At least 1,063 records · Page 59

Effects of applied pressure on hot-pressing of Beta-SiC

The effects of applied pressure on the densification during hot pressing of beta-SiC compacts were investigated. Beta-SiC powder is Starck made and has the average particle size of about 0.7 micrometer. Hot pressing experiments were carried out in graphite dies at temperatures of 1700 deg to 2300 deg C and at the pressures up to 1000 kg/sq cm. The compacts containing 1 weight percent B4C were examined. Sintered compacts were examined for microstructure and the Rockwell A-scale hardness was measured. The B4C addition was very effective to mitigate the hot pressing conditions. It is found that densification goes with the strengthening of the bonding and does not occur in particle deformation due to concentrated stress.

Kinoshita, M.↗

Processing of sintered alpha SiC

Processing methods of sintered alpha SiC for engine applications are developed in a cost effective manner, using a submicron sized powder blended with sintering aids (boron and carbon). The processes for forming a green powder compact, such as dry pressing, cold isostatic pressing and green machining, slip casting, aqueous extrusion, plastic extrusion, and injection molding, are described. Dry pressing is the simplest route to component fabrication, and is carried out at approximately 10,000 psi pressure, while in the cold isostatic method the pressure could go as high as 20,000 psi. Surfactants are added to control settling rates and casting characteristics in the slip casting. The aqueous extrusion process is accomplished by a hydraulic ram forcing the aqueous mixture through a die. The plastic forming processes of extrusion and injection molding offer the potential of greater diversity in shape capacity. The physical properties of sintered alpha SiC (hardness, Young's modulus, shear modulus, and thermal diffusivity) are extensively tested. Corrosion resistance test results of silicon carbide are included.

Storm, R. S.↗

Reactive sintering of SiC

Investigation of the sintering processes involved in the sintering of SiC revealed a connection between the types and quantities of sintering additives or catalysts and densification, initial shrinkage, and weight loss of the sintered SiC material. By sintering processes, is meant the methods of mass transport, namely solid vapor transport and grain boundary diffusion.

Kim, Y. W.↗

Creep of chemically vapor deposited SiC fibers

The creep, thermal expansion, and elastic modulus properties for chemically vapor deposited SiC fibers were measured between 1000 and 1500 C. Creep strain was observed to increase logarithmically with time, monotonically with temperature, and linearly with tensile stress up to 600 MPa. The controlling activation energy was 480 + or - 20 kJ/mole. Thermal pretreatments near 1200 and 1450 C were found to significantly reduce fiber creep. These results coupled with creep recovery observations indicate that below 1400 C fiber creep is anelastic with neglible plastic component. This allowed a simple predictive method to be developed for describing fiber total deformation as a function of time, temperature, and stress. Mechanistic analysis of the property data suggests that fiber creep is the result of beta-SiC grain boundary sliding controlled by a small percent of free silicon in the grain boundaries.

Dicarlo, J. A.↗

Parametric evaluation of ball milling of SiC in water

A statistically designed experiment was conducted to determine optimum conditions for ball milling alpha-SiC in water. The influence of pH adjustment, volume percent solids loading, and mill rotational speed on grinding effectiveness was examined. An equation defining the effect of those milling variables on specific surface area was obtained. The volume percent solids loading of the slurry had the greatest influence on the grinding effectiveness in terms of increase in specific surface area. As grinding effectiveness improved, mill and media wear also increased. Contamination was minimized by use of sintered alpha-SiC milling hardware.

Kiser, J. D.↗

Mechanical properties of SiC fiber-reinforced reaction-bonded Si3N4 composites

The room temperature mechanical and physical properties of silicon carbide fiber reinforced reaction-bonded silicon nitride composites (SiC/RBSN) have been evaluated. The composites contained 23 and 40 volume fraction of aligned 140 micro m diameter chemically vapor deposited SiC fibers. Preliminary results for composite tensile and bend strengths and fracture strain indicate that the composites displayed excellent properties when compared with unreinforced RBSN of comparable porosity. Fiber volume fraction showed little influence on matrix first cracking strain but did influence the stressed required for matrix first cracking and for ultimate composite fracture strength. It is suggested that by reducing matrix porosity and by increasing the volume fraction of the large diameter SiC fiber, it should be possible to further improve the composite stress at which the matrix first cracks.

