need to create pathways for gas escape during curing, fiber beds with high saturation after impregnation show the largest reductions in saturation during curing. Notwithstanding, saturation after curing increases with instantaneous capillary number. Voids tend to form in the largest channels between fibers, where the local fiber bed porosity is high, during both impregnation and curing. Here, void formation is typically accompanied by fiber movement that increases both the local fiber bed porosity near voids and the overall non-uniformity in the fiber bed, as measured by local porosity entropy.

(A - Material) fibers↗

Real-time cure monitoring of fiber-reinforced polymer composites using infrared thermography and recursive Bayesian filtering

Despite the desirable characteristics of fiber-reinforced polymer (FRP) composites, their utilization in high volume production industries is limited by a lack of efficient manufacturing techniques. Monitoring the curing process of these composites can help with improving the quality and efficiency of the manufacturing process. This article discusses a method that uses Kalman-filter-based fusion of the information obtained from infrared thermography (surface temperature measurements) and a heat conduction model to estimate degrees of cure and internal temperatures of curing FRP composite parts in real time. The effectiveness of the methodology is demonstrated by successfully monitoring the curing of an FRP composite part in a laboratory experiment. Finally, the proposed methodology is a crucial step towards identifying anomalies in the curing process that negatively impact the quality of FRP composite parts.

36 MATERIALS SCIENCE↗

Reactions of DGEBA epoxy cured with diethanolamine: Isoconversional kinetics and implications to network structure

The curing of diglycidyl ether of bisphenol A (DGEBA) epoxy with diethanolamine (DEA) is studied. DEA has three reactive groups, a secondary amine hydrogen and two hydroxyls. The secondary amine reacts rapidly, forming an adduct containing tertiary amines, epoxides and hydroxyls. The epoxides and hydroxyls then react in the presence of the amines to crosslink and vitrify the epoxy in the “gelation” reaction. The gelation reaction, the subject of this study, is not simple. The reaction exhibits unusual dependencies on both temperature and degree of cure. Previously, the general mechanisms of this curing process were explored by a number of us. In the present paper, both differential scanning calorimetry (DSC) and isothermal microcalorimetry (IMC) are used to determine a number of characteristic times associated with the reaction. The characteristic times show that the reaction rate has different functional forms at different temperatures and extents of reaction. This results from the reaction rate not depending solely upon the temperature and over-all extent-of-reaction. The concentration of a number of auxiliary reactive species that are generated in the course of the reaction (as well as their mobility and steric hindrance) appear to be key factors in defining the reaction kinetics. The dependence of the final network structure on cure schedule for this type of tertiary amine activated reaction is then discussed in the context of the literature. Lastly, in the Supplementary Material, Kamal-like functions are fit to the isothermal reaction kinetics, with the reader cautioned in applying the functions to non-isothermal cures.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Infrared curing simulations of liquid composites molding

Infrared radiation is an effective energy source to cure thermosetting polymers. Its usage is expected to reduce curing time in comparison with thermal heating and mold thermally regulated. In addition, because of the polymerization mechanism and instant on-off control of this power, an improvement in the final properties of the material is also expected. In this paper, we studied the infrared interaction with carbon (or glass) fibers reinforced epoxy matrix, where Liquid resin infusion (LRI) is used to manufacture the composite. Temperature of the composite is a key parameter that affects its mechanical properties and is controlled by the infrared emitters and the exothermic heat released from the polymerization. Radiative heat flux is computed using the in-lab developed software RAYHEAT. Then, the heat flux (or absorbed energy for glass fibers) is exported to the finite element based program COMSOLMULTIPHYSICS where heat balance equation is solved. This equation is coupled with the exothermic heat released during the curing process in order to predict the composite temperature versus time and degree of cure. Numerical simulations will be performed on planar parts (sheet shape) as well as curvilinear shapes. Experimental validations of the infrared curing carbon (glass)-epoxy composite system are presented in this paper Sheet surface temperature distribution are measured thanks to infrared camera. Kinetic parameters were estimated from differential scanning calorimeter (DSC) experimental data.

36 MATERIALS SCIENCE↗

Importance of microstructural features in mechanical response of cast-cured HMX formulations

We report that cast-cure formulations of plastic-bonded explosives (PBX) present some advantages in manufacturing and application compared to traditional pressed slurry formulated materials. For example, these formulations can be cast to specific shapes and then cured in place, avoiding the need for machining precision parts. However, the microstructure of these materials can be greatly affected by the specific manufacturing process. Here, we evaluate the effect of minor changes to the formulation and manufacturing process on several cyclotetramethylene-tetranitramine (HMX) PBXs. The binders were based on hydroxyl-terminated polybutadiene (HTPB) and cast-cured using diphenylmethane diisocyanate (isonate) as a curing agent. We examined the materials using X-ray computed tomography (CT) imaging and uniaxial compression testing. The isonate content was found to significantly affect the modulus and strength of the binder. The presence of significant void content could be controlled by adding a centrifuging step during the curing process, but the resulting effect on mechanical properties was relatively minor. Finally, mesoscale simulations showed that differences in the mechanical strength of the binder were not sufficient to describe the differences observed in mechanical testing, indicating that the HMX-binder adhesion was also being changed by the manufacturing process.

36 MATERIALS SCIENCE↗

Effect of post cure time and temperature on the properties of two phenolic-fiber composites

Some effects of post-cure time and temperature on the physicomechanical properties of a phenolic-asbestos and a phenolic-glass composite are studied. The molding and post-curing procedures are discussed along with physical and mechanical test results. It is found that the specific gravity of the panels tested decreased slightly but the hardness always increased with post cure, and that the mechanical properties had different patterns of response to increasing post-cure time and temperature. For tensile properties, strength decreased, modulus increased, and elongation at break exhibited little change. In general, the phenolic-asbestos showed more positive response to post cure than did the phenolic-glass. Mold venting is found to impart better properties to the composites concerned.

Lucy, M. H.↗

Acoustic characterization of composite cure

The relationship between the time evolution of ultrasonic longitudinal velocities, measured in the course of the cure of 3501-6 neat and fiber-reinforced resin, and the time evolution of the degree of cure was studied. The resin samples were placed in a mold, one side of which was a graphite plate, while the rest was made of stainless steel. After placing the mold in a press and applying a single-cycle 5-MHz pulse to the transducer bonded to the outer side of the graphite plate, the echo resulting from the resin-graphite interface and the subsequent echoes from within the resin layer were recorded with a 200-MHz, 8-bit digitizer. The degree of cure was calculated from the acoustic response, using the relationships derived by Winfree and Parker (1986). The calculated degree of cure had the expected time dependence, and the agreement between the degree of cure measured for the neat resin and the prepreg was reasonable.

Parker, F. R.↗

Differential Curing In Fiber/Resin Laminates

Modified layup schedule counteracts tendency toward delamination. Improved manufacturing process resembles conventional process, except prepregs partially cured laid on mold in sequence in degree of partial cure decreases from mold side to bag side. Degree of partial cure of each layer at time of layup selected by controlling storage and partial-curing temperatures of prepreg according to Arrhenius equation for rate of gel of resin as function of temperature and time from moment of mixing. Differential advancement of cure in layers made large enough to offset effect of advance bag-side heating in oven or autoclave. Technique helps prevent entrapment of volatile materials during manufacturing of fiber/resin laminates.

Webster, Charles N.↗