Effects of aging on the characteristics of TiNiPd shape memory alloy thin films

TiNiPd thin films have been deposited on glass substrate using R.F. magnetron sputtering. Effects of annealing and aging on the microstructure, phase transformation behaviors and shape memory effects of these thin films have been studied by X-ray diffractometry, differential scanning calorimeter, tensile tests and internal friction characteristics. The TiNiPd thin films annealed at 750 deg. C exhibit uniform martensite/austenite transformations and shape memory effect. Aging at 450 deg. C for 1 h improved the uniformity of transformations and shape memory effect. Long time aging decreased transformation temperatures and increased the brittleness of TiNiPd thin films.

36 MATERIALS SCIENCE↗

Compositional analysis and depth profiling of thin film CrO{sub 2} by heavy ion ERDA and standard RBS: a comparison

Chromium dioxide (CrO{sub 2}) thin film has generated considerable interest in applied research due to the wide variety of its technological applications. It has been extensively investigated in recent years, attracting the attention of researchers working on spintronic heterostructures and in the magnetic recording industry. However, its synthesis is usually a difficult task due to its metastable nature and various synthesis techniques are being investigated. In this work a polycrystalline thin film of CrO{sub 2} was prepared by electron beam vaporization of Cr{sub 2}O{sub 3} onto a Si substrate. The polycrystalline structure was confirmed through XRD analysis. The stoichiometry and elemental depth distribution of the deposited film were measured by ion beam nuclear analytical techniques heavy ion elastic recoil detection analysis (ERDA) and Rutherford backscattering spectrometry (RBS), which both have relative advantage over non-nuclear spectrometries in that they can readily provide quantitative information about the concentration and distribution of different atomic species in a layer. Moreover, the analysis carried out highlights the importance of complementary usage of the two techniques to obtain a more complete description of elemental content and depth distribution in thin films. - Graphical abstract: Heavy ion elastic recoil detection analysis (ERDA) and Rutherford backscattering spectrometry (RBS) both have relative advantage over non-nuclear spectrometries in that they can readily provide quantitative information about the concentration and distribution of different atomic species in a layer. Highlights: Black-Right-Pointing-Pointer Thin films of CrO{sub 2} have been grown by e-beam evaporation of Cr{sub 2}O{sub 3} target in vacuum. Black-Right-Pointing-Pointer The composition was determined by heavy ion-ERDA and RBS. Black-Right-Pointing-Pointer HI-ERDA and RBS provided information on the light and heavy elements, respectively.

36 MATERIALS SCIENCE↗

X-ray microstructural analysis of nanocrystalline TiZrN thin films by diffraction pattern modeling

A detailed microstructural characterization of nanocrystalline TiZrN thin films grown at different substrate temperatures (T{sub S}) was carried out by X-ray diffraction (XRD). Total diffraction pattern modeling based on more meaningful microstructural parameters, such as crystallite size distribution and dislocation density, was performed to describe the microstructure of the thin films more precisely. This diffraction modeling has been implemented and used mostly to characterize powders, but the technique can be very useful to study hard thin films by taking certain considerations into account. Nanocrystalline films were grown by using the cathodic pulsed vacuum arc technique on stainless steel 316L substrates, varying the temperature from room temperature to 200 °C. Further surface morphology analysis was performed to study the dependence of grain size on substrate temperature using atomic force microscopy (AFM). The crystallite and surface grain sizes obtained and the high density of dislocations observed indicate that the films underwent nanostructured growth. Variations in these microstructural parameters as a function of T{sub S} during deposition revealed a competition between adatom mobility and desorption processes, resulting in a specific microstructure. These films also showed slight anisotropy in their microstructure, and this was incorporated into the diffraction pattern modeling. The resulting model allowed for the films' microstructure during synthesis to be better understood according to the experimental results obtained. - Highlights: • Mobility and desorption competition generates a critical temperature. • A microstructure anisotropy related to the local strain was observed in thin films. • Adatom mobility and desorption influence grain size and microstrain.

