Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “COERCIVE FORCE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Effect of the Ce Content on the Magnetic Properties and Microstructure of CeCo{sub 5}-based Sintered Bulk Magnets

CeCo{sub 5}-based magnets have recently attracted much attention due to their moderate magnetic performance and low cost. Nevertheless, there have been few studies on the effects of Ce content on the magnetic properties and microstructures of CeCo{sub 5}-based magnets. In response to this, the magnetic properties of sintered bulk magnets with nominal compositions of Ce(Co{sub 0.73}Cu{sub 0.135}Fe{sub 0.135}){sub z} (z = 4.95, 5.15, 5.35, and 5.55), prepared by the conventional powder metallurgy method, were investigated here. Based on experimental findings, it was shown that Ce(Co{sub 0.73}Cu{sub 0.135}Fe{sub 0.135}){sub 5.15} sintered bulk magnets had comprehensive magnetic properties—maximum energy product of 80 kJ m{sup − 3} (10 MGOe) and intrinsic coercivity (H{sub cj}) of 452 kA m{sup − 1} (5.69 kOe)—superior to those previously reported by us. For z = 5.35 and 5.55, due to the presence of the minor Ce{sub 2}Co{sub 17} phase (which has a Curie temperature (T{sub c}) < 20 °C), magnets had low H{sub cj} values. Based on x-ray diffraction and scanning electron microscopy observations, it was suggested that the volume fraction of the 1:5 matrix phase was the main factor determining the H{sub cj} of CeCo{sub 5}-based sintered bulk magnets obtained with different Ce contents. Furthermore, the importance of the dispersion characteristics of the Ce{sub 2}O{sub 3} phase within the matrix was emphasized. Uniform dispersion of the Ce{sub 2}O{sub 3} phase can significantly improve the overall magnetic performance of CeCo{sub 5}-based magnets.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microwave-Hydrothermal Synthesis of Y{sub 3}Fe{sub 5}O{sub 12} Nanoparticles: Sintering Temperature Effect on Structural, Magnetic and Dielectric Properties

Herein, we report a facile microwave-assisted hydrothermal method for the preparation of yttrium iron garnet (YIG, Y{sub 3}Fe{sub 5}O{sub 12})nanocrystals and realized the synergy between its structural and magnetic properties. The as-prepared powder thermal stability was characterized in detail by using thermogravimetric-differential thermal analysis (TG-DTA). The synthesized powder was microwave sintered at six different temperatures ranging from 973 to 1373 K for 60 min and characterized using X-ray diffraction (XRD) and field emission scanning electron microscopy (FESEM). Magnetic properties were investigated by vibrating-sample magnetometer (VSM) and ferromagnetic resonance (FMR) studies. The frequency variation of dielectric and magnetic properties was measured in the frequency range of 100 kHz–1.8 GHz. The observed magnetic and dielectric parameters such as saturation magnetization, coercivity, permeability, linewidth, dielectric constant and magnetodielectric losses are strongly affected by sintering temperature. The saturation magnetization and coercivity of YIG were found in the range 14.4–28.0 emu/g and 35–87 Oe, respectively. Furthermore, the FMR linewidth decreases from 844 to 204 Oe. This analysis undoubtedly demonstrates that the synthesis method and sintering temperature have the prominent effect on the electrical and magnetic properties of YIG and would be very useful for the garnet-based microwave device applications.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Ti Capping Layer Effects in Microstructure and Magnetic Properties of Sputter-Deposited FePt Thin Film

Ti/FePt/Fe nano-thin films were fabricated by a DC facing-target magnetron sputtering method onto glass substrates at room temperature and were subsequently annealed in situ in vacuum. The impacts of the Ti capping layer on microstructural and magnetic properties of the FePt films were investigated in detail. X-ray diffraction (XRD) patterns demonstrate that the film is deposited onto glass substrates and the addition of a Ti layer forms ternary TiFePt, and binary PtTi and FeTi alloys. The results reveal refined granularity, decreased roughness, and enhanced coercivity and degree of squareness after the introduction of a Ti capping layer.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of NaOH Concentration and Adding Sequences on Structural and Magnetic Properties of Ni{sub 0.4}Co{sub 0.6}Fe{sub 2}O{sub 4} Nanopowders Prepared Via Co-precipitation Route

