Genesis of Nanogalvanic Corrosion Revealed in Pearlitic Steel

Nanoscale, localized corrosion underpins billions of dollars in damage and material costs each year; however, the processes responsible have remained elusive due to the complexity of studying degradative material behavior at nanoscale liquid–solid interfaces. Recent improvements to liquid cell scanning/transmission electron microscopy and associated techniques enable this first look at the nanogalvanic corrosion processes underlying this widespread damage. Nanogalvanic corrosion is observed to initiate at the near-surface ferrite/cementite phase interfaces that typify carbon steel. In minutes, the corrosion front delves deeper into the material, claiming a thin layer of ferrite around all exposed phase boundaries before progressing laterally, converting the ferrite to corrosion product normal to each buried cementite grain. Over the following few minutes, the corrosion product that lines each cementite grain undergoes a volumetric expansion, creating a lateral wedging force that mechanically ejects the cementite grains from their grooves and leaves behind percolation channels into the steel substructure.

36 MATERIALS SCIENCE↗

Thermophysical properties of low cost lithium nitrate salts produced in northern Chile for thermal energy storage

In recent years, lithium containing salts have been studied for thermal energy storage (TES) applications because of their excellent thermophysical properties. In solar power plants, lithium is seen as a way to improve the properties of state-of-the art molten salts used today. Lithium nitrate is a good candidate for sensible heat storage, because of its ability to increase the salt mixture's working temperature range. In the present research, thermophysical properties characterization of lithium nitrate containing salts, produced in Chile, have been carried out. Corrosion evaluations at 390° and 565 °C for 1000 h were performed for low chromium steel T22 and stainless steels (AISI 430 and AISI 316), respectively. Chemical composition of the salts including identification of corrosion products and impurities was determined and an estimation of the Chilean production costs is reported. The study shows a loss of thermal properties after the corrosion tests. The heat capacity was reduced, possibly caused by the formation of oxides at high temperatures. As a result, the partial thermal decomposition of the salt was probably produced by the incorporation of corrosion products from the steel.

25 ENERGY STORAGE↗

Hydro-chemo-mechanical phase field formulation for corrosion induced cracking in reinforced concrete

Steel corrosion induced cracking in reinforced concrete structures is often caused by volumetric straining at the steel-concrete interface. This volumetric strain is mainly controlled by the rate of generation of corrosion product, which depends on the diffusion of Cl{sup −} and dissolved O{sub 2} as well as the chemical reaction at the steel-concrete interface. While many numerical modeling techniques have been proposed to tackle this complex phenomenon, most have been limited to using staggered solution schemes, where the diffusion, chemical reaction, mechanical strain, and crack fields are solved for separately. Unfortunately, such approaches introduce numerical errors that can lead to unrealistic predictions. Therefore, a coupled solution, is needed to remove the formulation induced errors and understand this complex phenomenon. To provide a unifying solution framework for corrosion induced cracking in reinforced concrete, a phase field formulation is presented and implemented with FEM algorithms. The governing equations are derived from the system's free energy and Fick's law of diffusion. The proposed formulation was first validated in 1D by comparing the modeling results with the semi-analytical solution approximated via Laurent series to avoid singularities in the complex domain. 2D plane strain solutions to the embedded rebar undergoing corrosion induced cracking with pre-cracks are also presented and compared with the approximated solutions from linear elastic fracture mechanics theory (LEFM). The modeling of crack propagation enabled by the proposed formulation is also presented along with parametric studies to reveal the roles of the fracture toughness and permeability of the concrete on the corrosion induced cracking. A case study was also conducted on H-pile steel with concrete jackets to demonstrate the feasibility of modeling corrosion induced fracture in reinforced concrete structures with complex steel-concrete interfaces.