36 MATERIALS SCIENCE↗

Crystallization study of amorphous sputtered NiTi bi-layer thin film

The crystallization of Ni-rich/NiTiCu bi-layer thin film deposited by magnetron sputtering from two separate alloy targets was investigated. To achieve the shape memory effect, the NiTi thin films deposited at room temperature with amorphous structure were annealed at 773 K for 15, 30, and 60 min for crystallization. Characterization of the films was carried out by differential scanning calorimetry to indicate the crystallization temperature, grazing incidence X-ray diffraction to identify the phase structures, atomic force microscopy to evaluate surface morphology, scanning transmission electron microscopy to study the cross section of the thin films. The results show that the structure of the annealed thin films strongly depends on the temperature and time of the annealing. Crystalline grains nucleated first at the surface and then grew inward to form columnar grains. Furthermore, the crystallization behavior was markedly affected by composition variations. - Highlights: • A developed bi-layer Ni45TiCu5/Ni50.8Ti was deposited on Si substrate and crystallized. • During crystallization, The Ni{sub 45}TiCu{sub 5} layer is thermally less stable than the Ni-rich layer. • The activation energy is 302 and 464 kJ/mol for Cu-rich and Ni-rich layer in bi-layer, respectively.

36 MATERIALS SCIENCE↗

Deposition of transparent conductive mesoporous indium tin oxide thin films by a dip coating process

Cetyltrimethyl ammonium bromide (CTAB) templated mesoporous indium tin oxide (ITO) thin films were deposited on quartz plates by an evaporation-induced self-assembly (EISA) process using a dip coating method. The starting solution was prepared by mixing indium chloride, tin chloride, and CTAB dissolved in ethanol. Five to fifty mole percent Sn-doped ITO films were prepared by heat-treatment at 400 deg. C for 5 h. The structural, adsorptive, electrical, and optical properties of mesoporous ITO thin films were investigated. Results indicate that the mesoporous ITO thin films have an ordered two-dimensional hexagonal (p6mm) structure, with nanocrystalline domains in the inorganic oxide framework. The continuous thin films have highly ordered pore sizes (>20 A), high Brunauer-Emmett-Teller (BET) surface area up to 340 m{sup 2}/g, large pore volume (>0.21 cm{sup 3}/g), outstanding transparency in the visible range (>80%), and show a minimum resistivity of {rho} = 1.2 x 10{sup -2} {omega} cm.

36 MATERIALS SCIENCE↗

Electric and magnetic properties of Pb(Zr{sub 0.52}Ti{sub 0.48})O{sub 3}-CoFe{sub 2}O{sub 4} particle composite thin film on the SrTiO{sub 3} substrate

We deposited a thin epitaxial Pb(Zr{sub 0.52}Ti{sub 0.48})O{sub 3} (PZT) layer on the (0 0 1) SrTiO{sub 3} (STO) substrate doped with Nb (0.5 wt.%), then grew composite thin film of CoFe{sub 2}O{sub 4} (CFO) and PZT phases on it. X-ray diffraction and high resolution transmission electron microscopy showed that the PZT and CFO phases in the film had perfect epitaxial structures. CFO nanoparticles were embedded in PZT matrix randomly, which was useful to enhance the insulativity of the composite film. The composite thin film exhibited good ferromagnetic and ferroelectric properties. The dielectric constants of the composite thin film kept unchangeable in a wide bias electric field, but increased in a magnetic field, namely, magnetodielectric effect. The possible reasons for the magnetodielectric effect were discussed.