Ni{sub 0.4}Co{sub 0.6}Fe{sub 2}O{sub 4} nanopowders were prepared via the co-precipitation route followed by annealing treatment. The structural and magnetic properties of the as-synthesized samples were determined by XRD, FT-IR, TG-DSC, and PPMS measurements, respectively. The XRD patterns indicated a single-phase cubic spinel structure for all the Ni-Co ferrite samples, regardless of adding sequences of the reactants or NaOH concentration. The analysis of the XRD patterns revealed that the enhancement in lattice constant with increasing NaOH concentration is related to the prevention of oxidization of Co{sup 2+} ions in the Ni-Co ferrite lattice. The FT-IR spectra indicated that samples prepared in the B process have fewer impurities than those prepared in the A process. The enhancement in saturation magnetization with the increase in sodium hydroxide concentration could be attributed to the strengthening of super-exchange interaction between A and B sublattices, due to replacements of Co{sup 3+} ions (magnetic moment of 0 μ{sub B}) by Co{sup 2+} ions (magnetic moment of 3 μ{sub B}) at B sublattices. The obvious increase in the coercivity field with the increase in concentration of NaOH solutions can be interpreted in terms of enhancement of magneto-crystalline anisotropy that originated from gradual substitutions of Co{sup 3+} ions with Co{sup 2+} ions at the octahedral sites.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Random Magnetic Anisotropy Studies in SmCo{sub 5} Thin Films

SmCo{sub 5} thin films with different thicknesses were prepared by electron beam evaporation on Kapton substrates. The out-of-plane hysteresis loops for different thicknesses reveal a maximum coercive field when the thickness is 15 nm. Using random magnetic anisotropy model, the thickness dependence of magnetic properties was studied in SmCo{sub 5} nanocrystalline films and several fundamental magnetic parameters were extracted. We have determined the local magnetic anisotropy constant K{sub 1} which is found to increase with increasing film thickness except for t = 7 nm which is thought to arise from the structural imperfection of the SmCo{sub 5} films.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effects of Microwave-Assisted Annealing on the Structure and Magnetic Properties of (Nd{sub 0.75}Pr{sub 0.25}){sub 9}Fe{sub 72}Ti{sub 1}Zr{sub 3}Mn{sub x} Mo{sub 4−x}B{sub 10.5}C{sub 0.5} Amorphous Ribbons

The amorphous as-spun ribbons with nominal composition (Nd{sub 0.75}Pr{sub 0.25}){sub 9}Fe{sub 72}Ti{sub 1}Zr{sub 3}Mn{sub x}Mo{sub 4−x}B{sub 10.5}C{sub 0.5}(x = 1, 2, 3) were annealed by microwave-assisted annealing. The effects of the Mn-doped alloys on glass-forming ability (GFA), crystallization, and magnetic properties of the Nd{sub 2}Fe{sub 14}B/α-Fe nanocomposite magnets were examined by thermal differential scanning calorimetry (DSC), X-ray diffraction (XRD), and vibrating sample magnetometry (VSM). An appropriate amount of Mn was beneficial to the optimization of the structure and magnetic properties. Compared with conventional annealing, the microwave-assisted annealing has contributed to the precipitation of hard magnetic phases and adjusted the proportion of hard and soft magnetic phases. The optimum magnetic properties with coercivity up to 805 kA/m were found for ribbons (with composition x = 1) annealed under the microwave power of 2000 W for 10 min.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effects of Nd, Er Doping on the Structure and Magnetic Properties of YFeO{sub 3}

Nd, Er co-doped YFeO{sub 3} compounds were synthesized by sol-gel method. The prepared compounds were characterized by powder x-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), scanning electron microscopy (SEM), energy-dispersive x-ray (EDX), and vibrating sample magnetometer (VSM) integrated in a physical property measurement system (PPMS-9), respectively. The results show that the compounds possess orthorhombic perovskite structure. The Y{sub 0.5}Er{sub 0.1}Nd{sub 0.4}FeO{sub 3} compound mainly consists of five elements (Er, Nd, Y, Fe, and O) and atom ratio matched well with the formula. With the increase of Nd{sup 3+} doping content in Y{sub 0.5}Er{sub 0.5−x}Nd{sub x}FeO{sub 3} (x = 0, 0.1, 0.2, 0.3, and 0.4), the coercivity increases gradually while the saturation magnetization and remanent magnetization decrease at the same time. Introducing Nd{sup 3+} and Er{sup 3+} ions into YFeO{sub 3} will make a change on a structure distortion, resulting in the decrease of the Fe–O–Fe angle and the consequent reduction of superexchange effect. From our research results, the relationship between the r (R{sup 3+}) and the superexchange bond angle is different from pure-phase orthoferrites R FeO{sub 3}.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetic Features of Boron Doping on Hf{sub 2}Co{sub 11} Thin Films