36 MATERIALS SCIENCE↗

Assessing High-energy, Laser-driven, X-ray Sources as a Technique to Analyse ILW Containers - 18242

The principle concern regarding intermediate level waste (ILW) containers is the internal volumetric expansion due to the formation of corrosion products. To tackle this (via non-destructive testing) the development of a new technique to identify problematic containers was initiated by radiographic imaging and neutron assay of small scale, simulated, nuclear waste packages. This was achieved using a high-energy laser pulse to produce a bright burst of high-energy Bremsstrahlung radiation for imaging and a pulse of thermal energy neutrons for isotopic quantification. The small scale, simulated, nuclear waste packages (typically a quarter of a 28 mm natural uranium penny encased in grout) were produced with corrosion from oxygen and hydrogen rich environments to simulate the potential effects of long term storage. These samples were characterised using electron and ion beam techniques prior to encapsulation to establish the extent of corrosion and sample morphology. The small-scale samples were analysed using high-resolution x-ray tomography (XRT). These 3D pictures identified the corrosion state of the material and the effect on the surrounding grout matrix. These data sets were used as a baseline to compare with the 2D images obtained from the high-energy radiography to ascertain the imaging quality and potential capability of a laser driven inspection system. The study established the non-destructive imaging capability of a high-energy laser driven x-ray source for identifying fine features such as corrosion products on uranium samples encased in grout and cracks, and for penetrative imaging through large thicknesses of grout. In addition, generation of laser-driven neutrons of thermal energy required for active interrogation of uranium isotopes is demonstrated experimentally and simulations of the neutron inspection method are presented, thus paving the way for criticality testing of ILW containers. This current study is single pulse exposure acquisition, but the data can be used to predict the potential capability of a diode-pumped laser-driven system operating at, or above, 10 Hz by utilising, for example, the Dipole laser technology recently delivered by the STFC Central Laser Facility. Such a system will enable 3D tomography of nuclear waste containers and also greatly reduced signal to noise ratio via multiple acquisition and image stacking. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Determination of the Corrosive Conditions Present within Aircraft Lap-Splice Joints

The complexity of airframe structure lends itself to damage resulting from crevice corrosion. Fuselage lap-splice joints are a particularly important structural detail in this regard because of the difficulty associated with detection and measurement of corrosion in these occluded regions. The objective of this work is to develop a laboratory corrosion test protocol to identify the chemistry to which lap joints are exposed and to develop a model of the corrosion within the joints. A protocol for collecting and identifying the chemistry of airframe crevice corrosion has been developed. Capillary electrophoresis (CE) is used to identify the ionic species contained in corrosion product samples removed from fuselage lap splice joints. CE analysis has been performed on over sixty corrosion product samples removed from both civilian and military aircraft. Over twenty different ions have been detected. Measurements of pH of wetted corroded surfaces indicated an alkaline occluded solution. After determining the species present and their relative concentrations, the resultant solution was reproduced in bulk and electrochemical tests were performed to determine the corrosion rate. Electrochemical analyses of the behavior of AA2024-T3 in these solutions gave corrosion rates of up to 250 microns per year (10 mpy). Additional tests have determined the relative importance of each of the detected ions in model solutions used for future predictive tests. The statistically significant ions have been used to create a second generation solution. Laboratory studies have also included exposure tests involving artificial lap joints exposed to various simulated bulk and crevice environments. The extent and morphology of the attack in artificial lap joints has been compared to studies of corroded samples from actual aircraft. Other effects, such as temperature and potential, as well as the impact of the environment on fatigue crack growth have also been studied.