36 MATERIALS SCIENCE↗

A simple chemical method for deposition of electrochromic Prussian blue thin films

Highlights: Black-Right-Pointing-Pointer Prussian blue thin films were prepared by a simple chemical deposition method. Black-Right-Pointing-Pointer The films can be easily prepared from aqueous solution of Fe{sub 2}(SO{sub 4}){sub 3} and K{sub 4}[Fe(CN){sub 6}]. Black-Right-Pointing-Pointer The films show good electrochromic properties. Black-Right-Pointing-Pointer They change from deep blue color into green, and then back to blue and colorless. Black-Right-Pointing-Pointer The PB thin films exhibit stability and excellent reversibility. -- Abstract: This paper is about a recently developed new chemical method for deposition of Prussian blue thin films. The films are easily prepared by successive immersion of the substrates into an acidic aqueous solution of Fe{sub 2}(SO{sub 4}){sub 3} and K{sub 4}[Fe(CN){sub 6}]. It is calculated of the results from AFM analysis that the growth in the film thickness by one immersion cycle corresponds to an average increase of 6 nm. The characterization of the films with X-ray diffraction, SEM-EDS analysis and FTIR spectroscopy shows that the deposited material is amorphous hydrated Fe{sub 4}[Fe(CN){sub 6}]{sub 3}. The electrochromic properties are characterized by cyclic voltammetry and VIS spectrophotometry. The PB thin films exhibit stability and excellent reversibility, which make these films favorable for electrochromic devices.

36 MATERIALS SCIENCE↗

Novel microwave assisted sol–gel synthesis (MW-SGS) and electrochromic performance of petal like h-WO{sub 3} thin films

Graphical abstract: Electrochromic intercalation and deintercalation of Li{sup +} ions and electrons is facilitated by providing hexagonal tunnel, trigonal cavity and square window which allows easy and fast insertion and extraction of ions. Highlights: ► Novel two step MW-SGS is first time employed to prepare WO{sub 3} thin films. ► MW-SGS is simple and cost effective technique for preparation of nanostructures. ► Petal-like hexagonal WO{sub 3} nanodisks were successfully deposited. ► O/W ratio calculated by XPS studies is 2.89. ► Good electrochromic performance suggests practical usability of proposed technique. -- Abstract: Use of domestic microwave oven is first time employed for chemical deposition of nanocrystalline hexagonal WO{sub 3} (h-WO{sub 3}) thin films. Low cost precursors like sodium tungstate, hydrochloric acid, oxalic acid and potassium sulfate signifies cost effectiveness of this thin film fabrication route. Scanning electron microscopy images reveal formation of petal like nanodisks. A number of analytical techniques were used to characterize the WO{sub 3} petal like nanodisks, including X-ray diffraction (XRD), energy dispersive X-ray spectroscopy (EDX), X-ray photoelectron spectroscopy, FT-IR spectroscopy, Raman scattering spectroscopy, UV–visible spectrophotometry and cyclic voltammetry (CV). The X-ray photoelectron spectroscopic studies revealed 2.89 O/W atomic ratio. The electrical transport studies on WO{sub 3} thin films show semiconducting behavior with n-type semiconductivity. The value of determined coloration efficiency is 57.90 cm{sup 2}/C. The mechanism of Li{sup +} intercalation and deinercalation in h-WO{sub 3} matrix is proposed for enhanced electrochromism.

36 MATERIALS SCIENCE↗

Morphology dependent electrochemical performance of sputter deposited Sn thin films

Graphical abstract: Smooth homogenous anode surface results in better electrochemical performance in terms of capacity and cycle life. Highlights: ► Controlling rate of deposition of Sn thin films for different surface morphology. ► Higher deposition rate results in poor capacity retention. ► Lower deposition rate of 0.25 nm s{sup −1} helps in higher capacity retention. ► Electrochemical performance correlated homogeneity and interparticle contact area. -- Abstract: This study deals with tailoring of the surface morphology, microstructure, and electrochemical properties of Sn thin films deposited by magnetron sputtering with different deposition rates. Scanning electron microscopy and atomic force microscopy are used to characterize the film surface morphology. Electrochemical properties of Sn thin film are measured and compared by cyclic voltammetry and charge–discharge cycle data at a constant current density. Sn thin film fabricated with a higher deposition rate exhibited an initial discharge capacity of 798 mAh g{sup −1} but reduced to 94 mAh g{sup −1} at 30th cycle. Film deposited with lower deposition rate delivered 770 mAh g{sup −1} during 1st cycle with improved capacity retention of 521 mAh g{sup −1} on 30th cycle. Comparison of electrochemical performances of these films has revealed important distinctions, which are associated with the surface morphology and hence on rate of deposition.