The effect of boron (B) doping on the structural and magnetic properties is studied systematically in the Hf{sub 2}Co{sub 11} thin films. The modified crystal microstructure and annealing process enhanced the coercive field up to 1754 Oe. In order to obtain superior magnetic properties, the optimum doping ratios should be properly controlled attentively. To identify the structure, B-doped Hf{sub 2}Co{sub 11} thin films were investigated by temperature-dependent X-ray diffraction analysis for the first time. The hard magnetic phase of Hf{sub 2}Co{sub 11}B{sub x} thin films was formed to orthorhombic phase with some Co impurities and had a crystallization temperature around 823 K.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetic Behavior of Iron-Rich Permalloy Nanoparticles

Iron-rich permalloy Fe{sub x}Ni{sub 1−x} nanoparticles (NPs) were fabricated using a low-temperature wet chemistry method involving the hydrothermal growth of the NPs. Three Fe–Ni NPs (Fe{sub 0.5}Ni{sub 0.5}, Fe{sub 0.625}Ni{sub 0.375}, and Fe{sub 0.83}Ni{sub 0.17}) were fabricated and studied by X-ray diffraction (XRD), scanning electron microscopy (SEM), and vibrating sample magnetometer (VSM). After the initial formations, the three Fe–Ni NPs were annealed at 200, 400, and 600 °C; the XRD showed that all three FeNi NPs had a bcc structure (not the fcc structure of the standard Fe{sub 20}Ni{sub 80} permalloy). The SEM images showed that the NPs had spherical shapes. The VSM measurements showed that none of the Fe–Ni nanoparticles were superparamagnets but were ferromagnets. The heat treatments cause the work needed to the flip the spin (coercivity (H{sub c})) to increase and the values of the saturation magnetizations to fluctuate.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Evolution of Micro-structure and Magnetic Properties in L1{sub 0} CoPt Nanoparticles by Au Addition

L1{sub 0} CoPt-Au nanoparticles with face-centered tetragonal (FCT) structure were synthesized by sol-gel technique at 700°C. The micro-structure and magnetism of L1{sub 0} CoPt-Au were measured by different measuring technologies. The influences of Au on the micro-structure and magnetism of L1{sub 0} CoPt nanoparticles were investigated. The Au addition promoted the formation of ordered L1{sub 0} phase CoPt nanoparticles and improved the grain size of L1{sub 0} CoPt nanoparticles When the Au content increased to 10 at.%, coercivity increased and saturation magnetization decreased, which may be originated from the increased order degree and ferrimagnetic nature of L1{sub 0} CoPt nanoparticles. Interestingly, when the Au addition was more than 10 at.%, the coercivity decreased due to the decrease of the order degree.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effects of Fe Ion Vacancy on Magnetic Properties of NiFe{sub 2}O{sub 4} Ferrite Nanoparticles

The effects of Fe ion vacancy on structural and magnetic properties of NiFeO{sub 4} nanoparticles are investigated using X-ray diffraction, Fourier transform infrared, morphological, and magnetic measurements. The introduction of Fe ion vacancy leads to the increase of the lattice parameter and decrease of the particle size. Moreover, vibrating sample magnetometer measurement results revealed that the values of the magnetization decreased and that coercivity had no regular behavior with increasing Fe ion vacancy content. These behaviors could be explained by considering cation distribution in the spinel structure. The estimated cation distribution results show that the Fe ion vacancy mostly occurred at the B sites which is in good agreement with the theoretical calculations.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Tailoring the Structural, Optical and Magnetic Properties of NiFe{sub 2}O{sub 4} by Varying Annealing Temperature

Magnetic nanocrystalline NiFe{sub 2}O{sub 4} nanoparticles of size ranging between 13 and 19 nm were synthesized by the hydrothermal method using polyethylene glycol (PEG) as surfactant. The role of annealing on phase, crystallite size, and morphology was determined by X-ray diffraction (XRD) and transmission electron microscopy (TEM). Energy-dispersive X-ray spectroscopy (EDX) was used for qualitative analysis. X-ray diffraction confirmed the single phase of as-obtained particles. TEM revealed a spherical morphology having an average particle size of 13.73 nm at 523 K and rises to 14.89, 16.42, and 21.14 nm at 623, 723, and 823 K respectively, which is approximately the same as the crystallite size determined from XRD. EDX results confirmed that elemental ratios were in stoichiometry. Fourier transform infrared (FTIR) spectral analysis demonstrates the formation of M-O bond in NiFe{sub 2}O{sub 4} nanoparticles. The optical spectra obtained from UV-visible spectroscopy revealed that nanoparticles have direct allowed energy band gap of 2.34, 2.47, 2.70, and 2.20 eV at 523, 623, 723, and 823 K respectively. A vibrating sample magnetometer (VSM) was used at room temperature for magnetic measurements which further showed ferromagnetic behavior of as-synthesized material. In addition, it was found that saturation magnetization increases with an increase of annealing temperature while coercivity decreases with temperature.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Facile Synthesis of Spinel Ferrites with Enhanced Magnetic Properties from Two Intractable Metallurgical Resources: Zinc-Bearing Dust and Nickel Laterite Ore