Lewis, Karen S.↗

Exploring the speciation of actinide salts in the presence of contaminants related to molten salt reactors

Molten salt reactors (MSR) are up-and-coming Generation IV nuclear reactors with either coolant and/or radioactive fuel in molten salt form. Due to their improved safety, efficiency, affordability and convenient waste processing system, these reactors are considered a superior alternative to conventional ones. However, prior to commercial implementation, it is necessary to have an extensive understanding of the reactions occurring in the MSR. The safety parameters of the MSR are determined by the rheological properties such as density and viscosity of the molten salt and these properties are governed by the local structure of the molten salts. Due to the high operational temperatures of MSR's, corrosion plays an important role. Because of their influence, the container corrosion products become part of the fuel salt matrix. In this work, we are investigating how these corrosion products, e.g., Mo, Ni, Cr, would impact the speciation of the actinide metal centers. For the initial studies, lanthanides are used as a surrogate for actinides. Lanthanide chloride salts (LnCl3) are mixed with transition metals and excess of alkali or alkali earth metal salts or salt mixtures (LiCl, NaCl, KCl). These are added to an alumina crucible, placed in a quartz tube, and sealed under a vacuum. This is heated up to around 1000 °C and slowly cooled to a temperature above the melting point of the salt and at that temperature, the reaction is taken out of the furnace. The excess salt is removed, and the resulting product is analyzed using X-ray diffraction techniques, scanning electron microscopy, and spectroscopic methods such as Raman, UV-Visible, and FTIR spectroscopy.

37 - INORGANIC, ORGANIC, PHYSICAL AND ANALYTICAL C↗

Electrochemical Behavior of Cu{sub 60}Zr{sub 25}Ti{sub 15} Bulk Metallic Glass with the Addition of Nb and Mo

This paper reports the changes in the electrochemical behavior of Cu{sub 60}Zr{sub 25}Ti{sub 15} bulk metallic glass (BMG) with the addition of 1 at.% Mo and Nb in 3.5 wt.% NaCl aqueous solution. Electrochemical methods employed for the study are open-circuit potential (OCP) and potentiodynamic polarization. The OCP values of the parent BMG and minor-alloyed BMGs differ only marginally. However, potentiodynamic studies show slightly higher corrosion resistance for the minor-alloyed BMGs than that of the parent alloy. Polarized surfaces of all the samples, examined under a scanning electron microscope (SEM), reveal pits formed due to corrosion. Corrosion products are analyzed by energy-dispersive spectroscopy (EDS) and X-ray photoelectron spectroscopy (XPS). Higher corrosion resistance observed for Nb- or Mo-added BMGs is attributed to the formation of NbO{sub 2}/Nb{sub 2}O{sub 5} and MoO{sub 2}, respectively, besides the oxides of other constituent elements.

36 MATERIALS SCIENCE↗

Friction and wear of iron in sulfuric acid

Elemental iron sliding on aluminum oxide in aerated sulfuric acid concentrations ranging from very dilute (0.000007 N; i.e., 4 ppm) to very concentrated (96 percent acid) was studied. Load and reciprocating sliding speeds were kept constant. With the most dilute acid of 0.7 to 0.0002 N, a complex corrosion product formed that was friable and often increased friction and wear. At concentrations of 0.001 N, metal losses were essentially by wear alone. Because no buildup of corrosion products occurred, this acid concentration became the standard from which to separate metal loss from direct corrosion and mechanical wear losses. When the acid concentration was increased to 5 percent, the high corrosion rate of iron in sulfuric acid strongly dominated the total wear loss. This strong corrosion increased to 30 percent acid, and decreased somewhat at 50 percent in accordance with expectations. However, the low corrosion of iron expected at acid concentrations of 65 to 96 percent was not observed in the wear area. It is apparent that the normal passivating film was being worn away and a galvanic cell established which rapidly attached to the wear area.