36 MATERIALS SCIENCE↗

Synthesis of TiO{sub 2} thin films using single molecular precursors by MOCVD method for dye-sensitized solar cells application and study on film growth mechanism

For dye-sensitized solar cells application, in this study, we have synthesized TiO{sub 2} thin films at deposition temperature in the range of 300–750 °C by metalorganic chemical vapor deposition (MOCVD) method. Titanium(IV) isopropoxide, (TIP, Ti(O{sup i}Pr){sub 4}) and Bis(dimethylamido)titanium diisopropoxide, (BTDIP, (Me{sub 2}N){sub 2}Ti(O{sup i}Pr){sub 2}) were used as single source precursors that contain Ti and O atoms in the same molecule, respectively. Crack-free, highly oriented TiO{sub 2} polycrystalline thin films with anatase phase were deposited on Si(1 0 0) with TIP at temperature as low as 450 °C. XRD and TED data showed that below 500 °C, the TiO{sub 2} thin films were dominantly grown in the [2 1 1] direction on Si(1 0 0), whereas with increasing the deposition temperature to 700 °C, the main film growth direction was changed to [2 0 0]. Above 700 °C, however, rutile phase TiO{sub 2} thin films have only been obtained. In the case of BTDIP, on the other hand, only amorphous film was grown on Si(1 0 0) below 450 °C while a highly oriented anatase TiO{sub 2} film in the [2 0 0] direction was obtained at 500 °C. With further increasing deposition temperatures over 600 °C, the main film growth direction shows a sequential change from rutile [1 0 1] to rutile [4 0 0], indicating a possibility of getting single crystalline TiO{sub 2} film with rutile phase. This means that the precursor together with deposition temperature can be one of important parameters to influence film growth direction, crystallinity as well as crystal structure. To investigate the CVD mechanism of both precursors in detail, temperature dependence of growth rate was also carried out, and we then obtained different activation energy of deposition to be 77.9 and 55.4 kJ/mol for TIP and BTDIP, respectively. Also, we are tested some TiO{sub 2} film synthesized with BTDIP precursor to apply dye-sensitized solar cell.

36 MATERIALS SCIENCE↗

In–Ga–Zn–O thin film transistor with HfO{sub 2} gate insulator prepared using various O{sub 2}/(Ar + O{sub 2}) gas ratios

We have investigated the effect of the deposition of an HfO{sub 2} thin film as a gate insulator with different O{sub 2}/(Ar + O{sub 2}) gas ratios using RF magnetron sputtering. The HfO{sub 2} thin film affected the device performance of amorphous indium–gallium–zinc oxide transistors. The performance of the fabricated transistors improved monotonously with increasing O{sub 2}/(Ar + O{sub 2}) gas ratio: at a ratio of 0.35, the field effect mobility of the amorphous InGaZnO thin film transistors was improved to 7.54 cm{sup 2}/(V s). Compared to those prepared with an O{sub 2}/(Ar + O{sub 2}) gas ratio of 0.05, the field effect mobility of the amorphous InGaZnO thin film transistors was increased to 1.64 cm{sup 2}/(V s) at a ratio of 0.35. This enhancement in the field effect mobility was attributed to the reduction of the root mean square roughness of the gate insulator layer, which might result from the trap states and surface scattering of the gate insulator layer at the lower O{sub 2}/(Ar + O{sub 2}) gas ratio.