Nickel laterite ore and zinc-bearing dust are multi-metal-associated and intractable resources. Comprehensive and cooperative utilization of zinc-bearing dust and nickel laterite ore for the preparation of spinel ferrites with enhanced magnetic properties by a facile process was proposed. The structure and magnetic properties of as-prepared spinel ferrites were characterized by X-ray diffraction (XRD), Raman spectroscopy, and Physical Property Measurement System (PPMS). The effect of mass ratios of zinc-bearing dust to nickel laterite ore, calcination temperature, and Zn substitution content on the as-prepared samples was investigated in detail. A single phase of Zn-substituted spinel ferrites (x= 0.00, 0.10, 0.20, and 0.30) could be obtained when the mass ratios were controlled at 1:0.4, 1:4:1.8, 1:2:1.5, and 1:1:1.2 after being calcined at 900 {sup ∘}C for 30 min, respectively. The magnetic property tests present that the as-prepared spinel ferrite exhibits enhanced magnetic properties with the saturation magnetization (Ms) value of 66.8 emu g{sup − 1} and the coercivity (Hc) value of 26 Oe when the mass ratio was controlled at 1:1:1.2. This research could provide an effective way to transfer two intractable resources into soft magnetic materials.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Evolution of Intrinsic and Magnetic Field-Induced Magnetic Anisotropies in Strongly Phase-Separated Manganite Thin Films

Single crystalline thin film (∼ 100 nm) of La{sub 0.18}Pr{sub 0.40}Ca{sub 0.42}MnO{sub 3} is grown on (001) oriented LaAlO{sub 3} substrates and the evolution of anisotropy associated with the supercooling behaviour of the magnetic liquid is studied as a function of temperature and magnetic field. The angle-dependent magnetization measurements ascertain that the easy magnetic axis lies in the plane of the film while the hard axis is along the plane normal. The ratio of the easy and hard axes magnetizations (M{sub ||} and M{sub ⊥}) measured at 10 K, viz., M{sub ||}/M{sub ⊥} (10 K) = 2.6, confirms the strongly anisotropic nature of the film. The easy axis ferromagnetic (FM) transition temperature (T{sub C}) is smaller than that along the hard axis. The giant hysteresis in FCC–FCW M–T, which manifests the magnetic liquid behaviour of the strongly phase-separated manganites is appreciably narrowed along the hard axis. The strain glass state is also less dominant along the easy axis. The analysis of the M–H data brings out that the easy axis remanence (M{sub r||}) shows a nonlinear temperature dependence, while the one corresponding to the hard axis (M{sub r⊥}) shows a nearly linear behaviour. The coercivity (H{sub C}) follows a law of the type H{sub C}(T)=H{sub C}(0)(1−AT{sup b}). The value of exponent b ∼ 0.5 for single-domain particles, but in the present case, the best fit to the experimental data yields the exponent b ≈ 0.25 for both H{sub C||} and H{sub C⊥}. The smaller value of the exponent is attributed to the non-canonical nature of the ferromagnetic state and the associated strongly phase-separated nature of the LPCMO thin film.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of Si on the Glass Formation and Magnetic Properties of High-Iron Fe–Zr–Si Alloys

High-iron Fe–Zr–Si amorphous ribbons were fabricated through the melt-spun technique. Then, the effects of Si content on the glass-forming ability and magnetic properties of Fe{sub 90−x}Zr{sub 10}Si{sub x} (x = 1, 2, 3, 4, 5, 10) alloys were investigated. Results showed that the amorphous structure only formed in an alloy composition of 3 at.% Si. Moreover, α-Fe(Si) and Fe{sub 3}Zr phase appeared gradually when Si was added. Fe{sub 87}Zr{sub 10}Si{sub 3} alloy is a unique amorphous structure in Fe{sub 90−x}Zr{sub 10}Si{sub x} ribbons. The peak temperatures of the two crystallization stages were 464 and 600 {sup ∘}C. The saturation magnetization (M{sub s}) values of the alloys ranged from 91.2 to 132.3 emu/g, and all had an initial increase before decreasing and their coercivity (H{sub c}) values increased with increased Si content. The Fe{sub 87}Zr{sub 10}Si{sub 3} amorphous alloy exhibited a low H{sub c} value of approximately 39.1 A/m, which shows good magnetic properties in the as-quenched state. After annealing, the M{sub s} of the amorphous sample considerably improved, particularly reaching 165.3 emu/g at 600 {sup ∘}C.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