Rengstorff, G. W. P.↗

The effect of tempering temperature on pitting corrosion resistance of 420 stainless steels

The AISI Type 420 stainless steels are commonly used to steam generators, mixer blades, etc. These stainless steels are most prone to pitting in dissolved Cl{sup −} containing environments. In this paper, the effect of tempering temperature on pitting corrosion resistance of AISI Type 420 stainless steels was studied. The AISI Type 420 stainless steels specimens were heat treated at the temperature of 1050°C for 1 hour to reach austenite stabilization and then quench in the oil. After that, the specimens were tempered at the temperature of 150, 250, 350 and 450°C for 30 minutes and then air cooled to the room temperature. The electrochemical potentiodynamic polarization test was conducted at 3.5% sodium chloride solution to evaluate corrosion rate and pitting corrosion behaviour. The Scanning Electron Microscope (SEM), Energy Dispersive X-Ray Spectroscopy (EDS) were used to evaluate the pitting corrosion product. The result have shown that highest pitting potential was found in the sample tempered at 250°C and corrosion pits were found to initiate preferentially around chromium carbides.

36 MATERIALS SCIENCE↗

Interaction of sulfuric acid corrosion and mechanical wear of iron

Friction and wear experiments were conducted with elemental iron sliding on aluminum oxide in aerated sulfuric acid at concentrations ranging from very dilute (0.00007 N; i.e., 4 ppm) to very concentrated (96 percent acid). Load and reciprocating sliding speed were kept constant. With the most dilute acid concentration of 0.00007 to 0.0002 N, a complex corrosion product formed that was friable and often increased friction and wear. At slightly higher concentrations of 0.001 N, metal losses were essentially by wear alone. Because no buildup of corrosion products occurred, this acid concentration became the standard from which to separate metal loss from direct corrosion and mechanical wear losses. When the acid concentration was increased to 5 percent (1 N), the well-established high corrosion rate of iron in sulfuric acid strongly dominated the total wear loss. This strong corrosion increased to 30 percent acid and decreased somewhat to 50 percent acid in accordance with expectations. However, the low corrosion of iron expected at acid concentrations of 65 to 96 percent was not observed in the wear area. It was apparent that the normal passivating film was being worn away and a galvanic cell established that rapidly attacked the wear area. Under the conditions where direct corrosion losses were highest, the coefficient of friction was the lowest.

Rengstorff, G. W. P.↗

Interaction of sulfuric acid corrosion and mechanical wear of iron

Friction and wear experiment were conducted with elemental iron sliding on aluminum oxide in aerated sulfuric acid at concentrations ranging from very dilute (0.00007 N; i.e., 4 ppm) to very concentrated (96 percent acid). Load and reciprocating sliding speed were kept constant. With the most dilute acid concentration of 0.00007 to 0.0002 N, a complex corrosion product formed that was friable and often increased friction and wear. At slightly higher concentrations of 0.001 N, metal losses were essentially by wear alone. Because no buildup of corrosion products occurred, this acid concentration became the standard from which to separate metal loss from direct corrosion and mechanical wear losses. When the acid concentration was increased to 5 percent (1 N), the well-established high corrosion rate of iron in sulfuric acid strongly dominated the total wear loss. This strong corrosion increased to 30 percent acid and decreased somewhat to 50 percent acid in accordance with expectations. However, the low corrosion of iron expected at acid concentrations of 65 to 96 percent was not observed in the wear area. It was apparent that the normal passivating film was being worn away and a galvanic cell established that rapidly attacked the wear area. Under the conditions where direct corrosion losses were highest, the coefficient of friction was the lowest.

Rengstorff, G. W. P.↗

Multielectrode Array Sensors to Enable Long-Duration Corrosion Monitoring and Control of Concentrating Solar Power Systems

Molten mixtures of MgCl2-KCl-NaCl are promising heat transfer fluid (HTF) candidates for the next generation of concentrating solar power systems (Gen3 CSP), because of their low cost, high decomposition temperature, and favorable heat transfer characteristics. However, if the chemistry of the salts is not properly controlled, molten chlorides can cause corrosion of high-temperature metal alloys, such as Inconel (R), in CSP systems. Here we demonstrate a corrosion monitoring system that can be used to monitor the health of the structural alloys over long durations. The monitoring system includes a multielectrode array voltammetry sensor that measures the redox potential of molten MgCl2-KCl-NaCl mixture as well as the presence of corrosion products and impurities. The sensors have been successfully operated in static molten salt environments for long durations, and are capable of detecting corrosion products, such as Cr2+ and Fe2+, quantitatively at low concentrations (i.e., approximately 100 ppm) with less than 4% error.