Bhatt, R. T.↗

Comparison of the contact stress and friction behavior of SiC and ZrO2 materials

Studies were performed to further elucidate the friction and contact-stress characteristics of structural ceramic materials. New data for fully stabilized and partially stabilized zirconia ceramics are compared with prior test results for sintered SiC. The comparison provides further evidence that the high temperature friction characteristics of sintered SiC are strongly influenced by the presence of a viscous surface layer. The results also show that a ceramic material with lower coefficient of friction and higher fracture toughness has increased resistance to strength-reducing surface damage due to contact stress.

Lindberg, L. J.↗

Parametric evaluation of ball milling of SiC in water

A statistically designed experiment was conducted to determine optimum conditions for ball milling alpha-SiC in water. The influence of pH adjustment, volume percent solids loading, and mill rotational speed on grinding effectiveness was examined. An equation defining the effect of those milling variables on specific surface area was obtained. The volume percent solids loading of the slurry had the greatest influence on the grinding effectiveness in terms of increase in specific surface area. As grinding effectiveness improved, mill and media wear also increased. Contamination was minimized by use of sintered alpha-SiC milling hardware.

Kiser, J. D.↗

Creep of chemically vapour deposited SiC fibres

The creep, thermal expansion, and elastic modulus properties for chemically vapor deposited SiC fibers were measured between 1000 and 1500 C. Creep strain was observed to increase logarithmically with time, monotonically with temperature, and linearly with tensile stress up to 600 MPa. The controlling activation energy was 480 + or - 20 kJ/mole. Thermal pretreatments near 1200 and 1450 C were found to significantly reduce fiber creep. These results coupled with creep recovery observations indicate that below 1400 C fiber creep is anelastic with negligible plastic component. This allowed a simple predictive method to be developed for describing fiber total deformation as a function of time, temperature, and stress. Mechanistic analysis of the property data suggests that fiber creep is the result of beta-SiC grain boundary sliding controlled by a small percent of free silicon in the grain boundaries.

Dicarlo, J. A.↗

Thermal expansion of the hexagonal (4H) polytype of SiC

The principal axial coefficients of thermal expansion, alpha(11) and alpha(33), of the (4H) polytype of hexagonal alpha SiC have been determined by X-ray diffraction measurements in the temperature range 20-1000 C. Alpha(11) and alpha(33), derived from the lattice parameter measurements, were expressed as the second-order polynomials in temperature. Alpha(11) was found to be larger than alpha(33) over the entire temperature range, with a thermal expansion anisotropy factor A increasing from 0.04 at room temperature to 0.11 at 1000 C. The thermal expansion results for the (4H) structure were compared with previously published results for the cubic (3C) and the hexagonal (6H) SiC polytypes.

Li, Z.↗

Processing of laser formed SiC powder

Processing research was undertaken to demonstrate that superior SiC characteristics could be achieved through the use of ideal constituent powders and careful post-synthesis processing steps. Initial research developed the means to produce approximately 1000 A uniform diameter, nonagglomerated, spherical, high purity SiC powders. Accomplishing this goal required major revision of the particle formation and growth model from one based on classical nucleation and growth to one based on collision and coalescence of Si particles followed by their carburization. Dispersions based on pure organic solvents as well as steric stabilization were investigated. Test parts were made by the colloidal pressing technique; both liquid filtration and consolidation (rearrangement) stages were modeled. Green densities corresponding to a random close packed structure were achieved. After drying, parts were densified at temperatures ranging from 1800 to 2100 C. This research program accomplished all of its major objectives. Superior microstructures and properties were attained by using powders having ideal characteristics and special post-synthesis processing procedures.

Haggerty, J. S.↗

Compensation in epitaxial cubic SiC films

Hall measurements on four n-type cubic SiC films epitaxially grown by chemical vapor deposition on (100) Si substrates are presented, and the temperature-dependent carrier concentrations are analyzed. Samples are found to be highly compensated (greater than 90 percent) contrary to the assumption made in previously published work, and the donor ionization energies, E(D), are shown to be less than one-half the values quoted previously. New E(D) and donor concentration values, however, provide evidence for identifying the donors as nitrogen in cubic SiC.

Segall, B.↗

TEM investigation of beta-SiC grown epitaxially on Si substrate by CVD

A transmission electron microscopy study is being conducted on the microstructure of beta-SiC films grown epitaxially on 001-plane silicon by chemical vapor deposition. Observations have been made in plain view and in cross-section. A high density of stacking faults has been found in the bulk of the epilayer which are bounded by partials of the Shockley type with Burgers vectors 1/6 211-line. Cross-sectional high resolution electron microscopy of the interface has shown it to be semicoherent with misfit dislocations to accommodate the lattice parameter difference between the substrate and the epilayer. In addition to misfit dislocations, a high density of twins and some stacking faults are present in the SiC near the interface. Mechanisms for the nucleation and growth of these defects are discussed.