36 MATERIALS SCIENCE↗

In situ fabricate Cu{sub 2}S thin film with hierarchical petal-like nanostructures

Graphical abstract: - Highlights: • Cu{sub 2}S thin films with hierarchical nanostructures have been synthesized by solvothermal method using DMSO as reactant. • The band gap is estimated to be 1.0 eV of the Cu{sub 2}S hierarchical nanostructures. • The form process of Cu{sub 2}S and the possible mechanism of hierarchical nanostructures were proposed. - Abstract: In this paper, Cu{sub 2}S thin film with hierarchical petal-like nanostructures has been successfully in situ synthesized via a solvothermal method using DMSO as reactant under appropriate reaction conditions. The crystalline phase, morphology and optical properties of the resulting products were characterized by X-ray diffraction, energy-dispersive X-ray spectrometry, scanning electron microscopy and UV–vis absorption spectroscopy, respectively. The band gap is estimated to be about 1.0 eV by the results of UV–vis absorption spectroscopy of the Cu{sub 2}S thin film with hierarchical nanostructures that consisted of nanoslices with the thickness of 15 nm. The formation process of Cu{sub 2}S and the possible mechanism of hierarchical nanostructures were also proposed. These findings are valuable since Cu{sub 2}S thin film with hierarchical petal-like nanostructures are promising candidate as lithium ion battery and solar cell materials.

36 MATERIALS SCIENCE↗

Room temperature multiferroic properties of (Bi{sub 0.95}La{sub 0.05})(Fe{sub 0.97}Mn{sub 0.03})O{sub 3}/NiFe{sub 2}O{sub 4} double layered thin film

Graphical abstract: - Highlights: • Chemical solution deposition of (Bi{sub 0.95}La{sub 0.05})(Fe{sub 0.97}Mn{sub 0.03})O{sub 3}–NiFe{sub 2}O{sub 4} double layered thin film. • Studies on structural, electrical and multiferroic properties. • NiFe{sub 2}O{sub 4} acts as both resistive buffer layer and magnetic source. - Abstract: (Bi{sub 0.95}La{sub 0.05})(Fe{sub 0.97}Mn{sub 0.03})O{sub 3}/NiFe{sub 2}O{sub 4} double layered thin film was prepared on a Pt(111)/Ti/SiO{sub 2}/Si(100) substrate by a chemical solution deposition method. X-ray diffraction and Raman scattering spectroscopy studies confirmed the formation of the distorted rhombohedral perovskite and the inverse spinel cubic structures for the (Bi{sub 0.95}La{sub 0.05})(Fe{sub 0.97}Mn{sub 0.03})O{sub 3}/NiFe{sub 2}O{sub 4} double layered thin film. The (Bi{sub 0.95}La{sub 0.05})(Fe{sub 0.97}Mn{sub 0.03})O{sub 3}/NiFe{sub 2}O{sub 4} double layered thin film exhibited well saturated ferromagnetic (2 M{sub r} of 18.1 emu/cm{sup 3} and 2H{sub c} of 0.32 kOe at 20 kOe) and ferroelectric (2P{sub r} of 60 μC/cm{sup 2} and 2E{sub c} of 813 kV/cm at 866 kV/cm) hysteresis loops with low order of leakage current density (4.5 × 10{sup −6} A/cm{sup 2} at an applied electric field of 100 kV/cm), which suggest the ferroelectric and ferromagnetic multi-layers applications in real devices.