Concentrated solar power↗

Assessing corrosion problems in photovoltaic cells via electrochemical stress testing

A series of accelerated electrochemical experiments to study the degradation properties of polyvinylbutyral-encapsulated silicon solar cells has been carried out. The cells' electrical performance with silk screen-silver and nickel-solder contacts was evaluated. The degradation mechanism was shown to be electrochemical corrosion of the cell contacts; metallization elements migrate into the encapsulating material, which acts as an ionic conducting medium. The corrosion products form a conductive path which results in a gradual loss of the insulation characteristics of the encapsulant. The precipitation of corrosion products in the encapsulant also contributes to its discoloration which in turn leads to a reduction in its transparency and the consequent optical loss. Delamination of the encapsulating layers could be attributed to electrochemical gas evolution reactions. The usefulness of the testing technique in qualitatively establishing a reliability difference between metallizations and antireflection coating types is demonstrated.

Shalaby, H.↗

The manufacture and use of sludge test materials for R and D purposes in the treatment and processing of magnox based sludge

Among the Intermediate Level Waste materials in store and awaiting treatment and processing in the UK are quantities of magnesium hydroxide sludge. This sludge is a product of radioactive Magnox Swarf which arose from the de-canning of used magnox fuel element rods. As the Swarf was stored underwater, a corrosion reaction occurred over the course of time between the magnox and the water resulting in a magnesium hydroxide based sludge. The differing conditions and materials present in the various storage areas means that the sludge can range in consistency from that of a slurry through to a thick clay. Sludge test materials are required to underpin and validate the research and development equipment and processes that are to be used to treat the waste material. Necessary restrictions imposed on the sampling and testing of the radioactive waste means that the available data on the properties and behaviour of the sludge is limited. The raw materials used to create the sludge test materials are based upon magnesium hydroxide so that as far as possible the chemical behaviour will be similar to that of the waste material. The most representative sludge test material is manufactured by the corrosion of non-radioactive magnox or magnesium. However, time constraints make it impractical to supply this material in sufficient quantities for full scale validation trials. An alternative is to use sludge manufactured from commercially available magnesium hydroxide. The particle shape of commercially available materials differs from corrosion product magnesium hydroxide which means that properties such as the rheological behaviour cannot be replicated. Nevertheless, valuable trial data can be obtained, giving a greater degree of confidence in the waste treatment process than would be possible if only the more representative but less available corrosion product materials were to be used. Key test material parameters used in the trials have been identified as the particle size distribution and the sludge thickness (measured as yield shear strength). Other properties including cohesion, adhesion and rheological behaviour are also considered. The use of different mixers for sludge manufacture has the potential to affect the behavioural properties and a brief description of each of these mixers is included. The scale of mixing has been found to make a significant difference to the ageing. A chemical impurity in the commercially available materials has been successfully exploited, so that sludge mixed at comparatively low yield shear strengths can thicken into the consistency of clay. This aids manufacture and allows large quantities of thick material to be produced relatively easily. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Corrosion Behavior of Candidate Materials Used for Urea Hydrolysis Equipment in Coal-Fired Selective Catalytic Reduction Units

Corrosion tests were performed in the laboratory in order to assess the corrosion resistance of candidate materials used in urea hydrolysis equipment. The materials to be evaluated were exposed at 145 °C for 1000 h. Alloys 316L, 316L Mod., HR3C, Inconel 718, and TC4 were evaluated. Additionally, aluminide and chromate coatings applied to a 316L substrate were examined. After exposure, the mass changes in the test samples were measured by a discontinuous weighing method, and the morphologies, compositions, and phases of the corrosion products were analyzed using scanning electron microscopy, energy-dispersive spectroscopy, and x-ray diffraction. Results indicated that continuous pitting and dissolution corrosion were the main failure modes for 316L stainless steel. 316L Mod. and HR3C alloy showed better corrosion resistance than 316L due to their relatively high Cr contents, but HR3C exhibited a strong tendency toward intergranular corrosion. Inconel 718, TC4, and aluminide and chromate coating samples showed similar corrosion processes: only depositions formed by hydrothermal reactions were observed. Based on these results, a possible corrosion process in the urea hydrolysis environment was discussed for these candidate materials and questions to be clarified were proposed.