Chorey, C. M.↗

Growth and characterization of cubic SiC single-crystal films on Si

Morphological and electrical characterization results are presented for cubic SiC films grown by chemical vapor deposition on single-crystal Si substrates. The films, up to 40 microns thick, were characterized by optical microscopy, (SEM), (TEM), electron channeling, surface profilometry, and Hall measurements. A variety of morphological features observed on the SiC films are described. Electrical measurements showed a decrease in the electron mobility with increasing electron carrier concentration, similar to that observed in Si. Room-temperature electron mobilities up to 520 sq cm/V-s (at an electron carrier concentration of 5 x 10 to the 16th/cu cm) were measured. Finally, a number of parameters believed to be important in the growth process were investigated, and some discussion is given of their possible effects on the film characteristics.

Powell, J. Anthony↗

Mechanical properties of SiC fiber-reinforced reaction-bonded Si3N4 composites

The room temperature mechanical and physical properties of silicon carbide fiber reinforced reaction-bonded silicon nitride composites (SiC/RBSN) have been evaluated. The composites contained 23 and 40 volume fraction of aligned 140 micro m diameter chemically vapor deposited SiC fibers. Preliminary results for composite tensile and bend strengths and fracture strain indicate that the composites displayed excellent properties when compared with unreinforced RBSN of comparable porosity. Fiber volume fraction showed little influence on matrix first cracking strain but did influence the stressed required for matrix first cracking and for ultimate composite fracture strength. It is suggested that by reducing matrix porosity and by increasing the volume fraction of the large diameter SiC fiber, it should be possible to further improve the composite stress at which the matrix first cracks.

Bhatt, Ramakrishna T.↗

SiC fiber reinforced reaction-bonded Si3N4 composites

A technique for fabricating strong and tough SiC fiber reinforced reaction bonded Si3N4 matrix composites (SiC/RBSN) was developed. Using this technique, composites containing approximately 23, 30, and 40 volume fractions of aligned 140 micron diameter, chemically vapor deposited SiC fibers were fabricated. The room temperature physical and mechanical properties were evaluated. The results for composite tensile strength, bend strength, and fracture strain indicate that the composite displays excellent properties when compared with the unreinforced matrix of comparable porosity. The composite stress at which the matrix first cracks and the ultimate composite fracture strength increase with increasing volume fraction of fibers, and the composite fails gracefully. The mechanical property data of this ceramic composite are compared with similar data for unreinforced commercially available Si3N4 materials and for SEP SiC/SiC composites.

Bhatt, Ramakrishna T.↗

High frequency ultrasonic characterization of sintered SiC

High frequency (60 to 160 MHz) ultrasonic nondestructive evaluation was used to characterize variations in density and microstructural constituents of sintered SiC bars. Ultrasonic characterization methods included longitudinal velocity, reflection coefficient, and precise attenuation measurements. The SiC bars were tailored to provide bulk densities ranging from 90 to 98 percent of theoretical, average grain sizes ranging from 3.0 to 12.0 microns, and average pore sizes ranging from 1.5 to 4.0 microns. Velocity correlated with specimen bulk density irrespective of specimen average grain size, average pore size, and average pore orientation. Attenuation coefficient was found to be sensitive to both density and average pore size variations, but was not affected by large differences in average grain size.

Baaklini, George Y.↗

Effect of high-temperature hydrogen exposure on sintered alpha-SiC

Sintered alpha-silicon carbide was exposed to pure, dry hydrogen at high temperatures for times up to 500 hr. Weight loss and corrosion were seen after 50 hr at temperatures as low as 1000 C. Corrosion of SiC by hydrogen produced grain boundary deterioration at 1100 C and a mixture of grain and grain boundary deterioration at 1300 C. Statistically significant strength reductions were seen in samples exposed to hydrogen for times greater than 50 hr and temperatures above 1100 C. Critical fracture origins were identified by fractography as either general grain boundary corrosion at 1100 C or as corrosion pits at 1300 C. A maximum strength decrease of approximately 33 percent was seen at 1100 and 1300 C after 500 hr exposure to hydrogen. A computer assisted thermodynamic program was also used to predict possible reaction species of SiC and hydrogen.

Hallum, Gary W.↗