36 MATERIALS SCIENCE↗

Growth, structural and optoelectronic properties tuning of nitrogen-doped ZnO thin films synthesized by means of reactive pulsed laser deposition

Highlights: • PLD technique has been used to elaborate N doped ZnO. • A maximum incorporation of 0.7 at.% has been achieved at a pressure of 25 mTorr. • Increasing the N{sub 2} pressure decreases the nitrogen content with the creation of more defects. • Optical transmission and PL spectra have confirmed the band gap narrowing. - Abstract: Pulsed laser deposition has been successfully used to achieve in-situ nitrogen doping of zinc oxide thin films at a temperature as low as 300 °C. Nitrogen-doped zinc oxide (ZnO:N) thin films with a maximum nitrogen content of 0.7 at.% were obtained by varying the nitrogen background pressure in the range of 0–150 mTorr. The ZnO:N thin films were found to present hexagonal crystalline structure with dense and smooth surface. X-ray photoelectron spectroscopy analysis confirms the effective incorporation of nitrogen into ZnO thin films. Optical transmission together with room temperature photoluminescence measurements show that the band gap of the ZnO:N films shifts from 3.3 eV to 3.1 eV as nitrogen concentration varies in the range of 0.2–0.7 at.%. The narrower band gap is obtained at an optimal nitrogen concentration of 0.22 at.%. This band gap narrowing is found to be caused by both nitrogen incorporation and nitrogen-induced defects in the ZnO:N films.

36 MATERIALS SCIENCE↗

Structural and vibrational investigations of Nb-doped TiO{sub 2} thin films

Highlights: • We studied the evolutions of structure for TiO{sub 2} thin film as changes with Nb doping and temperatures. • Up to 800 °C, the grain size of Nb{sub 0.1}Ti{sub 0.9}O{sub 2} is smaller than for pure TiO{sub 2} because doped Nb hinders the growth of the TiO{sub 2} grains. • There was no formation of the rutile phase at high temperature. • Nb doped TiO{sub 2} films have high electron densities at 400–700 °C. • Nb dope extends the absorbance spectra of TiO{sub 2} which leads to the band gap reduce. - Abstract: Acid-catalyzed sol–gel and spin-coating methods were used to prepare Nb-doped TiO{sub 2} thin film. In this work, we studied the effect of niobium doping on the structure, surface, and absorption properties of TiO{sub 2} by energy-dispersive X-ray spectroscopy (EDX), X-ray diffraction (XRD), X-ray reflectometry (XRR), X-ray photoelectron spectroscopy (XPS), Raman, and UV–vis absorption spectroscopy at various annealing temperatures. EDX spectra show that the Nb:Ti atomic ratios of the niobium-doped titania films are in good agreement with the nominal values (5 and 10%). XPS results suggest that charge compensation is achieved by the formation of Ti vacancies. Specific niobium phases are not observed, thus confirming that niobium is well incorporated into the titania crystal lattice. Thin films are amorphous at room temperature and the formation of anatase phase appeared at an annealing temperature close to 400 °C. The rutile phase was not observed even at 900 °C (XRD and Raman spectroscopy). Grain sizes and electron densities increased when the temperature was raised. Nb-doped films have higher electron densities and lower grain sizes due to niobium doping. Grain size inhibition can be explained by lattice stress induced by the incorporation of larger Nb{sup 5+} ions into the lattice. The band gap energy of indirect transition of the TiO{sub 2} thin films was calculated to be about 3.03 eV. After niobium doping, it decreased to 2.40 eV.

36 MATERIALS SCIENCE↗

Optical and structural properties of sputtered CdS films for thin film solar cell applications

Graphical abstract: Photo current–voltage curves (a) and the quantum efficiency (QE) (b) for the solar cell with CdS film grown at 300 °C. - Highlights: • CdS thin films were grown by a RF magnetron sputtering method. • Influence of growth temperature on the properties of CdS films was investigated. • At higher T{sub g}, the crystallinity of the films improved and the grains enlarged. • CdS/CdTe solar cells with efficiencies of 9.41% were prepared at 300 °C. - Abstract: CdS thin films were prepared by radio frequency magnetron sputtering at various temperatures. The effects of growth temperature on crystallinity, surface morphology and optical properties of the films were characterized with X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), Raman spectra, UV–visible spectrophotometry, and photoluminescence (PL) spectra. As the growth temperature was increased, the crystallinity of the sputtered CdS films was improved and the grains were enlarged. The characteristics of CdS/CdTe thin film solar cell appeared to be significantly influenced by the growth temperature of the CdS films. Thin film CdS/CdTe solar cells with efficiencies of 9.41% were prepared at a growth temperature of 300 °C.