36 MATERIALS SCIENCE↗

Calorimetric Measurements of the Thermodynamic Properties of RE-Silicate Coating Materials

Thermodynamic quantities of coatings materials and siliceous debris-induced corrosion products are crucial to understand in order to develop mitigation strategies necessary to improve the durability of gas-turbine engines. Siliceous induced corrosion can occur when debris consisting mainly of CaO-MgO-Al2O3-SiO2 (CMAS) is ingested by aircraft engines during and after take-off, which sticks to hot surfaces and forms calcium rare-earth silicate oxyapatites. In this work, high-temperature oxide melt drop solution calorimetry (HT drop solution calorimetry) was used to obtain the enthalpies of formation for RE silicate (RE2Si2O7, RE2SiO5 where RE = Yb, Er, Y, Dy, Nd, Lu and Gd) environmental barrier coatings (EBCs) and the calcium RE silicate oxyapatite Ca2RE8(SiO4)6O2 (RE = Yb, Er, Y, Dy, Nd, Gd and Sm) corrosion products. Trends in the enthalpy of formation as a function of the ionic potential of the rare-earth cations in their related crystallographic sites are discussed.

Costa, Gustavo↗

Near-Field Corrosion Interactions between Glass and Corrosion Resistant Alloys

This study explores the corrosion interactions between model nuclear waste glass materials and corrosion resistant alloys, under conditions that simulate the near field of a nuclear waste repository. The interactions between the corrosion of stainless steel (SS) 316, alloy G30, or alloy 625, and international simple glass or soda-lime silica glass are systematically studied. The dissimilar materials were exposed in close proximity to each other in different electrolytes at 90 oC. After exposure, the glass surface exposed near metals showed different regimes of corrosion, with distinct surface morphologies and chemistries that were likely affected by the local environment created by the localized corrosion of metals. Surface and solution analyses showed that the corrosion rate of glass was enhanced by the presence of metals. Infrared spectroscopy data suggested the local build-up of stresses in the contact area of glass, which may lead to the mechanical instability of the glass alteration layer. On the other hand, the effect of glass on metal corrosion is strongly dependent on the leaching solution. In electrolytes containing abundant aggressive anions such as Cl-, glass seems to suppress the localized corrosion of SS by the precipitation of a Si-rich surface film that protects the SS substrate from solutions. However, in less aggressive electrolytes, the corrosion rate of SS was increased by the presence of glass corrosion products. Overall, our study showed that the hidden and localized damage on glass in contact with metals may enhance the release of incorporated radionuclides compared to typical uniform glass corrosion. Therefore, more attention should be paid to the corrosion interactions between metals and glass under repository conditions.

Guo, Xiaolei↗

Microstructure analysis for chemical interaction between cesium and SUS 316 steel in fast breeder reactor application

In this study the corrosion products on a surface after cesium corrosion examination at 650 deg. C for 100 hrs were characterized by TEM observation around the corroded area on the surface in order to understand the corrosion mechanism of cesium fission product for cladding materials in fast reactor. The experimental results suggest the main corrosion mechanism occurred in the process of the separation of cesium chromate and metal (Fe, Ni). The main reaction of corrosion process was considered to be equation, 2Cs + 7/2 O{sub 2} + 2Cr {yields} Cs{sub 2}Cr{sub 2}O{sub 7}(L). (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