The Role of Wheel Surface Quality on Structural and Hard Magnetic Properties of Nd–Fe–B Permanent Magnet Powders

Rapidly solidified Nd{sub 15}Fe{sub 77}B{sub 8} magnetic alloy powders have been produced by using melt-spinning method. Different wheel surface structures such as smooth and textured were tested to investigate the effect of wheel surface morphology on powder shape, microstructure, Curie temperature, and magnetic properties. Produced powders were subjected to surfactant-active ball-milling process for powder size reduction and to enhance magnetic and thermal properties. Generally, flaky-shaped powders were obtained with smooth surface wheels and spherical-shaped powders were produced with textured surface wheel. Microstructure of flaky-shaped powders consisted of polygonal fine equiaxed grains with an average grain size of 0.45 µm. Spherical-shaped powders had dendritic microstructure regardless of their sizes. Both flaky and spherical powders involved hard magnetic Nd{sub 2}Fe{sub 14}B phase located in the grain interior and a fine network of Nd-rich phase at the grain boundaries. Surfactant-active ball-milling process significantly contributed to magnetic and thermal properties of powders. The coercivity values of flaky-shaped powders milled for 90, 150, 210, 270, 330, and 390 min milling times were substantially higher than that of spherical-shaped powders milled for the same period of times. The Curie temperatures of Nd{sub 15}Fe{sub 77}B{sub 8} ingot alloy and spherical- and flaky-shaped powders were found as 279, 305, and 321 {sup ∘}C, respectively. On the other hand, the Curie temperatures of flaky- and spherical-shaped powders milled for 390 min were measured as 331 and 311 {sup ∘}C, respectively.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

The Structural and Magnetic Characteristics of Nanocrystalline Co{sub 82}Zr{sub 18} Alloy

In the present study, the structural and magnetic characteristics of nanocrystalline Co{sub 82}Zr{sub 18} alloy with different structure and crystallite sizes were investigated. In this regard, the nanocrystalline Co{sub 82}Zr{sub 18} sample with different structure and crystallite sizes were prepared using a copper boat vacuum induction melting plus melt spinning and subsequent annealing processes. The prepared samples were characterized using X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), differential scanning calorimetry (DSC), and vibrating scanning magnetometer (VSM). According to achieved results, single-phase structure of Zr{sub 2}Co{sub 11} can successfully form by means of melt spinning process at wheel speed of 40 m/s. The melt-spun ribbons exhibit hard magnetic properties with the coercivity and saturation of magnetization in the range of 2.3 kOe and 58 emu/g, respectively. The highest value of coercivity in Co{sub 82}Zr{sub 18} alloy was estimated to be about 3 kOe in annealed sample at 500{sup ∘}C for 1 h.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structural and Soft Magnetic Properties of Nickel-Substituted Co-Zn Nanoferrites

Nickel-substituted cobalt-zinc nanoferrites (Co{sub 0.5−x}Zn{sub 0.5}Ni{sub x}Fe{sub 2}O{sub 4}, x = 0.05 to 0.25 in steps of 0.05) were synthesized in a citric acid auto-combustion method. Divalent strong paramagnetic nickel ions substituted in place of ferromagnetic cobalt ions resulted in slight modifications over structural and significant changes in magnetic properties of the system. All samples were characterized with X-ray diffraction technique for structure determination. Crystallite sizes were calculated using the Williamson-Hall plot and size-strain plots, from these lattice strain and microstrain were discussed. Transmission electron microscopy measurements were done for the base sample (x = 0), and they showed well-developed spherical particles with an average size of 35 nm. SEM micrograph was recorded for the base sample to observe surface morphology, and it was observed to be stoichiometric, as evident from EDAX measurements. Saturation magnetization, remanence, coercivity and remanence ratio were measured using M-H loops recorded using a vibrating sample magnetometer at room temperature. Magnetocrystalline anisotropy was discussed with the help of magnetocrystalline anisotropy constant (K{sub 1}) obtained from the law of approach to saturation method.

36 MATERIALS SCIENCE↗