36 MATERIALS SCIENCE↗

Ferroelectric and piezoelectric responses of (110) and (001)-oriented epitaxial Pb(Zr{sub 0.52}Ti{sub 0.48})O{sub 3} thin films on all-oxide layers buffered silicon

Graphical abstract: The cross sections show a very dense structure in the (001)-oriented films (c,d), while an open columnar growth structure is observed in the case of the (110)-oriented films (a,b). The (110)-oriented PZT films show a significantly larger longitudinal piezoelectric coefficient (d33{sub ,f}), but smaller transverse piezoelectric coefficient (d31{sub ,f}) than the (001) oriented films. - Highlights: • We fabricate all-oxide, epitaxial piezoelectric PZT thin films on Si. • The orientation of the films can be controlled by changing the buffer layer stack. • The coherence of the in-plane orientation of the grains and grain boundaries affects the ferroelectric properties. • Good cycling stability of the ferroelectric properties of (001)-oriented PZT thin films. The (110)-oriented PZT thin films show a larger d33{sub ,f} but smaller d31{sub ,f} than the (001)-oriented films. - Abstract: Epitaxial ferroelectric Pb(Zr{sub 0.52}Ti{sub 0.48})O{sub 3} (PZT) thin films were fabricated on silicon substrates using pulsed laser deposition. Depending on the buffer layers and perovskite oxide electrodes, epitaxial films with different orientations were grown. (110)-oriented PZT/SrRuO{sub 3} (and PZT/LaNiO{sub 3}) films were obtained on YSZ-buffered Si substrates, while (001)-oriented PZT/SrRuO{sub 3} (and PZT/LaNiO{sub 3}) were fabricated with an extra CeO{sub 2} buffer layer (CeO{sub 2}/YSZ/Si). There is no effect of the electrode material on the properties of the films. The initial remnant polarizations in the (001)-oriented films are higher than those of (110)-oriented films, but it increases to the value of the (001) films upon cycling. The longitudinal piezoelectric d33{sub ,f} coefficients of the (110) films are larger than those of the (001) films, whereas the transverse piezoelectric d31{sub ,f} coefficients in the (110)-films are less than those in the (001)-oriented films. The difference is ascribed to the lower density (connectivity between grains) of the former films.

36 MATERIALS SCIENCE↗

Estimation of electron–phonon coupling and Urbach energy in group-I elements doped ZnO nanoparticles and thin films by sol–gel method

Highlights: • Comparison of group-I elements doped ZnO nanoparticles and thin films. • Calculation of electron–phonon coupling and phonon lifetime from Raman spectroscopy. • Estimation of interband states from Urbach energy. - Abstract: Group-I (Li, Na, K & Cs) elements doped ZnO nanoparticles (NPs) and thin films were prepared using sol–gel method. XRD data and TEM images confirm the absence of any other secondary phase different from wurtzite type ZnO. Spherical shapes of grains are observed from the surfaces of doped ZnO films by atomic force microscope images (AFM) and presences of dopants are confirmed from energy dispersive X-ray spectra. The Raman active E{sub 2} (high), E{sub 2} (low), E{sub 1} and A{sub 1} (LO) modes are observed from both ZnO NPs and thin films. First-order longitudinal optical (LO) phonon is found to have contributions from direct band transition and localized excitons. Electron–phonon coupling, phonon lifetime and deformation energy of ZnO are calculated based on the effect of dopants with respect to the multiple Raman LO phonon scattering. Presence of localized interbands states in doped ZnO NPs and thin films are found from the Urbach energy calculations.

36 MATERIALS SCIENCE↗